Inhibitor and Secondary Recrystallization Behavior of Giant Magnetostriction of Fe-Ga Thin Sheet
Received date: 2022-09-13
Revised date: 2023-02-17
Online published: 2023-04-23
Supported by
National Natural Science Foundation of China(52004164);National Natural Science Foundation of China(51931002);National Natural Science Foundation of China(51671049);Education Department Program of Liaoning Province(LQGD2020013)
The core issue in the study of giant magnetostriction of Fe-Ga alloy thin sheet is to obtain preferential texture through secondary recrystallization. In this work, the evolution of the texture, precipitation, and grain boundary characteristics of an Fe-Ga alloy thin sheet during the annealing process were investigated using XRD, SEM, EBSD, and TEM. The mechanism of the secondary recrystallization of the Goss ({110}<001>) texture in the Fe-Ga alloy thin sheet was analyzed. The results show that the primary recrystallized thin sheet is composed of strong γ-fibers and has a weak Goss texture. Moreover, high-density MnS and NbC precipitates of size 20-40 nm are dispersedly distributed in the matrix grains after primary recrystallization. The coarsening of the precipitates and a decrease in the volume fraction and density weaken the inhibiting force during the annealing process. The density of the precipitates inside the Goss grains is lower than that of the precipitates in the matrix grains with γ-texture during the process from primary recrystallization to secondary recrystallization. Before the occurrence of secondary recrystallization, Goss grains do not exhibit a number and size advantages over the matrix grains but are surrounded by higher-energy grain boundaries than the matrix grains. The differences between the Goss and matrix grains in terms of precipitation and high-energy grain boundary characteristics during primary recrystallization provide an additional driving force for the secondary recrystallization of Goss grains. Therefore, a perfect secondary recrystallization of the Goss texture with a saturation magnetostriction coefficient of 250 × 10‒6 is produced in the Fe-Ga alloy thin sheet without the introduction of the surface energy effect using a special annealing atmosphere.
Key words: Fe-Ga alloy; thin sheet; secondary recrystallization; texture; magnetostriction
ZHAI Xinya , HE Zhenghua , SHA Yuhui , ZHU Xiaofei , LI Feng , CHEN Lijia , ZUO Liang . Inhibitor and Secondary Recrystallization Behavior of Giant Magnetostriction of Fe-Ga Thin Sheet[J]. Acta Metall Sin, 2024 , 60(11) : 1559 -1570 . DOI: 10.11900/0412.1961.2022.00455
| 1 | Guruswamy S, Srisukhumbowornchai N, Clark A E, et al. Strong, ductile, and low-field-magnetostrictive alloys based on Fe-Ga [J]. Scr. Mater., 2000, 43: 239 |
| 2 | Kellogg R A, Russell A M, Lograsso T A, et al. Tensile properties of magnetostrictive iron-gallium alloys [J]. Acta Mater., 2004, 52: 5043 |
| 3 | Fu Q, Sha Y H, Zhang F, et al. Correlative effect of critical parameters for η recrystallization texture development in rolled Fe81Ga19 sheet: Modeling and experiment [J]. Acta Mater., 2019, 167: 167 |
| 4 | Ma T Y, Hu S S, Bai G H, et al. Structural origin for the local strong anisotropy in melt-spun Fe-Ga-Tb: Tetragonal nanoparticles [J]. Appl. Phys. Lett., 2015, 106: 112401 |
| 5 | Srisukhumbowornchai N, Guruswamy S. Crystallographic textures in rolled and annealed Fe-Ga and Fe-Al alloys [J]. Metall. Mater. Trans., 2004, 35A: 2963 |
| 6 | Na S M, Yoo J H, Flatau A B. Abnormal (110) grain growth and magnetostriction in recrystallized galfenol with dispersed niobium carbide [J]. IEEE Trans. Magn., 2009, 45: 4132 |
| 7 | Li J H, Gao X X, Zhu J, et al. Texture and magnetostriction in rolled Fe-Ga alloy [J]. Acta Metall. Sin., 2008, 44: 1031 |
| 李纪恒, 高学绪, 朱 洁 等. 轧制Fe-Ga合金的织构及磁致伸缩 [J]. 金属学报, 2008, 44: 1031 | |
| 8 | He Z H, Sha Y H, Fu Q, et al. Secondary recrystallization and magnetostriction in binary Fe81Ga19 thin sheets [J]. J. Appl. Phys., 2016, 119: 123904 |
| 9 | He Z H, Sha Y H, Shan N, et al. Secondary recrystallization Goss texture development in a binary Fe81Ga19 sheet induced by inherent grain boundary mobility [J]. Metals, 2019, 9: 1254 |
