Microstructure and Mechanical Properties of As-Cast and Laser Powder Bed Fused AlCoCrFeNi2.1 Eutectic High-Entropy Alloy
Received date: 2023-07-14
Revised date: 2023-09-07
Online published: 2023-12-19
Supported by
National Natural Science Foundation of China(U21A2043);Youth Innovation Promotion Association, CAS(2022191);Bintech-IMR Research and Development Program(GYY-JSBU-2022-010)
Eutectic high-entropy alloys (EHEAs), as a typical kind of in situ composite, have become a potential alternative for conventional alloys because of their advantages in high-entropy alloys and eutectic alloys. Casting is the conventional preparation method of EHEAs, which is a well-established process with low production efficiency. Laser powder bed fusion (LPBF) is an economical and effective preparation technology that provides a novel way to directly form fine and complex EHEA components. In this study, considering the different application requirements and technical characteristics, AlCoCrFeNi2.1 EHEA was prepared by vacuum induction melting and LPBF, respectively. The effect of the preparation process on the microstructure of the alloy was investigated. In addition, tensile properties of the samples at 20, 500, and 700°C were investigated. Results showed that as-cast and LPBF-formed AlCoCrFeNi2.1 exhibited a eutectic structure composed of alternating fcc and bcc/B2 phases. The high heating and cooling rates during the LPBF process were conducive to the formation of ultrafine and uniform eutectic lamellae, which significantly reduced element segregation. During tensile deformation at room temperature, considering the strong phase boundary strengthening and dual-phase synergistic deformation, the ultimate tensile strength of the LPBF-formed sample was enhanced by about 28% compared with that of the as-cast sample, and a satisfactory elongation of 10% was obtained. At 500°C, the mechanical properties of the as-cast and LPBF-formed samples decreased probably because of the severe phase transformation in the alloy. When the testing temperature was increased to 700°C, the mechanical properties of the as-cast sample continued to decrease. The LPBF-formed samples showed a low tensile strength and superior elongation that should be attributed to the eutectic lamellae sliding along the phase boundaries at high temperatures. Meanwhile, the fracture mechanism of the LPBF-formed sample was dominated by ductile fracture. This work could provide a theoretical basis for the optimization of the microstructure and mechanical properties of EHEAs, thereby promoting their industrial application.
TANG Xu , ZHANG Hao , XUE Peng , WU Lihui , LIU Fengchao , ZHU Zhengwang , NI Dingrui , XIAO Bolv , MA Zongyi . Microstructure and Mechanical Properties of As-Cast and Laser Powder Bed Fused AlCoCrFeNi2.1 Eutectic High-Entropy Alloy[J]. Acta Metall Sin, 2024 , 60(11) : 1461 -1470 . DOI: 10.11900/0412.1961.2023.00301
| 1 | Leong Z, Ramamurty U, Tan T L. Microstructural and compositional design principles for Mo-V-Nb-Ti-Zr multi-principal element alloys: A high-throughput first-principles study [J]. Acta Mater., 2021, 213: 116958 |
| 2 | Kies F, Wu X X, Hallstedt B, et al. Enhanced precipitation strengthening of multi-principal element alloys by κ- and B2-phases [J]. Mater. Des., 2021, 198: 109315 |
| 3 | Chen Y J, Chen D K, An X H, et al. Unraveling dual phase transformations in a CrCoNi medium-entropy alloy [J]. Acta Mater., 2021, 215: 117112 |
