Similarities and Differences of Microstructure and Mechanical Properties Between High γ' Content Powder and Wrought Superalloys
Received date: 2023-07-07
Revised date: 2023-12-10
Online published: 2024-01-24
Supported by
National Natural Science Foundation of China(52271087);National Science and Technology Major Project(J2017-VI-0017-089)
The turbine disk is a crucial heat-resistant component of aeronautical engines. An investigation into the similarities and differences in the microstructure and mechanical properties of superalloys fabricated using powder metallurgy and conventional casting and wrought methods could provide a theoretical framework for ensuring the production and operational reliability of turbine disks that are difficult to deform. GH4720Li (Udimet720Li) alloy is a commonly used nickel-based superalloy reinforced through precipitation. The volume fraction of γ' precipitation in GH4720Li alloy is 45%. It is mainly used to make compressor and turbine disks for use at 650-750 oC, as well as turbine disks for use at 900 oC in a short time. The mechanical properties of the GH4720Li alloy are closely associated with its microstructure. The mechanical properties of the alloy, including hardness, yield strength, and tensile strength, are influenced by factors such as grain size and orientation, distribution of the γ′ phase, presence of twins, and arrangement of grain boundaries. To investigate the similarities and differences of the microstructure and mechanical properties between powder alloy (FGH4720Li alloy) and wrought alloy (GH4720Li alloy), which were prepared by powder metallurgy and traditional cast and wrought processes, the microstructure characteristics of FGH4720Li alloy and GH4720Li alloy were observed and analyzed by SEM, TEM, and EBSD (FGH4720Li alloy). The mechanical properties of both alloys were studied via Vickers hardness and high-temperature tensile tests. Furthermore, the relationship between the microstructure and mechanical properties of both alloys was thoroughly discussed. Results show that the distribution characteristics of dislocation, twin substructure morphology, grain orientation concentration, and twin boundary in both alloys are similar. Wide twins (0.5-1 μm) and some narrow twins (< 100 nm) were observed in both two alloys, and the type of twin boundary is primarily Σ3. No obvious preferred orientation was noticed in both alloys. The difference is that the size of γ
WANG Hongying , YAO Zhihao , LI Dayu , GUO Jing , YAO Kaijun , DONG Jianxin . Similarities and Differences of Microstructure and Mechanical Properties Between High γ' Content Powder and Wrought Superalloys[J]. Acta Metall Sin, 2025 , 61(9) : 1364 -1374 . DOI: 10.11900/0412.1961.2023.00291
| [1] | Fan H Y, Jiang H, Dong J X, et al. An optimization method of upsetting process for homogenized, nickel-based superalloy Udimet 720Li ingot considering both cracking and recrystallization [J]. J. Mater. Process. Technol., 2019, 269: 52 |
| [2] | Zhao C L, Wang Q, Tang Y, et al. Microstructure and property stability of powder metallurgy nickel-based U720Li superalloy during long-term aging [J]. Rare Met. Mater. Eng., 2022, 51: 2356 |
| 赵春玲, 王 强, 汤 悦 等. 粉末镍基U720Li高温合金长期时效下的组织与性能稳定性[J]. 稀有金属材料与工程, 2022, 51: 2356 | |
| [3] | Zhang H K, Li Y, Ma H C, et al. A novel short-process manufacturing method of γ′-strengthened superalloy: Modulation of nano-scaled γ′ precipitates during hot deformation [J]. Mater. Sci. Eng., 2022, A846: 143257 |
| [4] | Wan Z P. Hot deformation behavior and microstructure & properties control of Ni-based alloy GH4720LI [D]. Harbin: Harbin Institute of Technology, 2019 |
| 万志鹏. GH4720LI镍基合金高温变形行为及组织性能控制研究 [D]. 哈尔滨: 哈尔滨工业大学, 2019 | |
| [5] | Qu J L, Yi C S, Chen J W, et al. Research progress of precipitated phases in GH4720Li superalloy [J]. J. Mater. Eng., 2020, 48(8): 73 |
| 曲敬龙, 易出山, 陈竞炜 等. GH4720Li合金中析出相的研究进展 [J]. 材料工程, 2020, 48(8): 73 | |
| [6] | Yao Z H, Hou J, Chen Y, et al. Effect of micron-sized particles on the crack growth behavior of a Ni-based powder metallurgy superalloy [J]. Mater. Sci. Eng., 2022, A860: 144242 |
| [7] | Jiang R, Zhang W T, Zhang L C, et al. Strain localization and crack initiation behavior of a PM Ni-based superalloy: SEM-DIC characterization and crystal plasticity simulation [J]. Fatigue Fract. Eng. Mater. Struct., 2022, 45: 1635 |
| [8] | Liu J, Ye F, Wang X Q, et al. Precipitation behavior of γ′ phase in P/M superalloy Udimet720Li [J]. Powder Metall. Technol., 2021, 39: 499, 525 |
