Effect of Electron Beam Smelting Power on Microstructure, Segregation, and γ′ Phase Precipitation Behavior of GH4068 Alloy
Received date: 2023-06-19
Revised date: 2023-11-15
Online published: 2024-01-19
Supported by
National Key Research and Development Program of China(2019YFA0705300)
The as-cast structure of high-alloyed wrought superalloys exhibits disadvantages such as high microscopic segregation and poor microstructure uniformity, severely affecting their subsequent hot working and deformation properties. To optimize the as-cast structure of the wrought superalloy, GH4068 alloy was smelted via electron beam smelting (EBS), and its ingots with low segregation were prepared by setting different EBS powers for 10 min. The results show that the bottom of the ingots after EBS appeared to be fine grain regions, with the presence of only cellular segregation structure and cellular dendritic crystal; the large area in the middle became vertically growing columnar crystal regions, the direction of secondary dendrite crystal growth was parallel to that of the columnar crystal growth; a small amount of equiaxed crystal was observed at the top, and the growth direction of dendritic crystals was disordered. Analyzing the compositions of ingots revealed that Cr volatilization in this alloy was the most obvious; the Cr content decreased by 1.97% when the EBS power was 17 kW. The ingot structure prepared via EBS was more highly distributed than that obtained using the traditional vacuum induction melting + electroslag remelting duplex process. When the EBS power was 12 kW, the secondary dendrite spacing λ2 was 44.6 μm, which was 32.2% less than that yielded using the duplex process, the degree of the microscopic segregation of the ingot dendrite region decreased considerably, and the degree of the microscopic segregation of the typical easily segregated elements Ti and W reduced by 20.4% and 18.6%, respectively. Furthermore, the massive precipitation of large interdendritic γ′ phases were observed, while the γ′ phases in the dendritic core were spherical and smaller in size than those in the interdendritic. Meanwhile, the ingot prepared with an EBS power of 12 kW achieved the smallest size for γ′ phases and least irregular γ′ phases in the interdendritic. In the EBS process, the actual melt temperature was considerably higher than the alloy melting temperature. After the overheating of the melt, the cluster structure effectively decomposed, elements were uniformly distributed, the degree of subcooling increased in the solidification process, and the uniformity of the melt was inherited to the solidification structure to refine the as-cast structure and reduce the degree of microscopic segregation. Meanwhile, during the EBS process, local high temperature generated due to the electron beam bombardment on the surface of the molten pool effectively reduced the N content in the alloy.
BAI Rusheng , TAN Yi , CUI Hongyang , NING Lidan , CUI Chuanyong , WANG Yunpeng , LI Pengting . Effect of Electron Beam Smelting Power on Microstructure, Segregation, and γ′ Phase Precipitation Behavior of GH4068 Alloy[J]. Acta Metall Sin, 2024 , 60(9) : 1189 -1199 . DOI: 10.11900/0412.1961.2023.00263
| 1 | Reed R C, Tao T, Warnken N. Alloys-by-design: Application to nickel-based single crystal superalloys [J]. Acta Mater., 2009, 57: 5898 |
| 2 | Gu Y, Harada H, Cui C, et al. New Ni-Co-base disk superalloys with higher strength and creep resistance [J]. Scr. Mater., 2006, 55: 815 |
| 3 | Cui C Y, Gu Y F, Yuan Y, et al. Enhanced mechanical properties in a new Ni-Co base superalloy by controlling microstructures [J]. Mater. Sci. Eng., 2011, A528: 5465 |
| 4 | Zhou Z J, Zhang R, Cui C Y, et al. Effects of homogenization treatment on the microsegregation of a Ni-Co based superalloy produced by directional solidification [J]. Acta Metall. Sin. (Engl. Lett.), 2021, 34: 943 |
| 5 | Gu Y F, Cui C Y, Yuan Y, et al. Research progress in a high performance cast & wrought superalloy for turbine disc applications [J]. Acta Metall. Sin., 2015, 51: 1191 |
| 谷月峰, 崔传勇, 袁 勇 等. 一种高性能航空涡轮盘用铸锻合金的研究进展 [J]. 金属学报, 2015, 51: 1191 | |
