Research paper

Phase Transformation Behaviors in the Heat-Affected Zones of Ferritic Heat-Resistant Steels Enabled by In Situ CSLM Observation

  • SHEN Yang ,
  • GU Zhengman ,
  • WANG Cong
Expand
  • 1 School of Metallurgy, Northeastern University, Shenyang 110819, China
    2 Jiangxi Key Laboratory of Forming and Joining Technology for Aerospace Components, Nanchang Hangkong University, Nanchang 330063, China
WANG Cong, professor, Tel: 15702435155, E-mail: wangc@smm.neu.edu.cn

Received date: 2023-02-07

  Revised date: 2023-04-06

  Online published: 2023-04-23

Supported by

National Key Research and Development Program of China(2022YFE0123300);National Natural Science Foundation of China(U20A20277;52050410341;52150610494);Jiangxi Provincial Natural Science Foundation(20232BAB214054)

Abstract

Fossil-fired thermal power generation has dominated China's electricity production for a long time, contributing to around 70% of the total capacity. Developing long-life ultra-supercritical thermal power units is essential for improving coal-fired power generation efficiency, reducing harmful gas emissions, and achieving national energy conservation and emission reduction targets. The assembly and manufacture of advanced heat-resistant steel grades are required to address the above demands, serving as crucial components driving the technological advancement of thermal power units. Heat-resistant steel grades P11, P22, and P91, which are Cr-Mo based ferritic, possess a range of highly attractive properties, such as excellent mechanical properties, excellent corrosion resistance, and relatively low construction costs. These steel grades are widely used in pressure vessels and pipelines focused on high-temperature applications. Fusion welding techniques are invariably necessary to weld such heat-resistant-grade steels before they are positioned in high-temperature service. However, it is worth noting that drastic solid-state phase transformations in the heat-affected zones (HAZs) during thermal welding cycles can profoundly influence the heterogeneous microstructures of welded joints, determining their final mechanical properties to a large extent. Furthermore, it seriously threatens the safe and stable operation of thermal power plants. High-temperature confocal scanning laser microscopy (CSLM) revolutionized traditional metallographic experiments, enabling real-time morphology and quantitative analysis tracking. This innovation has facilitated investigations into the kinetic phase transformation process and microstructure evolution in steels at high temperatures. In this work, the kinetics of phase transformation and microstructural evolution in the HAZs of P11, P22, and P91 ferritic heat-resistant steels during continuous cooling processes were systematically investigated using CSLM. The results revealed that bainite laths preferentially nucleate in the order of increasing difficulty in the energy barrier on austenite grain boundaries, inclusions, internal grain distortion areas, previous bainite laths, and grain interiors. Meanwhile, the growth characteristics of bainite/martensite laths were documented as the phase transformation progressed. It is revealed that bainite laths attach to prior austenite grain boundaries and the previous bainite, while martensite laths grow radially inside the prior austenite grains. Both bainite and martensite laths cease growing when they encounter grain boundaries or other laths, eventually forming an interlocking microstructure. Additionally, the growth rates of bainite/martensite laths in the HAZs of P11, P22, and P91 ferritic heat-resistant steels exhibited considerable variations as the temperature decreased. The analysis revealed that as the temperature decreased, the growth rate of laths in the coarse-grained heat-affected zone was considerably higher than that in the fine-grained heat-affected zone, which can be attributed to the increase in the degree of supercooling and prior austenite grain size.

Cite this article

SHEN Yang , GU Zhengman , WANG Cong . Phase Transformation Behaviors in the Heat-Affected Zones of Ferritic Heat-Resistant Steels Enabled by In Situ CSLM Observation[J]. Acta Metall Sin, 2024 , 60(6) : 802 -816 . DOI: 10.11900/0412.1961.2023.00045

