Research paper

Biologically Inspired Xanthium-Like Spherical Texture in Superhydrophobic Ni-Co-Zn Coatings and Their Anti-Icing Performances

  • ZHOU Xiaowei ,
  • Guo Yun ,
  • JING Xueyan ,
  • WANG Yuxin
Expand
  • School of Materials Science and Engineering, Jiangsu University of Science and Technology, Zhenjiang 212003, China
ZHOU Xiaowei, associate professor, Tel: (0511)84401188, E-mail: zhouxiaowei901@just.edu.cn

Received date: 2023-02-18

  Revised date: 2023-06-02

  Online published: 2023-12-18

Supported by

National Natural Science Foundation of China(51605203);Natural Science Foundation of Jiangsu Province(BK20211344)

Abstract

Superhydrophobic surfaces are promising anti-icing solutions for industrial applications such as spacecraft wings and wind turbine fans. However, the complexity of traditional processes, poor durability, and low interfacial adhesion between the substrate and fluorocarbon polymer films restrict their widespread use. This study validates a one-step electroplating method for Ni0.12Co0.88 - x Znx (x = 0-0.36, %, mass fraction) coatings on honeycomb porous Ti surfaces, achieving super hydrophobicity without secondary modifications. SEM, XRD, and wettability tests are employed to characterize the surface features and hydrophobic properties. Optimized conditions (50 g/L Zn2+ (x = 0.24) and 5 g/L Na3Cit concentration) resulted in a compact microstructural texture and refined crystal size (300 nm), enhancing the interfacial bonding strength. The as-deposited coating exhibited hydrophobic features, with a maximum water contact angle (WCA) of 126.3° and a sliding angle (SA) of 17.5° after 14 d of natural aging. The textural evolution from Zn nanocrystals to ZnO dendrites with a multi-antenna structure was attributed to this phenomenon. Artificial aging at 100, 200, and 300 oC achieved a superhydrophobic surface in less than 7 d. The sample aged at 200 oC displayed a WCA exceeding 153.2° and an SA below 7.8° due to out-migration of the active ZnO phase and self-assembly evolution, forming xanthium-like spherical structures with nanocrystalline Ni or Co shells and multi-tentacle ZnO dendrites. Comparatively, anti-icing performances were assessed at -10 oC, showing a peach blossom ice shape on all coating samples. The sample aged at 200 oC exhibited an ice-resistant time of over 1418 s, 20 times longer than that of the porous Ti substrate, indicating excellent anti-icing performances. In summary, electroplating Ni-Co-Zn coatings onto porous Ti is a practical solution that meets the evolving requirements for superhydrophobic films in spacecraft shells for anti-icing and warship surfaces for anti-salt spray corrosion.

Cite this article

ZHOU Xiaowei , Guo Yun , JING Xueyan , WANG Yuxin . Biologically Inspired Xanthium-Like Spherical Texture in Superhydrophobic Ni-Co-Zn Coatings and Their Anti-Icing Performances[J]. Acta Metall Sin, 2025 , 61(5) : 783 -796 . DOI: 10.11900/0412.1961.2023.00066

