Overview

Recent Advances in Open-Cell Porous Metal Materials for Electrocatalytic and Biomedical Applications

  • Wence XU ,
  • Zhenduo CUI ,
  • Shengli ZHU
Expand
  • School of Materials Science and Engineering, Tianjin University, Tianjin 300350, China
ZHU Shengli, professor, Tel: 18920951755, E-mail: slzhu@tju.edu.cn

Received date: 2022-08-04

  Revised date: 2022-09-27

  Online published: 2022-10-12

Supported by

National Natural Science Foundation of China(51771131);National Natural Science Foundation of China(52001172)

Abstract

Open-cell porous metal materials are multifunctional lightweight materials that have attracted considerable attention in electrocatalysis and biomedicine owing to their large specific surface area, low bulk density, good specific strength, high conductivity, and high mass transfer. The morphology, porosity, composition, crystal structure, and other properties of open-cell porous metal materials can be controlled precisely by designing different metal systems and developing efficient preparation technologies. Therefore, the corresponding functional performance of open-cell porous metal materials, such as catalytic activity, selectivity, stability, and biocompatibility, can be improved further. This paper briefly describes the fabrication methods and principles of open-cell porous metal materials for electrocatalysis and biomedicine. In addition, the recent developments in open-cell porous metal materials for electrocatalysis and biomedicine are summarized. Finally, the future development directions of open-cell porous metal materials for electrocatalysis and biomedicine are proposed.

Cite this article

Wence XU , Zhenduo CUI , Shengli ZHU . Recent Advances in Open-Cell Porous Metal Materials for Electrocatalytic and Biomedical Applications[J]. Acta Metall Sin, 2022 , 58(12) : 1527 -1544 . DOI: 10.11900/0412.1961.2022.00369

References

1 Shi S, Li Y, Ngo-Dinh B N, et al. Scaling behavior of stiffness and strength of hierarchical network nanomaterials [J]. Science, 2021, 371: 1026
2 Lang X Y, Hirata A, Fujita T, et al. Nanoporous metal/oxide hybrid electrodes for electrochemical supercapacitors [J]. Nat. Nanotechnol., 2011, 6: 232
3 Smith A J, Trimm D L. The preparation of skeletal catalysts [J]. Annu. Rev. Mater. Res., 2005, 35: 127
4 Knyrim J S, Becker P, Johrendt D, et al. A new non-centrosymmetric modification of BiB3O6 [J]. Angew. Chem. Int. Ed., 2006, 45: 8239
5 Biener J, Biener M M, Madix R J, et al. Nanoporous gold: Understanding the origin of the reactivity of a 21st century catalyst made by pre-columbian technology [J]. ACS Catal., 2015, 5: 6263
6 Wang X G, Wang W M, Qi Z, et al. Fabrication, microstructure and electrocatalytic property of novel nanoporous palladium composites [J]. J. Alloys Compd., 2010, 508: 463
7 Wang D H, Engle K M, Shi B F, et al. Ligand-enabled reactivity and selectivity in a synthetically versatile aryl C-H olefination [J]. Science, 2010, 327: 315
8 Wittstock A, Biener J, B?umer M. Nanoporous gold: A new material for catalytic and sensor applications [J]. Phys. Chem. Chem. Phys., 2010, 12: 12919
9 Dixon M C, Daniel T A, Hieda M, et al. Preparation, structure, and optical properties of nanoporous gold thin films [J]. Langmuir, 2007, 23: 2414
10 He R, Wang Y C, Wang X Y, et al. Facile synthesis of pentacle gold-copper alloy nanocrystals and their plasmonic and catalytic properties [J]. Nat. Commun., 2014, 5: 4327
11 Chapman C A R, Wang L, Chen H, et al. Nanoporous gold biointerfaces: Modifying nanostructure to control neural cell coverage and enhance electrophysiological recording performance [J]. Adv. Funct. Mater., 2017, 27: 1604631
12 Liu D Q, Yang Z B, Wang P, et al. Preparation of 3D nanoporous copper-supported cuprous oxide for high-performance lithium ion battery anodes [J]. Nanoscale, 2013, 5: 1917