References

1 Liu Z D, Chen Z Z, He X K, et al. Systematical innovation of heat resistant materials used for 630-700oC advanced ultra-supercritical (A-USC) fossil fired boilers [J]. Acta Metall. Sin., 2020, 56: 539
  刘正东, 陈正宗, 何西扣 等. 630~700℃超超临界燃煤电站耐热管及其制造技术进展 [J]. 金属学报, 2020, 56: 539
2 He H S, Yu L M, Liu C X, et al. Research progress of a novel martensitic heat-resistant steel G115 [J]. Acta Metall. Sin., 2022, 58: 311
  何焕生, 余黎明, 刘晨曦 等. 新一代马氏体耐热钢G115的研究进展 [J]. 金属学报, 2022, 58: 311
3 Liu Z D, Cheng S C, Bao H S, et al. Localization of boiler steel technology in China used for ultra super critical power plants [J]. Iron Steel, 2009, 44(6): 1
  刘正东, 程世长, 包汉生 等. 超超临界火电机组用锅炉钢技术国产化问题 [J]. 钢铁, 2009, 44(6): 1
4 Liu Z D, Cheng S C, Tang G B, et al. The state-of-the-art of steel technology used for Chinese power plants and its future [J]. Iron Steel, 2011, 46(3): 1
  刘正东, 程世长, 唐广波 等. 中国电站用钢技术现状和未来发展 [J]. 钢铁, 2011, 46(3): 1
5 Laha K, Chandravathi K S, Parameswaran P, et al. Type IV cracking susceptibility in weld joints of different grades of Cr-Mo ferritic steel [J]. Metall. Mater. Trans., 2009, 40A: 386
6 Hua Y, Chen J G, Yu L M, et al. Microstructure evolution and mechanical properties of dissimilar material diffusion-bonded joint for high Cr ferrite heat-resistant steel and austenitic heat-resistant steel [J]. Acta Metall. Sin., 2022, 58: 141
  化 雨, 陈建国, 余黎明 等. 高Cr铁素体耐热钢与奥氏体耐热钢的异种材料扩散连接接头组织演变及力学性能 [J]. 金属学报, 2022, 58: 141
7 Zou X D, Zhao D P, Sun J C, et al. An integrated study on the evolution of inclusions in EH36 shipbuilding steel with Mg addition: From casting to welding [J]. Metall. Mater. Trans., 2018, 49B: 481
8 Shen Y, Leng J, Wang C. On the heterogeneous microstructure development in the welded joint of 12MnNiVR pressure vessel steel subjected to high heat input electrogas welding [J]. J. Mater. Sci. Technol., 2019, 35: 1747
9 Wu Y W, Yuan X B, Kaldre I, et al. TiO2-assisted microstructural variations in the weld metal of EH36 shipbuilding steel subject to high heat input submerged arc welding [J]. Metall. Mater. Trans., 2023, 54B: 50
10 Wang Y Y, Kannan R, Zhang L, et al. Microstructural analysis of the as-welded heat-affected zone of a grade 91 steel heavy section weldment [J]. Weld. J., 2017, 96: 203
11 Lee K, Lee S, Na H, et al. Ghost microstructure evolution and identification in the coarse grain heat affected zone of 2.25Cr-1Mo-V-Ti steel using tint etching [J]. Mater. Charact., 2016, 121: 31
12 Abd El-Azim M E, Ibrahim O H, El-Desoky O E. Long term creep behaviour of welded joints of P91 steel at 650oC [J]. Mater. Sci. Eng., 2013, A560: 678
13 Wang X, Wang X, Zhang Y L, et al. Microstructure and creep fracture behavior in HR3C/T92 dissimilar steel welds [J]. Mater. Sci. Eng., 2021, A799: 140128
14 Wang C, Zhang J. Fine-tuning weld metal compositions via flux optimization in submerged arc welding: an overview [J]. Acta Metall. Sin., 2021, 57: 1126
  王 聪, 张 进. 埋弧焊中焊剂对焊缝金属成分调控的研究进展 [J]. 金属学报, 2021, 57: 1126
15 Wang Y Y, Kannan R, Li L J. Characterization of as-welded microstructure of heat-affected zone in modified 9Cr-1Mo-V-Nb steel weldment [J]. Mater. Charact., 2016, 118: 225
16 Quidort D, Brechet Y J M. A model of isothermal and non isothermal transformation kinetics of bainite in 0.5%C steels [J]. ISIJ Int., 2002, 42: 1010
17 Ueshima Y, Mizoguchi S, Matsumiya T, et al. Analysis of solute distribution in dendrites of carbon steel with δ/γ transformation during solidification [J]. Metall. Mater. Trans., 1986, 17B: 845
