Research paper

Microstructural Stability and Stress Rupture Properties of a Third-Generation Ni Base Single Crystal Supalloy

  • LIU Jinlai ,
  • SUN Jingxia ,
  • MENG Jie ,
  • LI Jinguo
Expand
  • 1 Shi -changxu Innovation Center for Advanced Materials, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
    2 School of Materials Science and Engineering, University of Science and Technology of China, Shenyang 110016, China
LIU Jinlai, senior engineer, Tel: (024)23971767, E-mail: jlliu@imr.ac.cn

Received date: 2022-07-09

  Revised date: 2022-11-08

  Online published: 2023-02-23

Supported by

National Key Research and Development Program of China(2019-Ⅶ-0019-0161);National Key Research and Development Program of China(2017YFA0700704);National Natural Science Foundation of China(51971214);Sichuan Science and Technology Program(2022YFSY0016)

Abstract

Single-crystal superalloys have been developed to the 5th generation to improve their temperature capacity. Thus, a rare metal Ru is doped to the 4th and 5th generations based on the 6%Re (with the same mass fraction) contained in third-generation superalloys. Compared with Re addition in low-generation superalloys, improvement of temperature capacity decreases with Ru addition in high-generation superalloys; however, the cost of superalloys containing Ru has increased significantly. Therefore, considerable attention must be paid to the development of third-generation single-crystal superalloys because of their superior cost performance. Thus, considering the slight precipitation of the topologically close-packed (TCP) phase and low properties at the intermediate temperature of third-generation single-crystal superalloys, Al is considered as a significant element affecting microstructure stability, which is determined by calculating the number of electron vacancy (Nv). By reducing 0.4%Al, no TCP phase is precipitated in the superalloy after long-term thermal exposure at 1100oC for 1000 h; therefore, good microstructure stability is obtained. The concentration of Re and Co is decreased slightly to increase the stacking fault energy of the superalloy and to enhance the properties at intermediate temperature. The stress rupture life at 760oC and 800 MPa extends from 40 h to 150 h by reducing 0.4%Al followed with reduction of 0.25%Re and 1%Co. Moreover, the stress rupture properties at high temperature remain unchanged. Based on the abovementioned research, a third-generation single-crystal superalloy is developed, and the causes of stabilization of the microstructure and improvement to properties at intermediate temperature are also discussed.

Cite this article

LIU Jinlai , SUN Jingxia , MENG Jie , LI Jinguo . Microstructural Stability and Stress Rupture Properties of a Third-Generation Ni Base Single Crystal Supalloy[J]. Acta Metall Sin, 2024 , 60(6) : 770 -776 . DOI: 10.11900/0412.1961.2022.00337

