Multiscale Residual Stress Evaluation of Engineering Materials/Components Based on Neutron and Synchrotron Radiation Technology
Received date: 2023-04-09
Revised date: 2023-05-20
Online published: 2023-06-07
Supported by
National Key Research and Development Program of China(2021YFA1600600);National Natural Science Foundation of China(U2141206);National Natural Science Foundation of China(52171098);National Natural Science Foundation of China(51921001)
Multiscale residual stress exists throughout the manufacturing process of engineering components, from design and production to processing and servicing. This stress can impact the machining accuracy, structural load capacity, and fatigue lifespan of these components. Therefore, accurate measurement and regulation of residual stress are critical for ensuring the longevity and reliability of engineering components. However, precise characterization of residual stress is challenging owing to its multilevel and cross-scale distribution traits and dynamic evolution under various conditions, such as temperature and load. Compared with laboratory X-ray measurement methods, neutron diffraction (ND), synchrotron-based high-energy X-ray diffraction (HE-XRD), and synchrotron-based X-ray microbeam diffraction (μ-XRD) techniques offer increased penetration depth and better time and spatial resolutions. In addition, the ability to attach environmental devices enables nondestructive and accurate in situ characterization of three types of residual stresses: macroscopic residual stress, intergranular or interphase microscopic stress, and intragranular ultramicroscopic stress. ND is currently the only nondestructive method capable of accurately measuring three-dimensional (3D) stress at centimeter-level depths within engineering components. HE-XRD, due to its high flux, excellent collimation, and millimeter-level penetration depth for metals, can be utilized for in situ studies of intergranular and interphase stress evolution and partitioning during deformation. The μ-XRD employs a submicron focused beam and differential aperture technology to analyze depth information of a sample. By conducting point-by-point scanning, it can capture 3D distribution of microscopic stress inside a single grain. Furthermore, our group has developed a novel method and device for depth stress characterization based on differential aperture technology under synchrotron-based high-energy monochromatic X-ray transmission geometry, and can measure stress gradients with high precision from the surface to the interior of engineering materials at millimeter-level depths. This study presents the measurement principles, application ranges, and applications of the above-mentioned multiscale stress characterization technologies based on the neutron/synchrotron facilities as well as envisaging the future development of related technologies.
LI Shilei , LI Yang , WANG Youkang , WANG Shengjie , HE Lunhua , SUN Guang'ai , XIAO Tiqiao , WANG Yandong . Multiscale Residual Stress Evaluation of Engineering Materials/Components Based on Neutron and Synchrotron Radiation Technology[J]. Acta Metall Sin, 2023 , 59(8) : 1001 -1014 . DOI: 10.11900/0412.1961.2023.00157
| 1 | Ghosh S, Rana V P S, Kain V, et al. Role of residual stresses induced by industrial fabrication on stress corrosion cracking susceptibility of austenitic stainless steel [J]. Mater. Des., 2011, 32: 3823 |
| 2 | Capello E. Residual stresses in turning: Part I: Influence of process parameters [J]. J. Mater. Process. Technol., 2005, 160: 221 |
| 3 | Navas G V, Gonzalo O, Bengoetxea I. Effect of cutting parameters in the surface residual stresses generated by turning in AISI 4340 steel [J]. Int. J. Mach. Tools Manuf., 2012, 61: 48 |
| 4 | Bussu G, Irving P E. The role of residual stress and heat affected zone properties on fatigue crack propagation in friction stir welded 2024-T351 aluminium joints [J]. Int. J. Fatigue, 2003, 25: 77 |
| 5 | Webster G A, Ezeilo A N. Residual stress distributions and their influence on fatigue lifetimes [J]. Int. J. Fatigue, 2001, 23: 375 |
| 6 | Torres M A S, Voorwald H J C. An evaluation of shot peening, residual stress and stress relaxation on the fatigue life of AISI 4340 steel [J]. Int. J. Fatigue, 2002, 24: 877 |
| 7 | Miao B R, Luo Y X, Peng Q M, et al. Multidisciplinary design optimization of lightweight carbody for fatigue assessment [J]. Mater. Des., 2020, 194: 108910 |
| 8 | Niu C L, Xie S M, Zhang T. Research on anti-fatigue design method of welded structure oriented to stiffness coordination strategy [J]. Int. J. Struct. Integr., 2022, 13: 196 |
