Research paper

Mechanical Alloying Fabrication of Nano-ZrB2-Reinforced CoNiCrAlY Composite Powders and Microstructure-Property Characterization of the Resultant Coatings

  • YANG Kang ,
  • XIN Yue ,
  • JIANG Zitao ,
  • LIU Xia ,
  • XUE Zhaolu ,
  • ZHANG Shihong
Expand
  • Key Laboratory of Green Fabrication and Surface Technology of Advanced Metal Materials, Ministry of Education, Anhui University of Technology, Ma'anshan 243002, China
ZHANG Shihong, professor, Tel: (0555)2315291, E-mail: shzhang@ahut.edu.cn

Received date: 2023-04-21

  Revised date: 2023-05-24

  Online published: 2023-08-30

Supported by

National Natural Science Foundation of China(U22A20110);Outstanding Youth Fund of Anhui Province(2108085J22)

Abstract

High-temperature furnace rolls are subjected to extreme conditions, including high temperatures and heavy loads, rendering them susceptible to oxidation, wear, and other forms of failure. To address these issues, this study investigates the preparation and properties of CoNiCrAlY-ZrB2 composite powders and coatings. CoNiCrAlY serves as the metal matrix, and ZrB2 acts as the ceramic reinforcement phase. Two variants of CoNiCrAlY-20%ZrB2 (mass fraction) composite powders were fabricated using one-step and step-fashion mechanical alloying (MA) techniques (marked by MA-1 and MA-2, respectively). The microstructure and phase composition of the coatings were studied using SEM, XRD, and TEM. Mechanical properties were also investigated. High-temperature friction and wear tests were conducted at 550-950 oC. Results indicate that the particle size of the composite powder decreases with increasing MA time. Step-fashion MA successfully produced ZrB2-reinforced CoNiCrAlY composite powder, with ZrB2 particles evenly distributed throughout the CoNiCrAlY matrix. When alloyed for 35 h, the average particle size (D50 = 38.6 μm) met the specifications for high-velocity oxygen-fuel (HVOF) spraying. CoNiCrAlY-20%ZrB2 composite coatings were then prepared via HVOF spraying. Coatings derived from MA-2 powders exhibited higher melting states, denser microstructures, and lower porosity (0.28%) compared to those made with MA-1 powders. These coatings also displayed superior hardness (738 HV0.3) and fracture toughness (5.21 MPa·m1/2). High-temperature wear resistance was tested for both MA-1 and MA-2 composite coatings. At 950 oC, a protective glazing layer of Al2O3, Cr2O3, and CoCr2O4 was formed on the surface of the composite coatings. The coatings demonstrated effective self-lubrication at 750 oC due to the formation of the “glazing layer”. Above 750 oC, the MA-2 composite coating outperformed the one-step coating in wear resistance. Specifically, at 950 oC, the wear rate of the MA-2 composite coating was 1.71 × 10-14 m3·N-1·m-1, considerably lower than that of the MA-1 composite coating (4.28 × 10-14 m3·N-1·m-1). In conclusion, the addition of ZrB2 nanoparticles to the CoNiCrAlY coating considerably enhanced its friction and wear properties at high temperatures. The step-fashion mechanical alloying method demonstrated superior coating density, hardness, and high-temperature wear resistance.

Cite this article

YANG Kang , XIN Yue , JIANG Zitao , LIU Xia , XUE Zhaolu , ZHANG Shihong . Mechanical Alloying Fabrication of Nano-ZrB2-Reinforced CoNiCrAlY Composite Powders and Microstructure-Property Characterization of the Resultant Coatings[J]. Acta Metall Sin, 2025 , 61(4) : 619 -631 . DOI: 10.11900/0412.1961.2023.00177