13 Ryan G, Pandit A, Apatsidis D P. Fabrication methods of porous metals for use in orthopaedic applications [J]. Biomaterials, 2006, 27: 2651
14 Wang M Y, Yu X T, Wang Z, et al. Hierarchically 3D porous films electrochemically constructed on gas-liquid-solid three-phase interface for energy application [J]. J. Mater. Chem., 2017, 5A: 9488
15 Zhang J T, Li C M. Nanoporous metals: Fabrication strategies and advanced electrochemical applications in catalysis, sensing and energy systems [J]. Chem. Soc. Rev., 2012, 41: 7016
16 Fujita T, Guan P F, McKenna K, et al. Atomic origins of the high catalytic activity of nanoporous gold [J]. Nat. Mater., 2012, 11: 775
17 Nagels J, Stokdijk M, Rozing P M. Stress shielding and bone resorption in shoulder arthroplasty [J]. J. Shoulder Elbow Surg., 2003, 12: 35
18 Torres Y, Trueba P, Pavón J, et al. Designing, processing and characterisation of titanium cylinders with graded porosity: An alternative to stress-shielding solutions [J]. Mater. Des., 2014, 63: 316
19 Anselme K. Osteoblast adhesion on biomaterials [J]. Biomaterials, 2000, 21: 667
20 Zhang Z, Jones D, Yue S, et al. Hierarchical tailoring of strut architecture to control permeability of additive manufactured titanium implants [J]. Mater. Sci. Eng., 2013, C33: 4055
21 Xiao J, Qiu G B. Research review of space holders of sintered titanium foams with large pores and high porosity [J]. Mater. China, 2018, 37: 372
21 肖健, 邱贵宝. 大孔径高孔隙率烧结泡沫钛的造孔剂研究述评 [J]. 中国材料进展, 2018, 37: 372
22 Qiao J C, Xi Z P, Tang H P, et al. Current status of metal porous materials by powder metallurgy technology [J]. Rare Met. Mater. Eng., 2008, 37: 2054
22 乔吉超, 奚正平, 汤慧萍 等. 粉末冶金技术制备金属多孔材料研究进展 [J]. 稀有金属材料与工程, 2008, 37: 2054
23 Li Y X, Cui Z D, Yang X J, et al. The porous TiNb24Zr4 alloys with controllable porosity fabricated by conventional sintering [J]. Adv. Mater. Res., 2011, 335-336: 797
24 Lu Z L, Xu W L, Cao J W, et al. Microstructures and properties of porous TiAl-based intermetallics prepared by freeze-casting [J]. Trans. Nonferrous Met. Soc. China, 2020, 30: 382
25 Li J R, Yu C L, Xu Z J, et al. Preparing a novel gradient porous metal fiber sintered felt with better manufacturability for hydrogen production via methanol steam reforming [J]. Int. J. Hydrogen Energy, 2019, 44: 23983
26 Zou C M, Zhang E L, Zeng S Y. Porous titanium by fiber sintering and its biomimetic Ca-P coating [J]. Rare Met. Mater. Eng., 2007, 36: 1394
26 邹鹑鸣, 张二林, 曾松岩. 纤维烧结多孔钛及其表面生长仿生Ca-P涂层 [J]. 稀有金属材料与工程, 2007, 36: 1394
27 Munir Z A, Anselmi-Tamburini U, Ohyanagi M. The effect of electric field and pressure on the synthesis and consolidation of materials: A review of the spark plasma sintering method [J]. J. Mater. Sci., 2006, 41: 763
28 Zhang F M, Otterstein E, Burkel E. Spark plasma sintering, microstructures, and mechanical properties of macroporous titanium foams [J]. Adv. Eng. Mater., 2010, 12: 863
29 McCue I, Benn E, Gaskey B, et al. Dealloying and dealloyed materials [J]. Annu. Rev. Mater. Res., 2016, 46: 263
30 Newman R C, Corcoran S G, Erlebacher J, et al. Alloy corrosion [J]. MRS Bull., 1999, 24: 24
31 Joo S H, Bae J W, Park W Y, et al. Beating thermal coarsening in nanoporous materials via high-entropy design [J]. Adv. Mater., 2020, 32: 1906160
32 Yang X X, Xu W C, Cao S, et al. An amorphous nanoporous PdCuNi-S hybrid electrocatalyst for highly efficient hydrogen production [J]. Appl. Catal., 2019, 246B: 156
33 Fujita T. Hierarchical nanoporous metals as a path toward the ultimate three-dimensional functionality [J]. Sci. Technol. Adv. Mater., 2017, 18: 724
34 Chuang A, Erlebacher J. Challenges and opportunities for integrating dealloying methods into additive manufacturing [J]. Materials, 2020, 13: 3706
35 Ding Y, Kim Y J, Erlebacher J. Nanoporous gold leaf: "Ancient technology"/advanced material [J]. Adv. Mater., 2004, 16: 1897
36 Kertis F, Snyder J, Govada L, et al. Structure/processing relationships in the fabrication of nanoporous gold [J]. JOM, 2010, 62(6): 50
