Research paper

Effect of Flash Heating on Microstructure and Mechanical Properties of 2000 MPa Hot Stamping Steel

  • XIE Zedong ,
  • DING Cancan ,
  • WEN Pengyu ,
  • LUO Haiwen
Expand
  • School of Metallurgical and Ecological Engineering, University of Science and Technology Beijing, Beijing 100083, China
LUO Haiwen, professor, Tel: (010)62332911, E-mail: luohaiwen@ustb.edu.cn

Received date: 2023-02-02

  Revised date: 2023-03-11

  Online published: 2023-05-15

Supported by

National Natural Science Foundation of China(51831002);National Natural Science Foundation of China(52233018);Fundamental Research Founds for the Central Universities(FRF-TP-18-002C2)

Abstract

Hot stamping steels (HSSs) have been widely used in automobiles, to reduce weight and improve safety due to their ultrahigh strength and ease of synthesis at high temperatures. At present, steel sheets with high strength and good ductility are needed to further reduce the weight of manufactured products. The most popular HSS grade in use at present is 22MnB5, which has an ultimate tensile strength (UTS) of 1500 MPa, but it has a ductility of less than 7%, which is quite poor. Driven by the demand for weight reduction in the automotive industries, a 2000 MPa HSS have been developed by employing a new alloying design and an ultrafast heating process. The latter has received much less attention than the former, although it demonstrates huge potential for improving mechanical properties and production efficiency of HSSs. In this study, the effect of heating processes, including conventional and flash heating, at a ramp of 150oC/s in the temperature range of 850-950oC before tempering at 150oC on the microstructures and mechanical properties of a new type of 2000 MPa HSS were studied. Compared with the conventional heating at a relatively low ramp rate, the flash heating improved the strength and ductility of 2000 MPa HSS, simultaneously. Moreover, their best tensile properties were achieved after flash heating to 950oC: UTS was 2180 MPa and total elongation was 13%, which were approximately 200 MPa and 4% higher than those obtained using conventional heating, respectively. This is because flash heating results in the formation of a more refined hierarchical martensite structure after quenching, with a higher dislocation density and a larger fraction of retained austenite (RA). RA was formed by dissolving cementite particles containing high C/Mn concentrations, which were then inherited in the formed austenite after quenching due to insufficient time for the homogenization of solute C/Mn by diffusion during the flash heating. The volume fraction of RA increased gradually with an increase in the flash heating temperature, then, more cementite particles were dissolved. This was also confirmed by kinetic simulations that reversed the austenitization on the dissolving cementite. Finally, it was proposed that flash heating technology is a promising technology for the production of ultra-strong and ductile HSS sheets.

Cite this article

XIE Zedong , DING Cancan , WEN Pengyu , LUO Haiwen . Effect of Flash Heating on Microstructure and Mechanical Properties of 2000 MPa Hot Stamping Steel[J]. Acta Metall Sin, 2024 , 60(12) : 1667 -1677 . DOI: 10.11900/0412.1961.2023.00036

