Recrystallization Controlling in a Cold-Rolled Medium Mn Steel and Its Effect on Mechanical Properties
Received date: 2022-07-20
Revised date: 2022-09-18
Online published: 2022-09-30
Supported by
National Natural Science Foundation of China(52071322)
Owing to the excellent combination of specific strength and ductility, medium Mn steels (MMSs) with Mn contents of 3%-12% (mass fraction) are considered the most promising candidates for the third-generation advanced high-strength steel. The combination of excellent strength-ductility is mainly attributed to the active transformation-induced plasticity effect of the metastable retained austenite during deformation. Therefore, producing a considerable amount of retained austenite with reasonable stabilities in the steel by various heat treatment schedules is always important. In this study, granular- and lamellar-structured retained austenites were developed in a cold-rolled 0.15C-5Mn MMS by introducing a technical process of precontrolling ferrite recrystallization in the annealing schedule. The microstructures of the annealed samples were analyzed using SEM, EBSD, and TEM. The results show that duplex microstructures comprising various amounts of recrystallized ferrite and fresh martensite can be obtained in the cold-rolled MMS when controlling the occurrence of recrystallization at different intercritical temperatures by a preannealing process. When this microstructure is used for the final austenite reverted transformation annealing, the resultant ultrafine duplex microstructure with recrystallized ferrite and two types of heterogeneous retained austenite, i.e., lamellar and granular, is produced. The heterogeneous-structured austenite shows more sensitivity to increasing strain, i.e., various mechanical stabilities, which enable an excellent strength-ductility combination and reduced Lüders strain in the cold-rolled medium Mn steel.
HU Baojia , ZHENG Qinyuan , LU Yi , JIA Chunni , LIANG Tian , ZHENG Chengwu , LI Dianzhong . Recrystallization Controlling in a Cold-Rolled Medium Mn Steel and Its Effect on Mechanical Properties[J]. Acta Metall Sin, 2024 , 60(2) : 189 -200 . DOI: 10.11900/0412.1961.2022.00350
| 1 | Yang D P, Du P J, Wu D, et al. The microstructure evolution and tensile properties of medium-Mn steel heat-treated by a two-step annealing process [J]. J. Mater. Sci. Technol., 2021, 75: 205 |
| 2 | Huang L, Deng X T, Liu J, et al. Relationship between retained austenite stability and cryogenic impact toughness in 0.12C-3.0Mn low carbon medium manganese steel [J]. Acta Metall. Sin., 2017, 53: 316 |
| 黄 龙, 邓想涛, 刘 佳 等. 0.12C-3.0Mn低碳中锰钢中残余奥氏体稳定性与低温韧性的关系 [J]. 金属学报, 2017, 53: 316 | |
| 3 | Chen S, Hu J, Shan L Y, et al. Characteristics of bainitic transformation and its effects on the mechanical properties in quenching and partitioning steels [J]. Mater. Sci. Eng., 2021, A803: 140706 |
| 4 | Hu B J, Zheng Q Y, Jia C N, et al. Improvement of mechanical properties of a medium-Mn TRIP steel by precursor microstructure control [J]. Acta Metall. Sin. (Engl. Lett.), 2022, 35: 1068 |
| 5 | Cai M H, Huang H S, Pan H J, et al. Microstructure and tensile properties of a Nb-Mo microalloyed 6.5Mn alloy processed by intercritical annealing and quenching and partitioning [J]. Acta Metall. Sin. (Engl. Lett.), 2017, 30: 665 |
| 6 | Lu Q, Lai Q Q, Chai Z S, et al. Revolutionizing car body manufacturing using a unified steel metallurgy concept [J]. Sci. Adv., 2021, 7: eabk0176 |
| 7 | Yang F, Luo H W, Dong H. Effects of intercritical annealing temperature on the tensile behavior of cold rolled 7Mn steel and the constitutive modeling [J]. Acta Metall. Sin., 2018, 54: 859 |
| 阳 锋, 罗海文, 董 瀚. 退火温度对冷轧7Mn钢拉伸行为的影响及模拟研究 [J]. 金属学报, 2018, 54: 859 | |
| 8 | Cai M H, Huang H S, Su J H, et al. Enhanced tensile properties of a reversion annealed 6.5Mn-TRIP alloy via tailoring initial microstructure and cold rolling reduction [J]. J. Mater. Sci. Technol., 2018, 34: 1428 |
| 9 | Hu J, Du L X, Xu W, et al. Ensuring combination of strength, ductility and toughness in medium-manganese steel through optimization of nano-scale metastable austenite [J]. Mater. Charact., 2018, 136: 20 |
