Research paper

Stress Corrosion Behavior of Ni-Cr-Mo-V Steel in 3.5%NaCl Solution Under the Interaction of Hydrostatic Pressure and Tensile Stress

  • SONG Yushan ,
  • LIU Rui ,
  • CUI Yu ,
  • LIU Li ,
  • WANG Fuhui
Expand
  • 1 Shenyang National Laboratory for Materials Science, Northeastern University, Shenyang 110819, China
    2 Shi -changxu Innovation Center for Advanced Materials, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
LIU Rui, associate professor, Tel: 18842505442, E-mail: liurui@mail.neu.edu.cn
LIU Li, professor, Tel: 15904072057, E-mail: liuli@mail.neu.edu.cn

Received date: 2023-03-02

  Revised date: 2023-04-05

  Online published: 2023-09-18

Supported by

National Key Research and Development Program of China(2022YFB3808800);China Postdoctoral Science Foundation(2021M700711);National Natural Science Foundation of China

Abstract

With the promotion of the deep-sea strategy of China, the safety of metallic structural materials in deep sea is considered critical for development of deep-sea engineering equipment. High-strength low-alloy (HSLA) steel is widely used in pressure hulls of deep-sea submarines and oil platforms. However, HSLA steel is affected by the complex mechanical environment during its long-term service in the deep sea, leading to severe corrosion failure. Therefore, research on the effects of the hydrostatic pressure and tensile stress in deep sea on the stress corrosion behavior of HSLA steel is beneficial for the development, application, and lifetime prediction of deep-sea engineering equipment. Here, experiments were conducted using Ni-Cr-Mo-V steel, and the electrochemical measurement system and slow strain rate tensile (SSRT) test system in a simulated deep-sea environment were established in laboratory. The electric double-layer structure at the metal-solution interface was investigated using the differential capacitance curve, and the corrosion current density of the alloy was characterized with the linear polarization curve. The morphology of pits at local corrosion sites and fracture after the SSRT test were observed through SEM, and the size of the pits was analyzed using white-light interferometry. The stress corrosion cracking (SCC) sensitivity of the alloy was studied utilizing the SSRT test. The effects of the hydrostatic pressure and deformation on the concentration of H+ near the alloy surface were determined via the hydrolysis of metal cations. The results illustrated that the hydrostatic pressure can improve the SCC susceptibility of Ni-Cr-Mo-V steel in 3.5%NaCl solution, which can be affected by the dual effects of the interaction of the hydrostatic pressure and tensile stress on the local corrosion behavior. On the one hand, the interaction of the tensile stress and hydrostatic pressure affects the expansion and structure of pits and suppresses the adhesion of corrosion products to the alloy surface. On the other hand, the hydrostatic pressure and tensile stress affect the electric double layer at the metal-solution interface and subsequently promote the hydrolysis of metal cations, increasing the H+ concentration near the alloy surface. Additionally, the fracture mode of Ni-Cr-Mo-V steel in 3.5%NaCl solution is independent of the hydrostatic pressure; however, the hydrostatic pressure determines the shallow and small structure of the dimples in the fracture.

Cite this article

SONG Yushan , LIU Rui , CUI Yu , LIU Li , WANG Fuhui . Stress Corrosion Behavior of Ni-Cr-Mo-V Steel in 3.5%NaCl Solution Under the Interaction of Hydrostatic Pressure and Tensile Stress[J]. Acta Metall Sin, 2025 , 61(2) : 309 -322 . DOI: 10.11900/0412.1961.2023.00087

