Research paper

Influence of Spray Forming Process on Carbide Characteristics and Mechanical Properties of M3 High-Speed Steel

  • LIU Jihao ,
  • CHI Hongxiao ,
  • WU Huibin ,
  • MA Dangshen ,
  • ZHOU Jian ,
  • GU Jinbo
Expand
  • 1.Institute for Special Steels, Central Iron and Steel Research Institute, Beijing 100081, China
    2.Collaborative Innovation Center of Steel Technology, University of Science and Technology Beijing, Beijing 100083, China
CHI Hongxiao, professor, Tel: (010)62182268, E-mail: chihongxiao@163.com

Received date: 2023-07-29

  Revised date: 2023-11-14

  Online published: 2024-01-24

Abstract

High-speed steel typically comprises a high carbon content with an abundance of alloying elements, leading to a solidified microstructure rich in carbides. The refinement of these carbides in the microstructure is the most effective method for enhancing the mechanical properties of high-speed steel, and it remains a primary focus of the high-speed steel research. The prevalent industrial production methods for high-speed steel include traditional casting and forging, powder metallurgy, and spray forming. Traditional casting and forging methods are often constrained by segregation issues, hindering the application of high-quality cast and forged high-speed steel. Powder metallurgy high-speed steel exhibits remarkable mechanical properties; however, its high production costs have restricted its broader development. Conversely, spray forming is an advanced manufacturing method characterized by cost effectiveness, efficient production, and environmental friendliness. Although China has successfully implemented the mass production of spray-formed tool and die steel, systematic research on the microstructure and properties of such steel in actual industrial preparation is lacking. This study conducts a comparative analysis of the microstructure and mechanical properties of the M3 high-speed steel prepared via three distinct methods: electroslag remelting, spray forming, and powder metallurgy. The experimental results show that although the different preparation methods exert minimal impact on the carbide type within the annealed microstructure of the M3 high-speed steel, they considerably affect the morphology, size, and distribution of the carbides. Spray-formed and powder metallurgy high-speed steels display a dispersed, particulate carbide distribution across transverse and longitudinal sections, with spray-formed steel exhibiting coarser carbide sizes. Electroslag remelted high-speed steel exhibits a network-like distribution of carbides in the transverse sections and a distinct banded arrangement in the longitudinal sections. The mechanical properties of powder metallurgy high-speed steel were superior to those of electroslag remelted and spray-formed high-speed steels. The more uniform and finer the distribution of carbides within the steel microstructure, the higher will be their hardness, bending strength, and impact toughness. Regarding wear resistance, spray-formed high-speed steel outperforms the others, which is attributed to the presence of large-sized MC-type carbides in its microstructure. These carbides not only provide better wear resistance, but also change the formation of the oxidation layer from diffusion mechanism to sintering mechanism, thereby reducing crack propagation in the matrix and enhancing wear resistance. This study delves into the carbide precipitation behavior of the M3 high-speed steel during the spray forming process based on the microstructural characteristics of the spray-formed steel.

Cite this article

LIU Jihao , CHI Hongxiao , WU Huibin , MA Dangshen , ZHOU Jian , GU Jinbo . Influence of Spray Forming Process on Carbide Characteristics and Mechanical Properties of M3 High-Speed Steel[J]. Acta Metall Sin, 2025 , 61(8) : 1229 -1244 . DOI: 10.11900/0412.1961.2023.00318

