Plastic Deformation Behaviors of VCoNi Medium-Entropy Alloy Under Nanoindentation

  • WANG Fangyuan ,
  • ZHANG Yulong ,
  • WANG Zhangwei ,
  • XIONG Zhiping ,
  • WANG Hui ,
  • SONG Min ,
  • XIA Wenzhen
Expand
  • 1 State Key Laboratory of Powder Metallurgy, Central South University, Changsha 410083, China
    2 Institute of Microstructure and Micro/nano-mechanics, School of Metallurgical Engineering, Anhui University of Technology, Ma'anshan 243032, China
    3 National Key Laboratory of Science and Technology on Materials Under Shock and Impact, Beijing Institute of Technology, Beijing 100081, China
    4 State Key Laboratory for Advance Metals and Materials, University of Science and Technology Beijing, Beijing 100083, China

Received date: 2023-12-29

  Revised date: 2024-01-27

  Online published: 2024-02-29

Supported by

National Key Research and Development Program of China(2022YFE0134400);Young Scientists Fund of National Natural Science Foundation of China(52201057);National Key Laboratory Foundation of Science and Technology on Materials under Shock and Impact(6142902220101);State Key Laboratory for Advanced Metals and Materials(2023-Z05)

Abstract

High- and medium-entropy alloys have attracted considerable attention because of their innovative design concepts. The VCoNi medium-entropy alloy with equiatomic ratio, a distinctive type of medium-entropy alloy, is characterized by a fcc structure. As it exhibits remarkable mechanical properties such as strength and plasticity across a broad temperature spectrum, it is suitable for versatile applications. Current research on VCoNi medium-entropy alloys predominantly focuses on the alloy design and the manipulation of heat treatment technologies to enhance mechanical properties with relatively less emphasis on elucidating plastic deformation mechanisms. A profound understanding of these mechanisms is imperative for controlling their properties. Although previous studies have revealed plastic deformation mechanisms mediated by dislocations in VCoNi medium-entropy alloys, the impact of grain orientation on dislocation movement and interaction mechanisms remains elusive. Nanoindentation technology has been widely used to assess plastic deformation behavior and dislocation evolution in materials. Grain orientation profoundly influences the mechanical properties and plastic deformation behavior of materials at the microscale. Therefore, investigating the influence of grain orientation on the plastic deformation mechanism in the VCoNi medium-entropy alloy is of great importance. A comprehensive understanding of plastic deformation and dislocation interactions can be achieved by analyzing slip steps generated by nanoindentation. This study delves into the plastic deformation behavior of VCoNi medium-entropy alloy in {101}, {111}, and {001} grains using nanoindentation. By analyzing the evolution of slip steps and load-displacement curves, it concentrates on the influence of crystal orientation on plastic deformation behavior and explores the intricate relationship among dislocation interactions, load-displacement behavior, and dislocation motion. The grain orientation in the VCoNi medium-entropy alloy dictates the activation and sequence of slip systems induced by nanoindentation, thereby substantially influencing the morphology of indentations, surrounding slip steps, and load-displacement behavior. The slip steps on the same slip plane in each grain preferentially appear on a positively inclined slip plane. On {101} grains, the slip steps appear on the (111) and (111¯) slip planes initially, and then on the (11¯1¯) and (11¯1) slip planes. In {111} grains, the slip steps appear on the (111¯), (11¯1¯), and (11¯1) slip planes. On {001} grains, the slip steps appear on the four {111} slip planes. {101}, {111}, and {001} grains exhibit butterfly-shaped, nested triangle-shaped, and cross-shaped overall indentation morphologies, respectively. Additionally, only a limited occurrence of double cross-slip is observed at the edges of the slip steps in {101} and {001} grains. The analysis of dislocation interactions revealed that on {101} grains, dislocation reactions tended to form Lomer-Cottrell locks and Glissile junctions, in {111} grains they tended to form Collinear junctions and Lomer-Cottrell locks, and in {001} grains they tended to form Glissile junctions. This determination influences the subsequent pop-in behavior in the load-displacement curves of different grains.