37 Vega A A, Newman R C. Nanoporous metals fabricated through electrochemical dealloying of Ag-Au-Pt with systematic variation of Au:Pt ratio [J]. J. Electrochem. Soc., 2014, 161: C1
38 Ye X L, Lu N, Li X J, et al. Primary and secondary dealloying of Au(Pt)-Ag: Structural and compositional evolutions, and volume shrinkage [J]. J. Electrochem. Soc., 2014, 161: C517
39 Wang Z L, Liu P, Han J H, et al. Engineering the internal surfaces of three-dimensional nanoporous catalysts by surfactant-modified dealloying [J]. Nat. Commun., 2017, 8: 1066
40 Erlebacher J, Aziz M J, Karma A, et al. Evolution of nanoporosity in dealloying [J]. Nature, 2001, 410: 450
41 Xu W C, Zhu S L, Liang Y Q, et al. A nanoporous metal phosphide catalyst for bifunctional water splitting [J]. J. Mater. Chem., 2018, 6A: 5574
42 Wang Z L, Ning S C, Liu P, et al. Tuning surface structure of 3D nanoporous gold by surfactant-free electrochemical potential cycling [J]. Adv. Mater., 2017, 29: 1703601
43 Fu J T, Corsi J S, Welborn S S, et al. Eco-friendly synthesis of nanoporous magnesium by air-free electrolytic dealloying with recovery of sacrificial elements for energy conversion and storage applications [J]. ACS Sustain. Chem. Eng., 2021, 9: 2762
44 Shi H, Zhou Y T, Yao R Q, et al. Spontaneously separated intermetallic Co3Mo from nanoporous copper as versatile electrocatalysts for highly efficient water splitting [J]. Nat. Commun., 2020, 11: 2940
45 Xu W C, Fan G L, Zhu S L, et al. Electronic structure modulation of nanoporous cobalt phosphide by carbon doping for alkaline hydrogen evolution reaction [J]. Adv. Funct. Mater., 2021, 31: 2107333
46 Lan J, Peng M, Liu P, et al. Scalable synthesis of nanoporous boron for high efficiency ammonia electrosynthesis [J]. Mater. Today, 2020, 38: 58
47 Tan Y W, Wang H, Liu P, et al. 3D nanoporous metal phosphides toward high-efficiency electrochemical hydrogen production [J]. Adv. Mater., 2016, 28: 2951
48 Tan Y W, Wang H, Liu P, et al. Versatile nanoporous bimetallic phosphides towards electrochemical water splitting [J]. Energy Environ. Sci., 2016, 9: 2257
49 Guo X Y, Zhang C X, Tian Q H, et al. Liquid metals dealloying as a general approach for the selective extraction of metals and the fabrication of nanoporous metals: A review [J]. Mater. Today Commun., 2021, 26: 102007
50 Harrison J D, Wagner C. The attack of solid alloys by liquid metals and salt melts [J]. Acta Metall., 1959, 7: 722
51 Wada T, Yubuta K, Inoue A, et al. Dealloying by metallic melt [J]. Mater. Lett., 2011, 65: 1076
52 Okulov I V, Okulov A V, Volegov A S, et al. Tuning microstructure and mechanical properties of open porous TiNb and TiFe alloys by optimization of dealloying parameters [J]. Scr. Mater., 2018, 154: 68
53 Okulov I V, Okulov A V, Soldatov I V, et al. Open porous dealloying-based biomaterials as a novel biomaterial platform [J]. Mater. Sci. Eng., 2018, C88: 95
54 Kim J W, Tsuda M, Wada T, et al. Optimizing niobium dealloying with metallic melt to fabricate porous structure for electrolytic capacitors [J]. Acta Mater., 2015, 84: 497
55 Hadden M, Martinez-Martin D, Yong K T, et al. Recent advancements in the fabrication of functional nanoporous materials and their biomedical applications [J]. Materials, 2022, 15: 2111
56 Han J H, Li C, Lu Z, et al. Vapor phase dealloying: A versatile approach for fabricating 3D porous materials [J]. Acta Mater., 2019, 163: 161
57 Lu Z, Li C, Han J H, et al. Three-dimensional bicontinuous nanoporous materials by vapor phase dealloying [J]. Nat. Commun., 2018, 9: 276
58 Li J, Li L J, Gao Y F, et al. Preparation of nanomaterials employing template method [J]. Mater. Rep., 2011, 25(2): 5
58 李静, 李利军, 高艳芳 等. 模板法制备纳米材料 [J]. 材料导报, 2011, 25(2): 5
59 Krishnan M R, Chien Y C, Cheng C F, et al. Fabrication of mesoporous polystyrene films with controlled porosity and pore size by solvent annealing for templated syntheses [J]. Langmuir, 2017, 33: 8428
