Research paper

Long-Term Oxidation Behavior and Microstructural Evolution of γ-TiAl Alloys at 700 oC in Air

  • ZHOU Zhichun ,
  • LIU Renci ,
  • ZHANG Jianda ,
  • YANG Chao ,
  • CUI Yuyou ,
  • YANG Rui
Expand
  • 1.Shi -changxu Innovation Center for Advanced Materials, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
    2.School of Materials Science and Engineering, University of Science and Technology of China, Shenyang 110016, China
    3.School of Materials Science and Engineering, Shenyang University of Technology, Shenyang 110870, China
    4.AECC Commercial Aero-Engine Co. Ltd., Shanghai 200241, China
LIU Renci, professor, Tel: (024)83970951, E-mail: rcliu@imr.ac.cn

Received date: 2023-11-13

  Revised date: 2023-12-10

  Online published: 2024-01-02

Supported by

Major Special Science and Technology Project of Yunnan Province(202302AB080009);CAS Project for Young Scientists in Basic Research(YSBR-025);National Key Research and Development Program of China(2021YFB3702605);National Science and Technology Major Projects of China(J2019-VII-0002-0142)

Abstract

γ-TiAl alloys are a new generation of high-temperature lightweight materials characterized by low density, high specific modulus of elasticity, excellent high-temperature strength, and creep resistance, making them highly suitable for aviation, aerospace, and automotive engine applications. A typical application of the alloys is in the low-pressure turbine blades of aero-engines, such as GEnx and Trent XWB developed by the General Electric and Rolls-Royce, respectively. Their alloy compositions are Ti-48Al-2Cr-2Nb and Ti-45Al-2Nb-2Mn-1B (atomic fraction, %), respectively. γ-TiAl alloys are required for long-term service at 600-700 oC; however, they react readily with oxygen to form oxide scale when exposed in air at high temperatures, compromising service safety and reliability. Thus, understanding the long-term oxidation behavior of γ-TiAl alloys during service at high temperatures is imperative. In this study, the oxide scale and microstructural evolution of cast Ti-45Al-2Nb-2Mn-1B alloy (45XD alloy) and Ti-48Al-2Nb-2Cr alloy (4822 alloy) at 700 oC in air for 0-2000 h were investigated using SEM and TEM. The mass gain of both alloys was measured during oxidation, and their oxidation behaviors were compared. The 4822 alloy exhibited a notably higher mass gain than the 45XD alloy. Both alloys demonstrated periodic mass gain behavior during oxidation for 0-2000 h—alternating rapid and slow gains—with stabilization in the later stages. The oxide scales formed layered structures, primarily of TiO2 and Al2O3, on the surface of both alloys; the scale of 45XD alloy was continuous and dense, whereas that of the 4822 alloy was porous. Additionally, the study revealed that α2 lamellae in the subsurface of the 45XD alloy decomposed during oxidation, forming an Al-rich and Ti-lean γ zone on the subsurface. α2 lamellae in the bulk microstructure of the 45XD alloy were also decomposed and transformed into γ phase. The 4822 alloy experienced a significant reduction in the volume fractions of α2 in equiaxed γ grains and α2 + β0 at equiaxed γ grain boundaries.

Cite this article

ZHOU Zhichun , LIU Renci , ZHANG Jianda , YANG Chao , CUI Yuyou , YANG Rui . Long-Term Oxidation Behavior and Microstructural Evolution of γ-TiAl Alloys at 700 oC in Air[J]. Acta Metall Sin, 2025 , 61(8) : 1217 -1228 . DOI: 10.11900/0412.1961.2023.00443