Cite this article

WANG Fangyuan , ZHANG Yulong , WANG Zhangwei , XIONG Zhiping , WANG Hui , SONG Min , XIA Wenzhen . Plastic Deformation Behaviors of VCoNi Medium-Entropy Alloy Under Nanoindentation[J]. Acta Metall Sin, 2025 , 61(10) : 1567 -1578 . DOI: 10.11900/0412.1961.2023.00499

References

[1] George E P, Raabe D, Ritchie R O. High-entropy alloys [J]. Nat. Rev. Mater., 2019, 4: 515
[2] Ma E, Wu X L. Tailoring heterogeneities in high-entropy alloys to promote strength-ductility synergy [J]. Nat. Commun., 2019, 10: 5623
[3] Wang Z W, Lu W J, Zhao H, et al. Ultrastrong lightweight compositionally complex steels via dual-nanoprecipitation [J]. Sci. Adv., 2020, 6: eaba9543
[4] Miracle D B, Senkov O N. A critical review of high entropy alloys and related concepts [J]. Acta Mater., 2017, 122: 448
[5] Liu J P, Chen H, Zhang C, et al. Progress of cryogenic deformation and strengthening-toughening mechanisms of high-entropy alloys [J]. Acta Metall. Sin., 2023, 59: 727
  刘俊鹏, 陈 浩, 张 弛 等. 高熵合金的低温塑性变形机制及强韧化研究进展 [J]. 金属学报, 2023, 59: 727
[6] An Z B, Mao S C, Zhang Z, et al. Strengthening-toughening mechanism and mechanical properties of span-scale heterostructure high-entropy alloy [J]. Acta Metall. Sin., 2022, 58: 1441
  安子冰, 毛圣成, 张 泽 等. 高熵合金跨尺度异构强韧化及其力学性能研究进展 [J]. 金属学报, 2022, 58: 1441
[7] Sohn S S, Da Silva A K, Ikeda Y, et al. Ultrastrong medium-entropy single-phase alloys designed via severe lattice distortion [J]. Adv. Mater., 2019, 31: 1807142
[8] Chen X F, Yuan F P, Zhou H, et al. Structure motif of chemical short-range order in a medium-entropy alloy [J]. Mater. Res. Lett., 2022, 10: 149
[9] Cai W J, He J Y, Wang L, et al. Characterization of chemical short-range order in VCoNi medium-entropy alloy processed by spark plasma sintering [J]. Scr. Mater., 2023, 231: 115463
[10] Liu G D, Luo X M, Zou J P, et al. Effects of grain size and cryogenic temperature on the strain hardening behavior of VCoNi medium-entropy alloys [J]. Acta Metall. Sin. (Engl. Lett.), 2023, 36: 973
[11] Yang D C, Jo Y H, Ikeda Y, et al. Effects of cryogenic temperature on tensile and impact properties in a medium-entropy VCoNi alloy [J]. J. Mater. Sci. Technol., 2021, 90: 159
[12] Luo H, Sohn S S, Lu W J, et al. A strong and ductile medium-entropy alloy resists hydrogen embrittlement and corrosion [J]. Nat. Commun., 2020, 11: 3081
[13] Lee S, Vaid A, Im J, et al. In-situ observation of the initiation of plasticity by nucleation of prismatic dislocation loops [J]. Nat. Commun., 2020, 11: 2367
[14] Habiyaremye F, Guitton A, Sch?fer F, et al. Plasticity induced by nanoindentation in a CrCoNi medium-entropy alloy studied by accurate electron channeling contrast imaging revealing dislocation-low angle grain boundary interactions [J]. Mater. Sci. Eng., 2021, A817: 141364
[15] Ye Y X, Lu Z P, Nieh T G. Dislocation nucleation during nanoindentation in a body-centered cubic TiZrHfNb high-entropy alloy [J]. Scr. Mater., 2017, 130: 64
[16] Hua D P, Xia Q S, Wang W, et al. Atomistic insights into the deformation mechanism of a CoCrNi medium entropy alloy under nanoindentation [J]. Int. J. Plast., 2021, 142: 102997
[17] Zhang Y W, Li S J, Hao Y L, et al. Nanoindentation study on Ti-24Nb-4Zr-8Sn single crystals [J]. Chin. J. Nonferrous Met., 2010, 20(Spec.1) : S528
  张晏玮, 李述军, 郝玉琳 等. Ti-24Nb-4Zr-8Sn合金单晶纳米压痕研究 [J]. 中国有色金属学报, 2010(专辑)825S :02,1
[18] Salehinia I, Lawrence S K, Bahr D F. The effect of crystal orientation on the stochastic behavior of dislocation nucleation and multiplication during nanoindentation [J]. Acta Mater., 2013, 61: 1421
