Effect of V Distribution Characteristics on the Hardenability of a Novel 980 MPa Grade Extra-Thick Steel Plate for Marine Engineering
Received date: 2024-01-15
Revised date: 2024-02-13
Online published: 2024-03-13
Supported by
National Natural Science Foundation of China(52171050);Natural Science Foundation—Steel and Iron Foundation of Hebei Province(E2020203195);Shanghai Engineering Technology Research Center for Hot Manufacturing of Heavy Forgings(18DZ2253400)
Improving the hardenability of a ferrous alloy to achieve uniform microstructures and mechanical properties along the direction of the plate thickness is a key challenge in the production of high-grade extra-thick steel plates suitable for marine engineering (hereinafter referred to as “marine steel”). Hence, in this study, the effect of V distribution on the microstructures and hardenability of marine steel was investigated by employing the following procedure: a novel 980 MPa grade extra-thick steel plate was subjected to austenitization at 850 and 910 oC; subsequently, through thermal expansion and Jominy end-quench tests combined with fixed nitrogen treatment with aluminum. The microstructures and state of V atoms in the marine steel sample were characterized using SEM, EPMA, and TEM. Results showed that the occurrence of AlN during austenitizing at 910 oC promoted the segregation of V atoms on the original austenite grain boundaries, improved the stability of undercooled austenite, and delayed the transformation of proeutectoid ferrite. Thus, this study showed that the incorporation of V in marine steel substantially improved the hardenability of marine steel over a wide range of cooling rates (corresponding to steel plates with thicker cross-sections) and facilitated better microstructure uniformity, performance in marine environments, and matching between the required strength and toughness.
Key words: extra-thick plate; hardenability; V segregation; AlN; Jominy test
FU Wantang , WANG Wei , REN Liguo , BAI Xinghong , LV Zhiqing , LI Rongbin , LIU Haonan , QI Jianjun . Effect of V Distribution Characteristics on the Hardenability of a Novel 980 MPa Grade Extra-Thick Steel Plate for Marine Engineering[J]. Acta Metall Sin, 2025 , 61(9) : 1344 -1352 . DOI: 10.11900/0412.1961.2024.00010
| [1] | Xu L Z, Qiao G Y, Gong X, et al. Effect of through-thickness microstructure inhomogeneity on mechanical properties and strain hardening behavior in heavy-wall X70 pipeline steels [J]. J. Mater. Res. Technol., 2023, 25: 4216 |
| [2] | Han J, Li H J, Zhu Z X, et al. Effects of processing optimisation on microstructure, texture, grain boundary and mechanical properties of Fe-17Cr ferritic stainless steel thick plates [J]. Mater. Sci. Eng., 2014, A616: 20 |
| [3] | Zang C Y, Xiao W L, Fu Y, et al. Enhanced properties and homogeneity of Al-Zn-Mg-Cu alloy thick plate by non-isothermal aging [J]. J. Alloys Compd., 2023, 952: 170023 |
| [4] | Zhang L, Shi Y, Hu L, et al. Impact of multi-level microstructures on the strength and yield ratio of extra-thick ultra-high-strength steel [J]. J. Mater. Eng. Perform., 2023, 32: 10344 |
| [5] | Xue H, Peng W J, Yu L, et al. Effect of hardenability on microstructure and property of low alloy abrasion-resistant steel [J]. Mater. Sci. Eng., 2020, A793: 139901 |
| [6] | Nosovi V B, Yurasov S A. Calculation of hardenability of structural steels from their chemical composition [J]. Met. Sci. Heat Treat., 1995, 37: 16 |
| [7] | Grange R A. Estimating the hardenability of carbon steels [J]. Metall. Trans., 1973, 4: 2231 |
| [8] | Brown G T, James B A. Superhardening in medium-carbon steel [J]. Met. Technol., 1980, 7: 261 |
| [9] | Shimotori K, Kawai M, Tokoro H. Effects of Al and Ti on age-hardenability of 40Cr-Ni alloy [J]. J. Jpn. Inst. Met. Mater., 1972, 36: 685 |
| 霜鳥一三, 河合光雄, 野老博和. 40%Cr-Ni合金の時効硬化性におよぼすAlとTiの単独添加の影響 [J]. 日本金属学会誌, 1972, 36: 685 | |
| [10] | Cias W W. Phase transformational kinetics and hardenability of low-carbon, boron-treated steels [J]. Metall. Trans., 1973, 4: 603 |
| [11] | Aaron H B, Kotler G R. Second phase dissolution [J]. Metall. Trans., 1971, 2: 393 |
| [12] | Garbarz B, Pickering F B. Relationship between hardness and microstructure of continuously cooled C-Mn-V steels [J]. Mater. Sci. Technol., 1986, 2: 1016 |
