Research paper

Combustion Behavior of GH4061 Alloy in High Pressure and Oxygen-Enriched Atmosphere

  • CAO Shuting ,
  • ZHANG Shaohua ,
  • ZHANG Jian
Expand
  • 1Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
    2School of Materials Science and Engineering, University of Science and Technology of China, Shenyang 110016, China
ZHANG Jian, professor, Tel: (024)23971196, E-mail: jianzhang@imr.ac.cn;ZHANG Shaohua, associate professor, Tel: (024)23748882, E-mail: zhangshaohua@imr.ac.cn

Received date: 2022-10-31

  Revised date: 2022-12-13

  Online published: 2023-02-08

Supported by

National Natural Science Foundation of China(52150233);Key Research Program of Chinese Academy of Sciences(ZDRW-CN-2021-2-1)

Abstract

Liquid oxygen (LOX)/kerosene rocket engines are the main power system of heavy launch vehicles around the globe, and the turbine materials are usually exposed to elevated temperatures, high pressure, and oxygen-enriched environment in gas generators. Metal combustion may occur under these working conditions. GH4061 is a newly developed Ni-based superalloy that is used in turbine materials because of its excellent mechanical properties. However, its combustion resistance property has rarely been studied. Recently, several studies on metal combustion have been conducted, but they mainly focus on exploring the rules of metal combustion. Furthermore, the domestically promoted ignition-combustion (PIC) experiment equipment only supports the test under 2 MPa pressure, which has significantly limited the study of metal combustion at higher pressure. Therefore, the analysis of the metal combustion mechanism remains incomplete. In this study, the 3.5-25 MPa high pressure and oxygen-enriched combustion experiments of GH4061 alloy were performed on the basis of independently-developed PIC equipment with a maximum pressure of 25 MPa. A high-speed camera was used to observe and record the combustion process. The postcombustion microstructure was characterized using SEM and EDS, and the combustion product was identified using XRD. The length and rate of burning increase as the oxygen pressure increases. The critical burning pressure of GH4061 under 99.5% oxygen (when igniting at 25oC) is about 5 MPa, according to ASTM-G124. After testing, the transition zone, melting zone, ignition interface, and oxide zone in the samples were characterized. The burning process is due to elements with a higher heat of combustion. During combustion, lower-density molten oxides float up to the melting zone. After testing, small O/Al/Ti-rich particles and large complex oxide particles with dendritic morphology were observed in the melting zone. The effect of oxygen pressure was analyzed using thermodynamics.

Cite this article

CAO Shuting , ZHANG Shaohua , ZHANG Jian . Combustion Behavior of GH4061 Alloy in High Pressure and Oxygen-Enriched Atmosphere[J]. Acta Metall Sin, 2023 , 59(4) : 547 -555 . DOI: 10.11900/0412.1961.2022.00551

