Basal Stacking Faults of μ Phase in Ni-Based Superalloy GH4151
Received date: 2023-01-16
Revised date: 2023-02-26
Online published: 2023-04-27
Supported by
National Natural Science Foundation of China(52171020);National Natural Science Foundation of China(91960202);National Science and Technology Major Project of China(2019VI00060120)
Wrought Ni-based superalloys are widely used in aviation and energy fields because of their excellent creep resistance, thermal stability, heat corrosion resistance, and oxidation resistance at high temperatures. The mechanical properties of wrought Ni-based superalloys are significantly affected by grain boundary precipitation. Among the grain boundary second phases, the topologically close-packed (TCP) phase is usually discovered in wrought superalloys with the addition of refractory metal elements. As a complex intermetallic compound with only tetrahedral interstices, the TCP phase is stacked with a high packing density of atoms, embodying low plasticity and high brittleness. Given these characteristics, the TCP phase tends to promote crack initiation and propagation during creep, thereby reducing the alloy's creep strength. Additionally, the formation of the TCP phase requires several refractory elements, thereby weakening the effect of the solid solution strengthening of the matrix. As a ubiquitous TCP phase in wrought superalloys, μ phases are represented by rectangular and parallelogram structural subunits, which are parallel to the basal plane of μ phases. Basal stacking faults (SFs) are the most common defects in the μ phase, and SFs with different stacking sequences will form different phases with corresponding structures and mechanical properties. The μ phases and their basal SFs in wrought Ni-based superalloy GH4151 were systematically studied by multifarious electron microscopy techniques, such as EDS and atomic-resolution high-angle annular dark-field scanning transmission electron microscopy (HAADF-STEM) of aberration-corrected TEM, revealing the structure and composition of the μ phase and the structure and distribution of numerous basal SFs in the μ phase. Based on the different arrangements of structural subunits, the basal SFs were divided into four types. Type I basal SF is equivalent to the μ phase with a layer of parallelogram structural subunit reversing to form two layers of microsymmetric structures, the reversed parallelogram structural subunit is symmetrical to the rectangular one; type II basal SF is equivalent to type I basal SF in the absence of a layer of the rectangular structural subunit, forming a C14 structure and microsymmetric structure; type III basal SF results from the absence of a layer of the parallelogram structural subunit in the μ phase, forming a complete Zr4Al3 phase; and type IV basal SF results from the absence of a layer of the rectangular structural subunit in the μ phase, forming a C15 structure. Among the four types of basal SFs, type II and type IV basal SFs form Laves phases, but the occurrence of the former is more than that of the latter. This finding is related to the stability of type II basal SF (C14 structure) over type IV basal SF (C15 structure) revealed by the first-principle calculations.
LONG Jiangdong , DUAN Huichao , ZHAO Peng , ZHANG Rui , ZHENG Tao , QU Jinglong , CUI Chuanyong , DU Kui . Basal Stacking Faults of μ Phase in Ni-Based Superalloy GH4151[J]. Acta Metall Sin, 2024 , 60(2) : 167 -178 . DOI: 10.11900/0412.1961.2023.00026
| 1 | Reed R C. The Superalloys: Fundamentals and Applications [M]. Cambridge: Cambridge University Press, 2006: 10 |
| 2 | Guo J T. Materials Science and Engineering for Superalloys [M]. Beijing: Science Press, 2008: 286 |
| 郭建亭. 高温合金材料学 [M]. 北京: 科学出版社, 2008: 286 | |
| 3 | Kuo K H, Ye H Q, Li D X. Tetrahedrally close-packed phases in superalloys: New phases and domain structures observed by high-resolution electron microscopy [J]. J. Mater. Sci., 1986, 21: 2597 |
| 4 | Giessen B C. Developments in the Structural Chemistry of Alloy Phases [M]. Cleveland: Springer, 1969: 30 |
| 5 | Tian S G, Wang M G, Li T, et al. Influence of TCP phase and its morphology on creep properties of single crystal nickel-based superalloys [J]. Mater. Sci. Eng., 2010, A527: 5444 |
| 6 | Volek A, Singer R F, Buergel R, et al. Influence of topologically closed packed phase formation on creep rupture life of directionally solidified nickel-base superalloys [J]. Metall. Mater. Trans., 2006, 37A: 405 |
