Inhomogeneity Analyses of Microstructure and Mechanical Properties of TC21 Titanium Alloy Variable Cross-section Die Forgings for Aviation
Received date: 2022-06-23
Revised date: 2022-09-11
Online published: 2022-10-08
Supported by
National Natural Science Foundation of China(51871225);National Natural Science Foundation of China(U2106215);Deyang City Science and Technology Project(2021JBJZ011)
TC21 titanium alloy has been successfully used in the structural die forgings of aviation owing to its excellent damage tolerance. However, because of the difference in the equivalent strains of die forgings, the microstructure and properties of variable cross-sections are considerably different, affecting the service life of the structural parts. Therefore, the microstructure and mechanical properties of β-forged TC21 titanium alloy die forgings with variable cross-sections were characterized using Deform software simulation, OM, SEM, XRD, EBSD, and tensile and impact tests, and the primary factors affecting the tensile and impact properties as well as their anisotropy were comprehensively analyzed. The results showed that the overall shape of the die forgings was complex and the effective strain was concentrated in the range of 0.75-1.20. The evidence of the flow was obvious at high strain, the substructure increased, and the narrow cross-section led to a faster cooling rate. This resulted in the decrease of αp content and refinement of αs, which together led to the increase in strength. The evolution of various texture components under high strain during thermal deformation and heat treatment was analyzed, and finally the strong texture of residual β phase <110>//LD and {0002} weak texture of transformed α phase were formed. The strength anisotropy caused by the strong texture was analyzed from α phase slip system and β phase densely packed plane. The impact load-displacement curves showed that the impact energy was mainly consumed via the initiation energy. Combining with the prior β grain arrangement, the fracture modes of impact and tensile fracture in different orientations were discussed. Finally, a tensile fracture model was proposed, which explained the reason that there was a good strength and plastic matching at a high strain of 1.20. This work provides material research support for optimizing the uniformity design of TC21 alloy variable cross-section die forgings.
Key words: TC21 titanium alloy; die forging; effective strain; texture; mechanical property
YANG Jie , HUANG Sensen , YIN Hui , ZHAI Ruizhi , MA Yingjie , XIANG Wei , LUO Hengjun , LEI Jiafeng , YANG Rui . Inhomogeneity Analyses of Microstructure and Mechanical Properties of TC21 Titanium Alloy Variable Cross-section Die Forgings for Aviation[J]. Acta Metall Sin, 2024 , 60(3) : 333 -347 . DOI: 10.11900/0412.1961.2022.00313
| 1 | Zhang F, Dou Z L, Zou Y B. Application status and development trend of aeronautical forging technology [J]. Aeronaut. Manuf. Technol., 2015, (7): 60 |
| 张 方, 窦忠林, 邹彦博. 航空锻造技术的应用现状及发展趋势 [J]. 航空制造技术, 2015, (7): 60 | |
| 2 | Gao L. Investigations on precision forming technology and manufacture of aviation large die forgings [D]. Chongqing: Chongqing University, 2019 |
| 高 林. 大型航空模锻件整体精密成形工艺技术研究与试制 [D]. 重庆: 重庆大学, 2019 | |
| 3 | Yang R, Ma Y J, Lei J F, et al. Toughening high strength titanium alloys through fine tuning phase composition and refining microstructure [J]. Acta Metall. Sin., 2021, 57: 1455 |
| 杨 锐, 马英杰, 雷家峰 等. 高强韧钛合金组成相成分和形态的精细调控 [J]. 金属学报, 2021, 57: 1455 | |
| 4 | Saurabh A, Meghana C M, Singh P K, et al. Titanium-based materials: Synthesis, properties, and applications [J]. Mater. Today Proc., 2022, 56: 412 |
| 5 | Banerjee D, Williams J C. Perspectives on titanium science and technology [J]. Acta Mater., 2013, 61: 844 |
| 6 | Tan C S, Sun Q Y, Zhang G J, et al. Remarkable increase in high-cycle fatigue resistance in a titanium alloy with a fully lamellar microstructure [J]. Int. J. Fatigue, 2020, 138: 105724 |
| 7 | Wang S, Liang Y L, Sun H, et al. Thermomechanical treatment-induced microstructure refinement to optimize mechanical properties of TC21 titanium alloys [J]. Mater. Sci. Eng., 2021, A812: 141095 |
| 8 | Shao H, Zhao Y Q, Ge P, et al. Crack initiation and mechanical properties of TC21 titanium alloy with equiaxed microstructure [J]. Mater. Sci. Eng., 2013, A586: 215 |
| 9 | Lei L, Zhao Q Y, Zhao Y Q, et al. Study on the intrinsic factors determining impact toughness of TC21 alloy [J]. Mater. Charact., 2021, 177: 111164 |
| 10 | Zhou X H, Liu W, Hao F, et al. Influence of quasi-β forging process on microstructure and properties of TC21 titanium alloy large forgings [J]. Forg. Stamp. Technol., 2020, 45: 29 |