60 Tang W X, Wu X F, Li S D, et al. Co-nanocasting synthesis of mesoporous Cu-Mn composite oxides and their promoted catalytic activities for gaseous benzene removal [J]. Appl. Catal., 2015, 162B: 110
61 Masuda H, Fukuda K. Ordered metal nanohole arrays made by a two-step replication of honeycomb structures of anodic alumina [J]. Science, 1995, 268: 1466
62 Zheng M, Yang J, Zhang H. Review on preparation and applications of porous metal materials [J]. Mater. Rep., 2022, 36(18): 78
62 郑敏, 杨瑾, 张华. 多孔金属材料的制备及应用研究进展 [J]. 材料导报, 2022, 36(18): 78
63 Zhao L J, Zhang F, Peng J, et al. Research progress and application of preparation technology of porous metal materials [J]. Powder Metall. Ind., 2022, 32(5): 110
63 赵立杰, 张芳, 彭军 等. 多孔金属材料的制备工艺研究进展及应用 [J]. 粉末冶金工业, 2022, 32(5): 110
64 Furumoto T, Koizumi A, Alkahari M R, et al. Permeability and strength of a porous metal structure fabricated by additive manufacturing [J]. J. Mater. Process. Technol., 2015, 219: 10
65 Thijs L, Verhaeghe F, Craeghs T, et al. A study of the microstructural evolution during selective laser melting of Ti-6Al-4V [J]. Acta Mater., 2010, 58: 3303
66 Liu Y J, Li S J, Zhang L C, et al. Early plastic deformation behaviour and energy absorption in porous β-type biomedical titanium produced by selective laser melting [J]. Scr. Mater., 2018, 153: 99
67 Li S J, Murr L E, Cheng X Y, et al. Compression fatigue behavior of Ti-6Al-4V mesh arrays fabricated by electron beam melting [J]. Acta Mater., 2012, 60: 793
68 Cansizoglu O, Harrysson O, Cormier D, et al. Properties of Ti-6Al-4V non-stochastic lattice structures fabricated via electron beam melting [J]. Mater. Sci. Eng., 2008, A492: 468
69 Liu Y J, Wang H L, Li S J, et al. Compressive and fatigue behavior of beta-type titanium porous structures fabricated by electron beam melting [J]. Acta Mater., 2017, 126: 58
70 Walter M G, Warren E L, McKone J R, et al. Solar water splitting cells [J]. Chem. Rev., 2010, 110: 6446
71 Hansen J N, Prats H, Toudahl K K, et al. Is there anything better than Pt for HER? [J]. ACS Energy Lett., 2021, 6: 1175
72 Liu S L, Mu X Q, Duan H Y, et al. Pd nanoparticle assemblies as efficient catalysts for the hydrogen evolution and oxygen reduction reactions [J]. Eur. J. Inorg. Chem., 2017, 2017: 535
73 Yu A, Kim S Y, Lee C, et al. Boosted electron-transfer kinetics of hydrogen evolution reaction at bimetallic RhCo alloy nanotubes in acidic solution [J]. ACS Appl. Mater. Interfaces, 2019, 11: 46886
74 Xie J F, Zhang H, Li S, et al. Defect-rich MoS2 ultrathin nanosheets with additional active edge sites for enhanced electrocatalytic hydrogen evolution [J]. Adv. Mater., 2013, 25: 5807
75 Sun J S, Wen Z, Han L P, et al. Nonprecious intermetallic Al7Cu4Ni nanocrystals seamlessly integrated in freestanding bimodal nanoporous copper for efficient hydrogen evolution catalysis [J]. Adv. Funct. Mater., 2018, 28: 1706127
76 Xu X S, Deng Y X, Gu M H, et al. Large-scale synthesis of porous nickel boride for robust hydrogen evolution reaction electrocatalyst [J]. Appl. Surf. Sci., 2019, 470: 591
77 Jiang B, Guo Y N, Kim J, et al. Mesoporous metallic iridium nanosheets [J]. J. Am. Chem. Soc., 2018, 140: 12434
78 Liu Z Y, Li J H, Zhang J, et al. Ultrafine Ir nanowires with microporous channels and superior electrocatalytic activity for oxygen evolution reaction [J]. ChemCatChem, 2020, 12: 3060
79 Yao Q, Huang B L, Zhang N, et al. Channel-rich RuCu nanosheets for pH-universal overall water splitting electrocatalysis [J]. Angew. Chem. Int. Ed., 2019, 58: 13983
80 Su X R, Li X W, Ong C Y A, et al. Metallization of 3D printed polymers and their application as a fully functional water-splitting system [J]. Adv. Sci., 2019, 6: 1801670
81 You B, Sun Y J. Hierarchically porous nickel sulfide multifunctional superstructures [J]. Adv. Energy Mater., 2016, 6: 1502333
