Research paper

Microstructure Evolution Near Interface and the Element Diffusion Dynamics of the Composite Stainless Steel Rebar

  • GUO Xingxing ,
  • SHUAI Meirong ,
  • CHU Zhibing ,
  • LI Yugui ,
  • XIE Guangming
Expand
  • 1 Engineering Research Center Heavy Machinery Ministry of Education, Taiyuan University of Science and Technology, Taiyuan 030024, China
    2 School of Mechanical Engineering, Taiyuan University of Science and Technology, Taiyuan 030024, China
    3 State Key Laboratory of Rolling and Automation, Northeastern University, Shenyang 110819, China
SHUAI Meirong, professor, Tel: 13935124835, E-mail: 2001041@tyust.edu.cn

Received date: 2023-01-20

  Revised date: 2023-08-08

  Online published: 2023-08-11

Supported by

National Natural Science Foundation of China(52075357);Key Research and Development Projects of Shanxi Province(201903D121043);Education and Innovation Subject of Graduate Student of Shanxi Province(20-21Y709; 2022Y709);Open Subject of State Key Laboratory of Rolling and Automation (Northeastern University)(2020RALKFKT013)

Abstract

The composite rebar of stainless steel is used as a new type of structural material and can meet the strict performance requirements of marine service, effectively solving the overcapacity problem of basic materials. The quality of the composite interface generally depends on the interface microstructure and the distribution of interface compounds. However, the deformation parameters also indicate the interface quality, and a composite product with a uniform interface and excellent performance could be obtained by controlling the reduction rate. Herein, high-temperature compression experiments were conducted on the composite materials of 304/Q235. The near-interface characteristics of the microstructure evolution were studied under a strain rate of 1 s-1 and reduction rates of 20%, 40%, and 60% to elucidate the dynamic nucleation mechanism and grain boundary migration of the stainless steel side of the interface. Based on Fick's second law of one-way flow under unsteady conditions, an element diffusion model of the composite interface transition region was established to explore the correlation between the interface microstructure evolution and element diffusion behavior. The results show that there is an uncoordinated dynamic recrystallization occured on both sides of the interface at the temperature of 1000 oC. The grains completely change during dynamic recrystallization at the carbon steel side of the interface, while the recrystallization dominated by the dislocation mechanism significantly occurs under the working condition with a high pressure rate (60%) at the stainless steel side. At a deformation temperature of 1100 oC, dynamic recrystallization is controlled by the dominant twinning mechanism at the stainless steel side, where Σ3 twinning accelerates the recrystallization process. At this time, the coordination of deformation is significantly improved on both sides of the interface. Further studies show that grain refinement and the movement of dislocation and twin defects have a positive effect on the element diffusion behavior. In addition, interfacial intermetallic compound evolution and cavity closure have a significant enhancement effect on interfacial elemental diffusion behavior. The Boltzmann-Matano method is employed to determine the position of the Matano surface, and the Levenberg-Marquardt method is employed to fit the multivariate nonlinear parameters. The established element diffusion model can accurately reflect the elemental concentration in the composite interface transition region, which provides theoretical support for the improvement of metallurgical bonding quality and interface performance control of composite materials.

Cite this article

GUO Xingxing , SHUAI Meirong , CHU Zhibing , LI Yugui , XIE Guangming . Microstructure Evolution Near Interface and the Element Diffusion Dynamics of the Composite Stainless Steel Rebar[J]. Acta Metall Sin, 2025 , 61(2) : 336 -348 . DOI: 10.11900/0412.1961.2023.00032