References

1 Jhajj K S, Slezak S R, Daun K J. Inferring the specific heat of an ultra high strength steel during the heating stage of hot forming die quenching, through inverse analysis [J]. Appl. Therm. Eng., 2015, 83: 98
2 Jin X J, Gong Y, Han X H, et al. A review of current state and prospect of the manufacturing and application of advanced hot stamping automobile steels [J]. Acta Metall. Sin., 2020, 56: 411
  金学军, 龚 煜, 韩先洪 等. 先进热成形汽车钢制造与使用的研究现状与展望 [J]. 金属学报, 2020, 56: 411
3 Karbasian H, Tekkaya A E. A review on hot stamping [J]. J. Mater. Process. Technol., 2010, 210: 2103
4 Wen P Y, Han J S, Luo H W. Application of flash processing in advanced high strength steels [J]. J. Iron Steel Res., 2020, 32: 1050
  温鹏宇, 韩建胜, 罗海文. 闪速加热工艺在先进高强钢领域的应用 [J]. 钢铁研究学报, 2020, 32: 1050
5 Karimi Y, Hossein Nedjad S, Shirazi H, et al. Cold rolling and intercritical annealing of C-Mn steel sheets with different initial microstructures [J]. Mater. Sci. Eng., 2018, A736: 392
6 Wen P Y, Hu B, Han J S, et al. A strong and ductile medium Mn steel manufactured via ultrafast heating process [J]. J. Mater. Sci. Technol., 2022, 97: 54
7 Wan X H, Liu G, Yang Z G, et al. Flash annealing yields a strong and ductile medium Mn steel with heterogeneous microstructure [J]. Scr. Mater., 2021, 198: 113819
8 Wen P Y, Han J S, Luo H W, et al. Effect of flash processing on recrystallization behavior and mechanical performance of cold-rolled IF steel [J]. Int. J. Miner. Metall. Mater., 2020, 27: 1234
9 Liu G, Li T, Yang Z G, et al. On the role of chemical heterogeneity in phase transformations and mechanical behavior of flash annealed quenching & partitioning steels [J]. Acta Mater., 2020, 201: 266
10 Mori K, Bariani P F, Behrens B A, et al. Hot stamping of ultra-high strength steel parts [J]. CIRP Ann., 2017, 66: 755
11 Min J Y, Lin J P, Min Y A, et al. On the ferrite and bainite transformation in isothermally deformed 22MnB5 steels [J]. Mater. Sci. Eng., 2012, A550: 375
12 Yi H L, Chang Z Y, Cai H L, et al. Strength, ductility and fracture strain of press-hardening steels [J]. Acta Metall. Sin., 2020, 56: 429
  易红亮, 常智渊, 才贺龙 等. 热冲压成形钢的强度与塑性及断裂应变 [J]. 金属学报, 2020, 56: 429
13 Hu K H, Mao X P, Zhou G F, et al. Effect of Si and Mn contents on the microstructure and mechanical properties of ultra-high strength press hardening steel [J]. Acta Metall. Sin., 2018, 54: 1105
  胡宽辉, 毛新平, 周桂峰 等. Si和Mn含量对超高强度热成形钢组织和性能的影响 [J]. 金属学报, 2018, 54: 1105
14 Liang J T, Lu H Z, Zhang L L, et al. A 2000 MPa grade Nb bearing hot stamping steel with ultra-high yield strength [J]. Mater. Sci. Eng., 2021, A801: 140419
15 Naderi M, Ketabchi M, Abbasi M, et al. Analysis of microstructure and mechanical properties of different high strength carbon steels after hot stamping [J]. J. Mater. Process. Technol., 2011, 211: 1117
16 Taylor T, Fourlaris G, Evans P, et al. New generation ultrahigh strength boron steel for automotive hot stamping technologies [J]. Mater. Sci. Technol., 2014, 30: 818
17 Ding C C, Hu K H, Chen H, et al. A dual-phase press-hardening steel with improved mechanical properties and superior oxidation resistance [J]. Metall. Mater. Trans., 2022, 53A: 1934
18 J?rvinen H, Isakov M, Nyyss?nen T, et al. The effect of initial microstructure on the final properties of press hardened 22MnB5 steels [J]. Mater. Sci. Eng., 2016, A676: 109
19 Han J, Lee Y K. The effects of the heating rate on the reverse transformation mechanism and the phase stability of reverted austenite in medium Mn steels [J]. Acta Mater., 2014, 67: 354
