Molecular Dynamics Simulation of Thermo-Kinetics of Tensile Deformation of α-Fe Single Crystal
Received date: 2022-11-30
Revised date: 2023-02-21
Online published: 2023-03-21
Supported by
National Natural Science Foundation of China(52130110)
The microstructure and deformation mechanisms determine the strength and plasticity of structural materials. Specifically, the nucleation and movement of dislocations play a crucial role in the plastic deformation processing of crystalline materials. Just like the phase transformation, the plastic deformation and evolution of dislocations can be described as a kinetic behavior resulting from a thermodynamic driving force. In recent years, this research group has introduced the concept of thermo-dynamic correlation,which reflects the correlation between thermodynamics and kinetics as a trade-off relationship between thermodynamic driving forces (ΔG) and kinetic energy barriers (Q). It was found that an increase in ΔG is always accompanied by a decrease in Q in the processes of phase transformations and plastic deformations, and vice versa. Based on the so-called synergy rule of thermodynamics and kinetics, a new idea for the design and optimization of mechanical properties of materials has been proposed, that is the generalized stability criteria for phase transformation and deformation. The ΔG and Q are correlated by the concept of generalized stability, and it was suggested by many cases of metallic materials design that high driving forces and high generalized stability correspond to high strength and high ductility. To understand the thermo-dynamic correlation in the material deformation process and apply the generalized stability criteria for materials design, it is essential to comprehend the law of dislocation movement and evolution, and quantitatively describe the relationship between the driving force and the energy barrier of dislocation movement. The molecular dynamics (MD) simulation method has become an important means of studying the deformation mechanism of materials, dispite some limitations such as high deformation rate and small size of the description object. In this work, the thermo-kinetic behaviors of α-Fe deformation along [010], [111], [1
Key words: α-Fe; molecular dynamics; dislocation; thermo-kinetics; generalized stability
BAI Zhiwen , DING Zhigang , ZHOU Ailong , HOU Huaiyu , LIU Wei , LIU Feng . Molecular Dynamics Simulation of Thermo-Kinetics of Tensile Deformation of α-Fe Single Crystal[J]. Acta Metall Sin, 2024 , 60(6) : 848 -856 . DOI: 10.11900/0412.1961.2022.00606
| 1 | Dever D J. Temperature dependence of the elastic constants in α-iron single crystals: Relationship to spin order and diffusion an-omalies [J]. J. Appl. Phys., 1972, 43: 3293 |
| 2 | Benito J A, Jorba J, Manero J M, et al. Change of Young's modulus of cold-deformed pure iron in a tensile test [J]. Metall. Mater. Trans.., 2005, 36A: 3317 |
| 3 | Zhang X Y, Chen J, Hu W Y, et al. Interactions of plasticity and phase transformation under shock in iron bicrystals [J]. J. Appl. Phys., 2019, 126: 045901 |
| 4 | Ma T, Xie H X. Formation mechanism of face-centered cubic phase in impact process of single crystal iron along [101] direction [J]. Acta Phys. Sin., 2020, 69: 130202 |
| 马 通, 谢红献. 单晶铁沿[101]晶向冲击过程中面心立方相的形成机制 [J]. 物理学报, 2020, 69: 130202 | |
| 5 | Sainath G, Choudhary B K. Deformation behaviour of body centered cubic iron nanopillars containing coherent twin boundaries [J]. Philos. Mag., 2016, 96: 3502 |
| 6 | Dutta A. Compressive deformation of Fe nanopillar at high strain rate: Modalities of dislocation dynamics [J]. Acta Mater., 2017, 125: 219 |
| 7 | Rawat S, Chaturvedi S. Effect of temperature on the evolution dynamics of voids in dynamic fracture of single crystal iron: A molecular dynamics study [J]. Philos. Mag., 2021, 101: 657 |
| 8 | Zhang Z S, Xu K, Lin Y W, et al. Simultaneous stiffening and strengthening of nanodiamond by fivefold twins [J]. MRS Bull., 2022, 47: 219 |
| 9 | Wu J Y, Nagao S, He J Y, et al. Role of five-fold twin boundary on the enhanced mechanical properties of fcc Fe nanowires [J]. Nano Lett., 2011, 11: 5264 |
| 10 | Zolnikov K P, Korchuganov A V, Kryzhevich D S. Anisotropy of plasticity and structural transformations under uniaxial tension of iron crystallites [J]. Comput. Mater. Sci., 2018, 155: 312 |
| 11 | Kocks U F, Argon A S, Ashby M F. Thermodynamics and kinetics of slip [M]. Oxford: Pergamon Presss, 1975: 1 |