References

1 Ban H Y, Mei Y X, Shi Y J. Research advances of stainless-clad bimetallic steel structures [J]. Eng. Mech., 2021, 38(6): 1
  班慧勇, 梅镱潇, 石永久. 不锈钢复合钢材钢结构研究进展 [J]. 工程力学, 2021, 38(6): 1
2 Xiang Y, Huang L, Zeng L F, et al. Development and application prospect of hot rolled stainless steel-carbon steel composite rebar [J]. Met. Mater. Metall. Eng., 2017, 45(suppl.1) : 84
  向 勇, 黄 玲, 曾麟芳 等. 热轧不锈钢-碳钢复合钢筋的开发和应用前景 [J]. 金属材料与冶金工程, 2017, 45(): 84
3 Liu X, Shuai M R, Li H B, et al. Effect of micro-tension on interfacial composite quality and atomic diffusion of stainless/carbon steel [J]. Mater. Rev., 2022, 36(23): 127
  刘 鑫, 帅美荣, 李海斌 等. 微张力对不锈钢/碳钢界面复合质量及原子扩散的影响 [J]. 材料导报, 2022, 36(23): 127
4 Song H, Shin H, Shin Y. Heat-treatment of clad steel plate for application of hull structure [J]. Ocean Eng., 2016, 122: 278
5 Mudhaffar M A, Saleh N A, Aassy A. Influence of hot clad rolling process parameters on life cycle of reinforced bar of stainless steel carbon steel bars [J]. Procedia Manuf., 2017, 8: 353
6 Wang S, Zhao G H, Li Y G, et al. Composite plate rolling technology of 304/Q345R based on a corrugated interface [J]. Materials, 2019, 12: 3866
7 Jiang L Y, Zhao C J, Yuan G, et al. Thicker steel plate shape-changing law and control method during the snake rolling process [J]. Metall. Res. Technol., 2016, 113: 309
8 Wu B N, Guo K, Yang X Y, et al. Effect of carbon content of substrate on the microstructure changes and tensile behavior of clad layer of stainless steel composites [J]. Mater. Sci. Eng., 2022, A831: 142201
9 Yang Y H, Jiang Z Z, Li S X, et al. Hot deformation behavior and microstructure evolution of stainless steel/carbon steel laminated composites [J]. Mater. Sci. Eng., 2022, A842: 142994
10 Noh S, Kimura A, Kim T K. Diffusion bonding of 9Cr ODS ferritic/martensitic steel with a phase transformation [J]. Fusion Eng. Des., 2014, 89: 1746
11 He P, Yue X, Zhang J H. Hot pressing diffusion bonding of a titanium alloy to a stainless steel with an aluminum alloy interlayer [J]. Mater. Sci. Eng., 2008, A486: 171
12 Lin Z M, Wang S, He J, et al. The effect of Ni interlayer on the hot-rolled and quenched stainless steel clad plate [J]. Materials, 2020, 13: 5455
13 Liu B X, Wang S, Fang W, et al. Microstructure and mechanical properties of hot rolled stainless steel clad plate by heat treatment [J]. Mater. Chem. Phys., 2018, 216: 460
14 Jin H R, Zhang L, Dai C, et al. Numerical simulation and experimental study on the interface bonding of stainless steel clad plate [J]. Strength Mater., 2018, 50: 29
15 Cho S H, Yoo Y C. Static recrystallization kinetics of 304 stainless steels [J]. J. Mater. Sci., 2001, 36: 4273
16 He W W, Li F, Zhang H Y, et al. The influence of cold rolling deformation on tensile properties and microstructures of Mn18Cr18N austenitic stainless steel [J]. Mater. Sci. Eng., 2019, A764: 138245
17 Yanushkevich Z, Belyakov A, Kaibyshev R. Microstructural evolution of a 304-type austenitic stainless steel during rolling at temperatures of 773-1273 K [J]. Acta Mater., 2015, 82: 244
18 Dehghan-Manshadi A, Barnett M R, Hodgson P D. Recrystallization in AISI 304 austenitic stainless steel during and after hot deformation [J]. Mater. Sci. Eng., 2008, A485: 664
19 Mirzadeh H, Cabrera J M, Prado J M, et al. Hot deformation behavior of a medium carbon microalloyed steel [J]. Mater. Sci. Eng., 2011, A528: 3876
20 Liu Y H, Yao Z K, Ning Y Q, et al. Effect of deformation temperature and strain rate on dynamic recrystallized grain size of a powder metallurgical nickel-based superalloy [J]. J. Alloys Compd., 2017, 691: 554
21 Yang Y H, Jiang Z Z, Chen Y T, et al. Interfacial microstructure and strengthening mechanism of stainless steel/carbon steel laminated composite fabricated by liquid-solid bonding and hot rolling [J]. Mater. Charact., 2022, 191: 112122
22 Giordani E J, Jorge Jr A M, Balancin O. Proportion of recovery and recrystallization during interpass times at high temperatures on a Nb-and N-bearing austenitic stainless steel biomaterial [J]. J. Alloys Compd., 2006, 55: 743
23 Ebrahimi G R, Keshmiri H, Momeni A, et al. Dynamic recrystallization behavior of a superaustenitic stainless steel containing 16%Cr and 25%Ni [J]. Mater. Sci. Eng., 2011, A528: 7488
24 El Wahabi M, Gavard L, Montheillet F, et al. Effect of initial grain size on dynamic recrystallization in high purity austenitic stainless steels [J]. Acta Mater., 2005, 53: 4605
25 Lin Y C, Wu X Y, Chen X M, et al. EBSD study of a hot deformed nickel-based superalloy [J]. J. Alloys Compd., 2015, 640: 101