20 Luo H W, Wang X H, Liu Z B, et al. Influence of refined hierarchical martensitic microstructures on yield strength and impact toughness of ultra-high strength stainless steel [J]. J. Mater. Sci. Technol., 2020, 51: 130
21 Zhou T, Lu J, Hedstr?m P. Mechanical behavior of fresh and tempered martensite in a CrMoV-alloyed steel explained by microstructural evolution and strength modeling [J]. Metall. Mater. Trans., 2020, 51A: 5077
22 Liu G, Dai Z B, Yang Z G, et al. Kinetic transitions and Mn partitioning during austenite growth from a mixture of partitioned cementite and ferrite: Role of heating rate [J]. J. Mater. Sci. Technol., 2020, 49: 70
23 Chen W J, Gao P F, Wang S, et al. Strengthening mechanisms of Nb and V microalloying high strength hot-stamped steel [J]. Mater. Sci. Eng., 2020, A797: 140115
24 Yong Q L. The Second Phase in Steel [M]. Beijing: Metallurgical Industry Press, 2006: 5
  雍岐龙. 钢铁材料中的第二相 [M]. 北京: 冶金工业出版社, 2006: 5
25 Shintani T, Murata Y. Evaluation of the dislocation density and dislocation character in cold rolled Type 304 steel determined by profile analysis of X-ray diffraction [J]. Acta Mater., 2011, 59: 4314
26 Wang Y J, Sun J J, Jiang T, et al. A low-alloy high-carbon martensite steel with 2.6?GPa tensile strength and good ductility [J]. Acta Mater., 2018, 158: 247
27 Hansen N. Hall-Petch relation and boundary strengthening [J]. Scr. Mater., 2004, 51: 801
28 Wang Y, Hu B, Liu X Y, et al. Influence of annealing temperature on both mechanical and damping properties of Nb-alloyed high Mn steel [J]. Acta Metall. Sin., 2021, 57: 1588
  王 玉, 胡 斌, 刘星毅 等. 退火温度对含Nb高锰钢力学和阻尼性能的影响 [J]. 金属学报, 2021, 57: 1588
29 Shibata A, Yonezawa H, Yabuuchi K, et al. Relation between martensite morphology and volume change accompanying fcc to bcc martensitic transformation in Fe-Ni-Co alloys [J]. Mater. Sci. Eng., 2006, A438-440: 241
30 Li S S, Wen P Y, Li S L, et al. A novel medium-Mn steel with superior mechanical properties and marginal oxidization after press hardening [J]. Acta Mater., 2021, 205: 116567
31 Luo H W, Liu J H, Dong H. A novel observation on cementite formed during intercritical annealing of medium Mn steel [J]. Metall. Mater. Trans., 2016, 47A: 3119
32 Shen G H, Hu B, Yang Z B, et al. Influence of tempering temperature on mechanical properties and microstructures of high-Al-contained medium Mn steel having δ-ferrite [J]. Acta Metall. Sin., 2022, 58: 165
  沈国慧, 胡 斌, 杨占兵 等. 回火温度对含δ铁素体高铝中锰钢力学性能和显微组织的影响 [J]. 金属学报, 2022, 58: 165
33 Liu G, Zhang S G, Li J, et al. Fast-heating for intercritical annealing of cold-rolled quenching and partitioning steel [J]. Mater. Sci. Eng., 2016, A669: 387
34 Azizi-Alizamini H, Militzer M, Poole W J. Formation of ultrafine grained dual phase steels through rapid heating [J]. ISIJ Int., 2011, 51: 958
35 Nakada N, Tsukahara M, Fukazawa K, et al. Very fine structured DP steel with tempered-martensite matrix fabricated by fast heating [J]. Mater. Trans., 2018, 59: 166
36 Xu D C, Li J, Meng Q G, et al. Effect of heating rate on microstructure and mechanical properties of TRIP-aided multiphase steel [J]. J. Alloys Compd., 2014, 614: 94
37 Mohanty R R, Girina O A, Fonstein N M. Effect of heating rate on the austenite formation in low-carbon high-strength steels annealed in the intercritical region [J]. Metall. Mater. Trans., 2011, 42A: 3680
Outlines

/