18 Mayr P, Palmer T A, Elmer J W, et al. Formation of delta ferrite in 9 wt pct Cr steel investigated by in-situ X-ray diffraction using synchrotron radiation [J]. Metall. Mater. Trans., 2010, 41A: 2462
19 Yu X H, Babu S S, Lippold J C, et al. In-situ observations of martensitic transformation in blast-resistant steel [J]. Metall. Mater. Trans., 2012, 43A: 1538
20 Mu W Z, Hedstr?m P, Shibata H, et al. High-temperature confocal laser scanning microscopy studies of ferrite formation in inclusion-engineered steels: A review [J]. JOM, 2018, 70: 2283
21 Shen Y, Chen B, Wang C. In situ observation and growth kinetics of bainite laths in the coarse-grained heat-affected zone of 2.25Cr-1Mo heat-resistant steel during simulated welding [J]. Metall. Mater. Trans., 2021, 52A: 14
22 Xuan C J, Mu W Z. Dissolution kinetics of arbitrarily-shaped alumina in oxide melt: An integration of phase-field modelling and real-time observation study [J]. J. Alloys Compd., 2020, 834: 155168
23 Mu W Z, Shibata H, Hedstr?m P, et al. Ferrite formation dynamics and microstructure due to inclusion engineering in low-alloy steels by Ti2O3 and TiN addition [J]. Metall. Mater. Trans., 2016, 47B: 2133
24 Zou X D, Sun J C, Matsuura H, et al. In situ observation of the nucleation and growth of ferrite laths in the heat-affected zone of EH36-Mg shipbuilding steel subjected to different heat inputs [J]. Metall. Mater. Trans., 2018, 49B: 2168
25 Ko T, Cottrell S A. The formation of bainite [J]. J. Iron Steel Inst., 1952, 172: 307
26 Terasaki H, Komizo Y I. Diffusional and displacive transformation behaviour in low carbon-low alloy steels studied by a hybrid in situ observation system [J]. Scr. Mater., 2011, 64: 29
27 Swallow E, Bhadeshia H K D H. High resolution observations of displacements caused by bainitic transformation [J]. Mater. Sci. Technol., 1996, 12: 121
28 Bhadeshia H K D H, Christian J W. Bainite in steels [J]. Metall. Mater. Trans., 1990, 21A: 767
29 Chang L C, Bhadeshia H K D H. Microstructure of lower bainite formed at large undercoolings below bainite start temperature [J]. Mater. Sci. Technol., 1996, 12: 233
30 Singh K, Kumar A, Singh A. Effect of prior austenite grain size on the morphology of nano-bainitic steels [J]. Metall. Mater. Trans., 2018, 49A: 1348
31 Ricks R A, Howell P R, Barritte G S. The nature of acicular ferrite in HSLA steel weld metals [J]. J. Mater. Sci., 1982, 17: 732
32 Mao C L, Liu C X, Yu L M, et al. Discontinuous lath martensite transformation and its relationship with annealing twin of parent austenite and cooling rate in low carbon RAFM steel [J]. Mater. Des., 2021, 197: 109252
33 Samanta S, Biswas P, Giri S, et al. Formation of bainite below the MS temperature: Kinetics and crystallography [J]. Acta Mater., 2016, 105: 390
34 Xu Z Y, Jin X J, Zhang J H, et al. Phase Transformation in Materials [M]. Beijing: Higher Education Press, 2013: 87
  徐祖耀, 金学军, 张骥华 等. 材料相变 [M]. 北京: 高等教育出版社, 2013: 87
35 Sarizam M, Komizo Y. Effects of holding temperature on bainite transformation in Cr-Mo steel [J]. J. Mech. Eng. Sci., 2014, 7: 1103
36 Zhang S H, Hattori N, Enomoto M, et al. Ferrite nucleation at ceramic/austenite interfaces [J]. ISIJ Int., 1996, 36: 1301
37 Mao G J, Cao R, Guo X L, et al. In situ observation of kinetic processes of lath bainite nucleation and growth by laser scanning confocal microscope in reheated weld metals [J]. Metall. Mater. Trans., 2017, 48A: 5783
38 Pan X Q, Zhi J J, Fan Z J, et al. Morphology and crystallography of microstructures in Mg-deoxidized offshore engineering steels after simulated welding thermal cycles [J]. Ironmak. Steelmak., 2022, 49: 541
