Research paper

Simulation of Core-Shell Structure Evolution of Cu-Co Immiscible Alloys

  • WANG Lin ,
  • WEI Chen ,
  • WANG Lei ,
  • WANG Jun ,
  • LI Jinshan
Expand
  • 1.State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072, China
    2.School of Materials Science and Engineering, Xi'an University of Technology, Xi'an 710048, China
WANG Jun, professor, Tel: (029)88460568, E-mail: nwpuwj@nwpu.edu.cn

Received date: 2023-03-03

  Revised date: 2023-04-10

  Online published: 2023-09-28

Supported by

National Natural Science Foundation of China(52174375);Innovation Capability Support Program of Shaanxi(2020KJXX-073);Independent Project of State Key Laboratory of Solidification Processing(2023-TS-13)

Abstract

Cu-Co alloys demonstrate immense potential for industrial applications due to their excellent properties, including high electrical conductivity and giant magnetoresistance effect. As typical immiscible alloys, Cu-Co alloys are prone to liquid-phase separation during their preparation; as a result, their components undergo severe segregation, limiting their applicability. Thus, investigating and elucidating the evolution mechanism of solidification structures of the Cu-Co alloys is imperative. However, liquid-phase separation in these alloys occurs on miniscule time and space scales, and complex physical processes such as diffusion, convection, and heat transfer are also involved. Hence, investigating the kinetic characteristics of alloy solidification and the mechanisms of microstructure formation solely by experimental methods using the existing technology is challenging. Nevertheless, with the continuous advancement of theoretical foundations and computational capabilities of materials, numerical simulations have emerged as an effective tool for investigating the microstructure evolution of immiscible alloys. This study investigates the mechanisms involved in the formation of core-shell structures during the solidification of Cu-Co alloys using a combination of experimental and numerical simulation techniques. Based on the phase-field method, three parallel simulations, incorporating fluid flow and Marangoni motion, were conducted. The microstructure evolution at various stages and under different conditions was systematically analyzed. The simulation results indicated that the fluid flow resulting from liquid-phase separation could expedite the coarsening of the second-phase droplets. Furthermore, Marangoni motion driven by temperature gradients resulted in the coalescence of second-phase droplets at the center (high temperatures), accelerating the coarsening process. The Ostwald ripening phenomenon and coagulation process between the second-phase droplets were simulated, and the growth kinetic mechanisms of the second phase were revealed. In addition, three Cu-Co alloys were used for simulations to investigate the impact of the volume fraction of Co-rich phase on the microstructure evolution. The validity of the simulation results was confirmed by comparing the simulated solidification structures with those obtained experimentally.

Cite this article

WANG Lin , WEI Chen , WANG Lei , WANG Jun , LI Jinshan . Simulation of Core-Shell Structure Evolution of Cu-Co Immiscible Alloys[J]. Acta Metall Sin, 2024 , 60(9) : 1239 -1249 . DOI: 10.11900/0412.1961.2023.00089

