Research paper

Phase Field Simulation of Viscous Sintering

  • GUO Songyuan ,
  • LIU Wenbo ,
  • YANG Qingcheng ,
  • QI Xiaoyong ,
  • YUN Di
Expand
  • 1 School of Energy and Power Engineering, Xi'an Jiaotong University, Xi'an 710049, China
    2 Shaanxi Key Laboratory of Advanced Nuclear Energy and Technology, Xi'an Jiaotong University, Xi'an 710049, China
    3 Shanghai Key Laboratory of Mechanics in Energy Engineering, Shanghai University, Shanghai 200072, China
LIU Wenbo, associate professor, Tel: (029)82668948, E-mail: liuwenbo@xjtu.edu.cn

Received date: 2022-09-09

  Revised date: 2023-03-01

  Online published: 2023-05-06

Supported by

Joint Fund of National Natural Science Foundation of China and China Academy of Engineering Physics (NSAF Joint Fund)(U2130105);Key Research Project of Zhejiang Lab(2021PE0AC02);Innovative Scientific Program of China National Nuclear Corporation

Abstract

The presence of a liquid phase, which provides capillary force during viscous sintering, can accelerate the evolution of sintered particles. Due to the difficulty of coupling about the Navier-Stokes equations, however, it is quite challenging to obtain simulation results that meet the laws of physics. In the present study, a phase field model of the viscous sintering process is established, and the morphology, velocity field, and pressure field evolutions of the sintered particles are analyzed. First, the Cahn-Hilliard and Navier-Stokes equations are solved using the finite difference method and the predictor-corrector method. In the finite difference method, the upwind and central difference schemes are combined. The simulation results show that under the drive of surface tension, two circular particles gradually merge into one. The velocity field is divided into a pure straining region and a rigid body motion region inside the particle; the pressure difference between the inside and outside of the particles is proportional to the curvature of the particles. Then, the contact radius and shrinkage of the two circular particles are calculated, and then a curve over time is drawn. The results show that they vary drastically at the beginning stage of evolution and satisfy the law of viscoelastic contact. In the later stage of evolution, the change becomes slower when the contact radius and shrinkage of the two circular particles are close to the values of the equilibrium state. With the increase in mobility, the evolution rate accelerates, but the morphology of the stable state is almost unchanged. The evolution of multiparticles and pores is also simulated. The results show that the pores in the viscous sintering process are initially spheroidized and then slowly disappear, resulting in densification. Under the same simulation conditions, the smaller pores evolve faster.

Cite this article

GUO Songyuan , LIU Wenbo , YANG Qingcheng , QI Xiaoyong , YUN Di . Phase Field Simulation of Viscous Sintering[J]. Acta Metall Sin, 2024 , 60(12) : 1691 -1700 . DOI: 10.11900/0412.1961.2022.00445