39 Hu H J, Xu G, Nabeel M, et al. In situ study on interrupted growth behavior and crystallography of bainite [J]. Metall. Mater. Trans., 2021, 52A: 817
40 Lee S J, Park J S, Lee Y K. Effect of austenite grain size on the transformation kinetics of upper and lower bainite in a low-alloy steel [J]. Scr. Mater., 2008, 59: 87
41 Chen R C, Zheng Z Z, Li N, et al. In-situ investigation of phase transformation behaviors of 300M steel in continuous cooling process [J]. Mater. Charact., 2018, 144: 400
42 Luo H W, Wang X H, Liu Z B, et al. Influence of refined hierarchical martensitic microstructures on yield strength and impact toughness of ultra-high strength stainless steel [J]. J. Mater. Sci. Technol., 2020, 51: 130
43 Furuhara T, Kawata H, Morito S, et al. Crystallography of upper bainite in Fe-Ni-C alloys [J]. Mater. Sci. Eng., 2006, A431: 228
44 Terasaki H, Komizo Y I. Correlation between the microstructural development of bainitic ferrite and the characteristics of martensite-austenite constituent [J]. Metall. Mater. Trans., 2013, 44A: 5289
45 Wright S I, Nowell M M, Field D P. A review of strain analysis using electron backscatter diffraction [J]. Microsc. Microanal., 2011, 17: 316
46 Saraf L. Kernel average misorientation confidence index correlation from FIB sliced Ni-Fe-Cr alloy surface [J]. Microsc. Microanal., 2011, 17: 424
47 Kang S, Yoon S, Lee S J. Prediction of bainite start temperature in alloy steels with different grain sizes [J]. ISIJ Int., 2014, 54: 997
48 Zheng Y F, Wu R M, Li X C, et al. Continuous cooling transformation behaviour and bainite formation kinetics of new bainitic steel [J]. Mater. Sci. Technol., 2017, 33: 454
49 Steven W, Haynes A G. The temperature of formation of martensite and bainite in low-alloy steels [J]. J. Iron Steel Inst., 1956, 183: 349
50 Andrews K W. Empirical formulae for the calculation of some transformation temperatures [J]. J. Iron Steel Inst., 1965, 203: 721
51 Hu Z W, Xu G, Hu H J, et al. In situ measured growth rates of bainite plates in an Fe-C-Mn-Si superbainitic steel [J]. Int. J. Miner. Metall. Mater., 2014, 21: 371
52 Lambert-Perlade A, Gourgues A F, Pineau A. Austenite to bainite phase transformation in the heat-affected zone of a high strength low alloy steel [J]. Acta Mater., 2004, 52: 2337
53 Endo A, Chauhan H S, Nakamura Y, et al. Relationship between growth rate and undercooling in Pt-added Y1Ba2Cu3O7 - x [J]. J. Mater. Res., 1996, 11: 1114
54 Liang G F, Ali Y, You G Q, et al. Effect of cooling rate on grain refinement of cast aluminium alloys [J]. Materialia, 2018, 3: 113
55 Celada-Casero C, Sietsma J, Santofimia M J. The role of the austenite grain size in the martensitic transformation in low carbon steels [J]. Mater. Des., 2019, 167: 107625
56 Hu F, Hodgson P D, Wu K M. Acceleration of the super bainite transformation through a coarse austenite grain size [J]. Mater. Lett., 2014, 122: 240
57 Xu G, Liu F, Wang L, et al. A new approach to quantitative analysis of bainitic transformation in a superbainite steel [J]. Scr. Mater., 2013, 68: 833
58 Liu D K, Yang J, Zhang Y H. In-situ observation of bainite transformation in CGHAZ of 420 MPa grade offshore engineering steel with different Mo contents [J]. ISIJ Int., 2022, 62: 714
59 Kong J H, Xie C S. Effect of molybdenum on continuous cooling bainite transformation of low-carbon microalloyed steel [J]. Mater. Des., 2006, 27: 1169
60 Hu H J, Xu G, Zhou M X, et al. Effect of Mo content on microstructure and property of low-carbon bainitic steels [J]. Metals, 2016, 6: 173
Outlines

/