| 刘 健, 叶 飞, 王旭青 等. 粉末高温合金Udimet720Li γ′强化相析出行为 [J]. 粉末冶金技术, 2021, 39: 499, 525 | |
| [9] | Liu C, Yao Z H, Guo J, et al. Microstructure evolution behavior of powder superalloy FGH4720Li at near service temperature [J]. Acta Metall. Sin., 2021, 57: 1549 |
| 刘 超, 姚志浩, 郭 婧 等. 粉末高温合金FGH4720Li在近服役温度下的组织演变规律 [J]. 金属学报, 2021, 57: 1549 | |
| [10] | Tian G F, Jia C C, Wen Y, et al. Effect of solution cooling rate on the γ′ precipitation behaviors of a Ni-based P/M superalloy [J]. J. Univ. Sci. Technol. Beijing Miner. Metall. Mater., 2008, 15: 729 |
| [11] | Huang Z L, Xie X F, Gu Y, et al. Tensile properties of Ni-based GH4720Li superalloys with different microstructures at 650 oC [J]. Chin. J. Rare Met., 2021, 45: 1269 |
| 黄子琳, 谢兴飞, 谷 雨 等. GH4720Li镍基合金显微组织对650 ℃拉伸性能影响 [J]. 稀有金属, 2021, 45: 1269 | |
| [12] | Hu D Y, Ma Q H, Shang L H, et al. Creep-fatigue behavior of turbine disc of superalloy GH720Li at 650 oC and probabilistic creep-fatigue modeling [J]. Mater. Sci. Eng., 2016, A670: 17 |
| [13] | Yu Q Y, Yao Z H, Dong J X. Deformation and recrystallization behavior of a coarse-grain, nickel-base superalloy Udimet720Li ingot material [J]. Mater. Charact., 2015, 107: 398 |
| [14] | Chen J Y, Dong J X, Zhang M C, et al. Deformation mechanisms in a fine-grained Udimet 720LI nickel-base superalloy with high volume fractions of γ′ phases [J]. Mater. Sci. Eng., 2016, A673: 122 |
| [15] | Zhang H K, Ma H C, Chang T X, et al. Deformation mechanisms of primary γ′ precipitates in nickel-based superalloy [J]. Scr. Mater., 2023, 224: 115109 |
| [16] | Qu J L, Bi Z N, Du J H, et al. Hot deformation behavior of nickel-based superalloy GH4720Li [J]. J. Iron Steel Res. Int., 2011, 18: 59 |
| [17] | Shen J Y, Hu L X, Sun Y, et al. Hot deformation behaviors and three-dimensional processing map of a nickel-based superalloy with initial dendrite microstructure [J]. J. Alloys Compd., 2020, 822: 153735 |
| [18] | Kan Z, Du L X, Hu J, et al. Influence of microstructure on mechanical property of GH4720 Li alloy [J]. J. Northeast. Univ. (Nat. Sci.), 2017, 38: 46 |
| 阚 志, 杜林秀, 胡 军 等. 微观组织对GH4720 Li合金力学性能的影响 [J]. 东北大学学报(自然科学版), 2017, 38: 46 | |
| [19] | Liu C. Evolution and interaction of microstructures of deformed superalloy during preparation process and thermo-mechnical coupling action [D]. Beijing: University of Science and Technology Beijing, 2022 |
| 刘 超. 变形高温合金制备过程和热力耦合作用下组织演变及互影响 [D]. 北京: 北京科技大学, 2022 | |
| [20] | Cayron C. Multiple twinning in cubic crystals: Geometric/algebraic study and its application for the identification of the Σ3 n grain boundaries [J]. Acta Crystallogr.: Found. Crystallogr., 2007, 63A: 11 |
| [21] | Ning Y Q, Wang T, Fu M W, et al. Competition between work-hardening effect and dynamic-softening behavior for processing as-cast GH4720Li superalloys with original dendrite microstructure during moderate-speed hot compression [J]. Mater. Sci. Eng., 2015, A642: 187 |
| [22] | Xie X F, Qu J L, Du J H. Effect of mixed grain structure on high temperature stress rupture property of Ni-based GH4720Li superalloy [J]. Mater. Rep., 2020, 34(suppl.1): 375 |
| 谢兴飞, 曲敬龙, 杜金辉. GH4720Li镍基合金混晶组织对高温持久性能的影响 [J]. 材料导报, 2020, 34(增刊1): 375 | |
| [23] | Mao J, Chang K M, Yang W H, et al. Cooling precipitation and strengthening study in powder metallurgy superalloy U720LI [J]. Metall. Mater. Trans., 2001, 32A: 2441 |
| [24] | Bhowal P R, Wright E F, Raymond E L. Effects of cooling rate and γ′ morphology on creep and stress-rupture properties of a powder metallurgy superalloy [J]. Metall. Trans., 1990, 21A: 1709 |
| [25] | Murakumo T, Kobayashi T, Koizumi Y, et al. Creep behaviour of Ni-base single-crystal superalloys with various γ′ volume fraction [J]. Acta Mater., 2004, 52: 3737 |
| [26] | Rao G A, Kumar M, Srinivas M, et al. Effect of standard heat treatment on the microstructure and mechanical properties of hot isostatically pressed superalloy Inconel 718 [J]. Mater. Sci. Eng., 2003, A355: 114 |
| [27] | Zhao G D. Effect of B and C on solidification segregation and hot ductility of U720Li alloy [D]. Hefei: University of Science and Technology of China, 2017 |
| 赵广迪. B和C对U720Li合金凝固偏析和热加工塑性的影响 [D]. 合肥: 中国科学技术大学, 2017 | |
| [28] | Viswanathan G B, Sarosi P M, Henry M F, et al. Investigation of creep deformation mechanisms at intermediate temperatures in René 88 DT [J]. Acta Mater., 2005, 53: 3041 |
| [29] | Sinharoy S, Virro-Nic P, Milligan W W. Deformation and strength behavior of two nickel-base turbine disk alloys at 650 oC [J]. Metall. Mater. Trans., 2001, 32A: 2021 |
/
| 〈 |
|
〉 |