Effect of Combined Addition of B and Zr on the Fluidity of IN718 Superalloy
Received date: 2022-10-12
Revised date: 2022-11-14
Online published: 2023-03-28
Supported by
National Natural Science Foundation of China(51904218);National Natural Science Foundation of China(52031012)
The fluidity of superalloy is an important property in the manufacture of large thin-walled and complex structure castings, but superalloys show high viscosity and a wide solidification temperature range, which may lead to serious defects, low yield, and poor performance. Therefore, the manufacturing of these castings is important to improve the fluidity by regulating the alloy composition. B and Zr, as common elements in superalloys, have important effects on solidification, microstructure, and mechanical properties. However, the effect of B and Zr on the fluidity and mechanism of superalloys remain unclear. In this study, the spiral fluidity test, high-temperature confocal laser scanning microscopy, and double-thermocouple method were used to investigate the fluidity, solidification, dendrite coherency point temperature, and stress rupture property of the IN718 superalloy with various B and Zr contents, whereas the mechanism of the effect of B and Zr on fluidity was also discussed. Results show that the combined addition of B and Zr can improve the fluidity and high-temperature stress rupture property of the IN718 superalloy. At different pouring temperatures, the fluidity of the alloy increases with the increase of B and Zr contents. The optimum fluidity is obtained with 0.0059%B and 0.042%Zr (mass fraction), respectively, which is about 90% higher than that of the original alloy and increases the stress rupture life by 77%. In the IN718 superalloy with a high content of B and Zr, the dendrite growth rate in the mushy zone is low, which reduces the dendrite coherency point temperature (TDCP), increases the difference between liquidus temperature (TL) and TDCP (TL- TDCP), delays the dendrite coherency, and improves the melt fluidity.
JIE Ziqi , LIU Dingyuan , $\boxed{\hbox{Zhang Jun}}$ . Effect of Combined Addition of B and Zr on the Fluidity of IN718 Superalloy[J]. Acta Metall Sin, 2024 , 60(12) : 1615 -1621 . DOI: 10.11900/0412.1961.2022.00508
| 1 | Zhang J, Jie Z Q, Huang T W, et al. Research and development of equiaxed grain solidification and forming technology for nickel-based cast superalloys [J]. Acta Metall. Sin., 2019, 55: 1145 |
| 张 军, 介子奇, 黄太文 等. 镍基铸造高温合金等轴晶凝固成形技术的研究和进展 [J]. 金属学报, 2019, 55: 1145 | |
| 2 | Sun B D, Wang J, Kang M D, et al. Investment casting technology and development trend of superalloy ultra limit components [J]. Acta Metall. Sin., 2022, 58: 412 |
| 孙宝德, 王 俊, 康茂东 等. 高温合金超限构件精密铸造技术及发展趋势 [J]. 金属学报, 2022, 58: 412 | |
| 3 | Zielińska M, Yavorska M, Por?ba M, et al. Thermal properties of cast nickel based superalloys [J]. Arch. Mater. Sci. Eng., 2010, 44: 35 |
| 4 | El-Bagoury N. Ni based superalloy: Casting technology, metallurgy, development, properties and applications [J]. Int. J. Eng. Sci. Res. Technol., 2016, 5: 108 |
| 5 | Jie Z Q, Zhang J, Huang T W, et al. Effects of boron and zirconium additions on the fluidity, microstructure and mechanical properties of IN718C superalloy [J]. J. Mater. Res., 2016, 31: 3557 |
| 6 | Moosavy H N, Aboutalebi M R, Seyedein S H, et al. A solidification model for prediction of castability in the precipitation-strengthened nickel-based superalloys [J]. J. Mater. Process. Technol., 2013, 213: 1875 |
| 7 | Zhang J, Singer R F. Effect of Zr and B on castability of Ni-based superalloy IN792 [J]. Metall. Mater. Trans., 2004, 35A: 1337 |
| 8 | Qi F, Yu L X, Zhao G D, et al. Effect of Zr on solidification segregation behavior of K417G alloy and its anomalous effect during rapid cooling process [J]. J. Alloys Compd., 2020, 835: 155243 |
| 9 | Zhao G D, Yu L X, Yang G L, et al. The role of boron in modifying the solidification and microstructure of nickel-base alloy U720Li [J]. J. Alloys Compd., 2016, 686: 194 |
| 10 | Zhou Y, Wang B, Li S P, et al. On the segregation behavior and influences of minor alloying element Zr in nickel-based superalloys [J]. J. Alloys Compd., 2022, 897: 163169 |
| 11 | Heydari D, Fard A S, Bakhshi A, et al. Hot tearing in polycrystalline Ni-based IN738LC superalloy: Influence of Zr content [J]. J. Mater. Process. Technol., 2014, 214: 681 |