References

1 Hu S B, Yuan X W, Liu L, et al. Influence of hydrostatic pressure on the corrosion and discharging behavior of Al-Zn-In-Mg-Ti alloy [J]. J. Alloys Compd., 2023, 936: 168197
2 Liu R, Liu L, Wang F H. The role of hydrostatic pressure on the metal corrosion in simulated deep-sea environments—A review [J]. J. Mater. Sci. Technol., 2022, 112: 230
3 Liu R, Song Y S, Cui Y, et al. Corrosion of high-strength steel in 3.5%NaCl solution under hydrostatic pressure: Understanding electrochemical corrosion with tensile stress coupling [J]. Corros. Sci., 2023, 219: 111204
4 Song Y S, Liu R, Cui Y, et al. Corrosion of high-strength steel in 3.5% NaCl solution under hydrostatic pressure: Initial corrosion with tensile stress coupling [J]. Corros. Sci., 2023, 219: 111229
5 Song L F, Liu Z Y, Hu J P, et al. Stress corrosion cracking of 2205 duplex stainless steel with simulated welding microstructures in simulated sea environment at different depths [J]. J. Mater. Eng. Perform., 2020, 29: 5476
6 Hu S B, Liu R, Liu L, et al. Influence of temperature and hydrostatic pressure on the galvanic corrosion between 90/10 Cu-Ni and AISI 316L stainless steel [J]. J. Mater. Res. Technol., 2021, 13: 1402
7 Liu R, Cui Y, Liu L, et al. Study on the mechanism of hydrostatic pressure promoting electrochemical corrosion of pure iron in 3.5% NaCl solution [J]. Acta Mater., 2021, 203: 116467
8 Hu S B, Liu R, Liu L, et al. Effect of hydrostatic pressure on the galvanic corrosion of 90/10 Cu-Ni alloy coupled to Ti6Al4V alloy [J]. Corros. Sci., 2020, 163: 108242
9 Ma H Y, Liu R, Ke P L, et al. Effect of hydrostatic pressure on the pitting corrosion of 17-4PH martensitic stainless steel [J]. Eng. Fail. Anal., 2022, 138: 106367
10 Zhang T, Yang Y G, Shao Y W, et al. A stochastic analysis of the effect of hydrostatic pressure on the pit corrosion of Fe-20Cr alloy [J]. Electrochim. Acta, 2009, 54: 3915
11 Yang Y G, Zhang T, Shao Y W, et al. Effect of hydrostatic pressure on the corrosion behaviour of Ni-Cr-Mo-V high strength steel [J]. Corros. Sci., 2010, 52: 2697
12 Liu R, Cui Y, Liu L, et al. A primary study of the effect of hydrostatic pressure on stress corrosion cracking of Ti-6Al-4V alloy in 3.5% NaCl solution [J]. Corros. Sci., 2020, 165: 108402
13 Yang Z X, Kan B, Li J X, et al. Hydrostatic pressure effects on stress corrosion cracking of X70 pipeline steel in a simulated deep-sea environment [J]. Int. J. Hydrogen Energy, 2017, 42: 27446
14 Hao W K, Liu Z Y, Wang X Z, et al. Present situation and prospect of studies on high strength steel and corrosion resistance in naval ship and submarine [J]. Equip. Environ. Eng., 2014, 11(1): 54
  郝文魁, 刘智勇, 王显宗 等. 舰艇用高强钢强度及其耐蚀性现状及发展趋势 [J]. 装备环境工程, 2014, 11(1): 54
15 Hao W K, Liu Z Y, Wang X Z, et al. Current situation and prospect of studies on strength and corrosion resistance of high strength steel for ocean platform [J]. Equip. Environ. Eng., 2014, 11(2): 50
  郝文魁, 刘智勇, 王显宗 等. 海洋平台用高强钢强度及其耐蚀性现状及发展趋势 [J]. 装备环境工程, 2014, 11(2): 50
16 Liu B, Zhang T, Shao Y W, et al. Effect of hydrostatic pressure on the corrosion behavior of pure nickel [J]. Int. J. Electrochem. Sci., 2012, 7: 1864
17 Xiong X L, Tao X, Zhou Q J, et al. Hydrostatic pressure effects on hydrogen permeation in A514 steel during galvanostatic hydrogen charging [J]. Corros. Sci., 2016, 112: 86
18 Xiong X L, Ma H X, Tao X, et al. Hydrostatic pressure effects on the kinetic parameters of hydrogen evolution and permeation in Armco iron [J]. Electrochim. Acta, 2017, 255: 230