References

[1] Barkalow R H, Kraft R W, Goldstein J I. Solidification of M2 high speed steel [J]. Metall. Trans., 1972, 3: 919
[2] Fischmeister H F, Riedl R, Karag?z S. Solidification of high-speed tool steels [J]. Metall. Trans., 1989, 20A: 2133
[3] Lee E S, Park W J, Baik K H, et al. Different carbide types and their effect on bend properties of a spray-formed high speed steel [J]. Scr. Mater., 1998, 39: 1133
[4] Holzgruber W, Holzgruber H. Recent innovations in electroslag remelting [J]. Iron Steelmaker, 1998, 25: 107
[5] Halfa H, Reda A M. Electroslag remelting of high technological steels [J]. J. Miner. Mater. Charact. Eng., 2015, 3: 444
[6] Bomba? D, Ter?elj M, Fazarinc M, et al. On the increase of intrinsic workability and hot working temperature range of M42 ledeburitic super high steel in as-cast and wrought states [J]. Mater. Sci. Eng., 2017, A703: 438
[7] Hwang K C, Lee S, Lee H C. Effects of alloying elements on microstructure and fracture properties of cast high speed steel rolls: Part II. Fracture behavior [J]. Mater. Sci. Eng., 1998, A254 : 296
[8] Hetzner D W. Refining carbide size distributions in M1 high speed steel by processing and alloying [J]. Mater. Charact., 2001, 46: 175
[9] Pan Y, Pi Z Q, Liu B W, et al. Influence of heat treatment on the microstructural evolution and mechanical properties of W6Mo5Cr4V2Co5Nb (825 K) high speed steel [J]. Mater. Sci. Eng., 2020, A787: 139480
[10] Du G, Li J, Wang Z B. Control of carbide precipitation during electroslag remelting-continuous rapid solidification of GCr15 steel [J]. Metall. Mater. Trans., 2017, 48B: 2873
[11] Li W M, Jiang Z H, Zang X M, et al. Carbide segregation control in electro-slag remelting withdrawal process of large cross-section high-speed steels [J]. J. Cent. South Univ. (Sci. Technol.), 2017, 48: 1697
  李万明, 姜周华, 臧喜民 等. 抽锭电渣重熔大截面高速钢过程的碳化物偏析控制 [J]. 中南大学学报(自然科学版), 2017, 48: 1697
[12] Kirk F A. Problems in high-speed steel manufacture and use: A challenge for economic powder metallurgy processing [J]. Powder Metall., 1981, 24: 70
[13] Wright C S, Wronski A S, Iturriza I. Development of robust processing routes for powder metallurgy high speed steels [J]. Mater. Sci. Technol., 2000, 16: 945
[14] Henein H. Why is spray forming a rapid solidification process? [J]. Materialwiss. Werkst., 2010, 41: 555
[15] Mesquita R A, Barbosa C A. High-speed steels produced by conventional casting, spray forming and powder metallurgy [J]. Mater. Sci. Forum, 2005, 498-499: 244
[16] Schulz A, Matthaei-Schulz E, Spangel S, et al. Analysis of spray formed tool steels [J]. Materialwiss. Werkst., 2003, 34: 478
[17] Schruff I, Schüler V, Spiegelhauer C, et al. Advanced tool steels produced via spray forming [A]. 6th International Tooling Conference [C]. Sweden, 2002: 1159
[18] Zhao S L. Research of microstructure and properities of spray formed high alloyed high speed steel [D]. Shanghai: Shanghai University, 2017
  赵顺利. 喷射成形高合金高速钢的组织与性能研究 [D]. 上海: 上海大学, 2017
[19] Wang H B, Hou L G, Zhang J X, et al. Microstructures and properties of spray formed Nb-containing M3 high speed steel [J]. Acta Metall. Sin., 2014, 50: 1421
  王和斌, 侯陇刚, 张金祥 等. 喷射成形含铌M3型高速钢组织与性能研究 [J]. 金属学报, 2014, 50: 1421
[20] Wei K, Xu Y, Liu X, et al. Microstructure and properties of high vanadium steel with 9% vanadium fabricated by spray forming- hot isostatic pressing [J]. Powder Metall. Ind., 2012, 22(3): 21
  魏 宽, 徐 轶, 刘 宪 等. 喷射成形—热等静压9V高钒钢的组织与性能研究 [J]. 粉末冶金工业, 2012, 22(3): 21
[21] Xu Y, Ge C C, Wei K, et al. Research on preparation technology of high-vanadium HSS by spray forming [J]. Powder Metall. Technol., 2012, 30: 22
  徐 轶, 葛昌纯, 魏 宽 等. 喷射成形高钒高速钢环坯制备技术研究 [J]. 粉末冶金技术, 2012, 30: 22
[22] Ghomashchi M R, Sellars C. Microstructural changes in as-cast M2 grade high speed steel during hot forging [J]. Metall. Trans., 1993, 24A: 2171
[23] Lee E S, Park W J, Jung J Y, et al. Solidification microstructure and M2C carbide decomposition in a spray-formed high-speed steel [J]. Metall. Mater. Trans., 1998, 29A: 1395
[24] Jia Y Z, Wu Y P, Kuang X G, et al. Tempering characteristics of conventional high-speed steel EM42 and powder metallurgical high-speed steel ASP2042 [J]. Heat Treat. Met., 2018, 43(6): 211
  贾寓真, 吴懿萍, 匡旭光 等. 传统冶炼高速钢EM42与粉末冶金高速钢ASP2042的回火特性 [J]. 金属热处理, 2018, 43(6): 211