| 12 | Liu F, Wang H F, Song S J, et al. Competitions correlated with nucleation and growth in non-equilibrium solidification and solid-state transformation [J]. Prog. Phys., 2012, 32: 57 |
| 刘 峰, 王海丰, 宋韶杰 等. 非平衡凝固与固态相变中有关形核和长大的竞争研究 [J]. 物理学进展, 2012, 32: 57 | |
| 13 | Peng H R, Huang L K, Liu F. A thermo-kinetic correlation for grain growth in nanocrystalline alloys [J]. Mater. Lett., 2018, 219: 276 |
| 14 | Liu F, Wang T L. Precipitation modeling via the synergy of thermo-dynamics and kinetics [J]. Acta Metall. Sin., 2021, 57: 55 |
| 刘 峰, 王天乐. 基于热力学和动力学协同的析出相模拟 [J]. 金属学报, 2021, 57: 55 | |
| 15 | Chen Z, Liu F, Yang X Q, et al. A thermokinetic description of nanoscale grain growth: Analysis of the activation energy effect [J]. Acta Mater., 2012, 60: 4833 |
| 16 | Peng H R, Liu B S, Liu F. A strategy for designing stable nanocrystalline alloys by thermo-kinetic synergy [J]. J. Mater. Sci. Technol., 2020, 43: 21 |
| 17 | Huang L K, Lin W T, Zhang Y B, et al. Generalized stability criterion for exploiting optimized mechanical properties by a general correlation between phase transformations and plastic deformations [J]. Acta Mater., 2020, 201: 167 |
| 18 | He Y Q, Song S J, Du J L, et al. Thermo-kinetic connectivity by integrating thermo-kinetic correlation and generalized stability [J]. J. Mater. Sci. Technol., 2022, 127: 225 |
| 19 | Hirel P. Atomsk: A tool for manipulating and converting atomic data files [J]. Comput. Phys. Commun., 2015, 197: 212 |
| 20 | Plimpton S. Fast parallel algorithms for short-range molecular dynamics [J]. J. Comput. Phys., 1995, 117: 1 |
| 21 | Mendelev M I, Han S, Srolovitz D J, et al. Development of new interatomic potentials appropriate for crystalline and liquid iron [J]. Philos. Mag., 2003, 83: 3977 |
| 22 | Jeon J B, Lee B J, Chang Y W. Molecular dynamics simulation study of the effect of grain size on the deformation behavior of nanocrystalline body-centered cubic iron [J]. Scr. Mater., 2011, 64: 494 |
| 23 | Yuan F P. Atomistic simulation study of tensile deformation in bulk nanocrystalline bcc iron [J]. Sci. China Phys. Mech. Astron., 2012, 55: 1657 |
| 24 | Zhao X, Lu C, Tieu A K, et al. Deformation mechanisms and slip-twin interactions in nanotwinned body-centered cubic iron by molecular dynamics simulations [J]. Comput. Mater. Sci., 2018, 147: 34 |
| 25 | Stukowski A. Visualization and analysis of atomistic simulation data with OVITO—The open visualization tool [J]. Modell. Simul. Mater. Sci. Eng., 2010, 18: 015012 |
| 26 | Stukowski A, Bulatov V V, Arsenlis A. Automated identification and indexing of dislocations in crystal interfaces [J]. Modell. Simul. Mater. Sci. Eng., 2012, 20: 085007 |
| 27 | Stukowski A. Structure identification methods for atomistic simulations of crystalline materials [J]. Modell. Simul. Mater. Sci. Eng., 2012, 20: 045021 |
| 28 | Ma B, Rao Q H, He Y H. Effect of crystal orientation on tensile mechanical properties of single-crystal tungsten nanowire [J]. Trans. Nonferrous Met. Soc. China, 2014, 24: 2904 |
| 29 | Sandoval L, Urbassek H M. Transformation pathways in the solid-solid phase transitions of iron nanowires [J]. Appl. Phys. Lett., 2009, 95: 191909 |
| 30 | Wen P, Tao G, Ren B X., et al. Molecular dynamics simulation on the uniaxial tension property of metal Fe interacting with C [J] Chin. J. Appl. Mech., 2015, 32: 915 |
| 闻 鹏, 陶 钢, 任保祥 等. C原子对Fe-C合金拉伸性能影响的分子动力学分析 [J]. 应用力学学报, 2015, 32: 915 | |
| 31 | Sandoval L, Urbassek H M. Finite-size effects in Fe-nanowire solid-solid phase transitions: A molecular dynamics approach [J]. Nano Lett., 2009, 9: 2290 |
| 32 | Sandoval L, Urbassek H M. Solid-solid phase transitions in Fe nanowires induced by axial strain [J]. Nanotechnology, 2009, 20: 5704 |
| 33 | Huang D, Zhang Q, Guo Y M. Molecular dynamics simulation for axial tension process of α-Fe and Ni nano wires [J]. Ordnance Mater. Sci. Eng., 2006, 29: 12 |
| 黄 丹, 章 青, 郭乙木. α-Fe和Ni纳米丝单向拉伸过程的分子动力学模拟 [J]. 兵器材料科学与工程, 2006, 29: 12 | |
| 34 | Wu Q, Wang Y, Han T, et al. Molecular dynamics simulations of the effect of temperature and strain rate on the plastic deformation of body-centered cubic iron nanowires [J]. J. Eng. Mater. Technol., 2021, 143: 031007 |
| 35 | Zepeda-Ruiz L A, Stukowski A, Oppelstrup T, et al. Probing the limits of metal plasticity with molecular dynamics simulations [J], Nature, 2017, 550: 492 |
/
| 〈 |
|
〉 |