| 4 | Kautz E J, Schreiber D K, Devaraj A, et al. Mechanistic insights into selective oxidation and corrosion of multi-principal element alloys from high resolution and in situ microscopy [J]. Materialia, 2021, 18: 101148 |
| 5 | Ding J L, Xu H J, Li X, et al. The similarity of elements in multi-principle element alloys based on a new criterion for phase constitution [J]. Mater. Des., 2021, 207: 109849 |
| 6 | Vikram R J, Murty B S, Fabijanic D, et al. Insights into micro-mechanical response and texture of the additively manufactured eutectic high entropy alloy AlCoCrFeNi2.1 [J]. J. Alloys Compd., 2020, 827: 154034 |
| 7 | Das S, Robi P S. Processing and characterization of W23Mo23V17Cr8-Ta7Fe22 and WMoVCrTa refractory high entropy alloys [J]. Int. J. Refract. Met. Hard Mater., 2021, 100: 105656 |
| 8 | Dada M, Popoola P, Mathe N, et al. The comparative study of the microstructural and corrosion behaviour of laser-deposited high entropy alloys [J]. J. Alloys Compd., 2021, 866: 158777 |
| 9 | He J Y, Wang H, Huang H L, et al. A precipitation-hardened high-entropy alloy with outstanding tensile properties [J]. Acta Mater., 2016, 102: 187 |
| 10 | Rogal ?. Semi-solid processing of the CoCrCuFeNi high entropy alloy [J]. Mater. Des., 2017, 119: 406 |
| 11 | Tang Z, Senkov O N, Parish C M, et al. Tensile ductility of an AlCoCrFeNi multi-phase high-entropy alloy through hot isostatic pressing (HIP) and homogenization [J]. Mater. Sci. Eng., 2015, A647: 229 |
| 12 | Wang M L, Cui H Z, Zhao Y Q, et al. A simple strategy for fabrication of an FCC-based complex concentrated alloy coating with hierarchical nanoprecipitates and enhanced mechanical properties [J]. Mater. Des., 2019, 180: 107893 |
| 13 | Huang H L, Wu Y, He J Y, et al. Phase-transformation ductilization of brittle high-entropy alloys via metastability engineering [J]. Adv. Mater., 2017, 29: 1701678 |
| 14 | Li R D, Niu P D, Yuan T C, et al. Selective laser melting of an equiatomic CoCrFeMnNi high-entropy alloy: Processability, non-equilibrium microstructure and mechanical property [J]. J. Alloys Compd., 2018, 746: 125 |
| 15 | Wang Q, Ma Y, Jiang B B, et al. A cuboidal B2 nanoprecipitation-enhanced body-centered-cubic alloy Al0.7CoCrFe2Ni with prominent tensile properties [J]. Scr. Mater., 2016, 120: 85 |
| 16 | Lu Y P, Dong Y, Guo S, et al. A promising new class of high-temperature alloys: Eutectic high-entropy alloys [J]. Sci. Rep., 2014, 4: 6200 |
| 17 | Lu Y P, Dong Y, Jiang H, et al. Promising properties and future trend of eutectic high entropy alloys [J]. Scr. Mater., 2020, 187: 202 |
| 18 | Shi P J, Ren W L, Zheng T X, et al. Enhanced strength-ductility synergy in ultrafine-grained eutectic high-entropy alloys by inheriting microstructural lamellae [J]. Nat. Commun., 2019, 10: 489 |
| 19 | Nassar A, Mullis A, Cochrane R, et al. Rapid solidification of AlCoCrFeNi2.1 high-entropy alloy [J]. J. Alloys Compd., 2022, 900: 163350 |
| 20 | Wang J T, Long Z P, Jiang P F, et al. Microstructure, crystallographic orientation and mechanical property in AlCoCrFeNi2.1 eutectic high-entropy alloy under magnetic field-assisted directional solidification [J]. Metall. Mater. Trans., 2020, 51A: 3504 |
| 21 | Gao X Z, Lu Y P, Zhang B, et al. Microstructural origins of high strength and high ductility in an AlCoCrFeNi2.1 eutectic high-entropy alloy [J]. Acta Mater., 2017, 141: 59 |
| 22 | Shi P J, Zhong Y B, Li Y, et al. Multistage work hardening assisted by multi-type twinning in ultrafine-grained heterostructural eutectic high-entropy alloys [J]. Mater. Today, 2020, 41: 62 |