References

1 German R M, translated by Jia C C, Chu K, Liu B W, et al. Sintering: From Empirical Observations to Scientific Principles [M]. Beijing: Chemical Industry Press, 2021: 5
  兰德尔·杰曼著, 贾成厂, 褚 克, 刘博文等译. 烧结实践与科学原理 [M]. 北京: 化学工业出版社, 2021: 5
2 German R M, Suri P, Park S J. Review: Liquid phase sintering [J]. J. Mater. Sci., 2009, 44: 1
3 Pi H L, Shi X L, Xu X X. Effect of SiC-ZrC coating prepared by SiZr liquid phase sintering on the oxidation resistance of C/SiC composites [J]. Acta Metall. Sin., 2021, 57: 791
  皮慧龙, 石小磊, 徐兴祥. SiZr液相烧结法制备SiC-ZrC涂层对C/SiC复合材料抗氧化性能的影响 [J]. 金属学报, 2021, 57: 791
4 Kraft T, Riedel H. Numerical simulation of solid state sintering; model and application [J]. J. Eur. Ceram. Soc., 2004, 24: 345
5 Van de Vorst G A L, Mattheij R M M. Numerical analysis of a 2-D viscous sintering problem with non-smooth boundaries [J]. Computing, 1992, 49: 239
6 Kuiken H K. Viscous sintering: The surface-tension-driven flow of a liquid form under the influence of curvature gradients at its surface [J]. J. Fluid Mech., 1990, 214: 503
7 Frenkel J J. Viscous flow of crystalline bodies under the action of surface tension [J]. J. Phys., 1945, 9: 385
8 Martínez-Herrera J I, Derby J J. Viscous sintering of spherical particles via finite element analysis [J]. J. Am. Ceram. Soc., 1995, 78: 645
9 Hiram Y, Nir A. A simulation of surface tension driven coalescence [J]. J. Colloid Interface Sci., 1983, 95: 462
10 Gross M, Steinbach I, Raabe D, et al. Viscous coalescence of droplets: A lattice Boltzmann study [J]. Phys. Fluids, 2013, 25: 052101
11 Braginsky M, Tikare V, Olevsky E. Numerical simulation of solid state sintering [J]. Int. J. Solids Struct., 2005, 42: 621
12 Yang Q C, Kirshtein A, Ji Y Z, et al. A thermodynamically consistent phase-field model for viscous sintering [J]. J. Am. Ceram. Soc., 2019, 102: 674
13 Landau L D, Khalatikow I M. The Selected Works of L.D. Landau (English Translation) [M]. Oxford: Pergamon, 1963: 1
14 Sun Z Y, Yang C, Liu W B. Phase field simulations of the sintering process of UO2 [J]. Acta Metall. Sin., 2020, 56: 1295
  孙正阳, 杨 超, 柳文波. UO2烧结过程的相场模拟 [J]. 金属学报, 2020, 56: 1295
15 Wang Y U. Computer modeling and simulation of solid-state sintering: A phase field approach [J]. Acta Mater., 2006, 54: 953
16 Chockalingam K, Kouznetsova V G, Van der Sluis O, et al. 2D phase field modeling of sintering of silver nanoparticles [J]. Comput. Meth. Appl. Mech. Eng., 2016, 312: 492
17 Zhang X, Liao Y L. A phase-field model for solid-state selective laser sintering of metallic materials [J]. Powder Technol., 2018, 339: 677
18 Kumar V, Fang Z Z, Fife P C. Phase field simulations of grain growth during sintering of two unequal-sized particles [J]. Mater. Sci. Eng., 2010, A528: 254
19 Tegze G, Pusztai T, Gránásy L. Phase field simulation of liquid phase separation with fluid flow [J]. Mater. Sci. Eng., 2005, A413-414: 418
20 Soligo G, Roccon A, Soldati A. Mass-conservation-improved phase field methods for turbulent multiphase flow simulation [J]. Acta Mech., 2019, 230: 683
21 Gao Y J, Lu Y J, Kong L Y, et al. Phase field crystal model and its application for microstructure evolution of materials [J]. Acta Metall. Sin., 2018, 54: 278
  高英俊, 卢昱江, 孔令一 等. 晶体相场模型及其在材料微结构演化中的应用 [J]. 金属学报, 2018, 54: 278
22 Zografos K, Afonso A M, Poole R J, et al. A viscoelastic two-phase solver using a phase-field approach [J]. J. Non-Newton. Fluid Mech., 2020, 284: 104364
23 Balemans C, Hulsen M A, Anderson P D. Sintering of two viscoelastic particles: A computational approach [J]. Appl. Sci., 2017, 7: 516
24 Kim J. Phase-field models for multi-component fluid flows [J]. Commun. Comput. Phys., 2012, 12: 613
25 Lin Y Y, Hui C Y, Jagota A. The role of viscoelastic adhesive contact in the sintering of polymeric particles [J]. J. Colloid Interface Sci., 2001, 237: 267
26 Kamyabi M, Sotudeh-Gharebagh R, Zarghami R, et al. Principles of viscous sintering in amorphous powders: A critical review [J]. Chem. Eng. Res. Des., 2017, 125: 328
27 Wakai F, Katsura K, Kanchika S, et al. Sintering force behind the viscous sintering of two particles [J]. Acta Mater., 2016, 109: 292
Outlines

/