| [13] | Pickering F B, Garbarz B. Strengthening in pearlite formed from thermomechanically processed austenite in vanadium steels and implications for toughness [J]. Mater. Sci. Technol., 1989, 5: 227 |
| [14] | Cai Z, Mao X P, Bao S Q, et al. Influence of vanadium microalloying on isothermal transformation behavior of eutectoid steel [J]. Phys. Met. Metall., 2019, 120: 936 |
| [15] | Garbarz B, Pickering F B. Effect of vanadium and austenitising temperature on hardenability of (0.2-0.3)C-1.6Mn steels with and without additions of titanium, aluminium, and molybdenum [J]. Mater. Sci. Technol., 1988, 4: 117 |
| [16] | Lagneborg R, Hutchinson B, Siwecki T, et al. The Role of Vanadium in Microalloyed Steels [M]. Sweden: Swerea KIMAB, 2014: 14 |
| [17] | Wang J L, Song S Q, Xue Z L, et al. Nitride-inclusion characterization in lightweight steel and re-precipitation behavior of AlN during heat treatment: Effect of Al content [J]. J. Iron Steel Res. Int., 2023 30: 350 |
| [18] | Lü C R, Xu L, Shi C, et al. Effect of Al on hardenability and microstructure of 42CrMo bolt steel [J]. Acta Metall. Sin., 2020, 56: 1324 |
| 吕超然, 徐 乐, 史 超 等. Al对42CrMo螺栓钢淬透性及组织的影响 [J]. 金属学报, 2020, 56: 1324 | |
| [19] | Guo Y H, Cao L, Wang G C, et al. Precipitation behaviors of AlN inclusion in high-Al steel [J]. Metall. Mater. Trans., 2023, 54B: 275 |
| [20] | Chen C, Zhang F C, Yang Z N, et al. Superhardenability behavior of vanadium in 40CrNiMoV steel [J]. Mater. Des., 2015, 83: 422 |
| [21] | Zhu Z, Chen Q W, Sun S H, et al. Effect of vanadium on superhardenability of 23MnNiMoCr54V steel for round-link chain in mining applications [J]. J. Mater. Eng. Perform., 2021, 30: 3884 |
| [22] | Qi J J. Fundamental research on composition design and manufacture process of super heavy link-chain steels for mining [D]. Qin-huangdao: Yanshan University, 2018 |
| 齐建军. 超大直径矿用圆环链钢的成分设计及制备工艺基础研究 [D]. 秦皇岛: 燕山大学, 2018 | |
| [23] | Grossman M A. Hardenability calculated from chemical composition [J]. Trans. AIME, 1942, 150: 227 |
| [24] | Garbarz B, Pickering F B. Effect of vanadium and austenitising temperature on hardenability of (0.2-0.3)C-1.6Mn steels with and without additions of titanium, aluminium, and molybdenum [J]. Mater. Sci. Technol., 1988, 4: 117 |
| [25] | St?ferle T, Spur G. Handbuch der Fertigungstechnik [M]. München: Carl Hanser Vlg., 1996: 272 |
| [26] | Vander Voort G F, Lampman S R, Sanders B R, et al. ASM Handbook. Volume 9: Metallography and Microstructures [M]. Materials Park, OH: ASM International, 2004: 1322 |
| [27] | Li??i? B, Tensi H M, Luty W. Theory and Technology of Quenching: A Handbook [M]. Berlin, Heidelberg: Springer, 1992: 390 |
| [28] | Jung S, Kim S, Kim S, et al. Quantitative laser-induced breakdown spectroscopy mapping of centerline segregation via optical emissions of Mn and Cr in steel wire rod products [J]. Mater. Today Commun., 2022, 33: 104867 |
| [29] | Li X X, Ramazani A, Prahl U, et al. Quantification of complex-phase steel microstructure by using combined EBSD and EPMA measurements [J]. Mater. Charact., 2018, 142: 179 |
| [30] | Li D L, Cai W Y, Liu Z X, et al. Elemental mapping and quantitative characterization of dendrite structure in IN718 supperalloy based on micro beam X-ray fluorescence and EPMA [J]. Vacuum, 2022, 198: 110859 |
| [31] | Zhang S Y, Wang X, Mo Y T, et al. Towards relieving center segregation in twin-roll cast Al-Mg-Si-Cu strips by controlling the thermal-mechanical process [J]. J. Mater. Sci. Technol., 2023, 148: 31 |
| [32] | Flori M, Gruzza B, Bideux L, et al. XPS, EPMA and microstructural analysis of a defective industrial plasma-nitrided steel [J]. Surf. Coat. Technol., 2008, 202: 5887 |
| [33] | Mostert R J, Van Rooyen G T. A quantitative assessment of the hardenability increase resulting from a superhardenability treatment [J]. Metall. Trans., 1984, 15A: 2185 |
| [34] | Lin H R, Cheng G H. Hardenability effect of boron on carbon steels [J]. Mater. Sci. Technol., 1987, 3: 855 |
| [35] | Dhara S, Van Bohemen S M C, Santofimia M J. Isothermal decomposition of austenite in presence of martensite in advanced high strength steels: A review [J]. Mater. Today Commun., 2022, 33: 104567 |
| [36] | Lv Z Q, Chen Z Y, Qi J J, et al. Boron-free medium-low nickel high-strength high-hardenability marine steel thick plate and preparation method [P]. Chin Pat, CN114086072A, 2022 |
| 吕知清, 陈振业, 齐建军 等. 无硼中低镍高强度高淬透性海工钢厚板及其制备方法 [P]. 中国专利, CN114086072A, 2022 |
/
| 〈 |
|
〉 |