References

1 Walston S, Cetel A, MacKay R, et al. Joint development of a fourth generation single crystal superalloy [A]. Superalloys 2004 [C]. Warrendale: TMS, 2004: 15
2 Sato A, Harada H, Yeh A C, et al. A 5th generation SC superalloy with balanced high temperature properties and processability [A]. Superalloys 2008 [C]. Champion: TMS, 2008: 131
3 Erickson G L. The development and application of CMSX?-10 [A]. Superalloys 1996 [C]. Warrendale: TMS, 1996: 35
4 Walston W S, O'Hara K S, Ross E W, et al. René N6: Third generation single crystal superalloy [A]. Superalloys 1996 [C]. Warrendale: TMS, 1996: 27
5 Argence D, Vemault C, Desvallees Y, et al. MC-NG: A 4th generation single-crystal superalloy for future aeronautical turbine blades and vanes [A]. Superalloys 2000 [C]. Warrrendale: TMS, 2000: 829
6 Rame J, Caron P, Locq D, et al. Development of AGAT, a third-generation nickel-based superalloy for single crystal turbine blade applications [A]. Proceedings of the 14th International Symposium on Superalloys [C]. Cham: Springer, 2020: 31
7 Fuchs G E. Improvement of creep strength of a third generation, single-crystal Ni-base superalloy by solution heat treatment [J]. J. Mater. Eng. Perform., 2002, 11: 19
8 Zhou H, Okada I, Ro Y, et al. Thermomechanical fatigue behavior of the third-generation, single-crystal superalloy TMS-75: Deformation structure [J]. Metall. Mater. Trans., 2004, 35A: 1779
9 Li J R, Liu S Z, Shi Z X, et al. Third generation single crystal superalloy DD9 [J]. J Iron Steel Res., 2011, 23(suppl. 2) : 337
  李嘉荣, 刘世忠, 史振学 等. 第三代单晶高温合金DD9 [J]. 钢铁研究学报, 2011, 23(): 337
10 Xiong J Y, Long A P, Zhang J T, et al. Microstructure and properties of third generation single crystal superalloy WZ30 [J]. Rare Met. Mater. Eng., 2021, 50: 3995
  熊江英, 龙安平, 张建庭 等. 一种新型第三代单晶高温合金WZ30组织与性能的研究 [J]. 稀有金属材料与工程, 2021, 50: 3995
11 Caldwell E C, Fela F J, Fuchs G E. Segregation of elements in high refractory content single crystal nickel based superalloys [A]. Superalloys 2004 [C]. Champion: TMS, 2004: 811
12 Kearsey R M, Beddoes J C, Jaansalu K M, et al. The effects of Re, W and Ru on microsegregation behaviour in single crystal superalloy systems [A]. Superalloys 2004 [C]. Champion: TMS, 2004: 801
13 Fuchs G E. Solution heat treatment response of a third generation single crystal Ni-base superalloy [J]. Mater. Sci. Eng., 2001, A300: 52
14 Diologent F, Caron P. On the creep behavior at 1033K of new generation single-crystal superalloys [J]. Mater. Sci. Eng., 2004, A385: 245
15 Wilson A S. Formation and effect of topologically close-packed phases in nickel-base superalloys [J]. Mater. Sci. Technol., 2017, 33: 1108
16 Seiser B, Drautz R, Pettifor D G. TCP phase predictions in Ni-based superalloys: Structure maps revisited [J]. Acta Mater., 2011, 59: 749
17 Huang S Y, An K, Gao Y, et al. Determination of γ/γ' lattice misfit in Ni-based single-crystal superalloys at high temperatures by neutron diffraction [J]. Metall. Mater. Trans., 2018, 49A: 740
18 Rae C M F, Matan N, Reed R C. The role of stacking fault shear in the primary creep of [001]-oriented single crystal superalloys at 750oC and 750 MPa [J]. Mater. Sci. Eng., 2001, A300: 125
19 Ma S, Carroll L, Pollock T M. Development of γ phase stacking faults during high temperature creep of Ru-containing single crystal superalloys [J]. Acta Mater., 2007, 55: 5802
20 Kumar K, Sankarasubramanian R, Waghmare U V. Tuning planar fault energies of Ni3Al with substitutional alloying: First-principles description for guiding rational alloy design [J]. Scr. Mater., 2018, 142: 74
21 Kong Y H, Chen Q Z. Effect of minor additions on the formation of TCP phases in modified RR2086 SX superalloys [J]. Mater. Sci. Eng., 2004, A366: 135
22 Gao S, Liu Z Q, Li C F, et al. In situ TEM investigation on the precipitation behavior of μ phase in Ni-base single crystal superalloys [J]. Acta Mater., 2016, 110: 268
23 Huis In't Veld A J, Boom G, Bronsveld P M, et al. Superlattice intrinsic stacking faults in γ′ precipitates [J]. Scr. Metall., 1985, 19: 1123
24 Milligan W W, Antolovich S D. The mechanisms and temperature dependence of superlattice stacking fault formation in the single-crystal superalloy PWA 1480 [J]. Metall. Trans., 1991, 22A: 2309
25 Knowles D M, Chen Q Z. Superlattice stacking fault formation and twinning during creep in γ/γ' single crystal superalloy CMSX-4 [J]. Mater. Sci. Eng., 2003, A340: 88
26 Gunturi S S K, MacLachlan D W, Knowles D M. Anisotropic creep in CMSX-4 in orientations distant from 〈001〉 [J]. Mater. Sci. Eng., 2000, A289: 289
27 Li J R, Dong J M, Han M, et al. Effects of sand blasting on surface integrity and high cycle fatigue properties of DD6 single crystal superalloy [J]. Acta Metall. Sin., 2023, 59: 1201
  李嘉荣, 董建民, 韩 梅 等. 吹砂对DD6单晶高温合金表面完整性和高周疲劳强度的影响 [J]. 金属学报, 2023, 59: 1201
28 Reppich B. Some new aspects concerning particle hardening mechanisms in γ' precipitating Ni-base alloys—I. Theoretical concept [J]. Acta Metall., 1982, 30: 87
29 Mackay R A, Maier R D. The influence of orientation on the stress rupture properties of nickel-base superalloy single crystals [J]. Metall. Trans., 1982, 13A: 1747
Outlines

/