| 10 | Liang J H, Zhao Z Z, Tang D, et al. Improved microstructural homogeneity and mechanical property of medium manganese steel with Mn segregation banding by alternating lath matrix [J]. Mater. Sci. Eng., 2018, A711: 175 |
| 11 | Yan S, Liu X H, Liang T S, et al. The effects of the initial microstructure on microstructural evolution, mechanical properties and reversed austenite stability of intercritically annealed Fe-6.1Mn-1.5Si-0.12C steel [J]. Mater. Sci. Eng., 2018, A712: 332 |
| 12 | Li Y, Li W, Min N, et al. Mechanical response of a medium manganese steel with encapsulated austenite [J]. Scr. Mater., 2020, 178: 211 |
| 13 | Luo L B, Li W, Liu S L, et al. Effect of intermediate temperature annealing on the stability of retained austenite and mechanical properties of medium Mn-TRIP steel [J]. Mater. Sci. Eng., 2019, A742: 69 |
| 14 | LI X, Song R B, Zhou N P, et al. An ultrahigh strength and enhanced ductility cold-rolled medium-Mn steel treated by intercritical annealing [J]. Scr. Mater., 2018, 154: 30 |
| 15 | Xu Y B, Zou Y, Hu Z P, et al. Correlation between deformation behavior and austenite characteristics in a Mn-Al type TRIP steel [J]. Mater. Sci. Eng., 2017, A698: 126 |
| 16 | Shen G H, Hu B, Yang Z B, et al. Influence of tempering temperature on mechanical properties and microstructures of high-Al-contained medium Mn steel having δ-ferrite [J]. Acta Metall. Sin., 2022, 58: 165 |
| 沈国慧, 胡 斌, 杨占兵 等. 回火温度对含δ铁素体高铝中锰钢力学性能和微观组织的影响 [J]. 金属学报, 2022, 58: 165 | |
| 17 | Zhou C, Ye Q B, Hu J, et al. Ultra-high-strength multi-alloyed steel with enhanced cryogenic toughness using thermally stable retained austenite [J]. Mater. Sci. Eng., 2022, A831: 142356 |
| 18 | Hui W J, Shao C W, Zhang Y J, et al. Microstructure and mechanical properties of medium Mn steel containing 3%Al processed by warm rolling [J]. Mater. Sci. Eng., 2017, A707: 501 |
| 19 | Cheng P, Hu B, Liu S L, et al. Influence of retained austenite and Cu precipitates on the mechanical properties of a cold-rolled and intercritically annealed medium Mn steel [J]. Mater. Sci. Eng., 2019, A746: 41 |
| 20 | Wei X, Zhang X L, Cai M H, et al. Stress-state-dependent deformation and fracture behaviors in a cold-rolled 7Mn steel [J]. Mater. Sci. Eng., 2022, A831: 142102 |
| 21 | Zhang Y, Ding H. Ultrafine also can be ductile: On the essence of Lüders band elongation in ultrafine-grained medium manganese steel [J]. Mater. Sci. Eng., 2018, A733: 220 |
| 22 | Hu B, Tu X, Wang Y, et al. Recent progress and future research prospects on the plastic instability of medium-Mn steels: A review [J]. Chin. J. Eng., 2020, 42: 48 |
| 胡 斌, 屠 鑫, 王 玉 等. 中锰钢塑性失稳现象的研究进展及未来研究展望 [J]. 工程科学学报, 2020, 42: 48 | |
| 23 | Yan S, Li T L, Liang T S, et al. By controlling recrystallization degree: A plain medium Mn steel overcoming Lüders deformation and low yield-to-tensile ratio simultaneously [J]. Mater. Sci. Eng., 2019, A758: 79 |
| 24 | Li Z C, Ding H, Misra R D K, et al. Deformation behavior in cold-rolled medium-manganese TRIP steel and effect of pre-strain on the Lüders bands [J]. Mater. Sci. Eng., 2017, A679: 230 |
| 25 | Zhao Z Z, Liang J H, Zhao A M, et al. Effects of the austenitizing temperature on the mechanical properties of cold-rolled medium-Mn steel system [J]. J. Alloys Compd., 2017, 691: 51 |
| 26 | Wang H S, Zhang Y X, Yuan G, et al. Significance of cold rolling reduction on Lüders band formation and mechanical behavior in cold-rolled intercritically annealed medium-Mn steel [J]. Mater. Sci. Eng., 2018, A737: 176 |
| 27 | Zou Y, Xu Y B, Hu Z P, et al. High strength-toughness combination of a low-carbon medium-manganese steel plate with laminated microstructure and retained austenite [J]. Mater. Sci. Eng., 2017, A707: 270 |
| 28 | Han J, Kang S H, Lee S J, et al. Fabrication of bimodal-grained Al-free medium Mn steel by double intercritical annealing and its tensile properties [J]. J. Alloys Compd., 2016, 681: 580 |
| 29 | Han J, Lee S J, Jung J G, et al. The effects of the initial martensite microstructure on the microstructure and tensile properties of intercritically annealed Fe-9Mn-0.05C steel [J]. Acta Mater., 2014, 78: 369 |
