Corrosion and Wear Behaviors of Fe-Based Composite Coating with Dual Amorphous Phases
Received date: 2023-11-13
Revised date: 2023-12-13
Online published: 2024-01-17
Supported by
National Natural Science Foundation of China(52371043);National Natural Science Foundation of China(51771005);National Natural Science Foundation of China(52171060)
Fe-based amorphous composite coatings have attracted great attention because their specific properties can be enhanced by introducing other metallic or ceramic particles. This work introduces a novel approach, distinct from traditional methods, by designing a composite coating with dual amorphous phases. The composite coating (named FH) was fabricated using high-velocity oxygen-fuel spraying of a blended amorphous powder. This powder comprised well-established Fe48Cr15Mo14C15B6Y2 (named FM) and Fe59Cr12Nb5B20Si4 (named FN) amorphous powders. This study focuses on investigating the corrosion and wear behaviors of the FH coating in comparison with those of monolithic amorphous coatings. The findings reveal that the FH coating possesses a high amorphous content and a compact structure. It features a uniform distribution of two types of amorphous splats, with no evident element diffusion. In 3.5%NaCl solution, the FH coating exhibits passivation behavior, similar to the two monolithic amorphous coatings, and yields a lower corrosion current and higher polarization resistance, indicating enhanced its corrosion resistance. This improved corrosion resistance of the FH coating is attributed to a harmonious balance between beneficial alloy elements and its compact structure, addressing the limitations of monolithic amorphous coatings. Furthermore, the FH coating displays a high friction coefficient under dry friction conditions and maintains a low wear rate, comparable to those of the FN coating. The wear mechanisms of the three amorphous coatings under dry friction primarily involve fatigue wear, supplemented by minor abrasive and oxidative wear. Compared to the monolithic amorphous coating, the FH coating shows enhanced interfacial bonding of splats and a balanced combination of strengthening and toughening, which effectively inhibit crack propagation caused by fatigue wear, thereby endowing the coating with superior wear resistance. Therefore, the composite coating with dual amorphous phases achieves a balance in cost efficiency, corrosion resistance, and wear resistance.
ZANG Bolin , YANG Yange , CAO Jingyi , XU Fengfeng , YAO Haihua , ZHOU Zheng . Corrosion and Wear Behaviors of Fe-Based Composite Coating with Dual Amorphous Phases[J]. Acta Metall Sin, 2025 , 61(8) : 1267 -1275 . DOI: 10.11900/0412.1961.2023.00449
| [1] | Si J J, Mei J N, Wang R S, et al. Fe-B-Si-Zr bulk metallic glasses with ultrahigh compressive strength and excellent soft magnetic properties [J]. Mater. Lett., 2016, 181: 282 |
| [2] | Li J F, Liu X, Zhao S F, et al. Fe-based bulk amorphous alloys with iron contents as high as 82 at% [J]. J. Magn. Magn. Mater., 2015, 386: 107 |
| [3] | Zhang W B, Li Q, Duan H M. Study of the effects of metalloid elements (P, C, B) on Fe-based amorphous alloys by ab initio molecular dynamics simulations [J]. J. Appl. Phys., 2015, 117: 104901 |
| [4] | Li H X, Lu Z C, Wang S L, et al. Fe-based bulk metallic glasses: Glass formation, fabrication, properties and applications [J]. Prog. Mater. Sci., 2019, 103: 235 |
| [5] | Lin C Y, Tien H Y, Chin T S. Soft magnetic ternary iron-boron-based bulk metallic glasses [J]. Appl. Phys. Lett., 2005, 86: 162501 |
| [6] | Dmowski W, Fan C, Morrison M L, et al. Structural changes in bulk metallic glass after annealing below the glass-transition temperature [J]. Mater. Sci. Eng., 2007, A471: 125 |
| [7] | Zhang S D, Wu J, Qi W B, et al. Effect of porosity defects on the long-term corrosion behaviour of Fe-based amorphous alloy coated mild steel [J]. Corros. Sci., 2016, 110: 57 |
| [8] | Inoue A, Takeuchi A. Recent development and application products of bulk glassy alloys [J]. Acta Mater., 2011, 59: 2243 |
| [9] | Suryanarayana C, Inoue A. Iron-based bulk metallic glasses [J]. Int. Mater. Rev., 2013, 58: 131 |
| [10] | Zhou Z, Wang L, Wang F C, et al. Formation and corrosion behavior of Fe-based amorphous metallic coatings by HVOF thermal spraying [J]. Surf. Coat. Technol., 2009, 204: 563 |