| 6 | Chen G S, Liu F J, Wang Q Z, et al. Triple-melted process and metallurgical quality of GH4169 alloy by the VIM + PESR + VAR processing [J]. J. Iron Steel Res., 2011, 23: 134 |
| 陈国胜, 刘丰军, 王庆增 等. GH4169合金VIM + PESR + VAR三联冶炼工艺及其冶金质量 [J]. 钢铁研究学报, 2011, 23: 134 | |
| 7 | Dong T W, Kou S Z, Pu Y L, et al. Microstructure and mechanical properties of K4169 alloy by the cold crucible levitation melting [J]. Foundry, 2015, 64: 1254 |
| 董天文, 寇生中, 蒲永亮 等. 水冷铜坩埚悬浮熔炼K4169合金的组织和力学性能 [J]. 铸造, 2015, 64: 1254 | |
| 8 | Trosch T, Str??ner J, V?lkl R, et al. Microstructure and mechanical properties of selective laser melted Inconel 718 compared to forging and casting [J]. Mater. Lett., 2016, 164: 428 |
| 9 | You Q F, Yuan H, You X G, et al. Segregation behavior of nickel-based superalloy after electron beam smelting [J]. Vacuum, 2017, 145: 116 |
| 10 | You X G, Tan Y, You Q F, et al. Preparation of Inconel 740 superalloy by electron beam smelting [J]. J. Alloys Compd., 2016, 676: 202 |
| 11 | Vutova K, Vassileva V, Koleva E, et al. Investigation of electron beam melting and refining of titanium and tantalum scrap [J]. J. Mater. Process. Technol., 2010, 210: 1089 |
| 12 | Choi G S, Lim J W, Munirathnam N R, et al. Preparation of 5N grade tantalum by electron beam melting [J]. J. Alloys Compd., 2009, 469: 298 |
| 13 | Yao K, Min X H, Shi S, et al. Volatilization behavior of β-type Ti-Mo alloy manufactured by electron beam melting [J]. Metals, 2018, 8: 206 |
| 14 | Zhuang X P, Tan Y, Zhao L H, et al. Microsegregation of a new Ni-Co-based superalloy prepared through electron beam smelting and its homogenization treatment [J]. J. Mater. Res. Technol., 2020, 9: 5422 |
| 15 | Wang Y L, Tan Y, Cui C Y, et al. Evaporation behavior of alloying elements and calculation of molten pool temperature in electron beam smelting of a new Ni-Co based superalloy [J]. Mater. Rep., 2023, 37(1): 176 |
| 王以霖, 谭 毅, 崔传勇 等. 电子束熔炼新型Ni-Co基高温合金过程中合金元素的挥发行为及熔池温度计算 [J]. 材料导报, 2023, 37(1): 176 | |
| 16 | Liu G Q, Feng L, Wang H M, et al. Statistics on the primary dendrite spacing of Ni-based single crystal super alloys [J]. Spec. Cast. Nonferrous Alloys, 2021, 41: 153 |
| 刘贵群, 冯 丽, 王贺明 等. 镍基单晶高温合金一次枝晶间距的统计研究 [J]. 特种铸造及有色合金, 2021, 41: 153 | |
| 17 | Zhao J. Fundamentals of Materials Science [M]. 2nd Ed., Dalian: Dalian University of Technology Press, 2015: 269 |
| 赵 杰. 材料科学基础 [M]. 第2版. 大连: 大连理工大学出版社, 2015: 269 | |
| 18 | Raghavan N, Dehoff R, Pannala S, et al. Numerical modeling of heat-transfer and the influence of process parameters on tailoring the grain morphology of IN718 in electron beam additive manufacturing [J]. Acta Mater., 2016, 112: 303 |
| 19 | Zhang W, Roy G G, Elmer J W, et al. Modeling of heat transfer and fluid flow during gas tungsten arc spot welding of low carbon steel [J]. J. Appl. Phys., 2003, 93: 3022 |
| 20 | He X, Elmer J W, Debroy T. Heat transfer and fluid flow in laser microwelding [J]. J. Appl. Phys., 2005, 97: 084909 |
| 21 | Cui H Y, Tan Y, Bai R S, et al. Microsegregation of a new Ni-Co-based superalloy prepared by electron beam smelting layered solidification technology and its homogenization behavior [J]. Mater. Charact., 2022, 184: 111668 |
| 22 | Yin F S, Sun X F, Guan H R, et al. Effect of thermal history on the liquid structure of a cast nickel-base superalloy M963 [J]. J. Alloys Compd., 2004, 364: 225 |
| 23 | Yin F S, Zheng Q, Sun X F, et al. Effect of melt treatment on carbides formation in a cast nickel-base superalloy M963 [J]. J. Mater. Process. Technol., 2007, 183: 440 |
| 24 | Wang H F, Su H J, Zhang J, et al. Effect of melt thermal history on solidification behavior and microstructural characteristics of a third-generation Ni-based single crystal superalloy [J]. J. Alloys Compd., 2016, 688: 430 |
| 25 | Calvo-dahlborg M, Popel P S, Kramer M J, et al. Superheat-dependent microstructure of molten Al-Si alloys of different compositions studied by small angle neutron scattering [J]. J. Alloys Compd., 2013, 550: 9 |
| 26 | Wang C S, Zhang J, Liu L, et al. Microstructure evolution of directionally solidified DZ125 superalloy with melt superheating treatment [J]. J. Alloys Compd., 2010, 508: 440 |
/
| 〈 |
|
〉 |