82 Wang X G, Li W, Xiong D H, et al. Fast fabrication of self-supported porous nickel phosphide foam for efficient, durable oxygen evolution and overall water splitting [J]. J. Mater. Chem., 2016, 4A: 5639
83 Shui J L, Chen C, Li J C M. Evolution of nanoporous Pt-Fe alloy nanowires by dealloying and their catalytic property for oxygen reduction reaction [J]. Adv. Funct. Mater., 2011, 21: 3357
84 Wang R Y, Xu C X, Bi X X, et al. Nanoporous surface alloys as highly active and durable oxygen reduction reaction electrocatalysts [J]. Energy Environ. Sci., 2012, 5: 5281
85 Snyder J, Fujita T, Chen M W, et al. Oxygen reduction in nanoporous metal-ionic liquid composite electrocatalysts [J]. Nat. Mater., 2010, 9: 904
86 Li J, Yin H M, Li X B, et al. Surface evolution of a Pt-Pd-Au electrocatalyst for stable oxygen reduction [J]. Nat. Energy, 2017, 2: 17111
87 Qiu H J, Fang G, Wen Y R, et al. Nanoporous high-entropy alloys for highly stable and efficient catalysts [J]. J. Mater. Chem., 2019, 7A: 6499
88 Oezaslan M, Heggen M, Strasser P. Size-dependent morphology of dealloyed bimetallic catalysts: Linking the nano to the macro scale [J]. J. Am. Chem. Soc., 2012, 134: 514
89 Xu C X, Zhang Y, Wang L Q, et al. Nanotubular mesoporous PdCu bimetallic electrocatalysts toward oxygen reduction reaction [J]. Chem. Mater., 2009, 21: 3110
90 Chen L Y, Guo H, Fujita T, et al. Nanoporous PdNi bimetallic catalyst with enhanced electrocatalytic performances for electro-oxidation and oxygen reduction reactions [J]. Adv. Funct. Mater., 2011, 21: 4364
91 Tominaka S, Hayashi T, Nakamura Y, et al. Mesoporous PdCo sponge-like nanostructure synthesized by electrodeposition and dealloying for oxygen reduction reaction [J]. J. Mater. Chem., 2010, 20: 7175
92 Tominaka S, Nakamura Y, Osaka T. Nanostructured catalyst with hierarchical porosity and large surface area for on-chip fuel cells [J]. J. Power Sources, 2010, 195: 1054
93 Lv H, Xu D D, Sun L Z, et al. Ternary palladium-boron-phosphorus alloy mesoporous nanospheres for highly efficient electrocatalysis [J]. ACS Nano, 2019, 13: 12052
94 Zeis R, Lei T, Sieradzki K, et al. Catalytic reduction of oxygen and hydrogen peroxide by nanoporous gold [J]. J. Catal., 2008, 253: 132
95 Chen C J, Zhu S L, Yang X J, et al. Electro-oxidation of ethylene glycol on nanoporous Ti-Cu amorphous alloy [J]. Electrochim. Acta, 2011, 56: 10253
96 Liu L F, Pippel E, Scholz R, et al. Nanoporous Pt-Co alloy nanowires: Fabrication, characterization, and electrocatalytic properties [J]. Nano Lett., 2009, 9: 4352
97 Liu L F, Scholz R, Pippel E, et al. Microstructure, electrocatalytic and sensing properties of nanoporous Pt46Ni54 alloy nanowires fabricated by mild dealloying [J]. J. Mater. Chem., 2010, 20: 5621
98 Deng K, Xu Y, Yang D D, et al. Pt-Ni-P nanocages with surface porosity as efficient bifunctional electrocatalysts for oxygen reduction and methanol oxidation [J]. J. Mater. Chem., 2019, 7A: 9791
99 Yin S L, Wang Z Q, Li C J, et al. Mesoporous Pt@PtM (M = Co, Ni) cage-bell nanostructures toward methanol electro-oxidation [J]. Nanoscale Adv., 2020, 2: 1084
100 Zhang J T, Liu P P, Ma H Y, et al. Nanostructured porous gold for methanol electro-oxidation [J]. J. Phys. Chem., 2007, 111C: 10382
101 Chen L Y, Lang X Y, Fujita T, et al. Nanoporous gold for enzyme-free electrochemical glucose sensors [J]. Scr. Mater., 2011, 65: 17
102 Liu Z N, Huang L H, Zhang L L, et al. Electrocatalytic oxidation ofD-glucose at nanoporous Au and Au-Ag alloy electrodes in alkaline aqueous solutions [J]. Electrochim. Acta, 2009, 54: 7286
103 Liu Z N, Du J G, Qiu C C, et al. Electrochemical sensor for detection of p-nitrophenol based on nanoporous gold [J]. Electrochem. Commun., 2009, 11: 1365
104 Chen L Y, Fujita T, Ding Y, et al. A three-dimensional gold-decorated nanoporous copper core-shell composite for electrocatalysis and nonenzymatic biosensing [J]. Adv. Funct. Mater., 2010, 20: 2279