| 9 | Oehlers D J, Ghosh A, Wahab M. Residual strength approach to fatigue design and analysis [J]. J. Struct. Eng., 1995, 121: 1271 |
| 10 | Zahl D B, McMeeking R M. The influence of residual stress on the yielding of metal matrix composites [J]. Acta Metall. Mater., 1991, 39: 1117 |
| 11 | Clifford S, Jansson N, Yu W, et al. Thermoviscoelastic anisotropic analysis of process induced residual stresses and dimensional stability in real polymer matrix composite components [J]. Composites, 2006, 37A: 538 |
| 12 | Samadi F, Mourya J, Wheatley G, et al. An investigation on residual stress and fatigue life assessment of T-shape welded joints [J]. Eng. Fail. Anal., 2022, 141: 106685 |
| 13 | Fan K F, Liu D X, Liu Y J, et al. Competitive effect of residual stress and surface roughness on the fatigue life of shot peened S42200 steel at room and elevated temperature [J]. Tribol. Int., 2023, 183: 108422 |
| 14 | Zhang W Q, Wang X L, Wang S Y, et al. Combined effects of machining-induced residual stress and external load on SCC initiation and early propagation of 316 stainless steel in high temperature high pressure water [J]. Corros. Sci., 2021, 190: 109644 |
| 15 | Abdul Jawwad A K, Mahdi M, Alshabatat N. The role of service-induced residual stresses in initiating and propagating stress corrosion cracking (SCC) in a 316 stainless steel pressure-relief-valve nozzle set [J]. Eng. Fail. Anal., 2019, 105: 1229 |
| 16 | Yazdanpanah A, Franceschi M, Bergamo G, et al. On the exceptional stress corrosion cracking susceptibility of selective laser melted 316L stainless steel under the individual effect of surface residual stresses [J]. Eng. Fail. Anal., 2022, 136: 106192 |
| 17 | Macherauch E. Residual stresses [A]. Application of Fracture Mechanics to Materials and Structures [M]. Dordrecht: Springer, 1984: 157 |
| 18 | Chava S, Namilae S. Continuous evolution of processing induced residual stresses in composites: An in-situ approach [J]. Composites, 2021, 145A: 106368 |
| 19 | Rossini N S, Dassisti M, Benyounis K Y, et al. Methods of measuring residual stresses in components [J]. Mater. Des., 2012, 35: 572 |
| 20 | Guo J, Fu H Y, Pan B, et al. Recent progress of residual stress measurement methods: A review [J]. Chin. J. Aeronaut., 2021, 34: 54 |
| 21 | Holmberg J, Steuwer A, Stormvinter A, et al. Residual stress state in an induction hardened steel bar determined by synchrotron- and neutron diffraction compared to results from lab-XRD [J]. Mater. Sci. Eng., 2016, A667: 199 |
| 22 | Ganguly S, Stelmukh V, Edwards L. et al. Analysis of residual stress in metal-inert-gas-welded Al-2024 using neutron and synchrotron X-ray diffraction [J]. Mater. Sci. Eng., 2008, A491: 248 |
| 23 | Paradowska A, Finlayson T R, Price J W H. et al. Investigation of reference samples for residual strain measurements in a welded specimen by neutron and synchrotron X-ray diffraction [J]. Physica, 2006, 385-386B: 904 |
| 24 | Aba-Perea P E, Pirling T, Preuss M. In-situ residual stress analysis during annealing treatments using neutron diffraction in combination with a novel furnace design [J]. Mater. Des., 2016, 110: 925 |
| 25 | Chen B, Skouras A, Wang Y Q, et al. In situ neutron diffraction measurement of residual stress relaxation in a welded steel pipe during heat treatment [J]. Mater. Sci. Eng., 2014, A590: 374 |
| 26 | Jia N, Cong Z H, Sun X, et al. An in situ high-energy X-ray diffraction study of micromechanical behavior of multiple phases in advanced high-strength steels [J]. Acta Mater., 2009, 57: 3965 |
| 27 | Zhang M H, Li L F, Ding J, et al. Temperature-dependent micromechanical behavior of medium-Mn transformation-induced-plasticity steel studied by in situ synchrotron X-ray diffraction [J]. Acta Mater., 2017, 141: 294 |
| 28 | Zhang Y B, Andriollo T, F?ster S, et al. Three-dimensional local residual stress and orientation gradients near graphite nodules in ductile cast iron [J]. Acta Mater., 2016, 121: 173 |
| 29 | Guo Y, Collins D M, Tarleton E, et al. Measurements of stress fields near a grain boundary: Exploring blocked arrays of dislocations in 3D [J]. Acta Mater., 2015, 96: 229 |
| 30 | Johnson M W, Edwards L, Withers P J. ENGIN—A new instrument for engineers [J]. Physica, 1997, 234-236B: 1141 |
| 31 | Withers P J, Webster P J. Neutron and synchrotron X-ray strain scanning [J]. Strain, 2001, 37: 19 |
| 32 | Pintschovius L, Jung V, Macherauch E, et al. Residual stress measurements by means of neutron diffraction [J]. Mater. Sci. Eng., 1983, 61: 43 |