19 Gutman E M. Thermodynamics of the mechanico-chemical effect: I. Derivation of basic equations. Nature of the effect [J]. Sov. Mater. Sci., 1968, 3: 190
20 Gutman E M. Thermodynamics of the mechanico-chemical effect: II. The range of operation of nonlinear laws [J]. Sov. Mater. Sci., 1967, 3: 293
21 Kan B, Wu W J, Yang Z X, et al. Stress-induced hydrogen redistribution and corresponding fracture behavior of Q960E steel at different hydrogen content [J]. Mater. Sci. Eng., 2020, A775: 138963
22 Lin B, Hu R G, Ye C Q, et al. A study on the initiation of pitting corrosion in carbon steel in chloride-containing media using scanning electrochemical probes [J]. Electrochim. Acta, 2010, 55: 6542
23 Liu C, Li X, Revilla R I, et al. Towards a better understanding of localised corrosion induced by typical non-metallic inclusions in low-alloy steels [J]. Corros. Sci., 2021, 179: 109150
24 Wei J, Dong J H, Ke W, et al. Influence of inclusions on early corrosion development of ultra-low carbon bainitic steel in NaCl solution [J]. Corrosion, 2015, 71: 1467
25 Wang L W, Xin J C, Cheng L J, et al. Influence of inclusions on initiation of pitting corrosion and stress corrosion cracking of X70 steel in near-neutral pH environment [J]. Corros. Sci., 2019, 147: 108
26 Wang L W, Liu Z Y, Cui Z Y, et al. In situ corrosion characterization of simulated weld heat affected zone on API X80 pipeline steel [J]. Corros. Sci., 2014, 85: 401
27 Liu Z Y, Li X G, Cheng Y F. In-situ characterization of the electrochemistry of grain and grain boundary of an X70 steel in a near-neutral pH solution [J]. Electrochem. Commun., 2010, 12: 936
28 Atrens A, Wang J Q, Stiller K, et al. Atom probe field ion microscope measurements of carbon segregation at an α:α grain boundary and service failures by intergranular stress corrosion cracking [J]. Corros. Sci., 2006, 48: 79
29 Zhao Y, Zhou E Z, Liu Y Z, et al. Comparison of different electrochemical techniques for continuous monitoring of the microbiologically influenced corrosion of 2205 duplex stainless steel by marine Pseudomonas aeruginosa biofilm [J]. Corros. Sci., 2017, 126: 142
30 Runci A, Provis J L, Serdar M. Revealing corrosion parameters of steel in alkali-activated materials [J]. Corros. Sci., 2023, 210: 110849
31 Sun H J, Liu L, Li Y, et al. Effect of hydrostatic pressure on the corrosion behavior of a low alloy steel [J]. J. Electrochem. Soc., 2013, 160: C89
32 Zhao Y, Zhang T, Xiong H, et al. Bridge for the thermodynamics and kinetics of electrochemical corrosion: Modeling on dissolution, ionization, diffusion and deposition in metal/solution interface [J]. Corros. Sci., 2021, 191: 109763
33 Venezuela J, Zhou Q J, Liu Q L, et al. The influence of microstructure on the hydrogen embrittlement susceptibility of martensitic advanced high strength steels [J]. Mater. Today Commun., 2018, 17: 1
34 Dwivedi S K, Vishwakarma M. Effect of hydrogen in advanced high strength steel materials [J]. Int. J. Hydrogen Energy, 2019, 44: 28007
35 Lynch S P. Environmentally assisted cracking: Overview of evidence for an adsorption-induced localised-slip process [J]. Acta Metall., 1988, 36: 2639
36 Shi R J, Ma Y, Wang Z D, et al. Atomic-scale investigation of deep hydrogen trapping in NbC/α-Fe semi-coherent interfaces [J]. Acta Mater., 2020, 200: 686
37 Takahashi J, Kawakami K, Kobayashi Y. Origin of hydrogen trapping site in vanadium carbide precipitation strengthening steel [J]. Acta Mater., 2018, 153: 193
38 Nagao A, Martin M L, Dadfarnia M, et al. The effect of nanosized (Ti, Mo)C precipitates on hydrogen embrittlement of tempered lath martensitic steel [J]. Acta Mater., 2014, 74: 244
Outlines

/