105 Ding Y, Chen M W, Erlebacher J. Metallic mesoporous nanocomposites for electrocatalysis [J]. J. Am. Chem. Soc., 2004, 126: 6876
106 Wang R Y, Wang C, Cai W B, et al. Ultralow-platinum-loading high-performance nanoporous electrocatalysts with nanoengineered surface structures [J]. Adv. Mater., 2010, 22: 1845
107 Ge X B, Yan X L, Wang R Y, et al. Tailoring the structure and property of Pt-decorated nanoporous gold by thermal annealing [J]. J. Phys. Chem., 2009, 113C: 7379
108 Yu J S, Ding Y, Xu C X, et al. Nanoporous metals by dealloying multicomponent metallic glasses [J]. Chem. Mater., 2008, 20: 4548
109 Xu C X, Liu A H, Qiu H J, et al. Nanoporous PdCu alloy with enhanced electrocatalytic performance [J]. Electrochem. Commun., 2011, 13: 766
110 Xu C X, Liu Y Q, Wang J P, et al. Nanoporous PdCu alloy for formic acid electro-oxidation [J]. J. Power Sources, 2012, 199: 124
111 Sa Y J, Lee C W, Lee S Y, et al. Catalyst-electrolyte interface chemistry for electrochemical CO2 reduction [J]. Chem. Soc. Rev., 2020, 49: 6632
112 Li D, Wu J, Liu T T, et al. Tuning the pore structure of porous tin foam electrodes for enhanced electrochemical reduction of carbon dioxide to formate [J]. Chem. Eng. J., 2019, 375: 122024
113 Kim H, Lee H, Lim T, et al. Facile fabrication of porous Sn-based catalysts for electrochemical CO2 reduction to HCOOH and syngas [J]. J. Ind. Eng. Chem., 2018, 66: 248
114 Wang J, Wang H, Han Z Z, et al. Electrodeposited porous Pb electrode with improved electrocatalytic performance for the electroreduction of CO2 to formic acid [J]. Front. Chem. Sci. Eng., 2015, 9: 57
115 Welch A J, DuChene J S, Tagliabue G, et al. Nanoporous gold as a highly selective and active carbon dioxide reduction catalyst [J]. ACS Appl. Energy Mater., 2019, 2: 164
116 Morimoto M, Takatsuji Y, Hirata K, et al. Visualization of catalytic edge reactivity in electrochemical CO2 reduction on porous Zn electrode [J]. Electrochim. Acta, 2018, 290: 255
117 Zhao Y, Liu X L, Chen D C, et al. Atomic-level-designed copper atoms on hierarchically porous gold architectures for high-efficiency electrochemical CO2 reduction [J]. Sci. China Mater., 2021, 64: 1900
118 Yan W Y, Zhang C, Liu L. Hierarchically porous CuAg via 3D printing/dealloying for tunable CO2 reduction to syngas [J]. ACS Appl. Mater. Interfaces, 2021, 13: 45385
119 Yang P P, Zhang X L, Gao F Y, et al. Protecting copper oxidation state via intermediate confinement for selective CO2 electroreduction to C2+ fuels [J]. J. Am. Chem. Soc., 2020, 142: 6400
120 Zhong M, Tran K, Min Y M, et al. Accelerated discovery of CO2 electrocatalysts using active machine learning [J]. Nature, 2020, 581: 178
121 Nazemi M, El-Sayed M A. Electrochemical synthesis of ammonia from N2 and H2O under ambient conditions using pore-size-controlled hollow gold nanocatalysts with tunable plasmonic properties [J]. J. Phys. Chem. Lett., 2018, 9: 5160
122 Pang F J, Wang Z F, Zhang K, et al. Bimodal nanoporous Pd3Cu1 alloy with restrained hydrogen evolution for stable and high yield electrochemical nitrogen reduction [J]. Nano Energy, 2019, 58: 834
123 Wang X J, Luo M, Lan J, et al. Nanoporous intermetallic Pd3Bi for efficient electrochemical nitrogen reduction [J]. Adv. Mater., 2021, 33: 2007733
124 Xu W C, Fan G L, Chen J L, et al. Nanoporous palladium hydride for electrocatalytic N2 reduction under ambient conditions [J]. Angew. Chem. Int. Ed., 2020, 59: 3511
125 Pang F J, Wang F, Yang L T, et al. Hierarchical nanoporous Pd1Ag1 alloy enables efficient electrocatalytic nitrogen reduction under ambient conditions [J]. Chem. Commun., 2019, 55: 10108
126 Fan G L, Xu W C, Li J H, et al. Nanoporous NiSb to enhance nitrogen electroreduction via tailoring competitive adsorption sites [J]. Adv. Mater., 2021, 33: 2101126
