Corrosion Behavior of NbC and Its Effect on Corrosion Layer Formation in Liquid Lead-Bismuth Eutectic of Nb-Containing Austenitic Stainless Steel
Received date: 2022-12-30
Revised date: 2023-02-28
Online published: 2023-04-23
Supported by
National Natural Science Foundation of China(51871218);LingChuang Research Project of China National Nuclear Corporation
The lead-cooled fast reactor is considered one of the promising Generation IV nuclear energy systems. Structural materials used in the construction of pressure vessels and internals for this reactor include 300 series austenitic stainless steels. Nb-containing austenitic stainless steels are developed to improve corrosion properties, mechanical properties, and irradiation resistance. However, coarse primary NbC carbides are formed during solidification in these steels and cannot be eliminated through subsequent hot working and heat treatment. Recently, researchers have found different oxidation behaviors between secondary phase particles and the matrix, which affect the material's corrosion properties. However, the oxidation behaviors of primary NbC are rarely reported. This study analyzes the corrosion behaviors of a solution-treated Nb-containing austenitic stainless steel plate after exposure to oxygen-saturated liquid lead-bismuth eutectic (LBE) at 550 and 600 oC using SEM, EPMA, XRD, and TEM. The results show that the oxidation probability of NbC is correlated with its location in the samples at 550 oC. NbC at the initial surface is easily oxidized, while NbC within the interior is difficult to oxidize due to the low equilibrium oxygen partial pressure in the inner oxide layer, which suppresses the oxidation of NbC. However, NbC at the initial surface and within the interior are prone to be oxidized as the temperature increases to 600 oC. Compared to the matrix, NbC oxidizes into Nb2O5, resulting in a higher Pilling-Bedworth ratio (PBR). This leads to high compressive stress and resultant microcrack formation in the surrounding oxide layer. Additionally, the presence of CO2 generated during the oxidation of NbC within the interior reduces the compactness of the oxide layer, leading to a higher growth rate.
WU Yang , XIE Ang , CHEN Shenghu , JIANG Haichang , RONG Lijian . Corrosion Behavior of NbC and Its Effect on Corrosion Layer Formation in Liquid Lead-Bismuth Eutectic of Nb-Containing Austenitic Stainless Steel[J]. Acta Metall Sin, 2025 , 61(2) : 287 -296 . DOI: 10.11900/0412.1961.2022.00650
| 1 | Alemberti A, Smirnov V, Smith C F, et al. Overview of lead-cooled fast reactor activities [J]. Prog. Nucl. Energy, 2014, 77: 300 |
| 2 | Yvon P, Carré F. Structural materials challenges for advanced reactor systems [J]. J. Nucl. Mater., 2009, 385: 217 |
| 3 | Chen S H, Xie A, Lv X L, et al. Tailoring microstructure of austenitic stainless steel with improved performance for generation-IV fast reactor application: A review [J]. Crystals, 2023, 13: 268 |
| 4 | Dalle F, Blat-Yrieix M, Dubiez-Le Goff S, et al. Conventional austenitic steels as out-of-core materials for Generation IV nuclear reactors [A]. Structural Materials for Generation IV Nuclear Reactors [M]. Amsterdam: Woodhead Publishing, 2017: 595 |
| 5 | Wang Q Y, Chen S H, Rong L J. δ-ferrite formation and its effect on the mechanical properties of heavy-section AISI 316 stainless steel casting [J]. Metall. Mater. Trans., 2020, 51A: 2998 |
| 6 | Wang Q Y, Chen S H, Lv X L, et al. Role of δ-ferrite in fatigue crack growth of AISI 316 austenitic stainless steel [J]. J. Mater. Sci. Technol., 2022, 114: 7 |
| 7 | Lv X L, Chen S H, Wang Q Y, et al. Temperature dependence of fracture behavior and mechanical properties of AISI 316 austenitic stainless steel [J]. Metals, 2022, 12: 1421 |
| 8 | Chen S H, Wang Q Y, Jiang H C, et al. Effect of δ-ferrite on hot deformation and recrystallization of 316KD austenitic stainless steel for sodium-cooled fast reactor application [J]. Acta Metall. Sin., 2024, 60: 367 |
| 陈胜虎, 王琪玉, 姜海昌 等. δ-铁素体对钠冷快堆用316KD奥氏体不锈钢热变形行为和动态再结晶的影响 [J]. 金属学报, 2024, 60: 367 | |
| 9 | Aydo?du G H, Aydinol M K. Determination of susceptibility to intergranular corrosion and electrochemical reactivation behaviour of AISI 316L type stainless steel [J]. Corros. Sci., 2006, 48: 3565 |