[25] El Rakayby A M, Mills B. Tempering and secondary hardening of M42 high-speed steel [J]. Mater. Sci. Technol., 1986, 2: 175
[26] Liu J H, Chi H X, Wu H B, et al. Heat treatment related microstructure evolution and low hardness issure of spray forming M3 high speed steel [J]. Chin. J. Mater. Res., 2023, 37: 625
  刘继浩, 迟宏宵, 武会宾 等. 喷射成形M3高速钢热处理过程中组织的演变和硬度偏低问题 [J]. 材料研究学报, 2023, 37: 625
[27] Xu Y. Microstructure and properties of spray forming FGH4095 superalloy and 9V high speed steel [D]. Southwest Jiaotong University, 2012
  徐 轶. 喷射成形FGH4095高温合金及9V高速钢组织性能研究 [D]. 成都: 西南交通大学, 2012
[28] Li J R, He T, Zhang P F, et al. Effect of large-size carbides on the anisotropy of mechanical properties in 11Cr-3Co-3W martensitic heat-resistant steel for turbine high temperature blades in ultra-supercritical power plants [J]. Mater. Charact., 2020, 159: 110025
[29] Johansson H, Sandstr?m R. Fracture behaviour and fracture toughness of M2 high speed steel [J]. Mater. Sci. Eng., 1978, 36: 175
[30] Xu Y W, Wang H M. Microstructure and room-temperature dry sliding wear behavior of Mo2Ni3Si/γ dual-phase alloy [J]. Acta Metall. Sin., 2006, 42: 722
  徐亚伟, 王华明. Mo2Ni3Si/γ双相合金的显微组织及室温干滑动磨损行为研究 [J]. 金属学报, 2006, 42: 722
[31] Fordyce I, Annasamy M, Sun S D, et al. The effect of heat treatment on the abrasive and erosive wear behaviour of laser metal deposited Fe-28Cr-2.7C alloy [J]. Wear, 2020, 458-459: 203410
[32] Wei S Z, Xu L J, Zhu J H, et al. Effect of carbon and vanadium content on microstructure and mechanical properties of high vanadium high speed steel [J]. J. Iron Steel Res., 2005, 17(5): 66
  魏世忠, 徐流杰, 朱金华 等. 碳、钒含量对高钒高速钢组织和力学性能的影响 [J]. 钢铁研究学报, 2005, 17(5): 66
[33] Liu H F, Liu Y H, Yu S R. Investigation of the wear resistance of high carbon high vanadium high speed steel [J]. Tribology, 2000, 20: 401
  刘海峰, 刘耀辉, 于思荣. 高碳高钒系高速钢的耐磨性研究 [J]. 摩擦学学报, 2000, 20: 401
[34] Rodenburg C, Rainforth W M. A quantitative analysis of the influence of carbides size distributions on wear behaviour of high-speed steel in dry rolling/sliding contact [J]. Acta Mater., 2007, 55: 2443
[35] Bergman F, Hedenqvist P, Hogmark S. The influence of primary carbides and test parameters on abrasive and erosive wear of selected PM high speed steels [J]. Tribol. Int., 1997, 30: 183
[36] Gore G J, Gates J D. Effect of hardness on three very different forms of wear [J]. Wear, 1997, 203-204: 544
[37] Wang Y, Su M, Chen C N. The influence of normal load and sliding speed on dry sliding friction of steel GCr15 [J]. Tribology, 1993, 13: 263
  王 铀, 苏 梅, 陈赤囡. 法向载荷和滑动速度对GCr15钢干滑动摩擦的影响 [J]. 摩擦学学报, 1993, 13: 263
[38] Stott F H, Wood G C. The influence of oxides on the friction and wear of alloys [J]. Tribol. Int., 1978, 11: 211
[39] Quinn T F J. Oxidational wear modelling Part III. The effects of speed and elevated temperatures [J]. Wear, 1998, 216: 262
[40] Wilson J E, Stott F H, Wood G C. The development of wear-protective oxides and their influence on sliding friction [J]. Proc. Roy. Soc., 1980, 369A: 557
[41] Vardavoulias M. The role of hard second phases in the mild oxidational wear mechanism of high-speed steel-based materials [J]. Wear, 1994, 173: 105
[42] Guo J, Feng Y L, Liu L G, et al. Investigation of microstructural damage to eutectic carbides from scratch tests of a heat-treated Fe-Cr-W-Mo-V-C alloy [J]. Wear, 2016, 358-359: 137
[43] Iakovakis E, Roy M J, Gee M, et al. Evaluation of wear mechanisms in additive manufactured carbide-rich tool steels [J]. Wear, 2020, 462-463: 203449
[44] Kumar K S, Lawley A, Koczak M J. Powder metallurgy T15 tool steel: Part I. Characterization of powder and hot isostatically pressed material [J]. Metall. Trans., 1991, 22A: 2733
[45] Zepon G, Ellendt N, Uhlenwinkel V, et al. Solidification sequence of spray-formed steels [J]. Metall. Mater. Trans., 2016, 47A: 842
[46] Liotti E, Arteta C, Zisserman A, et al. Crystal nucleation in metallic alloys using X-ray radiography and machine learning [J]. Sci. Adv., 2018, 4: eaar4004
[47] Li S S, Chen Y, Gong T Z, et al. Effect of cooling rate on the precipitation mechanism of primary carbide during solidification in high carbon-chromium bearing steel [J]. Acta Metall. Sin., 2022, 58: 1024
  李闪闪, 陈 云, 巩桐兆 等. 冷速对高碳铬轴承钢液析碳化物凝固析出机制的影响 [J]. 金属学报, 2022, 58: 1024
Outlines

/