127 Wang H J, Yu H J, Wang Z Q, et al. Electrochemical fabrication of porous Au film on Ni foam for nitrogen reduction to ammonia [J]. Small, 2019, 15: 1804769
128 Yang Y J, Wang S Q, Wen H M, et al. Nanoporous gold embedded ZIF composite for enhanced electrochemical nitrogen fixation [J]. Angew. Chem. Int. Ed., 2019, 58: 15362
129 Xiao L, Zhu S L, Liang Y Q, et al. Effects of hydrophobic layer on selective electrochemical nitrogen fixation of self-supporting nanoporous Mo4P3 catalyst under ambient conditions [J]. Appl. Catal., 2021, 286B: 119895
130 Rezwan K, Chen Q Z, Blaker J J, et al. Biodegradable and bioactive porous polymer/inorganic composite scaffolds for bone tissue engineering [J]. Biomaterials, 2006, 27: 3413
131 Geng Z, Cui Z D, Li Z Y, et al. Synthesis, characterization and the formation mechanism of magnesium- and strontium-substituted hydroxyapatite [J]. J. Mater. Chem., 2015, 3B: 3738
132 Geng Z, Cui Z D, Li Z Y, et al. Strontium incorporation to optimize the antibacterial and biological characteristics of silver-substituted hydroxyapatite coating [J]. Mater. Sci. Eng., 2016, C58: 467
133 Wu S L, Liu X M, Yeung K W K, et al. Biomimetic porous scaffolds for bone tissue engineering [J]. Mater. Sci. Eng., 2014, R80: 1
134 Niinomi M. Mechanical properties of biomedical titanium alloys [J]. Mater. Sci. Eng., 1998, A243: 231
135 Li Q, Niinomi M, Nakai M, et al. Improvements in the superelasticity and change in deformation mode of β-type TiNb24Zr2 alloys caused by aging treatments [J]. Metall. Mater. Trans., 2011, 42A: 2843
136 Deng S H, Yang X J, Zhu S L, et al. Biomedical properties of porous NiTi shape memory alloy and its prospect in medical application [J]. Heat Treat. Met., 2003, 28(12): 12
136 邓松华, 杨贤金, 朱胜利 等. 多孔NiTi形状记忆合金的生物医学特性及其医用前景 [J]. 金属热处理, 2003, 28(12): 12
137 Hu F, Zhu S L, Yang X J. Progress in research on normal sintering of porous TiNi alloys [J]. Heat Treat. Met., 2002, 27(7): 6
137 胡飞, 朱胜利, 杨贤金. 用粉末冶金法制备医用多孔TiNi合金的研究 [J]. 金属热处理, 2002, 27(7): 6
138 Liu S M, Yang X J, Cui Z D, et al. Effect of voltage on properties of the ceramic coatings prepared by micro-arc oxidation on titanium [J]. Mater. Rep., 2011, 25(16): 8
138 刘世敏, 杨贤金, 崔振铎 等. 电压对钛表面微弧氧化陶瓷层特性的影响 [J]. 材料导报, 2011, 25(16): 8
139 Zhu S L, Yang X J, Hu F, et al. Pore features of porous TiNi alloy sintered in argon atmosphere [J]. Trans. Met. Heat Treat., 2003, 24(4): 51
139 朱胜利, 杨贤金, 胡飞 等. 氩气保护烧结多孔TiNi合金孔隙特征的研究 [J]. 金属热处理学报, 2003, 24(4): 51
140 Chen M F, Yang X J, He F, et al. Effect of NaOH concentration on formation of bone-like apatite layer on NiTi shape memory alloy [J]. Acta Metall. Sin., 2003, 39: 859
140 陈民芳, 杨贤金, 何菲 等. NaOH浓度对NiTi形状记忆合金表面类骨磷灰石形成的影响 [J]. 金属学报, 2003, 39: 859
141 Hu R X, Yang X J, Chen M F, et al. Optimization of bioactive layer processing using chemical method on the surface of NiTi SMA [J]. Heat Treat. Met., 2003, 28(10): 42
141 胡荣香, 杨贤金, 陈民芳 等. NiTi形状记忆合金表面化学法制备生物活性层工艺的优化 [J]. 金属热处理, 2003, 28(10): 42
142 Li Y X, Cui Z D, Yang X J, et al. Corrosion behavior of porous Ti-24Nb-4Zr alloy in different simulated body fluids [J]. Adv. Mater. Res., 2012, 399-401: 1577
143 Liang C Y, Wang H S, Yang J J, et al. Femtosecond laser-induced micropattern and Ca/P deposition on Ti implant surface and its acceleration on early osseointegration [J]. ACS Appl. Mater. Interfaces, 2013, 5: 8179
144 Lai M, Gao Y, Yuan B, et al. Effect of pore structure regulation on the properties of porous TiNbZr shape memory alloys for biomedical application [J]. J. Mater. Eng. Perform., 2015, 24: 136
145 Kuczyńska-Zem?a D, Kijeńska-Gawrońska E, Pisarek M, et al. Effect of laser functionalization of titanium on bioactivity and biological response [J]. Appl. Surf. Sci., 2020, 525: 146492
146 Harrysson O L A, Cansizoglu O, Marcellin-Little D J, et al. Direct metal fabrication of titanium implants with tailored materials and mechanical properties using electron beam melting technology [J]. Mater. Sci. Eng., 2008, C28: 366