References

1 Huang J F, Zhao G P, Jiao L Y, et al. Combustion failure analysis of GH202 and GH586 superalloys for rocket engine [J]. J. Iron Steel Res., 2005, 17(3): 68
  黄进峰, 赵光普, 焦兰英 等. 火箭发动机用合金GH202和GH586燃烧事故分析 [J]. 钢铁研究学报, 2005, 17(3): 68
2 Grosse A V, Conway J B. Combustion of metals in oxygen [J]. Ind. Eng. Chem., 1958, 50: 663
3 Tekumalla S, Gupta M. An insight into ignition factors and mechanisms of magnesium based materials: A review [J]. Mater. Des., 2017, 113: 84
4 Shao L, Xie G L, Liu X H, et al. Combustion behaviour and mechanism of a Cu-Ni-Mn alloy in an oxygen enriched atmosphere [J]. Corros. Science., 2020, 163: 108253
5 Yoffe P. The burning of metals [J]. Proc. Roy. Soc., 1961, 261A: 357
6 Monroe R W, Bates C E, Pears C D. Metal combustion in high-pressure flowing oxygen [A]. The Symposium on Flammability and Sensitivity of Materials in Oxygen-Enriched Atmospheres [C]. Phoenix: ASTM, 1983: 126
7 Hill P R. High temperature oxidation and ignition of metals [R]. Washington: National Advisory Committee for Aeronautics, 1956
8 Stradling J S, Pippen D L, Frye G W. Techniques employed by the NASA White Sands Test Facility to ensure oxygen system component safety [A]. The Symposium on Flammability and Sensitivity of Materials in Oxygen-Enriched Atmospheres [C]. Phoenix: ASTM, 1983: 97
9 Neary R M. ASTM G 63: A milestone in a 60-year safety effort [A]. The Symposium on Flammability and Sensitivity of Materials in Oxygen-Enriched Atmospheres [C]. Phoenix: ASTM, 1983: 3
10 Million J F, Samant A, Zawierucha R, et al. Promoted ignition-combustion behavior of cobalt and nickel alloys in oxygen-enriched atmospheres [A]. The Symposium on Flammability and Sensitivity of Materials in Oxygen-Enriched Atmospheres: 12th Volume [C]. Berlin: ASTM, 2009: 10
11 American Society for Testing Material. Standard Test Method for Determining the Combustion Behavior of Metallic Materials in Oxygen-Enriched Atmospheres [S]. West Conshohocken: ASTM International, 2010
12 Benz F J, Shaw R C, Homa J M. Burn propagation rates of metals and alloys in gaseous oxygen [A]. The Symposium on Compatibility and Sensitivity of Materials in Oxygen-Enriched Atmospheres:Second Volume [C]. Washington: ASTM, 1986: 135
13 Zawierucha R, Million J F. Promoted ignition-combustion behavior of engineering alloys at elevated temperatures and pressures in oxygen gas mixtures [A]. The Symposium on Flammability and Sensitivity of Materials in Oxygen-Enriched Atmospheres: Fourth Volume [C]. Las Cruces: ASTM, 1989: 145
14 American Society for Testing Material. Standard Test Method for Determining the Combustion Behavior of Metallic Materials in Oxygen-Enriched Atmospheres [S]. West Conshohocken: ASTM International, 2018
15 Zabrenski J S, Werley B L, Slusser J W. Pressurized flammability limits of metals [A]. The Symposium on Flammability and Sensitivity of Materials in Oxygen-Enriched Atmospheres: Fourth Volume [C]. Las Cruces: ASTM, 1989: 178
16 Sircar S, Stoltzfus J, Bryan C, et al. Promoted combustion of pure metals in oxygen-enriched atmospheres [A]. The Symposium on Flammability and Sensitivity of Materials in Oxygen-Enriched Atmospheres: Seventh Volume [C]. Denver: ASTM, 1995: 100
17 Zawierucha R, Robert K, Mazzarella R B. Promoted ignition-combustion behavior of selected hastelloys in oxygen gas mixtures [A]. The Symposium on Flammability and Sensitivity of Materials in Oxygen-Enriched Atmospheres: Fifth Volume [C]. Cocoa Beach: ASTM 1989: 270
18 Bryan C J, Stoltzfus J M, Gunaji M V. An assessment of the flammability hazard of several corrosion resistant metal alloys [A]. The Symposium on Flammability and Sensitivity of Materials in Oxygen-Enriched Atmospheres: Sixth Volume [C]. Noordwijk: ASTM, 1993: 112
19 Stoltzfus J M, Homa J M, Williams R E, et al. ASTM committee G-4 metals flammability test program data and discussion [A]. The Symposium on Flammability and Sensitivity of Materials in Oxygen-Enriched Atmospheres: Fourth Volume [C]. Churchill College: ASTM, 1987: 33
20 Benz F, Steinberg T A, Janoff D. Combustion of 316 stainless steel in high-pressure gaseous oxygen [A]. The Symposium on Flammability and Sensitivity of Materials in Oxygen-Enriched Atmospheres: Fourth Volume [C]. Las Cruces: ASTM, 1989: 195
21 Gunaji M V, Sircar S, Beeson H D. Ignition and combustion of titanium and titanium alloys [A]. The Symposium on Flammability and Sensitivity of Materials in Oxygen-Enriched Atmospheres: Seventh Volume [C]. Denver: ASTM, 1995: 81
22 Janoff D, Pedley M D. Configurational effects on the combustion of several alloy systems in oxygen-enriched atmospheres [A]. The Symposium on Flammability and Sensitivity of Materials in Oxygen-Enriched Atmospheres: Eighth Volume [C]. West Conshohocken: ASTM, 1997: 147
23 Huang J F, Yu H Y, Li Y B, et al. Oxidation characteristic and mechanism of superalioys in oxygen-enriched atmosphere [J]. J. Iron Steel Res., 2009, 21(3): 51
  黄进峰, 余红燕, 李永兵 等. 富氧气氛下高温合金氧化特征及机理 [J]. 钢铁研究学报, 2009, 21(3): 51
24 Shi L F, Huang J F, Zhao G P, et al. Research on combustion characteristics and properties of superailoy in high-pressure and oxygen-enriched atmosphere [J]. Hot Working Tech., 2007, 36(4): 26
  施立发, 黄进峰, 赵光普 等. 高压富氧下几种高温合金的燃烧特征和性能研究 [J]. 热加工工艺, 2007, 36(4): 26
25 Wang H L, Huang J F, Lian Y, et al. Combustion behavior of GH4169 and GH4202 superalloys in oxygen-enriched atmosphere [J]. Chin. J. Eng., 2016, 38: 1288
  王宏亮, 黄进峰, 连 勇 等. 高温合金GH4169与GH4202在富氧气氛中的燃烧行为 [J]. 工程科学学报, 2016, 38: 1288
26 He Y W. Study on the effect and mechanism of V, Cu in a new Ni-Cr-Fe-Nb superalloy [D]. Shenyang: Northeastern University, 2016
  贺玉伟. V、Cu在新型Ni-Cr-Fe-Nb高温合金中的作用机理研究 [D]. 沈阳: 东北大学, 2016
27 American Society for Testing Material. Standard Guide for Evaluating Metals for Oxygen Service [S]. West Conshohocken: ASTM International, 2014
28 Bransford J W. Ignition and combustion temperatures determined by laser heating [A]. The Symposium on Compatibility and Sensitivity of Materials in Oxygen-Enriched Atmospheres: Second Volume [C]. Washington: ASTM, 1986: 78
29 Steinberg T A, Wilson D B, Benz F J. Microgravity and normal gravity combustion of metals and alloys in high pressure oxygen [A]. The Symposium on Flammability and Sensitivity of Materials in Oxygen-Enriched Atmospheres: Sixth Volume [C]. Noordwijk: ASTM, 1993: 136
30 Fueki K. T-G diagram and its applications to high temperature oxidation of pure metals [J]. Denkikagaku, 1958, 26: 292
31 Engel C D, Herald S D, Davis S E. Promoted metals combustion at ambient and elevated temperatures [A]. The Symposium on Flammability and Sensitivity of Materials in Oxygen-Enriched Atmospheres: Eleventh Volume [C]. Washington: ASTM, 2006: 62
32 Hirano T, Sato K, Sato Y, et al. Prediction of metal fire spread in high-pressure oxygen [J]. Combust. Sci. Technol., 1983, 32: 137
33 Hirano T, Sato Y, Sato K, et al. The rate determining process of iron oxidation at combustion in high pressure oxygen [J]. Oxid. Commun., 1984, 6: 113
Outlines

/