| 30 | Luo H W, Dong H, Huang M X. Effect of intercritical annealing on the Lüders strains of medium Mn transformation-induced plasticity steels [J]. Mater. Des., 2015, 83: 42 |
| 31 | Wan X H, Liu G, Yang Z G, et al. Flash annealing yields a strong and ductile medium Mn steel with heterogeneous microstructure [J]. Scr. Mater., 2021, 198: 113819 |
| 32 | Ma J W, Lu Q, Sun L, et al. Two-step intercritical annealing to eliminate Lüders band in a strong and ductile medium Mn steel [J]. Metall. Mater. Trans., 2018, 49A: 4404 |
| 33 | Kim M T, Park T M, Baik K H, et al. Effects of cold rolling reduction ratio on microstructures and tensile properties of intercritically annealed medium-Mn steels [J]. Mater. Sci. Eng., 2019, A752: 43 |
| 34 | Zhang X L, Yan J H, Liu T, et al. Microstructural evolution and mechanical behavior of a novel heterogeneous medium Mn cold-rolled steel [J]. Mater. Sci. Eng., 2021, A800: 140344 |
| 35 | Wan X H, Liu G, Ding R, et al. Stabilizing austenite via a core-shell structure in the medium Mn steels [J]. Scr. Mater., 2019, 166: 68 |
| 36 | Hu B J, Zheng C W, Zheng Q Y, et al. Ultra-fine heterogeneous microstructure enables high strength-ductility in a cold-rolled medium Mn steel [J]. Acta Metall. Sin. (Engl. Lett.), 2022, 35: 1712 |
| 37 | Wang C Y, Shi J, Cao W Q, et al. Characterization of microstructure obtained by quenching and partitioning process in low alloy martensitic steel [J]. Mater. Sci. Eng., 2010, A527: 3442 |
| 38 | Lee S, Lee K, De Cooman B C. Observation of the TWIP + TRIP plasticity-enhancement mechanism in Al-added 6 wt pct medium Mn steel [J]. Metall. Mater. Trans., 2015, 46A: 2356 |
| 39 | De Cooman B C, Lee S J, Shin S, et al. Combined intercritical annealing and Q&P processing of medium Mn steel [J]. Metall. Mater. Trans., 2017, 48A: 39 |
| 40 | Hu B, Shen X, Gao Q Y, et al. Yielding behavior of triplex medium Mn steel alternated with cooling strategies altering martensite/ferrite interfacial feature [J]. J. Mater. Sci. Technol., 2022, 126: 60 |
| 41 | Jeong M S, Park T M, Choi S, et al. Recovering the ductility of medium-Mn steel by restoring the original microstructure [J]. Scr. Mater., 2021, 190: 16 |
| 42 | Lai Q Q, Gouné M, Perlade A, et al. Mechanism of austenite formation from spheroidized microstructure in an intermediate Fe-0.1C-3.5Mn steel [J]. Metall. Mater. Trans., 2016, 47A: 3375 |
| 43 | Chen L S, Zhang J Y, Tian Y Q, et al. Effect of Mn pre-partitioning on C partitioning and retained austenite of Q&P Steels [J]. Acta Metall. Sin., 2015, 51: 527 |
| 陈连生, 张健杨, 田亚强 等. 预先Mn配分处理对Q&P钢中C配分及残余奥氏体的影响 [J]. 金属学报, 2015, 51: 527 | |
| 44 | Rao P M, Sarma V S, Sankaran S. Microstructure and mechanical properties of V-Nb microalloyed ultrafine-grained dual-phase steels processed through severe cold rolling and intercritical annealing [J]. Metall. Mater. Trans., 2017, 48A: 1176 |
| 45 | Hu J, Du L X, Sun G S, et al. The determining role of reversed austenite in enhancing toughness of a novel ultra-low carbon medium manganese high strength steel [J]. Scr. Mater., 2015, 104: 87 |
| 46 | Shao C W, Hui W J, Zhang Y J, et al. Microstructure and mechanical properties of a novel cold rolled medium-Mn steel with superior strength and ductility [J]. Acta Metall. Sin., 2019, 55: 191 |
| 邵成伟, 惠卫军, 张永健 等. 一种新型高强度高塑性冷轧中锰钢的组织和力学性能 [J]. 金属学报, 2019, 55: 191 | |
| 47 | Sun B H, Ma Y, Vanderesse N, et al. Macroscopic to nanoscopic in situ investigation on yielding mechanisms in ultrafine grained medium Mn steels: Role of the austenite-ferrite interface [J]. Acta Mater., 2019, 178: 10 |
| 48 | Hu J, Zhang J M, Sun G S, et al. High strength and ductility combination in nano-/ultrafine-grained medium-Mn steel by tuning the stability of reverted austenite involving intercritical annealing [J]. J. Mater. Sci., 2019, 54: 6565 |
| 49 | Ma J W, Liu H T, Lu Q, et al. Transformation kinetics of retained austenite in the tensile Lüders strain range in medium Mn steel [J]. Scr. Mater., 2019, 169: 1 |
/
| 〈 |
|
〉 |