26 Qin F M, Li Y J, He W W, et al. Effects of deformation microbands and twins on microstructure evolution of as-cast Mn18Cr18N austenitic stainless steel [J]. J. Mater. Res., 2017, 32: 3864
27 Zhong X T, Huang L K, Liu F. Discontinuous dynamic recrystallization mechanism and twinning evolution during hot deformation of Incoloy 825 [J]. J. Mater. Eng. Perform., 2020, 29: 6155
28 Liu B X, Wang S, Fang W, et al. Meso and microscale clad interface characteristics of hot-rolled stainless steel clad plate [J]. Mater. Charact., 2019, 148: 17
29 Yang X T, Fu X Y, Feng L, et al. NiCoCrAlY coating of in-situ synthesis by vacuum diffusion and its oxidation resistance [J]. Rare Met. Mater. Eng., 2020, 49: 1750
  杨效田, 付小月, 冯 力 等. 真空扩散原位合成NiCoCrAlY涂层及其抗氧化性能 [J]. 稀有金属材料与工程, 2020, 49: 1750
30 Lin Z M, Liu B X, Yu W X, et al. The evolution behavior and constitution characteristics of interfacial oxides in the hot-rolled stainless steel clad plate [J]. Corros. Sci., 2023, 211: 110866
31 Li L, Zhang X J, Liu H Y, et al. Formation mechanism of oxide inclusion on the interface of hot-rolled stainless steel clad plates [J]. J. Iron Steel Res., 2013, 25: 43
  李 龙, 张心金, 刘会云 等. 热轧不锈钢复合板界面氧化物夹杂的形成机制 [J]. 钢铁研究学报, 2013, 25: 43
32 Liu B X, Yin F X, Dai X L, et al. The tensile behaviors and fracture characteristics of stainless steel clad plates with different interfacial status [J]. Mater. Sci. Eng., 2017, A679: 172
33 Xie B J, Sun M Y, Xu B, et al. Evolution of interfacial characteristics and mechanical properties for 316LN stainless steel joints manufactured by hot-compression bonding [J]. J Mater. Process. Technol., 2020, 283: 116733.
34 Wang S, Liu B X, Chen C X, et al. Microstructure, mechanical properties and interface bonding mechanism of hot-rolled stainless steel clad plates at different rolling reduction ratios [J]. J. Alloys Compd., 2018, 766: 517
35 Wang H T, Han E H. Ab initio molecular dynamics simulation on interfacial reaction behavior of Fe-Cr-Ni stainless steel in high temperature water [J]. Comput. Mater. Sci., 2018, 149: 143
36 Ma X Y, Zhang Q, Chen X, et al. Inter-diffusion behavior of Ni/Fe/Ni laminated composite for magnetic and electromagnetic interference shielding [J]. Vacuum, 2015, 119: 196
37 Tian N N, Guan J T, Zhang C L, et al. Influence of high-current pulsed electron beam irradiation on element diffusion behavior and mechanical properties of TC4/304 stainless steel diffusion bonded joints [J]. Mater. Charact., 2023, 198: 112713
38 Chen C X, Liu M Y, Liu B X, et al. Tensile shear sample design and interfacial shear strength of stainless steel clad plate [J]. Fusion Eng. Des., 2017, 125: 431
39 Zhong Z H, Hinoki T, Jung H C, et al. Microstructure and mechanical properties of diffusion bonded SiC/steel joint using W/Ni interlayer [J]. Mater. Des., 2010, 31: 1070
40 Luo S G. Effect of grain size on grain boundary diffusion process and properties of sintered NdFeB [D]. Ganzhou: JiangXi University of Science and Technology, 2022
  罗三根. 晶粒尺寸对烧结钕铁硼晶界扩散行为及性能的影响 [D]. 赣州: 江西理工大学, 2022
41 Wu H. Microstructure evolution and element migration (diffusion) behavior of a Ni-based alloy processed by surface mechanical rolling treatment [D]. Nanjing: Nanjing University of Science and Technology, 2020
  吴 豪. 表面机械滚压处理镍基合金结构演化和元素迁移与扩散行为的研究 [D]. 南京: 南京理工大学, 2020
42 Liu B X, Wang S, Chen C X, et al. Interface characteristics and fracture behavior of hot rolled stainless steel clad plates with different vacuum degrees [J]. Appl. Surf. Sci., 2019, 463: 121
43 Eich S M, Kasprzak M, Gusak A, et al. On the mechanism of diffusion-induced recrystallization: Comparison between experiment and molecular dynamics simulations [J]. Acta Mater., 2012, 60: 3469
44 Velmurugan C, Senthilkumar V, Sarala S, et al. Low temperature diffusion bonding of Ti-6Al-4V and duplex stainless steel [J]. J. Mater. Process. Technol., 2016, 234: 272
45 Li Z, Zhao J W, Jia F H, et al. Interfacial characteristics and mechanical properties of duplex stainless steel bimetal composite by heat treatment [J]. Mater. Sci. Eng., 2020, A787: 139513
46 Tsai K Y, Tsai M H, Yeh J W. Sluggish diffusion in Co-Cr-Fe-Mn-Ni high-entropy alloys [J]. Acta Mater., 2013, 61: 4887
47 Zhang Q F, Zhao J C. Extracting interdiffusion coefficients from binary diffusion couples using traditional methods and a forward-simulation method [J]. Intermetallics, 2013, 34: 132 ***********************************************************************************************************
  作 者 勘 误
Outlines

/