Research paper

Crystallographic Understanding of the Effect of Ni Content on the Hardenability of High-Strength Low-Alloy Steel

  • SU Shuai ,
  • HAN Peng ,
  • YANG Shanwu ,
  • WANG Hua ,
  • JIN Yaohui ,
  • SHANG Chengjia
Expand
  • 1 Collaborative Innovation Center of Steel Technology, University of Science and Technology Beijing, Beijing 100083, China
    2 State Key Laboratory of Metal Material for Marine Equipment and Application, Ansteel Group Corporation, Anshan 114000, China
SHANG Chengjia, professor, Tel: (010)62332428, E-mail: cjshang@ustb.edu.cn

Received date: 2022-06-15

  Revised date: 2022-08-17

  Online published: 2023-02-15

Supported by

Liaoning Revitalization Talents Program(XLYC1907186)

Abstract

A matrix structure with high strength, such as lath martensite/bainite is created via quenching to achieve conventional high-strength low-alloy ultra-heavy plates. Subsequently, this structure is tempered to improve its toughness. However, it is usually impossible to avoid the low cooling rate in the center of the ultra-heavy plates during cooling, causing inhomogeneous microstructure and mechanical properties along the normal direction. Therefore, it is necessary to enhance the hardenability of the alloy. At lower cooling rates, granular bainite/ferrites are formed in the center of the plates with low hardenability. While this leads to the incompletely transformed martensite/austenite islands (M/A islands), which often cause cracks, fewer high angle grain boundaries (HAGBs) are also formed, which can effectively impede crack propagation. Therefore, improving the strength, toughness, and hardenability is crucial for the development of high-strength low-alloy steel. The addition of nickel can improve the hardenability as well as the toughness of the heavy plates. In this study, two high-strength low-alloy steels with different nickel contents are designed. In addition, the effect of nickel content on hardenability and phase transition temperature is tested using end quenching and thermal mechanical simulation testing. The effects of nickel content on the microstructure and crystallographic characteristics of coherent phase-transformed products are characterized using SEM and EBSD. The results reveal that the increased nickel content greatly improves the hardenability and significantly reduces the phase transition temperature. At a low cooling rate of 0.5oC/s, the microstructure of 2.94Ni steel is lath bainite, and the M/A islands are dispersed on a thin film, forming a phase transformation mode with higher HAGB density, block boundary density and V1/V2 variant pair content, and high hardness. This mode is dominated by the close-packed plane group. While the microstructure of 0.92Ni steel is granular bainite and the M/A islands are distributed in coarse blocks, forming a phase transformation mode with lower HAGB density, block boundary density and V1/V2 variant pair content, and significantly low hardness. Moreover, this mode is dominated by the Bain group. Additionally, the results demonstrate that at the cooling rate of 0.5oC/s, as nickel content increases, the driving force of phase transformation is greatly improved to obtain a higher transformation rate than the steel with low nickel content. The maximum carbon content of untransformed austenite is higher, which promotes the complete transformation of bainite and produces fewer M/A islands. Therefore, this research possesses great potential for the composition design and process control of high-strength low-alloy steel.

Cite this article

SU Shuai , HAN Peng , YANG Shanwu , WANG Hua , JIN Yaohui , SHANG Chengjia . Crystallographic Understanding of the Effect of Ni Content on the Hardenability of High-Strength Low-Alloy Steel[J]. Acta Metall Sin, 2024 , 60(6) : 789 -801 . DOI: 10.11900/0412.1961.2022.00297