| 10 | Sun A L, Liu J H, Jiang C B. Recrystallization, texture evolution, and magnetostriction behavior of rolled (Fe81Ga19)98B2 sheets during low-to-high temperature heat treatments [J]. J. Mater. Sci., 2014, 49: 4565 |
| 11 | Jiang L P, Yang J D, Hao H B, et al. Giant enhancement in the magnetostrictive effect of FeGa alloys doped with low levels of terbium [J]. Appl. Phys. Lett., 2013, 102: 222409 |
| 12 | Na S M, Flatau A B. Single grain growth and large magnetostriction in secondarily recrystallized Fe-Ga thin sheet with sharp Goss (011)[100] orientation [J]. Scr. Mater., 2012, 66: 307 |
| 13 | Na S M, Flatau A B. Global Goss grain growth and grain boundary characteristics in magnetostrictive galfenol sheets [J]. Smart Mater. Struct., 2013, 22: 125026 |
| 14 | Yuan C, Li J H, Zhang W L, et al. Secondary recrystallization behavior in the rolled columnar-grained Fe-Ga alloys [J]. J. Magn. Magn. Mater., 2015, 391: 145 |
| 15 | Yuan C, Li J H, Bao X Q, et al. Influence of annealing process on texture evolution and magnetostriction in rolled Fe-Ga based alloys [J]. J. Magn. Magn. Mater., 2014, 362: 154 |
| 16 | Li J H, Zhang W L, Yuan C, et al. Inhibition force of precipitates for promoting abnormal grain growth in magnetostrictive Fe83Ga17-(B, NbC) alloy sheets [J]. Rare Met., 2017, 36: 886 |
| 17 | He Z H, Du H J, Sha Y H, et al. Secondary recrystallization texture and magnetostriction in Fe-Ga alloy ultra-thin sheet [J]. IEEE Trans. Magn., 2022, 58: 2501906 |
| 18 | He Z H, Hao H B, Sha Y H, et al. Sharp secondary recrystallization and large magnetostriction in Fe81Ga19 sheet induced by composite nanometer-sized inhibitors [J]. J. Magn. Magn. Mater., 2019, 478: 109 |
| 19 | Lei F, Sha Y H, He Z H, et al. Rapid secondary recrystallization of the Goss texture in Fe81Ga19 sheets using nanosized NbC particles [J]. Materials, 2021, 14: 3818 |
| 20 | Liu Y Y, Li J H, Mu X, et al. Strong NbC particle pinning for promoting abnormal growth of Goss grain in Fe82Ga4.5Al13.5 rolled sheets [J]. J. Magn. Magn. Mater., 2017, 444: 364 |
| 21 | Mao W M, Li Y, Guo W, et al. Influence of MnS particles inside grains on the boundary migration before secondary recrystallization of grain oriented electrical steels [J]. Solid State Phenom., 2010, 160: 247 |
| 22 | Mao W M, An Z G, Li S X. Influence of MnS particles on the behaviors of grain boundary migration in Fe-3%Si alloys [J]. Chin. Sci. Bull., 2009, 54: 4537 |
| 23 | He Z H, Du H J, Sha Y H, et al. Secondary recrystallization behavior in magnetostrictive Fe-Ga thin sheets induced by nano-sized composite precipitates [J]. AIP Adv., 2021, 11: 035313 |
| 24 | Fu Q, Sha Y H, He Z H, et al. Recrystallization texture and magnetostriction in binary Fe81Ga19 sheets [J]. Acta Metall. Sin., 2017, 53: 90 |
| 付 全, 沙玉辉, 和正华 等. Fe81Ga19二元合金薄板的再结晶织构与磁致伸缩性能 [J]. 金属学报, 2017, 53: 90 | |
| 25 | Zhao L J, Tian X, Yao Z Q, et al. Enhanced magnetostrictive properties of lightly Pr-doped Fe83Ga17 alloys [J]. J. Rare Earths, 2020, 38: 257 |
| 26 | He Z H, Sha Y H, Zhang F, et al. Development of strong η fiber recrystallization texture in rolled Fe81Ga19 thin sheet [J]. Metall. Mater. Trans., 2014, 45A: 129 |
| 27 | Park J T, Szpunar J A. Evolution of recrystallization texture in nonoriented electrical steels [J]. Acta Mater., 2003, 51: 3037 |
| 28 | Dorner D, Zaefferer S, Raabe D. Retention of the Goss orientation between microbands during cold rolling of an Fe3%Si single crystal [J]. Acta Mater., 2007, 55: 2519 |
| 29 | Dorner D, Zaefferer S, Lahn L, et al. Overview of microstructure and microtexture development in grain-oriented silicon steel [J]. J. Magn. Magn. Mater., 2006, 304: 183 |
| 30 | Samajdar I, Cicale S, Verlinden B, et al. Primary recrystallization in a grain oriented silicon steel: On the origin of Goss {110}<001> grains [J]. Scr. Mater., 1998, 39: 1083 |
| 31 | Hayakawa Y, Szpunar J A. A new model of Goss texture development during secondary recrystallization of electrical steel [J]. Acta Mater., 1997, 45: 4713 |
| 32 | Lin P, Palumbo G, Harase J, et al. Coincidence site lattice (CSL) grain boundaries and Goss texture development in Fe-3%Si alloy [J]. Acta Mater., 1996, 44: 4677 |
/
| 〈 |
|
〉 |