Research paper

Low Cycle Fatigue Behavior of 9Cr-ODS Steel as a Fusion Blanket Structural Material at Room Temperature

  • WANG Qitao ,
  • LI Yanfen ,
  • ZHANG Jiarong ,
  • LI Yaozhi ,
  • FU Haiyang ,
  • LI Xinle ,
  • YAN Wei ,
  • SHAN Yiyin
Expand
  • 1 School of Materials Science and Engineering, University of Science and Technology of China, Shenyang 110016, China
    2 Shi -changxu Innovation Center for Advanced Materials, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
    3 CAS Key Laboratory of Nuclear Materials and Safety Assessment, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
LI Yanfen, professor, Tel: (024)23978990, E-mail: yfli@imr.ac.cn

Received date: 2023-01-31

  Revised date: 2023-04-28

  Online published: 2023-08-21

Supported by

National Key Research and Development Program of China(2019YFE03130000);National Natural Science Foundation of China(51971217)

Abstract

Adequate studies have not been conducted on the low cycle fatigue properties of oxide dispersion strengthened (ODS) steels that are typically used for fusion reactors worldwide. Moreover, the majority of the fatigue properties are examined with a small sample size due to the restricted manufacturing capacity, which is insufficient for determining the comprehensive properties of bulk materials. Research on the fatigue properties of Chinese ODS steels was conducted recently. However, it is quite uncommon to report the fatigue properties of self-produced 9Cr-ODS steel. Consequently, this work is the first to examine the effect of a cyclic strain on the low cycle fatigue behavior of a representative low-activation 9Cr-ODS martensitic steel. Hence, the strain control test method was employed here in a strain amplitude range of 0.3%-0.8% at room temperature. The cyclic stress response curves, hysteresis loops, relationships between strain amplitude and life, stress amplitude and plastic strain were obtained, and the corresponding fatigue parameters were summarized. Furthermore, the microstructural evolution, fatigue fracture morphology, and crack propagation characteristics during the fatigue process were analyzed. The results revealed that the cyclic stress response behavior of the 9Cr-ODS steel was related to the strain amplitude. With an increase in the strain amplitude, the peak stress in the tension zone of 9Cr-ODS steel increased and the fatigue life decreased. The relationship between cyclic strain and life agreed well with the Coffin-Manson model. Additionally, the 9Cr-ODS steel had no obvious cyclic hardening but revealed a cyclic softening under higher strain amplitudes of 0.5%-0.8%. The microstructure analysis showed that for higher cyclic strain amplitudes, the average grain size and the fraction of the large-angle grain boundaries increased gradually with a reduction in the dislocation density, leading to the cyclic softening of the material. The fatigue crack initiated at the surface and propagated inward by the transgranular mode. The fine grain boundaries and subgrain boundaries of the 9Cr-ODS steel could induce crack deflection, reduce crack propagation rate, and increase fatigue crack propagation life. Moreover, under the same strain amplitude, the peak stress in the tension zone of the steel was almost twice that of the China low activation martensitic (CLAM) steel without a reduction in the fatigue life, indicating a superior low cycle fatigue resistance of the 9Cr-ODS steel.

Cite this article

WANG Qitao , LI Yanfen , ZHANG Jiarong , LI Yaozhi , FU Haiyang , LI Xinle , YAN Wei , SHAN Yiyin . Low Cycle Fatigue Behavior of 9Cr-ODS Steel as a Fusion Blanket Structural Material at Room Temperature[J]. Acta Metall Sin, 2025 , 61(2) : 323 -335 . DOI: 10.11900/0412.1961.2023.00034