| 12 | Kontis P, Alabort E, Barba D, et al. On the role of boron on improving ductility in a new polycrystalline superalloy [J]. Acta Mater., 2017, 124: 489 |
| 13 | Hosseini S A, Madar K Z, Abbasi S M. Effect of homogenization heat treatments on the cast structure and tensile properties of nickel-base superalloy ATI 718Plus in the presence of boron and zirconium additions [J]. Mater. Sci. Eng., 2017, A689: 103 |
| 14 | Li X X, Ou M Q, Wang M, et al. Effect of boron addition on the microstructure and mechanical properties of K4750 nickel-based superalloy [J]. J. Mater. Sci. Technol., 2021, 60: 177 |
| 15 | Theska F, Buerstmayr R, Liu H, et al. Influence of grain boundary precipitation and segregation on cracking of cast and wrought superalloys containing B and Zr [J]. Mater. Charact., 2022, 187: 111881 |
| 16 | Zhang J, Jie Z Q, Liu M N, et al. A method for preparing fluidity testing mould and sample of superalloy [P]. Chin Pat, 114279802A, 2022 |
| 张 军, 介子奇, 刘淼楠 等. 一种高温合金流动性测试模具及测试试样的制备方法 [P]. 中国专利, 114279802A, 2022 | |
| 17 | Yan X W, Xu Q Y, Liu Q W, et al. Dendrite growth in nickel-based superalloy with in-situ observation by high temperature confocal laser scanning microscopy and numerical simulation [J]. Mater. Lett., 2021, 286: 129213 |
| 18 | Miao Z J, Shan A D, Wang W, et al. Solidification process of conventional superalloy by confocal scanning laser microscope [J]. Trans. Nonferrous Metals Soc. China, 2011, 21: 236 |
| 19 | Shin J S, Ko S H, Kim K T. Development and characterization of low-silicon cast aluminum alloys for thermal dissipation [J]. J. Alloys Compd., 2015, 644: 673 |
| 20 | Stangeland A, Mo A, Nielsen ?, et al. Development of thermal strain in the coherent mushy zone during solidification of aluminum alloys [J]. Metall. Mater. Trans., 2004, 35A: 2903 |
| 21 | Malekan M, Shabestari S G. Effect of grain refinement on the dendrite coherency point during solidification of the A319 aluminum alloy [J]. Metall. Mater. Trans., 2009, 40A: 3196 |
| 22 | Arnberg L, Chai G, Backerud L. Determination of dendritic coherency in solidifying melts by rheological measurements [J]. Mater. Sci. Eng., 1993, A173: 101 |
| 23 | Hong H U, Kim I S, Choi B G, et al. On the role of grain boundary serration in simulated weld heat-affected zone liquation of a wrought nickel-based superalloy [J]. Metall. Mater. Trans., 2012, 43A: 173 |
| 24 | Ebner A S, Jakob S, Clemens H, et al. Grain boundary segregation in Ni-base alloys: A combined atom probe tomography and first principles study [J]. Acta Mater., 2021, 221: 117354 |
| 25 | Yeh A C, Lu K W, Kuo C M, et al. Effect of serrated grain boundaries on the creep property of Inconel 718 superalloy [J]. Mater. Sci. Eng., 2011, A530: 525 |
| 26 | Tsai Y L, Wang S F, Bor H Y, et al. Effects of Zr addition on the microstructure and mechanical behavior of a fine-grained nickel-based superalloy at elevated temperatures [J]. Mater. Sci. Eng., 2014, A607: 294 |
| 27 | Yan B C, Zhang J, Lou L H. Effect of boron additions on the microstructure and transverse properties of a directionally solidified superalloy [J]. Mater. Sci. Eng., 2008, A474: 39 |
| 28 | Xiao L, Chaturvedi M C, Chen D L. Effect of boron and carbon on the fracture toughness of IN 718 superalloy at room temperature and 650oC [J]. J. Mater. Eng. Perform., 2005, 14: 528 |
| 29 | Flemings M C. Solidification processing [J]. Metall. Trans., 1974, 5: 2121 |
| 30 | Campbell J. Castings [M]. 2nd ed. Oxford: Butterworth-Heinemann, 2003: 70 |
| 31 | Farahany S, Idris M H, Ourdjini A, et al. Evaluation of the effect of grain refiners on the solidification characteristics of an Sr-modified ADC12 die-casting alloy by cooling curve thermal analysis [J]. J. Therm. Anal. Calorim., 2015, 119: 1593 |
| 32 | Grodzki J, Hartmann N, Rettig R, et al. Effect of B, Zr, and C on hot tearing of a directionally solidified nickel-based superalloy [J]. Metall. Mater. Trans., 2016, 47A: 2914 |
| 33 | Liu Q M, Huang S Z, Liu F, et al. Effect of boron content on microstructure evolution during solidification and mechanical properties of K417G alloy [J]. Acta Metall. Sin., 2019, 55: 720 |
| 刘巧沐, 黄顺洲, 刘 芳 等. B含量对K417G合金凝固过程中组织演变和力学性能的影响 [J]. 金属学报, 2019, 55: 720 |
/
| 〈 |
|
〉 |