| 周晓虎, 刘 卫, 郝 芳 等. 准β锻造工艺对TC21钛合金大型锻件组织及性能的影响 [J]. 锻压技术, 2020, 45: 29 | |
| 11 | Shi Z F, Guo H Z, Liu R, et al. Microstructure and mechanical properties of TC21 titanium alloy by near-isothermal forging [J]. Trans. Nonferrous Met. Soc. China, 2015, 25: 72 |
| 12 | Shi Z F, Guo H Z, Han J Y, et al. Microstructure and mechanical properties of TC21 titanium alloy after heat treatment [J]. Trans. Nonferrous Met. Soc. China, 2013, 23: 2882 |
| 13 | Zhu W G, Lei J, Su B, et al. The interdependence of microstructure, strength and fracture toughness in a novel β titanium alloy Ti-5Al-4Zr-8Mo-7V [J]. Mater. Sci. Eng., 2020, A782: 139248 |
| 14 | Chen W, Zeng W D, Zhao Y H, et al. Fracture toughness anisotropy of Ti17 billet processed by the β forging [J]. Mater. Sci. Eng., 2021, A807: 140825 |
| 15 | Liu Z, Liu J R, Zhao Z B, et al. Microstructure and tensile property of TC4 alloy produced via electron beam rapid manufacturing [J]. Acta Metall. Sin., 2019, 55: 692 |
| 刘 征, 刘建荣, 赵子博 等. 电子束快速成形制备TC4合金的组织和拉伸性能分析 [J]. 金属学报, 2019, 55: 692 | |
| 16 | Li W Y, Chen Z Y, Liu J R, et al. Rolling texture and its effect on tensile property of a near-α titanium alloy Ti60 plate [J]. J. Mater. Sci. Technol., 2019, 35: 790 |
| 17 | Wu Z H, Kou H C, Chen N N, et al. The effect of cubic-texture on fatigue cracking in a metastable β titanium alloy subjected to high-cycle fatigue [J]. Int. J. Fatigue, 2020, 141: 105872 |
| 18 | Chen J H, Li J S, Tang B, et al. Microstructure and texture evolution of a near β titanium alloy Ti-7333 during continuous cooling hot deformation [J]. Prog. Nat. Sci. Mater. Int., 2019, 29: 50 |
| 19 | Li J S, Dong R F, Kou H C, et al. Texture evolution and the recrystallization behavior in a near β titanium alloy Ti-7333 during the hot-rolling process [J]. Mater. Charact., 2020, 159: 109999 |
| 20 | Xu Z W, Liu A, Wang X S. Influence of macrozones on the fatigue cracking behavior and fracture mechanisms of rolled Ti-6Al-4V alloy [J]. Mater. Sci. Eng., 2021, A824: 141824 |
| 21 | Tchorzewski R M, Hutchinson W B. Effect of texture on fatigue crack path in titanium-6Al-4V [J]. Met. Sci., 1978, 12: 109 |
| 22 | Tchorzewski R M, Hutchinson W B. Anisotropy of fracture toughness in textured titanium-6Al-4V alloy [J]. Metall. Trans., 1978, 9A: 1113 |
| 23 | Yan M Q, Chen L Q, Yang P, et al. Effect of hot deformation parameters on the evolution of microstructure and texture of β phase in TC18 titanium alloy [J]. Acta Metall. Sin., 2021, 57: 880 |
| 颜孟奇, 陈立全, 杨 平 等. 热变形参数对TC18钛合金β相组织及织构演变规律的影响 [J]. 金属学报, 2021, 57: 880 | |
| 24 | Miyamoto H, Xiao T, Uenoya T, et al. Effect of simple shear deformation prior to cold rolling on texture and ridging of 16% Cr ferritic stainless steel sheets [J]. ISIJ Int., 2010, 50: 1653 |
| 25 | Li W Y. Study on texture and mechanical anisotropy of Ti60 high temperature titanium alloy plates [D]. Beijing: University of Chinese Academy of Sciences, 2017 |
| 李文渊. Ti60高温钛合金板材织构及力学性能各向异性研究 [D]. 北京: 中国科学院大学, 2017 | |
| 26 | Zhao Z B, Wang Q J, Hu Q M, et al. Effect of β (110) texture intensity on α-variant selection and microstructure morphology during β→α phase transformation in near α titanium alloy [J]. Acta Mater., 2017, 126: 372 |
| 27 | Lei L, Zhao Q Y, Wu C, et al. Variant selection, coarsening behavior of α phase and associated tensile properties in an α + β titanium alloy [J]. J. Mater. Sci. Technol., 2022, 99: 101 |
| 28 | Leo Prakash D G, Honniball P, Rugg D, et al. The effect of β phase on microstructure and texture evolution during thermomechanical processing of α + β Ti alloy [J]. Acta Mater., 2013, 61: 3200 |
| 29 | Germain L, Gey N, Humbert M, et al. Analysis of sharp microtexture heterogeneities in a bimodal IMI 834 billet [J]. Acta Mater., 2005, 53: 3535 |
| 30 | Wen X, Wan M P, Huang C W, et al. Strength and fracture toughness of TC21 alloy with multi-level lamellar microstructure [J]. Mater. Sci. Eng., 2019, A740-741: 121 |
| 31 | Ye X W, Wan M P, Huang C W, et al. Effect of aging temperature on mechanical properties of TC21 alloy with multi-level lamellar microstructure [J]. Mater. Sci. Eng., 2022, A840: 142825 |
| 32 | Won J W, Park K T, Hong S G, et al. Anisotropic yielding behavior of rolling textured high purity titanium [J]. Mater. Sci. Eng., 2015, A637: 215 |
| 33 | Dong R F, Li J S, Kou H C, et al. Dependence of mechanical properties on the microstructure characteristics of a near β titanium alloy Ti-7333 [J]. J. Mater. Sci. Technol., 2019, 35: 48 |
| 34 | Duan Q Q, Qu R T, Zhang P, et al. Intrinsic impact toughness of relatively high strength alloys [J]. Acta Mater., 2018, 142: 226 |
/
| 〈 |
|
〉 |