Research paper

Effect of Interstitial Element O on Cryogenic Mechanical Properties in β-Type Ti-15Mo Alloy

  • DAI Jincai ,
  • MIN Xiaohua ,
  • XIN Shewei ,
  • LIU Fengjin
Expand
  • 1 School of Materials Science and Engineering, Dalian University of Technology, Dalian 116024, China
    2 Northwest Institute for Non-Ferrous Metal Research, Xi'an 710016, China
MIN Xiaohua, professor, Tel: (0411)84708189, E-mail: minxiaohua@dlut.edu.cn

Received date: 2023-06-25

  Revised date: 2023-11-03

  Online published: 2023-11-27

Supported by

National Nature Science Foundation of China(52071051)

Abstract

Ti and titanium alloys are preferred for cryogenic applications, particularly at a liquid hydrogen temperature of 20 K, in aerospace due to their high specific strength, good corrosion resistance, low magnetic permeability, and low thermal expansion coefficient. Currently, the most common cryogenic titanium alloys are extra-low interstitial α-type and near α-type alloys. However, they exhibit inadequate age hardening and low cold-forming ability. Furthermore, they do not meet the enhanced strength-ductility requirements for cryogenic structural components. Metastable β-type titanium alloys with a {332}<113> twinning-induced plasticity (TWIP) effect have shown enhanced mechanical properties, such as a favorable balance of strength-ductility at ambient and cryogenic temperatures. Therefore, they are considered promising titanium alloy candidates for cryogenic applications. The content of interstitial elements, particularly the O content, has a substantial impact on the cryogenic ductility of titanium alloys. Therefore, all cryogenic titanium alloys have extremely rigorous requirements regarding the O content. However, the effect of O content on the cryogenic tensile behavior of {332}<113> TWIP alloys remains unclear. This study investigated the cryogenic tensile behavior of Ti-15Mo alloy with O contents of 0.2% and 0.4% (mass fraction, the same below) at 20 K. The tests were conducted using HRTEM, FIB, EBSD, SEM, OM, and a tensile testing machine fitted with a cryogenic system. Results show that the alloy comprising 0.2%O content (0.2O alloy) exhibits a good combination of tensile strength (1825 MPa) and elongation (7.5%). This alloy displays typical microvoid coalescence fracture characteristics. Alternatively, the alloy with 0.4%O content (0.4O alloy) presents a high tensile strength of 1973 MPa, a relatively low elongation of 1.5%, and typical cleavage fracture characteristics. The discrepancy in cryogenic tensile properties between the two alloys can be attributed to the effect of O content on the formation of {332}<113> twins. Several {332}<113> twins appear in the 0.2O alloy, whereas only a small number of twins are observed near the fracture region in the 0.4O alloy. The exceptional strength of the 0.2O alloy is attributed to the enhanced critically resolved shear stress of twinning, while the impressive elongation is attributed to the formation of numerous twins that impede local plastic deformation. The 0.2O alloy exhibits a noticeably serrated tensile curve and multiple necking. The activation of twins in the necking region hinders local plastic deformation and necking, thus enhancing the strength-ductility combination. Hence, by effectively using the interstitial element O, the cryogenic mechanical properties of metastable β-type titanium alloys can be effectively tailored as per requirements.

Cite this article

DAI Jincai , MIN Xiaohua , XIN Shewei , LIU Fengjin . Effect of Interstitial Element O on Cryogenic Mechanical Properties in β-Type Ti-15Mo Alloy[J]. Acta Metall Sin, 2025 , 61(2) : 243 -252 . DOI: 10.11900/0412.1961.2023.00268