References

1 Xie Z J, Fang Y P, Han G, et al. Structure-property relationship in a 960 MPa grade ultrahigh strength low carbon niobium-vanadium microalloyed steel: The significance of high frequency induction tempering [J]. Mater. Sci. Eng., 2014, A618: 112
2 Yu Y S, Hu B, Gao M L, et al. Determining role of heterogeneous microstructure in lowering yield ratio and enhancing impact toughness in high-strength low-alloy steel [J]. Int. J. Miner. Metall. Mater., 2021, 28: 816
3 Capdevila C, García-Mateo C, Chao J, et al. Advanced vanadium alloyed steel for heavy product applications [J]. Mater. Sci. Technol., 2009, 25: 1383
4 An F C, Zhao S X, Xue X K, et al. Incompleteness of bainite transformation in quenched and tempered steel under continuous cooling conditions [J]. J. Mater. Res. Technol., 2020, 9: 8985
5 Pan T, Wang X Y, Su H, et al. Effect of alloying element Al on hardenabilitity and mechanical properties of micro-B treated ultra-heavy plate steels [J]. Acta Metall. Sin., 2014, 50: 431
  潘 涛, 王小勇, 苏 航 等. 合金元素Al对微B处理特厚钢板淬透性及力学性能的影响 [J]. 金属学报, 2014, 50: 431
6 Zhou T, Yu H, Wang S Y. Microstructural characterization and mechanical properties across thickness of ultra-heavy steel plate [J]. Steel Res. Int., 2017, 88: 1700132
7 Al Hajeri K F, Garcia C I, Hua M J, et al. Particle-stimulated nucleation of ferrite in heavy steel sections [J]. ISIJ Int., 2006, 46: 1233
8 Wu B B. Study on crystallographic characteristics of high strength low alloy steel and its composition-process-performance relationship [D]. Beijing: University of Science and Technology Beijing, 2020
  吴彬彬. 高强度低合金钢晶体学特征及其成分-工艺-性能关系研究 [D]. 北京: 北京科技大学, 2020
9 Li W, Cao R, Zhu W C, et al. Microstructure evolution and impact toughness variation for high strength steel multi-pass weld metals with various cooling rates [J]. J. Manuf. Processes, 2021, 65: 245
10 Wang X L, Wang Z Q, Dong L L, et al. New insights into the mechanism of cooling rate on the impact toughness of coarse grained heat affected zone from the aspect of variant selection [J]. Mater. Sci. Eng., 2017, A704: 448
11 Wang X L, Ma X P, Wang Z Q, et al. Carbon microalloying effect of base material on variant selection in coarse grained heat affected zone of X80 pipeline steel [J]. Mater. Charact., 2019, 149: 26
12 Guo Z, Lee C S, Morris Jr J W. On coherent transformations in steel [J]. Acta Mater., 2004, 52: 5511
13 Wu B B, Wang Z Q, Wang X L, et al. Relationship between high angle grain boundaries and hardness after γα transformation [J]. Mater. Sci. Technol., 2019, 35: 1803
14 Huang S, Yu Y S, Wang Z Q, et al. Crystallographic insights into the role of nickel on hardenability of wear-resistant steels [J]. Mater. Lett., 2022, 306: 130961
15 Huang G, Wan X L, Wu K M, et al. Effects of small Ni addition on the microstructure and toughness of coarse-grained heat-affected zone of high-strength low-alloy steel [J]. Metals, 2018, 8: 718
16 Liu Z P, Yu Y S, Yang J, et al. Morphology and crystallography analyses of HSLA steels with hardenability enhanced by tailored C-Ni collocation [J]. Metals, 2021, 12: 32
17 Morris Jr J W, Guo Z, Krenn C R, et al. The limits of strength and toughness in steel [J]. ISIJ Int., 2001, 41: 599
18 Miyamoto G, Hori R, Poorganji B, et al. Crystallographic analysis of proeutectoid ferrite/austenite interface and interphase precipitation of vanadium carbide in medium-carbon steel [J]. Metall. Mater. Trans., 2013, 44A: 3436
19 Kawata H, Sakamoto K, Moritani T, et al. Crystallography of ausformed upper bainite structure in Fe-9Ni-C alloys [J]. Mater. Sci. Eng., 2006, A438-440: 140
20 Takayama N, Miyamoto G, Furuhara T. Effects of transformation temperature on variant pairing of bainitic ferrite in low carbon steel [J]. Acta Mater., 2012, 60: 2387
21 Yu Y S, Wang Z Q, Wu B B, et al. Tailoring variant pairing to enhance impact toughness in high-strength low-alloy steels via trace carbon addition [J]. Acta Metall. Sin. (Engl. Lett.), 2021, 34: 755
22 Yu Y S, Wang Z Q, Wu B B, et al. New insight into the hardenability of high strength low alloy steel from the perspective of crystallography [J]. Mater. Lett., 2021, 292: 129624
23 Huang S, Wu B B, Wang Z Q, et al. EBSD study on the significance of carbon content on hardenability [J]. Mater. Lett., 2019, 254: 412
24 Furuhara T, Chiba T, Kaneshita T, et al. Crystallography and interphase boundary of martensite and bainite in steels [J]. Metall. Mater. Trans., 2017, 48A: 2739
25 Miyamoto G, Iwata N, Takayama N, et al. Variant selection of lath martensite and bainite transformation in low carbon steel by ausforming [J]. J. Alloys Compd., 2013, 577 (): S528
26 Chiba T, Miyamoto G, Furuhara T. Comparison of variant selection between lenticular and lath martensite transformed from deformed austenite [J]. ISIJ Int., 2013, 53: 915
27 Morris Jr J W, Lee C S, Guo Z. The nature and consequences of coherent transformations in steel [J]. ISIJ Int., 2003, 43: 410
28 Wu B B, Wang Z Q, Yu Y S, et al. Thermodynamic basis of twin-related variant pair in high strength low alloy steel [J]. Scr. Mater., 2019, 170: 43
29 Quidort D, Brechet Y J M. A model of isothermal and non isothermal transformation kinetics of bainite in 0.5%C steels [J]. ISIJ Int., 2002, 42: 1010
30 You Y, Wang X M, Shang C J. Influence of austenitizing temperature on the microstructure and impact toughness of a high strength low alloy HSLA100 steel [J]. Acta Metall. Sin., 2012, 48: 1290
  由 洋, 王学敏, 尚成嘉. 奥氏体化温度对HSLA100高强度低合金钢组织及冲击韧性的影响 [J]. 金属学报, 2012, 48: 1290
31 Xu Z Y, Li X M. Diffusion of carbon during the formation of low-carbon martensite [J]. Acta Metall. Sin., 1983, 19(2): A83
  徐祖耀, 李学敏. 低碳马氏体形成时碳的扩散 [J]. 金属学报, 1983, 19(2): A83
32 Xu Z Y, Li X M. Diffusion of carbon during formation of low-carbon martensite (Continued) [J]. Acta Metall. Sin., 1983, 19(6): A505
  徐祖耀, 李学敏. 低碳马氏体形成时碳的扩散(续) [J]. 金属学报, 1983, 19(6): A505
33 Aaronson H I, Domian H A, Pound G M. Thermodynamics of the austenite-proeutectoid ferrite transformation: Fe-C alloys [J]. Trans. Metall. Soc. AIME, 1966, 236: 753
34 Bhadeshia H K D H, Honeycombe R W K. Steels: Microstructure and Properties [M]. 4th Ed., Oxford: Butterworth-Heinemann, 2017: 425
35 Bhadeshia H K D H. Thermodynamic analysis of isothermal transformation diagrams [J]. Met. Sci., 1982, 16: 159
Outlines

/