References

1 Wei C, Wang J, He Y X, et al. Liquid-liquid phase separation in immiscible Cu-Co alloy [J]. Mater. Lett., 2020, 268: 127585
2 Sun Z B, Song X P, Hu Z D, et al. Liquid separating behavior of Cu-Co alloys under deep supercooling [J]. Chin. J. Nonferrous Met., 2001, 11: 68
  孙占波, 宋晓平, 胡柱东 等. 深过冷条件下Cu-Co合金的液相分解 [J]. 中国有色金属学报, 2001, 11: 68
3 Hu Y, Cao W M, Yin R H, et al. Study of giant magnetoresistence of Co/Cu multilayers prepared by electrochemical deposition [J]. J. Funct. Mater., 2005, 36: 187
  胡 滢, 曹为民, 印仁和 等. Co/Cu纳米多层膜的制备及巨磁阻性能的研究 [J]. 功能材料, 2005, 36: 187
4 Yan Y J, Wei C, He Y X, et al. Effect of high magnetic field on solidification microstructure evolution of a Cu-Fe immiscible alloy [J]. China Foundry, 2022, 19: 335
5 Wei C, Li J S, Yan Y J, et al. Effect of high magnetic field on the microstructure evolution behavior of undercooled Cu-Co alloy [J]. Foundry Technol., 2022, 43: 180
  魏 晨, 李金山, 闫育洁 等. 强磁场对过冷Cu-Co合金组织演化行为的影响 [J]. 铸造技术, 2022, 43: 180
6 Jiang H X, Sun X J, Li S X, et al. Continuous solidification of Al-Bi immiscible alloys under the direct current [J]. Spec. Cast. Nonferrous Alloys, 2020, 40: 1045
  江鸿翔, 孙小钧, 李世欣 等. 直流电流作用下Al-Bi偏晶合金连续凝固研究 [J]. 特种铸造及有色合金, 2020, 40: 1045
7 Kolbe M, Cao C D, Lu X Y, et al. Solidification behaviour of undercooled Co-Cu alloys showing a metastable miscibility gap [J]. Mater. Sci. Eng., 2004, A375-377: 520
8 Mullis A M, Jegede O E, Bigg T D, et al. Dynamics of core-shell particle formation in drop-tube processed metastable monotectic alloys [J]. Acta Mater., 2020, 188: 591
9 Liu S C, Jie J C, Guo Z K, et al. Solidification microstructure evolution and its corresponding mechanism of metastable immiscible Cu80Fe20 alloy with different cooling conditions [J]. J. Alloys Compd., 2018, 742: 99
10 Shoji E, Isogai S, Suzuki R, et al. Neutron computed tomography of phase separation structures in solidified Cu-Co alloys and investigation of relationship between the structures and melt convection during solidification [J]. Scr. Mater., 2020, 175: 29
11 Anders D, Weinberg K. Numerical simulation of diffusion induced phase separation and coarsening in binary alloys [J]. Comput. Mater. Sci., 2011, 50: 1359
12 Bhattacharyya S, Abinandanan T A. A study of phase separation in ternary alloys [J]. Bull. Mater. Sci., 2003, 26: 193
13 Braga M H, Oliveira J C R E, Malheiros L F, et al. Phase field simulations in miscibility gaps [J]. Calphad, 2009, 33: 237
14 Hedstr?m P, Baghsheikhi S, Liu P, et al. A phase-field and electron microscopy study of phase separation in Fe-Cr alloys [J]. Mater. Sci. Eng., 2012, A534: 552
15 Kuwajima T, Saito Y, Suwa Y. Kinetics of phase separation in iron-based ternary alloys. II. Numerical simulation of phase separation in Fe-Cr-X (X = Mo, Cu) ternary alloys [J]. Intermetallics, 2003, 11: 1279
16 Guo C, Zhao Y P, Deng Y Y, et al. A phase-field study on interaction process of moving grain boundary and spinodal decomposition [J]. Acta Phys. Sin., 2022, 71(7): 078101
  郭 灿, 赵玉平, 邓英远 等. 运动晶界与调幅分解相互作用过程的相场法研究 [J]. 物理学报, 2022, 71(7): 078101
17 Guo C, Zhang Y C, Gao Y, et al. Atomic scale investigation of nucleation process by the phase field crystal model [J]. Foundry Technol., 2022, 43: 103
  郭 灿, 张一弛, 高 莹 等. 原子尺度形核过程的晶体相场法研究 [J]. 铸造技术, 2022, 43: 103
18 Qin T, Wang H P, Wei B B. Simulated evolution process of core-shell microstructures [J]. Sci. China, 2007, 50G: 546
19 Shi R P, Wang Y, Wang C P, et al. Self-organization of core-shell and core-shell-corona structures in small liquid droplets [J]. Appl. Phys. Lett., 2011, 98: 204106
20 Wang W L, Wu Y H, Li L H, et al. Homogeneous granular microstructures developed by phase separation and rapid solidification of liquid Fe-Sn immiscible alloy [J]. J. Alloys Compd., 2017, 693: 650
21 Cahn J W. On spinodal decomposition [J]. Acta Metall., 1961, 9: 795
22 Sun M M, Tian C Y, Mao L Y, et al. Reconfigurable magnetic slime robot: Deformation, adaptability, and multifunction [J]. Adv. Funct. Mater., 2022, 32: 2112508
23 Li X, Qiao Z H, Zhang H. A second-order convex splitting scheme for a Cahn-Hilliard equation with variable interfacial parameters [J]. J. Comput. Math., 2017, 35: 693
24 Maurits N M, Zvelindovsky A V, Sevink G J A, et al. Hydrodynamic effects in three-dimensional microphase separation of block copolymers: Dynamic mean-field density functional approach [J]. J. Chem. Phys., 1998, 108: 9150
25 Mauri R, Shinnar R, Triantafyllou G. Spinodal decomposition in binary mixtures [J]. Phys. Rev., 1996, 53E: 2613
26 Li J S, Wei C, Wang J, et al. A method for obtaining core-shell structure of immiscible alloy [P]. Chin Pat, 202310044747.6, 2023
  李金山, 魏 晨, 王 军 等. 一种难混溶合金获得核壳结构的方法 [P]. 中国专利, 202310044747.6, 2023)
Outlines

/