References

1 Xu A J, Wan H F, Liang C Z, et al. Application status and development trend of cryogenic titanium alloy [J]. J. Netshape Form. Eng., 2020, 12(6): 145
  许爱军, 万海峰, 梁春祖 等. 低温钛合金材料应用现状及发展趋势 [J]. 精密成形工程, 2020, 12(6): 145
2 Huang C W, Ge P, Zhao Y Q, et al. Research progress in titanium alloys at cryogenic temperatures [J]. Rare Met. Mater. Eng., 2016, 45: 254
  黄朝文, 葛 鹏, 赵永庆 等. 低温钛合金的研究进展 [J]. 稀有金属材料与工程, 2016, 45: 254
3 Osamu U. Review of the mechanical properties of high-strength alloys at cryogenic temperatures [J]. Mater. Perform. Charact., 2021, 10: 3
4 Yu Y, Jiang P, Li S K. Recent advances in the development and application of cryogenic titanium alloys [J]. Dev. Appl. Mater., 2014, 29(6): 118
  郁 炎, 蒋 鹏, 李士凯. 国内外低温钛合金的开发与应用现状 [J]. 材料开发与应用, 2014, 29(6): 118
5 Leyens C, Peters M. Titanium and titanium alloys [M]. Weinheim: Wiley-VCH Verlag GmbH & Co. KGaA, 2003: 36
6 Lei L, Zhao Q Y, Zhu Q W, et al. Twinning-induced high impact toughness of titanium alloy at cryogenic temperature [J]. Mater. Sci. Eng., 2022, A860: 144258
7 Lu Z C, Zhang X H, Ji W, et al. Investigation on the deformation mechanism of Ti-5Al-2.5Sn ELI titanium alloy at cryogenic and room temperatures [J]. Mater. Sci. Eng., 2021, A818: 141380
8 Nayan N, Singh G, Prabhu T A, et al. Cryogenic mechanical properties of warm multi-pass caliber-rolled fine-grained titanium alloys: Ti-6Al-4V (normal and ELI grades) and VT14 [J]. Metall. Mater. Trans., 2018, 49A: 128
9 Singh G, Bajargan G, Datta R, et al. Deformation and strength of Ti-6Al-4V alloyed with B at cryogenic temperatures [J]. Mater. Sci. Eng., 2014, A611: 45
10 Lu Z C, Sun Y C, Yao C G, et al. Microstructure and mechanical properties of novel Ti-Al-V-Zr-Mo-Nb cryogenic titanium alloy [J]. Rare Met. Mater. Eng., 2022, 51: 217
  陆子川, 孙亚超, 姚草根 等. 一种新型Ti-Al-V-Zr-Mo-Nb低温钛合金组织与性能研究 [J]. 稀有金属材料与工程, 2022, 51: 217
11 Zang M C, Niu H Z, Zhang H R, et al. Cryogenic tensile properties and deformation behavior of a superhigh strength metastable beta titanium alloy Ti-15Mo-2Al [J]. Mater. Sci. Eng., 2021, A817: 141344
12 Xiang L, Min X H, Mi G B. Application and research progress of body-centered-cubic Ti-Mo base alloys [J]. J. Mater. Eng., 2017, 45(7): 128
  向 力, 闵小华, 弭光宝. 体心立方Ti-Mo基钛合金应用研究进展 [J]. 材料工程, 2017, 45(7): 128
13 Zhang S J, Min X H, Li Y D, et al. Effects of deformation and phase transformation microstructures on springback behavior and biocompatibility in β-Type Ti-15Mo alloy [J]. Acta Metall. Sin. (Engl. Lett.), 2022, 35: 621
14 Dai J C, Min X H, Zhou K S, et al. Coupling effect of pre-strain combined with isothermal ageing on mechanical properties in a multilayered Ti-10Mo-1Fe/3Fe alloy [J]. Acta Metall. Sin., 2021, 57: 767
  戴进财, 闵小华, 周克松 等. 预变形与等温时效耦合作用下Ti-10Mo-1Fe/3Fe层状合金的力学性能 [J]. 金属学报, 2021, 57: 767
15 Yao K, Xin S W, Yang Y, et al. Ultrahigh cryogenic strength and exceptional ductility at 20 K in a TWIP Ti-15Mo alloy [J]. Scr. Mater., 2022, 213: 114595