| [11] | Zhou Z, Han F X, Yao H H, et al. Novel Fe-based amorphous composite coating with a unique interfacial layer improving thermal barrier application [J]. ACS Appl. Mater. Interfaces, 2021, 13: 23057 |
| [12] | Segu D Z, Choi J H, Yi S, et al. Dry sliding tribological properties of Fe-based bulk metallic glass [J]. Tribol. Lett., 2012, 47: 131 |
| [13] | Yao H H, Wang L, Zhou Z, et al. Thermal transport property correlated with microstructural evolution of Fe-based amorphous alloy [J]. Acta Mater., 2020, 200: 793 |
| [14] | Ye X Y, Shin Y C. Synthesis and characterization of Fe-based amorphous composite by laser direct deposition [J]. Surf. Coat. Technol., 2014, 239: 34 |
| [15] | Xu F F, Yao H H, Tang K Z, et al. Degeneration of thermal insulation property for Fe-based amorphous coating during long-term heat exposure [J]. J. Non-Cryst. Solids, 2023, 606: 122203 |
| [16] | Terajima T, Takeuchi F, Nakata K, et al. Composite coating containing WC/12Co cermet and Fe-based metallic glass deposited by high-velocity oxygen fuel spraying [J]. J. Alloys Compd., 2010, 504: S288 |
| [17] | Yasir M, Zhang C, Wang W, et al. Enhancement of impact resistance of Fe-based amorphous coating by Al2O3 dispersion [J]. Mater. Lett., 2016, 171: 112 |
| [18] | Zhou H, Zhang C, Wang W, et al. Microstructure and mechanical properties of Fe-based amorphous composite coatings reinforced by stainless steel powders [J]. J. Mater. Sci. Technol., 2014, 31: 43 |
| [19] | Yoon S, Kim J, Kim B D, et al. Tribological behavior of B4C reinforced Fe-base bulk metallic glass composite coating [J]. Surf. Coat. Technol., 2010, 205: 1962 |
| [20] | Yugeswaran S, Kobayashi A, Suresh K, et al. Characterization of gas tunnel type plasma sprayed TiN reinforced Fe-based metallic glass coatings [J]. J. Alloys Compd., 2013, 551: 168 |
| [21] | Cui C, Hou W A. Properties of Fe-based amorphous alloy coatings with Al2O3-13% TiO2 deposited by plasma spraying [J]. Rare Met. Mater. Eng., 2014, 43: 2576 |
| [22] | Wang S L, Cheng J C, Yi S H, et al. Corrosion resistance of Fe-based amorphous metallic matrix coating fabricated by HVOF thermal spraying [J]. Trans. Nonferrous Met. Soc. China, 2014, 24: 146 |
| [23] | Xu P, Zhang C, Wang W, et al. Pitting mechanism in a stainless steel-reinforced Fe-based amorphous coating [J]. Electrochim. Acta, 2016, 206: 61 |
| [24] | Zhou Z, Wang L, Wang F C, et al. Microstructure and properties of Fe-based amorphous alloy coatings [J]. Trans. Beijing Inst. Technol., 2008, 28: 817 |
| 周 正, 王 鲁, 王富耻 等. Fe基非晶合金涂层的微结构与性能研究 [J]. 北京理工大学学报自然版, 2008, 28: 817 | |
| [25] | Pang S J, Zhang T, Asami K, et al. Bulk glassy Fe-Cr-Mo-C-B alloys with high corrosion resistance [J]. Corros. Sci., 2002, 44: 1847 |
| [26] | Huang F, Kang J J, Yue W, et al. Corrosion behavior of FeCrMoCBY amorphous coating fabricated by high-velocity air fuel spraying [J]. J. Therm. Spray Technol., 2019, 28: 842 |
| [27] | Zhang H, Hu Y, Hou G L, et al. The effect of high-velocity oxy-fuel spraying parameters on microstructure, corrosion and wear resistance of Fe-based metallic glass coatings [J]. J. Non-Cryst. Solids, 2014, 406: 37 |
| [28] | Yao H H, Zhou Z, Xue Y F, et al. Microstructure and thermal conductivity of wire-arc sprayed FeCrNbBSiC amorphous coating [J]. J. Alloys Compd., 2019, 788: 514 |
| [29] | Liang X B, Chen Y X, Cheng J B, et al. Arc Spray Substable Composite Coating Technology [M]. Beijing: Science Press, 2014: 57 |
| 梁秀兵, 陈永雄, 程江波 等. 电弧喷涂亚稳态复合涂层技术 [M]. 北京: 科学出版社, 2014: 57 | |
| [30] | Zeng Z, Kuroda S, Era H. Comparison of oxidation behavior of Ni-20Cr alloy and Ni-base self-fluxing alloy during air plasma spraying [J]. Surf. Coat. Technol., 2009, 204: 69 |
| [31] | Farmer J C, Turchi P E A, Perepezko J H. Iron-based amorphous metals—An important family of high-performance corrosion-resistant materials [J]. Metall. Mater. Trans., 2009, 40A: 1288 |
| [32] | Guo R Q, Zhang C, Chen Q, et al. Study of structure and corrosion resistance of Fe-based amorphous coatings prepared by HVAF and HVOF [J]. Corros. Sci., 2011, 53: 2351 |
| [33] | Guo R Q, Zhang C, Yang Y, et al. Corrosion and wear resistance of a Fe-based amorphous coating in underground environment [J]. Intermetallics, 2012, 30: 94 |
/
| 〈 |
|
〉 |