References

1 Matthews S, James B. Review of thermal spray coating applications in the steel industry: Part 1—Hardware in steel making to the continuous annealing process [J]. J. Therm. Spray Technol., 2010, 19: 1267
2 Bolelli G, Candeli A, Lusvarghi L, et al. Tribology of NiCrAlY + Al2O3 composite coatings by plasma spraying with hybrid feeding of dry powder + suspension [J]. Wear, 2015, 344-345: 69
3 Hou G L, An Y L, Zhao X Q, et al. Effect of alumina dispersion on oxidation behavior as well as friction and wear behavior of HVOF-sprayed CoCrAlYTaCSi coating at elevated temperature up to 1000 oC [J]. Acta Mater., 2015, 95: 164
4 Taylor T A, Bettridge D F. Development of alloyed and dispersion-strengthened MCrAlY coatings [J]. Surf. Coat. Technol., 1996, 86-87: 9
5 Zhao L D, Parco M, Lugscheider E. Wear behaviour of Al2O3 dispersion strengthened MCrAlY coating [J]. Surf. Coat. Technol., 2004, 184: 298
6 Taha M A, Youness R A, Zawrah M F. Review on nanocomposites fabricated by mechanical alloying [J]. Int. J. Miner. Metall. Mater., 2019, 26: 1047
7 Suryanarayana C, Al-Joubori A A, Wang Z. Nanostructured materials and nanocomposites by mechanical alloying: An overview [J]. Met. Mater. Int., 2022, 28: 41
8 Liu C J, Sun W Y, Chen M H, et al. High-temperature oxidation behavior of spark plasma sintered Ni20Cr-xAl alloys [J]. Acta Metall. Sin., 2024, 60: 485
  刘丞济, 孙文瑶, 陈明辉 等. 放电等离子烧结Ni20Cr-xAl合金的高温氧化行为 [J]. 金属学报, 2024, 60: 485
9 Bi S, Li Z C, Sun H X, et al. Microstructure and mechanical properties of carbon nanotubes-reinforced 7055Al composites fabricated by high-energy ball milling and powder metallurgy processing [J]. Acta Metall. Sin., 2021, 57: 71
  毕 胜, 李泽琛, 孙海霞 等. 高能球磨结合粉末冶金法制备碳纳米管增强7055Al复合材料的微观组织和力学性能[J]. 金属学报, 2021, 57: 71
10 Niespodziana K, Jurczyk K, Jakubowicz J, et al. Fabrication and properties of titanium-hydroxyapatite nanocomposites [J]. Mater. Chem. Phys., 2010, 123: 160
11 Cen S B, Chen H, Liu Y, et al. Effect of CeO2 on corrosion behavior of WC-12Co coatings by high velocity oxygen fuel [J]. Acta Metall. Sin., 2016, 52: 1441
  岑升波, 陈 辉, 刘 艳 等. CeO2对超音速火焰喷涂WC-12Co涂层腐蚀行为的影响 [J]. 金属学报, 2016, 52: 1441
12 Hou G L, Zhou H D, An Y L, et al. Microstructure and high-temperature friction and wear behavior of WC-(W, Cr)2C-Ni coating prepared by high velocity oxy-fuel spraying [J]. Surf. Coat. Technol., 2011, 206: 82
13 Silveira L L, Sucharski G B, Pukasiewicz A G M, et al. Influence of particle size distribution on the morphology and cavitation resistance of high-velocity oxygen fuel coatings [J]. J. Therm. Spray Technol., 2018, 27: 695
14 Liu M T, Zhong X C, Wang J, et al. Microstructure and thermal stability of MoSi2-CoNiCrAlY nanocomposite feedstock prepared by high energy ball milling [J]. Surf. Coat. Technol., 2014, 239: 78
15 Richer P, Zú?iga A, Yandouzi M, et al. CoNiCrAlY microstructural changes induced during cold gas dynamic spraying [J]. Surf. Coat. Technol., 2008, 203: 364
16 Tahari M, Shamanian M, Salehi M. Microstructural and morphological evaluation of MCrAlY/YSZ composite produced by mechanical alloying method [J]. J. Alloys Compd., 2012, 525: 44
17 Hernández G I V, Albarrán M A G, de Anda E R, et al. Microstructural and high-temperature cyclic oxidation response of NiCoCrAlY coatings with and without SiC + ZrB2 reactive-element dispenser [J]. Corros. Sci., 2021, 189: 109617
18 Bobzin K, Schl?fer T, Richardt K, et al. Development of oxide dispersion strengthened MCrAlY coatings [J]. J. Therm. Spray Technol., 2008, 17: 853
19 Wang H Y, Zuo D W, Wang M D, et al. High temperature frictional wear behaviors of nano-particle reinforced NiCoCrAlY cladded coatings [J]. Trans. Nonferrous Met. Soc. China, 2011, 21: 1322
20 Houdková ?, Ka?parová M. Experimental study of indentation fracture toughness in HVOF sprayed hardmetal coatings [J]. Eng. Fract. Mech., 2013, 110: 468
21 Wood P D, Evans H E, Ponton C B. Investigation into the wear behaviour of Stellite 6 during rotation as an unlubricated bearing at 600 oC [J]. Tribol. Int., 2011, 44: 1589
22 Inman I A, Rose S R, Datta P K. Studies of high temperature sliding wear of metallic dissimilar interfaces Ⅱ: Incoloy MA956 versus Stellite 6 [J]. Tribol. Int., 2006, 39: 1361
23 Wood P D, Evans H E, Ponton C B. Investigation into the wear behaviour of Tribaloy 400 oC during rotation as an unlubricated bearing at 600 oC [J]. Wear, 2010, 269: 763
24 Wei Z, Wu Y P, Hong S, et al. Effects of temperature on wear properties and mechanisms of HVOF sprayed CoCrAlYTa-10%Al2O3 coatings and H13 steel [J]. Metals, 2019, 9: 1224
25 Zhou W T, Kong D J. Influence of Al2O3 mass fractions on microstructure, oxidation resistance and friction-wear behaviors of CoCrAlYTaSi coatings [J]. Surf. Coat. Technol., 2019, 379: 125058
Outlines

/