16 Chong Y, Poschmann M, Zhang R P, et al. Mechanistic basis of oxygen sensitivity in titanium [J]. Sci. Adv., 2020, 6: 4060
17 Wasz M L, Brotzen F R, Mclellan R B, et al. Effect of oxygen and hydrogen on mechanical properties of commercial purity titanium [J]. Int. Mater. Rev., 1996, 41: 1
18 Min X H, Emura S, Tsuchiya K, et al. Transition of multi-deformation modes in Ti-10Mo alloy with oxygen addition [J]. Mater. Sci. Eng., 2014, A590: 88
19 Min X H, Bai P F, Emura S, et al. Effect of oxygen content on deformation mode and corrosion behavior in β-type Ti-Mo alloy [J]. Mater. Sci. Eng., 2017, A684: 534
20 Kim J I, Kim H Y, Hosoda H, et al. Shape memory behavior of Ti-22Nb-(0.5-2.0)O (at%) biomedical alloys [J]. Mater. Trans., 2005, 46: 852
21 Min X H, Xiang L, Li M J, et al. Effect of {332}<113> twins combined with isothermal ω-phase on mechanical properties in Ti-15Mo alloy with different oxygen contents [J]. Acta Metall. Sin., 2018, 54: 1262
  闵小华, 向 力, 李明佳 等. {332}<113>孪晶与等温ω相的组合对不同O含量Ti-15Mo合金力学性能的影响 [J]. 金属学报, 2018, 54: 1262
22 Yao K, Min X H. Abnormal strain rate strengthening and strain hardening with constitutive modeling in body-centered cubic {332}<113> TWIP titanium alloy [J]. Acta Mater., 2022, 226: 117641
23 Li M J, Min X H, Yao K, et al. Novel insight into the formation of α″-martensite and ω-phase with cluster structure in metastable Ti-Mo alloys [J]. Acta Mater., 2019, 164: 322
24 Wang K G, Deng Z X, Tian Y Y, et al. Effect of cold rolling and solution treatment on β stability and mechanical properties of a metastable β-Ti alloy [J]. Mater. Sci. Eng., 2022, A861: 144366
25 Yao K, Min X H, Emura S, et al. Coupling effect of deformation mode and temperature on tensile properties in TWIP type Ti-Mo alloy [J]. Mater. Sci. Eng., 2019, A766: 138363
26 Qu L, Yang Y, Lu Y F, et al. A detwinning process of {332}<113> twins in beta titanium alloys [J]. Scr. Mater., 2013, 69: 389
27 Gutierrez-Urrutia I, Li C L, Emura S, et al. Study of {332}<113> twinning in a multilayered Ti-10Mo-xFe (x = 1-3) alloy by ECCI and EBSD [J]. Sci. Technol. Adv. Mater., 2016, 17: 220
28 Boyer R, Collings E W, Welsch G. Materials Properties Handbook: Titanium Alloys [M]. Materials Park: ASM International, 1994: 68
29 Zang M C, Niu H Z, Liu S, et al. Achieving highly promising strength-ductility synergy of powder bed fusion additively manufactured titanium alloy components at ultra-low temperatures [J]. Addit. Manuf., 2023, 65: 103444
30 Antony Prabhu T, Murugesan N, Thomas Tharian K, et al. Studies on mechanical properties of Ti-6Al-4V ELI at liquid hydrogen temperature [J]. Mater. Sci. Forum, 2015, 830-831: 207
31 Di iorio S, Briottet L, Rauch E F, et al. Plastic deformation, damage and rupture of PM Ti-6Al-4V at 20 K under monotonic loading [J]. Acta Mater., 2007, 55: 105
32 Hanada S, Izumi O. Transmission electron microscopic observations of mechanical twinning in metastable beta titanium alloys [J]. Metall. Trans., 1986, 17A: 1409
Outlines

/