[19] Chen T Y, Tan L Z, Lu Z Z, et al. The effect of grain orientation on nanoindentation behavior of model austenitic alloy Fe-20Cr-25Ni [J]. Acta Mater., 2017, 138: 83
[20] Csanádi T, Bl'anda M, Chinh N Q, et al. Orientation-dependent hardness and nanoindentation-induced deformation mechanisms of WC crystals [J]. Acta Mater., 2015, 83: 397
[21] Kang S, Jung Y S, Yoo B G, et al. Orientation-dependent indentation modulus and yielding in a high Mn twinning-induced plasticity steel [J]. Mater. Sci. Eng., 2012, A532: 500
[22] Sarvesha R, Gokhale A, Kumar K, et al. Effect of crystal orientation on indentation-induced deformation behavior of zinc [J]. Mater. Sci. Eng., 2020, A776: 139064
[23] McInteer W A, Thompson A W, Bernstein I M. The effect of hydrogen on the slip character of nickel [J]. Acta Metall., 1980, 28: 887
[24] Tromas C, Girard J C, Audurier V, et al. Study of the low stress plasticity in single-crystal MgO by nanoindentation and atomic force microscopy [J]. J. Mater. Sci., 1999, 34: 5337
[25] Nibur K A, Bahr D F. Identifying slip systems around indentations in fcc metals [J]. Scr. Mater., 2003, 49: 1055
[26] Nibur K A, Akasheh F, Bahr D F. Analysis of dislocation mechanisms around indentations through slip step observations [J]. J. Mater. Sci., 2007, 42: 889
[27] Xia W Z, Dehm G, Brinckmann S. Insight into indentation-induced plastic flow in austenitic stainless steel [J]. J. Mater. Sci., 2020, 55: 9095
[28] Xia W Z, Dehm G, Brinckmann S. Unraveling indentation-induced slip steps in austenitic stainless steel [J]. Mater. Des., 2019, 183: 108169
[29] Johnson K L. Contact Mechanics [M]. Cambridge: Cambridge University Press, 1985: 165
[30] Tuck J R, Korsunsky A M, Bull S J, et al. On the application of the work-of-indentation approach to depth-sensing indentation experiments in coated systems [J]. Surf. Coat. Technol., 2001, 137: 217
[31] Nguyen P C, Ryu I. Mesoscale dislocation dynamics modeling of incipient plasticity under nanoindentation [J]. Materialia, 2023, 32: 101956
[32] P?hl F. Pop-in behavior and elastic-to-plastic transition of polycrystalline pure iron during sharp nanoindentation [J]. Sci. Rep., 2019, 9: 15350
[33] Catoor D, Gao Y F, Geng J, et al. Incipient plasticity and deformation mechanisms in single-crystal Mg during spherical nanoindentation [J]. Acta Mater., 2013, 61: 2953
[34] Montagne A, Audurier V, Tromas C. Influence of pre-existing dislocations on the pop-in phenomenon during nanoindentation in MgO [J]. Acta Mater., 2013, 61: 4778
[35] Xiong K, Gu J F. Understanding pop-in phenomena in FeNi3 nanoindentation [J]. Intermetallics, 2015, 67: 111
[36] Li J Y, Yang S Q, Dong L G, et al. Effect of crystal orientation on the nanoindentation deformation behavior of TiN coating based on molecular dynamics [J]. Surf. Coat. Technol., 2023, 467: 129721
[37] Stricker M, Weygand D. Dislocation multiplication mechanisms-glissile junctions and their role on the plastic deformation at the microscale [J]. Acta Mater., 2015, 99: 130
[38] Katzer B, Zoller K, Bermuth J, et al. Characterization of Lomer junctions based on the Lomer arm length distribution in dislocation networks [J]. Scr. Mater., 2023, 226: 115232
[39] Kumar Panda A, Divakar R, Singh A, et al. Molecular dynamics studies on formation of stacking fault tetrahedra in fcc metals [J]. Comput. Mater. Sci., 2021, 186: 110017
[40] An D Y, Zhao H, Sun B H, et al. Direct observations of collinear dislocation interaction in a Fe-17.4Mn-1.50Al-0.29C (wt.%) austenitic steel under cyclic loading by in-situ electron channelling contrast imaging and cross-correlation electron backscatter diffraction [J]. Scr. Mater., 2020, 186: 341
Outlines

/