References

1 Wang Y X, Guan L L, He Z, et al. Preparation and characterisation of AAO/Ni/Ni superhydrophobic coatings on aluminium alloys [J]. Surf. Eng., 2021, 37: 1246
2 Lian F, Zang L P, Xiang Q K, et al. Tribological performance of super hydrophobic titanium alloy surface in artificial seawater [J]. Acta Metall. Sin., 2016, 52: 592
  连 峰, 臧路苹, 项秋宽 等. 超疏水钛合金表面在人工海水中的摩擦性能 [J]. 金属学报, 2016, 52: 592
3 Kang Z X, Guo M J. Fabrication of superhydrophobic Ti surface by thermal oxidation and its anticorrosion property [J]. Acta Metall. Sin., 2013, 49: 629
  康志新, 郭明杰. 热氧化法制备超疏水Ti表面及其耐腐蚀性 [J]. 金属学报, 2013, 49: 629
4 Shibuichi S, Onda T, Satoh N, et al. Super water-repellent surfaces resulting from fractal structure [J]. J. Phys. Chem., 1996, 100: 19512
5 Zhou X, Yu S R, Zang J, et al. Colorful nanostructured TiO2 film with superhydrophobic-superhydrophilic switchable wettability and anti-fouling property [J]. J. Alloys Compd., 2019, 798: 257
6 Jiang L, Wang R, Yang B, et al. Binary cooperative complementary nanoscale interfacial materials [J]. Pure Appl. Chem., 2000, 72: 73
7 Xi W J, Qiao Z M, Zhu C L, et al. The preparation of lotus-like super-hydrophobic copper surfaces by electroplating [J]. Appl. Surf. Sci., 2009, 255: 4836
8 Wang G W, Song D, Qiao Y X, et al. Developing super-hydrophobic and corrosion-resistant coating on magnesium-lithium alloy via one-step hydrothermal processing [J]. J. Magnes. Alloy., 2023, 11: 1422
9 Shang W, Wu F, Jiang S Q, et al. Effect of hydrophobicity on the corrosion resistance of microarc oxidation/self-assembly/nickel composite coatings on magnesium alloys [J]. J. Mol. Liq., 2021, 330: 115606
10 Hashjin R R, Ranjbar Z, Yari H, et al. Tuning up sol-gel process to achieve highly durable superhydrophobic coating [J]. Surf. Interfaces, 2022, 33: 102282
11 Liu Q W, Liu G D, Li Z H, et al. Preparation and properties of superhydrophobic surface of magnesium alloy by nanosecond laser [J]. Laser Optoelectron. Prog., 2022, 59: 224
  刘祁文, 刘国东, 李子航 等. 纳秒激光制备镁合金超疏水表面及其性能研究 [J]. 激光与光电子学进展, 2022, 59: 224
12 Liu Y H, Wang Z K. Superhydrophobic porous networks for enhanced droplet shedding [J]. Sci. Rep., 2016, 6: 33817
13 She Z X, Li Q, Wang Z W, et al. Highly anticorrosion, self-cleaning superhydrophobic Ni-Co surface fabricated on AZ91D magnesium alloy [J]. Surf. Coat. Technol., 2014, 251: 7
14 Peng Y J, Li P C, Li H, et al. Theoretical and experimental study of spontaneous adsorption-induced superhydrophobic Cu coating with hierarchical structures and its anti-scaling property [J]. Surf. Coat. Technol., 2022, 441: 128557
15 Wang L, Teng C, Liu J, et al. Robust anti-icing performance of silicon wafer with hollow micro-/nano-structured ZnO [J]. J. Ind. Eng. Chem., 2018, 62: 46
16 Xue C R, Dong L H, Liu T, et al. Preparation and anticorrosion performance of superhydrophobic TiO2 nanotube arrays on pure Ti [J]. Corros. Sci. Prot. Technol., 2012, 24: 37
  薛超瑞, 董丽华, 刘 通 等. TiO2纳米阵列超疏水膜的制备及耐腐蚀性能 [J]. 腐蚀科学与防护技术, 2012, 24: 37
17 S?kmen M, Tatl?dil ?, Breen C, et al. A new nano-TiO2 immobilized biodegradable polymer with self-cleaning properties [J]. J. Hazard. Mater., 2011, 187: 199
18 Zheng J X, Liu R, Liu D D, et al. Slippery liquid infused porous surfaces with anti-icing performance fabricated by direct laser interference lithography [J]. Prog. Org. Coat., 2023, 175: 107308
19 Tian Y, Xu Y C, Zhu Z T, et al. Hierarchical micro/nano/porous structure PVDF/hydrophobic GO photothermal membrane with highly efficient anti-icing/de-icing performance [J]. Colloids Surf., 2022, 651A: 129586
20 Guo P, Zheng Y M, Wen M X, et al. Icephobic/anti-icing properties of micro/nanostructured surfaces [J]. Adv. Mater., 2012, 24: 2642
21 Bhat R S, Shet V B. Development and characterization of Zn-Ni, Zn-Co and Zn-Ni-Co coatings [J]. Surf. Eng., 2020, 36: 429