| 23 | Xiong T, Zheng S J, Pang J Y, et al. High-strength and high-ductility AlCoCrFeNi2.1 eutectic high-entropy alloy achieved via precipitation strengthening in a heterogeneous structure [J]. Scr. Mater., 2020, 186: 336 |
| 24 | Wani I S, Bhattacharjee T, Sheikh S, et al. Tailoring nanostructures and mechanical properties of AlCoCrFeNi2.1 eutectic high entropy alloy using thermo-mechanical processing [J]. Mater. Sci. Eng., 2016, A675: 99 |
| 25 | Brif Y, Thomas M, Todd I. The use of high-entropy alloys in additive manufacturing [J]. Scr. Mater., 2015, 99: 93 |
| 26 | Tang X, Zhang S, Zhang C H, et al. Optimization of laser energy density and scanning strategy on the forming quality of 24CrNiMo low alloy steel manufactured by SLM [J]. Mater. Charact., 2020, 170: 110718 |
| 27 | Guo Y N, Su H J, Zhou H T, et al. Unique strength-ductility balance of AlCoCrFeNi2.1 eutectic high entropy alloy with ultra-fine duplex microstructure prepared by selective laser melting [J]. J. Mater. Sci. Technol., 2022, 111: 298 |
| 28 | He L, Wu S W, Dong A P, et al. Selective laser melting of dense and crack-free AlCoCrFeNi2.1 eutectic high entropy alloy: Synergizing strength and ductility [J]. J. Mater. Sci. Technol., 2022, 117: 133 |
| 29 | Ren J, Zhang Y, Zhao D X, et al. Strong yet ductile nanolamellar high-entropy alloys by additive manufacturing [J]. Nature, 2022, 608: 62 |
| 30 | Chen X S, Kong J, Li J L, et al. High-strength AlCoCrFeNi2.1 eutectic high entropy alloy with ultrafine lamella structure via additive manufacturing [J]. Mater. Sci. Eng., 2022, A854: 143816 |
| 31 | Miao J W, Wang M L, Zhang A J, et al. Tribological properties and wear mechanism of AlCr1.3TiNi2 eutectic high-entropy alloy at elevated temperature [J]. Acta Metall. Sin., 2023, 59: 267 |
| 苗军伟, 王明亮, 张爱军 等. AlCr1.3TiNi2共晶高熵合金的高温摩擦学性能及磨损机理 [J]. 金属学报, 2023, 59: 267 | |
| 32 | Tsai K Y, Tsai M H, Yeh J W. Sluggish diffusion in Co-Cr-Fe-Mn-Ni high-entropy alloys [J]. Acta Mater., 2013, 61: 4887 |
| 33 | Tang X, Zhang H, Zhu Z W, et al. Dual-phase synergistic deformation characteristics and strengthening mechanism of AlCoCrFeNi2.1 eutectic high entropy alloy fabricated by laser powder bed fusion [J]. J. Mater. Sci. Technol., 2023, 150: 75 |
| 34 | Mullins W W, Sekerka R F. Stability of a planar interface during solidification of a dilute binary alloy [J]. J. Appl. Phys., 1964, 35: 444 |
| 35 | Xiong M X, Liew J Y R. Mechanical properties of heat-treated high tensile structural steel at elevated temperatures [J]. Thin-Wall. Struct., 2016, 98: 169 |
| 36 | Qiang X H, Bijlaard F, Kolstein H. Dependence of mechanical properties of high strength steel S690 on elevated temperatures [J]. Constr. Build. Mater., 2012, 30: 73 |
| 37 | Jiang J, Bao W, Peng Z Y, et al. Experimental investigation on mechanical behaviours of TMCP high strength steel [J]. Constr. Build. Mater., 2019, 200: 664 |
| 38 | Shaheen M A, Presswood R, Afshan S. Application of machine learning to predict the mechanical properties of high strength steel at elevated temperatures based on the chemical composition [J]. Structures, 2023, 52: 17 |
| 39 | Yakel H L. Atom distribution in sigma phases. Ⅰ. Fe and Cr atom distribution in a binary sigma phase equilibrated at 1063, 1013 and 923K [J]. Acta Cryst., 1983, 39B: 20 |
| 40 | Chinese Society of Metals High Temperature Materials Branch. China Superalloys Handbook [M]. Beijing: Standards Press of China, 2012: 30 |
| 中国金属学会高温材料分会. 中国高温合金手册 [M]. 北京: 中国标准出版社, 2012: 30 |
/
| 〈 |
|
〉 |