References

1 Marmy P, Kruml T. Low cycle fatigue of Eurofer 97 [J]. J. Nucl. Mater., 2008, 377: 52
2 Nishimura A, Nagasaka T, Inoue N, et al. Low cycle fatigue properties of a low activation ferritic steel (JLF-1) at room temperature [J]. J. Nucl. Mater., 2000, 283-287: 677
3 Stubbins J F, Gelles D S. Fatigue performance and cyclic softening of F82H, a ferritic-martensitic steel [J]. J. Nucl. Mater., 1996, 233-237: 331
4 Hirose T, Tanigawa H, Ando M, et al. Radiation effects on low cycle fatigue properties of reduced activation ferritic/martensitic steels [J]. J. Nucl. Mater., 2002, 307-311: 304
5 Lindau R, M?eslang A, Rieth M, et al. Present development status of EUROFER and ODS-EUROFER for application in blanket concepts [J]. Fusion Eng. Des., 2005, 75-79: 989
6 Hu X, Huang L X, Wang W G, et al. Low cycle fatigue properties of CLAM steel at room temperature [J]. Fusion Eng. Des., 2013, 88: 3050
7 Chauhan A, Litvinov D, de Carlan Y, et al. Study of the deformation and damage mechanisms of a 9Cr-ODS steel: Microstructure evolution and fracture characteristics [J]. Mater. Sci. Eng., 2016, A658: 123
8 Cui C, Huang C, Su X P, et al. R&D on advanced cladding materials ODS alloys for fast reactor [J]. Nucl. Sci. Eng., 2011, 31: 305
  崔 超, 黄 晨, 苏喜平 等. 快堆先进包壳材料ODS合金发展研究 [J]. 核科学与工程, 2011, 31: 305
9 Li S F. Study on oxide strengthened dispersion alloys for Generation Ⅳ advanced nuclear systems [D]. Beijing: University of Science and Technology Beijing, 2016
  李少夫. 用于第四代先进核能系统的氧化物弥散强化合金的研究 [D]. 北京: 北京科技大学, 2016
10 Yamashita S, Watanabe S, Ohnuki S, et al. Effect of mechanical alloying parameters on irradiation damage in oxide dispersion strengthened ferritic steels [J]. J. Nucl. Mater., 2000, 283-287: 647
11 Lv Z. Development and prospect of nano-structured ODS steels for fusion reactor first wall application [J]. Atom. Energy Sci. Technol., 2011, 45: 1105
  吕 铮. 聚变堆第一壁用纳米结构ODS钢的发展与前瞻 [J]. 原子能科学技术, 2011, 45: 1105
12 Zinkle S J, Snead L L. Designing radiation resistance in materials for fusion energy [J]. Annu. Rev. Mater. Res., 2014, 44: 241
13 Lucas G E. High chromium ferritic and martensitic steels for nuclear applications: R. Klueh and D. Harries [J]. J. Nucl. Mater., 2002, 302: 232
14 Xu Y P, Lv Y M, Zhou H S, et al. A review on the development of the structural materials of the fusion blanket [J]. Mater. Rev., 2018, 32: 2897
  徐玉平, 吕一鸣, 周海山 等. 核聚变堆包层结构材料研究进展及展望 [J]. 材料导报, 2018, 32: 2897
15 Chauhan A, Hoffmann J, Litvinov D, et al. High-temperature low-cycle fatigue behavior of a 9Cr-ODS steel: Part 2 - hold time influence, microstructural evolution and damage characteristics [J]. Mater. Sci. Eng., 2018, A730: 197
16 Stra?berger L, Chauhan A, Czink S, et al. High-temperature low-cycle fatigue behavior and microstructural evolution of an ODS steel based on conventional T91 [J]. Int. J. Fatigue, 2017, 100: 50
17 Xu H J. Research on microstructure and mechanical property of 15Cr-ODS ferritic alloys [D]. Shenyang: Northeastern University, 2017
  徐海健. 15Cr-ODS铁素体合金微观结构及力学性能的研究 [D]. 沈阳: 东北大学, 2017
18 Chauhan A, Hoffmann J, Litvinov D, et al. High-temperature low-cycle fatigue behavior of a 9Cr-ODS steel: Part 1 - pure fatigue, microstructure evolution and damage characteristics [J]. Mater. Sci. Eng., 2017, A707: 207
19 Klueh R L, Gelles D S, Jitsukawa S, et al. Ferritic/martensitic steels—Overview of recent results [J]. J. Nucl. Mater., 2002, 307-311: 455
20 Mukhopadhyay D K, Froes F H, Gelles D S. Development of oxide dispersion strengthened ferritic steels for fusion [J]. J. Nucl. Mater., 1998, 258-263: 1209
21 Zhang J R, Li Y F, Rui X, et al. Study on microstructure and mechanical properties of 9Cr-ODS steel prepared by a powder hot forging process [J]. J. Iron Steel Res., 2021, 33(11): 1171
  张家榕, 李艳芬, 芮 祥 等. 粉末热锻制备9Cr-ODS钢的微观组织和力学性能研究 [J]. 钢铁研究学报, 2021, 33(11): 1171
22 Rui X, Li Y F, Zhang J R, et al. Microstructure and mechanical properties of a novel designed 9Cr-ODS steel synergically strengthened by nano precipitates [J]. Acta Metall Sin, 2023, 59: 1590
  芮 祥, 李艳芬, 张家榕 等. 新型纳米复合强化9Cr-ODS钢的设计、组织与力学性能 [J]. 金属学报, 2023, 59: 1590
23 Coffin L F. A study of the effects of cyclic thermal stresses on a ductile metal [J]. J. Fluids Eng., 1954, 76: 931
24 Kohyama A, Hishinuma A, Gelles D S, et al. Low-activation ferritic and martensitic steels for fusion application [J]. J. Nucl. Mater., 1996, 233-237: 138
25 Srivatsan T S, Al-Hajri M, Troxell J D. The tensile deformation, cyclic fatigue and final fracture behavior of dispersion strengthened copper [J]. Mech. Mater., 2004, 36: 99
26 Kuběna I, Kruml T, Sp?tig P, et al. Fatigue behaviour of ODS ferritic-martensitic Eurofer steel [J]. Procedia Eng., 2010, 2: 717
27 Li H L, Nishimura A, Li Z X, et al. Low cycle fatigue behavior of JLF-1 steel at elevated temperatures [J]. Fusion Eng. Des., 2006, 81: 241
28 Hu X, Huang L X, Yan W, et al. Microstructure evolution in CLAM steel under low cycle fatigue [J]. Mater. Sci. Eng., 2014, A607: 35
29 Msolli S. Thermoelastoviscoplastic modeling of RAFM steel JLF-1 using tensile and low cycle fatigue experiments [J]. J. Nucl. Mater., 2014, 451: 336
30 Bhattacharya A, Zinkle S J, Henry J, et al. Irradiation damage concurrent challenges with RAFM and ODS steels for fusion reactor first-wall/blanket: A review [J]. J. Phys. Energy, 2022, 4: 034003
31 Zhou H W, Bai F M, Yang L, et al. Low-cycle fatigue behavior of 1100 MPa grade high-strength steel [J]. Acta Metall. Sin., 2020, 56: 937
  周红伟, 白凤梅, 杨 磊 等. 1100 MPa级高强钢的低周疲劳行为 [J]. 金属学报, 2020, 56: 937
32 Zhao C, Huang J F, Zhang J, et al. Low-cycle fatigue behavior of 4Cr5MoSiV1 hot-work die steel at 700 oC [J]. Chin. J. Eng., 2020, 42: 602
  赵 超, 黄进峰, 张 津 等. 4Cr5MoSiV1热作模具钢700 ℃的低周疲劳行为 [J]. 工程科学学报, 2020, 42: 602
Outlines

/