22 Kapusta-Ko?odziej J, Syrek K, Pawlik A, et al. Effects of anodizing potential and temperature on the growth of anodic TiO2 and its photoelectrochemical properties [J]. Appl. Surf. Sci., 2017, 396: 1119
23 Zhou X W, Lu Z, Jing X Y. Pinning growth of TiN films toward porous Ti matrix [J]. J. Mater. Sci, 2022, 57: 18949
24 Zhou X W, Wu F J, Ouyang C. Electroless Ni-P alloys on nanoporous ATO surface of Ti substrate [J]. J. Mater. Sci, 2018, 53: 2812
25 Abou-Krisha M M, Rageh H M, Matter E A. Electrochemical studies on the electrodeposited Zn-Ni-Co ternary alloy in different media [J]. Surf. Coat. Technol., 2008, 202: 3739
26 Kazimierczak H, Ozga P, Socha R P. Investigation of electrochemical co-deposition of zinc and molybdenum from citrate solutions [J]. Electrochim. Acta, 2013, 104: 378
27 Eliaz N, Venkatakrishna K, Hegde A C. Electroplating and characterization of Zn-Ni, Zn-Co and Zn-Ni-Co alloys [J]. Surf. Coat. Technol., 2010, 205: 1969
28 Dikici T, Culha O, Toparli M. Study of the mechanical and structural properties of Zn-Ni-Co ternary alloy electroplating [J]. J. Coat. Technol. Res., 2010, 7: 787
29 Abou-Krisha M M. Influence of Ni2+ concentration and deposition potential on the characterization of thin electrodeposited Zn-Ni-Co coatings [J]. Mater. Chem. Phys., 2011, 125: 621
30 Jiang J W, Shen Y Z, Wang Z, et al. Anti/de-icing performance of the one-step electrodeposited superhydrophobic surfaces: Role of surface polarity regulated by hydrocarbon radical length [J]. Chem. Eng. J., 2022, 431: 133276
31 Yan Y X, Wang J H, Gao J, et al. TiO2-based slippery liquid-infused porous surfaces with excellent ice-phobic performance [J]. Colloids Surf., 2022, 654A: 129994
32 Shen Y Z, Wu Y, Tao J, et al. Spraying fabrication of durable and transparent coatings for anti-icing application: Dynamic water repellency, icing delay, and ice adhesion [J]. ACS Appl. Mater. Interfaces, 2019, 11: 3590
33 Khorasani M T, Mirzadeh H, Kermani Z. Wettability of porous polydimethylsiloxane surface: Morphology study [J]. Appl. Surf. Sci., 2005, 242: 339
34 Fu Q T, Wu X H, Kumar D, et al. Development of sol-gel icephobic coatings: Effect of surface roughness and surface energy [J]. ACS Appl. Mater. Interfaces, 2014, 6: 20685
35 Wei F F, Xiang T F, Liu J, et al. Fabrication of superhydrophobic surface by combination of electrodeposition and hydrothermal synthesis and its self-cleaning and anti-icing properties [J]. Electroplat. Finish., 2022, 41: 502
  魏菲菲, 项腾飞, 刘 剑 等. 电沉积-水热法构建超疏水表面及其自清洁和防结冰性能 [J]. 电镀与涂饰, 2022, 41: 502
36 Huang Y, Sarkar D K, Chen X G. Superhydrophobic nanostructured ZnO thin films on aluminum alloy substrates by electrophoretic deposition process [J]. Appl. Surf. Sci., 2015, 327: 327
37 Zhou X W, Guo Y, Lu Z. 3D Xanthium-like of Ni-Co-Zn ternary alloys as superhydrophobic coatings toward porous Ti surface for its anti-icing performances [J]. Surf. Coat. Technol., 2023, 473: 130034
38 Wang Z H, Li Y C, Zhang G J. Fabrication of superhydrophobic Zn-Ni coatings on LA43M magnesium alloy [J]. J. Mater. Eng. Perform., 2022, 31: 5333
39 Huang L J, Huang H, Guo W, et al. 3D urchin-like of Zn-Ni-Co ternary oxide microspheres as high-performance electrodes for supercapacitors [J]. Electrochim. Acta, 2022, 434: 141317
40 Wu C, Cai J J, Zhang Q B, et al. Hierarchical mesoporous zinc-nickel-cobalt ternary oxide nanowire arrays on nickel foam as high-performance electrodes for supercapacitors [J]. ACS Appl. Mater. Interfaces, 2015, 7: 26512
41 Zhu D Y, Dai P Q, Luo X B, et al. Novel characterization of wetting properties and the calculation of liquid-solid interface tension (I) [J]. Sci. Technol. Eng., 2007, 7: 3057
  朱定一, 戴品强, 罗晓斌 等. 润湿性表征体系及液固界面张力计算的新方法(Ⅰ) [J]. 科学技术与工程, 2007, 7: 3057
Outlines

/