| 10 | Padilha A F, Escriba D M, Materna-Morris E, et al. Precipitation in AISI 316L(N) during creep tests at 550 and 600 oC up to 10 years [J]. J. Nucl. Mater., 2007, 362: 132 |
| 11 | Vach M, Kuníková T, Dománková M, et al. Evolution of secondary phases in austenitic stainless steels during long-term exposures at 600, 650 and 800 oC [J]. Mater. Charact., 2008, 59: 1792 |
| 12 | Plaut R L, Herrera C, Escriba D M, et al. A short review on wrought austenitic stainless steels at high temperatures: Processing, microstructure, properties and performance [J]. Mater. Res., 2007, 10: 453 |
| 13 | Perron A, Toffolon-Masclet C, Ledoux X, et al. Understanding sigma-phase precipitation in a stabilized austenitic stainless steel (316Nb) through complementary CALPHAD-based and experimental investigations [J]. Acta Mater., 2014, 79: 16 |
| 14 | Carroll M C, Carroll L J. Fatigue and creep-fatigue deformation of an ultra-fine precipitate strengthened advanced austenitic alloy [J]. Mater. Sci. Eng., 2012, A556: 864 |
| 15 | Taylor M, Ramirez J, Charit I, et al. Creep behavior of Alloy 709 at 700 oC [J]. Mater. Sci. Eng., 2019, A762: 138083 |
| 16 | Uehira A, Mizuta S, Ukai S, et al. Irradiation creep of 11Cr-0.5 Mo-2W, V, Nb ferritic-martensitic, modified 316, and 15Cr-20Ni austenitic S.S. irradiated in FFTF to 103-206 dpa [J]. J. Nucl. Mater., 2000, 283-287: 396 |
| 17 | Xie A, Chen S H, Wu Y, et al. Homogenization temperature dependent microstructural evolution and mechanical properties in a Nb-stabilized cast austenitic stainless steel [J]. Mater. Charact., 2022, 194: 112384 |
| 18 | Proff C, Abolhassani S, Lemaignan C. Oxidation behaviour of zirconium alloys and their precipitates—A mechanistic study [J]. J. Nucl. Mater., 2013, 432: 222 |
| 19 | Wang Z, Zhou B X, Wang B Y, et al. Second phase particles and their corrosion behavior of Zr-0.72Sn-0.32Fe-0.15Cr-0.97Nb alloy [J]. Acta Metall. Sin., 2016, 52: 78 |
| 王 桢, 周邦新, 王波阳 等. Zr-0.72Sn-0.32Fe-0.15Cr-0.97Nb合金中的第二相及其腐蚀行为 [J]. 金属学报, 2016, 52: 78 | |
| 20 | Chen S H, Rong L J. Oxidation behavior of intermetallic phase and its contribution to the oxidation resistance in Fe-Cr-Zr ferritic alloy [J]. Metals, 2022, 12: 827 |
| 21 | Wu X Q, Rong L J, Tan J B, et al. Research advance on liquid lead-bismuth eutectic corrosion resistant Si enhanced ferritic/martensitic and austenitic stainless steels [J]. Acta Metall. Sin., 2023, 59: 502 |
| 吴欣强, 戎利建, 谭季波 等. 耐Pb-Bi腐蚀Si增强型铁素体/马氏体钢和奥氏体不锈钢的研究进展 [J]. 金属学报, 2023, 59: 502 | |
| 22 | Chen S H, Rong L J. Oxide scale formation on ultrafine-grained ferritic-martensitic steel during pre-oxidation and its effect on the corrosion performance in stagnant liquid Pb-Bi eutectic [J]. Acta Metall. Sin., 2021, 57: 989 |
| 陈胜虎, 戎利建. 超细晶铁素体-马氏体钢的高温氧化成膜特性及其对Pb-Bi腐蚀行为的影响 [J]. 金属学报, 2021, 57: 989 | |
| 23 | Martinelli L, Balbaud-Célérier F, Terlain A, et al. Oxidation mechanism of a Fe-9Cr-1Mo steel by liquid Pb-Bi eutectic alloy (Part I) [J]. Corros. Sci., 2008, 50: 2523 |
| 24 | Charalampopoulou E, Delville R, Verwerft M, et al. Transmission electron microscopy study of complex oxide scales on DIN 1.4970 steel exposed to liquid Pb-Bi eutectic [J]. Corros. Sci., 2019, 147: 22 |
| 25 | Moulder J F, Stickle W F, Sobol P E, et al. Handbook of X-ray Photoelectron Spectroscopy [M]. 2nd Ed., Eden Prairie, Minnesota: Perkin-Elmer Corporation, 1992: 28 |
| 26 | Martinelli L, Balbaud-Célérier F, Picard G, et al. Oxidation mechanism of a Fe-9Cr-1Mo steel by liquid Pb-Bi eutectic alloy (Part III) [J]. Corros. Sci., 2008, 50: 2549 |
| 27 | Wang J, Lu S P, Rong L J, et al. Effect of silicon on the oxidation resistance of 9 wt.% Cr heat resistance steels in 550 oC lead-bismuth eutectic [J]. Corros. Sci., 2016, 111: 13 |
| 28 | Hong J K, Park N K, Kim S J, et al. Microstructures of oxidized primary carbides on superalloy Inconel 718 [J]. Mater. Sci. Forum, 2005, 502: 249 |
| 29 | Ye Z F, Wang P, Li D Z, et al. M23C6 precipitates induced inhomogeneous distribution of silicon in the oxide formed on a high-silicon ferritic/martensitic steel [J]. Scr. Mater., 2015, 97: 45 |
| 30 | Li M S, Qian Y H, Xin L. Volume Ratio of an oxide to the metal [J]. Corros. Sci. Prot. Technol., 1999, 11: 284 |
| 李美栓, 钱余海, 辛 丽. 合金上氧化物的体积比的分析 [J]. 腐蚀科学与防护技术, 1999, 11: 284 | |
| 31 | Xu C H, Gao W. Pilling-Bedworth ratio for oxidation of alloys [J]. Mater. Res. Innov., 2000, 3: 231 |
/
| 〈 |
|
〉 |