References

[1] Kim Y W. Intermetallic alloys based on gamma titanium aluminide [J]. JOM, 1989, 41(7): 24
[2] Clemens H, Mayer S. Design, processing, microstructure, properties, and applications of advanced intermetallic TiAl alloys [J]. Adv. Eng. Mater., 2013, 15: 191
[3] Yang R. Advances and challenges of TiAl base alloys [J]. Acta Metall. Sin., 2015, 51: 129
  杨 锐. 钛铝金属间化合物的进展与挑战 [J]. 金属学报, 2015, 51: 129
[4] Kim Y W, Kim S L. Advances in gammalloy materials-processes-application technology: Successes, dilemmas, and future [J]. JOM, 2018, 70: 553
[5] Clemens H, Mayer S. Intermetallic titanium aluminides in aerospace applications—Processing, microstructure and properties [J]. Mater. High Temp., 2016, 33: 560
[6] Bewlay B P, Nag S, Suzuki A, et al. TiAl alloys in commercial aircraft engines [J]. Mater. High Temp., 2016, 33: 549
[7] Rahmel A, Schütze M, Quadakkers W J. Fundamentals of TiAl oxidation—A critical review [J]. Mater. Corros., 1995, 46: 271
[8] Mengis L, Ulrich A S, Watermeyer P, et al. Oxidation behaviour and related microstructural changes of two β0-phase containing TiAl alloys between 600 oC and 900 oC [J]. Corros. Sci., 2021, 178: 109085
[9] Shaaban A, Hayashi S, Takeyama M. A comparative study on the oxidation behaviours of a TNM alloy in argon and oxygen atmospheres at 650 oC [J]. Corros. Sci., 2021, 185: 109415
[10] Liu R C, Wang P, Cao R X, et al. Influence of thermal exposure at 700 oC on the microstructure and morphology in the surface of β-solidifying γ-TiAl alloys [J]. Acta Metall. Sin., 2022, 58: 1003
  刘仁慈, 王 鹏, 曹如心 等. 700 ℃热暴露对β凝固γ-TiAl合金表面组织及形貌的影响 [J]. 金属学报, 2022, 58: 1003
[11] Tian S W, He A R, Liu J H, et al. Oxidation resistance of TiAl alloy improved by hot-pack rolling and cyclic heat treatment [J]. Mater. Charact., 2021, 178: 111196
[12] Pan Y, Lu X, Hui T L, et al. High-temperature oxidation behaviour of TiAl alloys with Co addition [J]. J. Mater. Sci., 2021, 56: 815
[13] Cui Y Y, Xiang H F, Jia Q, et al. Effects of thermal exposure on the tensile and fatigue properties of cast Ti-47Al-2Cr-2Nb-0.15B alloy [J]. Acta Metall. Sin., 2005, 41: 108
  崔玉友, 项宏福, 贾 清 等. 热暴露对铸造Ti-47Al-2Cr-2Nb-0.15B合金的拉伸和疲劳性能的影响 [J]. 金属学报, 2005, 41: 108
[14] Dowling W E, Donlon W T. The effect of surface film formation from thermal exposure on the ductility of Ti-48A1-1V-0.2C (at%) [J]. Scr. Metall. Mater., 1992, 27: 1663
[15] Thomas M, Berteaux O, Popoff F, et al. Effects of exposure at 700 oC on RT tensile properties in a PM γ-TiAl alloy [J]. Intermetallics, 2006, 14: 1143
[16] Zhou Z C, Liu R C, Shen Y Y, et al. Microstructural evolution and embrittlement of a β-solidifying γ-TiAl alloy during exposure at 700 °C [J]. Mater. Sci. Eng., 2022, A852: 143704
[17] Pather R, Mitten W A, Holdway P, et al. The effect of high temperature exposure on the tensile properties of γ TiAl alloys [J]. Intermetallics, 2003, 11: 1015
[18] Draper S L, Lerch B A, Locci I E, et al. Effect of exposure on the mechanical properties of Gamma MET PX [J]. Intermetallics, 2005, 13: 1014
[19] Wu X H, Huang A, Hu D, et al. Oxidation-induced embrittlement of TiAl alloys [J]. Intermetallics, 2009, 17: 540
[20] Kelly T J, Austin C M, Fink P J, et al. Effect of elevated temperature exposure on cast gamma titanium aluminide (Ti-48Al-2Cr-2Nb) [J]. Scr. Metall. Mater., 1994, 30: 1105
[21] Wang F H, Tang Z L. Oxidation and protection of TiAl intermetallics [J]. Chin. J. Mater. Res., 1998, 12: 337
  王福会, 唐兆麟. TiAl金属间化合物的高温氧化与防护研究进展 [J]. 材料研究学报, 1998, 12: 337
[22] Rahmel A, Spencer P J. Thermodynamic aspects of TiAl and TiSi2 oxidation: The Al-Ti-O and Si-Ti-O phase diagrams [J]. Oxid. Met., 1991, 35: 53
[23] Becker S, Rahmel A, Schorr M, et al. Mechanism of isothermal oxidation of the intel-metallic TiAl and of TiAl alloys [J]. Oxid. Met., 1992, 38: 425
[24] Lin J P, Zhao L L, Li G Y, et al. Effect of Nb on oxidation behavior of high Nb containing TiAl alloys [J]. Intermetallics, 2011, 19: 131
[25] Garip Y, Ozdemir O. A study of the cycle oxidation behavior of the Cr/Mn/Mo alloyed Ti-48Al-based intermetallics prepared by ECAS [J]. J. Alloys Compd., 2020, 818: 152818
[26] Shida Y, Anada H. The effect of various ternary additives on the oxidation behavior of TiAl in high-temperature air [J]. Oxid. Met., 1996, 45: 197
[27] Stroosnijder M F, Haanappel V A C, Clemens H. Oxidation behaviour of TiAl-based intermetallics-influence of heat treatment [J]. Mater. Sci. Eng., 1997, A239-240: 842
[28] Haanappel V A C, Hofman R, Sunderk?tter J D, et al. The influence of microstructure on the isothermal and cyclic-oxidation behavior of Ti-48Al-2Cr at 800 oC [J]. Oxid. Met., 1997, 48: 263
[29] Pérez P, Jiménez J A, Frommeyer G, et al. The influence of the alloy microstructure on the oxidation behavior of Ti-46Al-1Cr-0.2Si alloy [J]. Oxid. Met., 2000, 53: 99
[30] Haanappel V A C, Clemens H, Stroosnijder M F. The effect of microstructure on the oxidation behaviour of Ti-46.5Al-4(Cr,Nb,Ta,B) and Ti-47Al-4(Cr,Nb,Mo,B) [J]. Mater. High Temp., 2002, 19: 19
[31] Maurice V, Despert G, Zanna S, et al. XPS study of the initial stages of oxidation of α2-Ti3Al and γ-TiAl intermetallic alloys [J]. Acta Mater., 2007, 55: 3315
[32] Li M S. High Temperature Corrosion of Metals [M]. Beijing: Metallurgical Industry Press, 2001: 5
  李美栓. 金属的高温腐蚀 [M]. 北京: 冶金工业出版社, 2001: 5
[33] Huang Z W, Sun C. On the role of thermal exposure on the stress controlled fatigue behaviour of a high strength titanium-aluminum alloy [J]. Mater. Sci. Eng., 2014, A615: 29
[34] Zhu H L, Seo D Y, Maruyama K, et al. Effect of microstructural stability on creep behavior of 47XD TiAl alloys with fine-grained fully lamellar structure [J]. Scr. Mater., 2005, 52: 45
[35] Huang Z W. Thermal stability of Ti-44Al-4Nb-4Hf-0.2Si-1B alloy [J]. Intermetallics, 2013, 37: 11
Outlines

/