147 Zhang J H, Sun Y Y, Guo A L, et al. Research progress of 3D printing magnesium-based biomaterials for bone defect repair [J]. Chin. J. Bone Joint Surg., 2021, 14: 826
147 张剑华, 孙元艺, 郭阿龙 等. 3D打印含镁生物医用材料用于骨缺损修复研究进展 [J]. 中华骨与关节外科杂志, 2021, 14: 826
148 Kiani F, Wen C E, Li Y C. Prospects and strategies for magnesium alloys as biodegradable implants from crystalline to bulk metallic glasses and composites—A review [J]. Acta Biomater., 2020, 103: 1
149 Anvari-Yazdi A F, Tahermanesh K, Hadavi S M M, et al. Cytotoxicity assessment of adipose-derived mesenchymal stem cells on synthesized biodegradable Mg-Zn-Ca alloys [J]. Mater. Sci. Eng., 2016, C69: 584
150 Gu X N, Zheng Y F, Cheng Y, et al. In vitro corrosion and biocompatibility of binary magnesium alloys [J]. Biomaterials, 2009, 30: 484
151 Li Y G, Jahr H, Zhou J, et al. Additively manufactured biodegradable porous metals [J]. Acta Biomater., 2020, 115: 29
152 Gu X N, Li N, Zhou W R, et al. Corrosion resistance and surface biocompatibility of a microarc oxidation coating on a Mg-Ca alloy [J]. Acta Biomater., 2011, 7: 1880
153 Yazdimamaghani M, Razavi M, Vashaee D, et al. Development and degradation behavior of magnesium scaffolds coated with polycaprolactone for bone tissue engineering [J]. Mater. Lett., 2014, 132: 106
154 Lai Y X, Li Y, Cao H J, et al. Osteogenic magnesium incorporated into PLGA/TCP porous scaffold by 3D printing for repairing challenging bone defect [J]. Biomaterials, 2019, 197: 207
155 Wang J L, Wu Y H, Li H F, et al. Magnesium alloy based interference screw developed for ACL reconstruction attenuates peri-tunnel bone loss in rabbits [J]. Biomaterials, 2018, 157: 86
156 Zheng Y F, Xia D D, Shen Y N, et al. Additively manufactured biodegrabable metal implants [J]. Acta Metall. Sin., 2021, 57: 1499
156 郑玉峰, 夏丹丹, 谌雨农 等. 增材制造可降解金属医用植入物 [J]. 金属学报, 2021, 57: 1499
157 Li Y, Jahr H, Pavanram P, et al. Additively manufactured functionally graded biodegradable porous iron [J]. Acta Biomater., 2019, 96: 646
158 Nie Y, Chen G, Peng H B, et al. In vitro and 48 weeks in vivo performances of 3D printed porous Fe-30Mn biodegradable scaffolds [J]. Acta Biomater., 2021, 121: 724
159 Liu Y, Zheng Y F, Chen X H, et al. Fundamental theory of biodegradable metals—Definition, criteria, and design [J]. Adv. Funct. Mater., 2019, 29: 1805402
160 Li Y, Pavanram P, Zhou J, et al. Additively manufactured biodegradable porous zinc [J]. Acta Biomater., 2020, 101: 609
161 Moon S K, Kim C K, Joo U H, et al. Biological evaluation of micro-nanoporous layer on Ti-Ag alloy for dental implant [J]. Int. J. Mater. Res., 2012, 103: 749
162 Xiong Y Z, Wang W, Gao R N, et al. Fatigue behavior and osseointegration of porous Ti-6Al-4V scaffolds with dense core for dental application [J]. Mater. Des., 2020, 195: 108994
163 Chahine G, Koike M, Okabe T, et al. The design and production of Ti-6Al-4V ELI customized dental implants [J]. JOM, 2008, 60(11): 50
164 He F, Zhang X, Peng W, et al. Research progress on porous tantalum coating in dental implants [J]. J. Dalian Med. Univ., 2019, 41: 458
164 何帆, 张新, 彭巍 等. 多孔钽涂层在牙种植体中的应用及研究进展 [J]. 大连医科大学学报, 2019, 41: 458
165 Balla V K, Bodhak S, Bose S, et al. Porous tantalum structures for bone implants: Fabrication, mechanical and in vitro biological properties [J]. Acta Biomater., 2010, 6: 3349
166 Wang Q, Zhang H, Li Q J, et al. Biocompatibility and osteogenic properties of porous tantalum [J]. Exp. Ther. Med., 2015, 9: 780
167 Lee J W, Wen H B, Gubbi P, et al. New bone formation and trabecular bone microarchitecture of highly porous tantalum compared to titanium implant threads: A pilot canine study [J]. Clin. Oral Implants Res., 2018, 29: 164
168 Wu L J, Dong Y W, Yao L T, et al. Nanoporous tantalum coated zirconia implant improves osseointegration [J]. Ceram. Int., 2020, 46: 17437
Outlines

/