| 7 | Carvalho P A, De Hosson J T M. Stacking faults in the Co7W6 isomorph of the μ phase [J]. Scr. Mater., 2001, 45: 333 |
| 8 | Chisholm M F, Kumar S, Hazzledine P. Dislocations in complex materials [J]. Science, 2005, 307: 701 |
| 9 | Wang D, Zhang J, Lou L H. On the role of μ phase during high temperature creep of a second generation directionally solidified superalloy [J]. Mater. Sci. Eng., 2010, A527: 5161 |
| 10 | Zhang Y C, Du K, Zhang W, et al. Shear deformation determined by short-range configuration of atoms in topologically close-packed crystal [J]. Acta Mater., 2019, 179: 396 |
| 11 | Zhang W, Yu R, Du K, et al. Undulating slip in Laves phase and implications for deformation in brittle materials [J]. Phys. Rev. Lett., 2011, 106: 165505 |
| 12 | Zhang Y C, Zhang W, Du B N, et al. Shuffle and glide mechanisms of prismatic dislocations in a hexagonal C14-type Laves-phase intermetallic compound [J]. Phys. Rev., 2020, 102B: 134117 |
| 13 | Yang Z Q, Chisholm M F, Yang B, et al. Role of crystal defects on brittleness of C15 Cr2Nb Laves phase [J]. Acta Mater., 2012, 60: 2637 |
| 14 | Frank F C, Kasper J S. Complex alloy structures regarded as sphere packings. I. Definitions and basic principles [J]. Acta Crystallogr., 1958, 11: 184 |
| 15 | Frank F C, Kasper J S. Complex alloy structures regarded as sphere packings. II. Analysis and classification of representative structures [J]. Acta Crystallogr., 1959, 12: 483 |
| 16 | Sinha A K. Topologically close-packed structures of transition metal alloys [J]. Prog. Mater. Sci., 1972, 15: 81 |
| 17 | Hiraga K, Yamamoto T, Hirabayashi M. Intermetallic compounds of the μ- and P-phases of Co7Mo6 studied by 1 MV electron microscopy [J]. Trans. Jpn Inst. Met., 1983, 24: 421 |
| 18 | Ye H Q, Li D X, Kuo K H. Domain structures of tetrahedrally close-packed phases with juxtaposed pentagonal antiprisms I. Structure description and HREM images of the C14 Laves and μ phases [J]. Philos. Mag., 1985, 51A: 829 |
| 19 | Heggen M, Houben L, Feuerbacher M. Plastic-deformation mechanism in complex solids [J]. Nat. Mater., 2010, 9: 332 |
| 20 | Feuerbacher M, Balanetskyy S, Heggen M. Novel metadislocation variants in orthorhombic Al-Pd-Fe [J]. Acta. Mater., 2008, 56: 1849 |
| 21 | Zhu J, Ye H Q. On the microstructure and its diffraction anomaly of the μ phase in superalloys [J]. Scr. Metall. Mater., 1990, 24: 1861 |
| 22 | Ma S Y, Li X Q, Zhang J X, et al. Atomic arrangement and formation of planar defects in the μ phase of Ni-base single crystal superalloys [J]. J. Alloys Compd., 2018, 766: 775 |
| 23 | Li D X, Kuo K H. Domain structures of tetrahedrally close-packed phases with juxtaposed pentagonal antiprisms III. Domain boundary structures in the μ phase [J]. Philos. Mag., 1985, 51A: 849 |
| 24 | Cheng Y X, Wang G L, Liu J D, et al. Atomic configurations of planar defects in μ phase in Ni-based superalloys [J]. Scr. Mater., 2021, 193: 27 |
| 25 | Gao S, Liu Z Q, Li C F, et al. In situ TEM investigation on the precipitation behavior of μ phase in Ni-base single crystal superalloys [J]. Acta. Mater., 2016, 110: 268 |
| 26 | Carvalho P A, Haarsma H S D, Kooi B J, et al. HRTEM study of Co7W6 and its typical defect structure [J]. Acta Mater., 2000, 48: 2703 |
| 27 | Shi T Y, Lu J C, Sun D S, et al. A high N and W heat-resistant martensitic cast steel with balanced tensile strength and creep resistance achieved by Laves and μ intermetallics [J]. J. Mater. Sci., 2022, 57: 12616 |
| 28 | Ye H Q, Wang D N, Kuo K H. Domain structures of tetrahedrally close-packed phases with juxtaposed pentagonal antiprisms II. Domain boundary structures of the CI4 Laves phase [J]. Philos. Mag., 1985, 51A: 839 |
| 29 | Liu L R, Zhou B X, Wang Q F, et al. Intergrowth structure of Laves within μ phases in Co-Al-W base superalloy [J]. J. Alloys Compd., 2020, 844: 155822 |
| 30 | Chen H, Ye L, Han Y, et al. Additive manufacturing of W-Fe composites using laser metal deposition: microstructure, phase transformation, and mechanical properties [J]. Mater. Sci. Eng., 2021, A811: 141036 |
| 31 | Mittemeijer E J. Fundamentals of Materials Science [M]. Berlin: Springer, 2010: 305 |
| 32 | Giannozzi P, Baroni S, Bonini N, et al. QUANTUM ESPRESSO: A modular and open-source software project for quantum simulations of materials [J]. J. Phys. Condens. Matter, 2009, 21: 395502 |
| 33 | Perdew J P, Burke K, Ernzerhof M. Generalized gradient approximation made simple [J]. Phys. Rev. Lett., 1996, 77: 3865 |
| 34 | Williams D B, Carter C B. Transmission Electron Microscopy [M]. 2nd Ed., New York: Springer, 2009: 419 |
/
| 〈 |
|
〉 |