| 33 | Wang X L, Holden T, Stoica A D, et al. First results from the VULCAN diffractometer at the SNS [J]. Mater. Sci. Forum, 2010, 652: 105 |
| 34 | Stefanus H, Takayoshi I, Kazuya A, et al. Current status of engineering materials diffractometer at J-PARC [J]. Mater. Sci. Forum, 2011, 681: 443 |
| 35 | Gao J B, Zhang S Y, Zhou L, et al. Novel engineering materials diffractometer fabricated at the China Spallation Neutron Source [J]. Nucl. Instrum. Methods Phys. Res., 2022, 1034A: 166817 |
| 36 | Mori T, Withers P J. Residual stress: Interphase stresses [A]. Encyclopedia of Materials: Science and Technology [M]. 2nd Ed., Amsterdam: Elsevier, 2001: 8113 |
| 37 | Withers P J, Bhadeshia H K D H. Residual stress. Part 1—Measurement techniques [J]. Mater. Sci. Technol., 2001, 17: 355 |
| 38 | Withers P J, Bhadeshia H K D H. Residual stress. Part 2—Nature and origins [J]. Mater. Sci. Technol., 2001, 17: 366 |
| 39 | Hutchings M T, Krawitz A D. Measurement of Residual and Applied Stress Using Neutron Diffraction [M]. Dordrecht: Springer, 1992: 1 |
| 40 | Hutchings M T, Withers P J, Holden T M, et al. Introduction to the Characterization of Residual Stress by Neutron Diffraction [M]. Boca Raton: CRC Press, 2005: 1 |
| 41 | Winholtz R A, Krawitz A D. Implications of equilibrium on principal macrostresses measured by neutron diffraction [J]. Mater. Sci. Eng., 1996, A221: 33 |
| 42 | Winholtz R A, Krawitz A D. The effect of assuming the principal directions in neutron diffraction measurement of stress tensors [J]. Mater. Sci. Eng., 1996, A205: 257 |
| 43 | Pratihar S, Turski M, Edwards L, et al. Neutron diffraction residual stress measurements in a 316L stainless steel bead-on-plate weld specimen [J]. Int. J. Press. Vessels Pip., 2009, 86: 13 |
| 44 | Gn?upel-Herold T, Creuziger A A, Iadicola M. A model for calculating diffraction elastic constants [J]. J. Appl. Cryst., 2012, 45: 197 |
| 45 | Gn?upel-Herold T. ISODEC: Software for calculating diffraction elastic constants [J]. J. Appl. Crystallogr., 2012, 45: 573 |
| 46 | Inspection and Quarantine of the People's Republic of China, AdministrationStandardization. Non-destructive testing—Standards test method for determining residual stresses by neutron diffraction. [S]. Beijing: Standards Press of China, 2011 |
| 中华人民共和国国家质量监督检验检疫总局, 中国国家标准化管理委员会. 无损检测 测量残余应力的中子衍射方法. [S]. 北京: 中国标准出版社, 2011 | |
| 47 | Withers P J, Preuss M, Steuwer A, et al. Methods for obtaining the strain-free lattice parameter when using diffraction to determine residual stress [J]. J. Appl. Crystallogr., 2007, 40: 891 |
| 48 | Liu X L, Luzin V, Qi H L, et al. Mapping of three-dimensional residual stresses by neutron diffraction in nickel-based superalloy discs prepared under different quenching conditions [J]. Mater. Today Commun., 2022, 32: 103876 |
| 49 | Zhang Z W. Study on the evolution of three-dimensional residual stress field in turbine discs by using neutron/X-ray diffraction and finite element method [D]. Beijing: University of Science and Technology Beijing, 2022 |
| 张哲维. 基于中子/X射线衍射与有限元法的涡轮盘模拟件三维残余应力场演变研究 [D]. 北京: 北京科技大学, 2022 | |
| 50 | Nishida M, Jing T, Muslih M R, et al. Residual stress measurement of titanium casting alloy by neutron diffraction [J]. AIP Conf. Proc., 2008, 989: 101 |
| 51 | Ren Y. High-energy synchrotron X-ray diffraction and its application to in situ structural phase-transition studies in complex sample environments [J]. JOM, 2012, 64: 140 |
| 52 | Rakowski R, Golovin G, O'Neal J, et al. Single-shot structural analysis by high-energy X-ray diffraction using an ultrashort all-optical source [J]. Sci. Rep., 2017, 7: 16603 |
| 53 | Wang T C. A study on microscopic mechanism of brittle fracture of thermally aged duplex stainless steels [D]. Beijing: University of Science and Technology Beijing, 2019 |
| 王天成. 热老化双相不锈钢脆性断裂的微观机制研究 [D]. 北京: 北京科技大学, 2019 | |
| 54 | Li R G, Wang Y K, Xu N, et al. Unveiling the origins of work-hardening enhancement and mechanical instability in laser shock peened titanium [J]. Acta Mater., 2022, 229: 117810 |
| 55 | Liu W J, Ice G E. X-ray laue diffraction microscopy in 3D at the advanced photon source [A]. Strain and Dislocation Gradients from Diffraction [C]. London: Imperial College Press, 2014: 53 |
| 56 | Liu W, Zschack P, Tischler J, et al. X‐ray Laue diffraction microscopy in 3D at the advanced photon source [J]. AIP Conf. Proc., 2011, 1365: 108 |
| 57 | Li R G. Localized deformation and damage of FCC/HCP metallic materials investigated by synchrotron-based X-ray diffraction [D]. Beijing: University of Science and Technology Beijing, 2020 |
| 李润光. FCC/HCP金属材料局域形变与损伤的同步辐射衍射研究 [D]. 北京: 北京科技大学, 2020 |
/
| 〈 |
|
〉 |