Research paper

Effect of δ-Ferrite on Hot Deformation and Recrystallization of 316KD Austenitic Stainless Steel for Sodium-Cooled Fast Reactor Application

  • CHEN Shenghu ,
  • WANG Qiyu ,
  • JIANG Haichang ,
  • RONG Lijian
Expand
  • 1CAS Key Laboratory of Nuclear Materials and Safety Assessment, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
    2School of Materials Science and Engineering, University of Science and Technology of China, Shenyang 110016, China
RONG Lijian, professor, Tel: (024)23971979, E-mail: ljrong@imr.ac.cn

Received date: 2022-01-27

  Revised date: 2022-03-16

  Online published: 2022-09-26

Supported by

National Natural Science Foundation of China(51871218);Youth Innovation Promotion Association CAS(2018227);CNNC Science Fund for Talented Young Scholars

Abstract

The sodium-cooled fast reactor is the most mature reactor among generation-IV nuclear reactors. A carbon/nitrogen-controlled 316KD austenitic stainless steel has been developed for the construction of pressure vessels and internals in Chinese CFR600 demonstration reactor. During their industrial production, δ-ferrite is present in large-scale billets because of the combined effect of non-equilibrium segregation and low cooling rate. For large-scale billets containing δ-ferrite, inhomogeneous grain-size distributions are observed in the product after hot working. Extensive studies on the recrystallization of the austenite phase in austenitic stainless steels during hot deformation were conducted. However, the effect of δ-ferrite on the recrystallization behavior of the austenite phase remains unclear. In this study, uniaxial hot compression tests of 316KD austenitic stainless steels involving as-cast and homogenized conditions were conducted at 1423 K and 0.1 s-1 using a Gleeble-3800 thermal-mechanical simulator, and the effect of δ-ferrite on hot deformation and recrystallization was analyzed by SEM, EBSD, and TEM. Results showed that δ-ferrite could be nearly eliminated through δ-ferrite→austenite transformation after homogenization at 1473 K for 14 h, whereas austenite grain showed evident growth. The elimination of δ-ferrite was a Cr-diffusion-controlled process through kinetic analysis. Plastic deformation occurred preferentially in δ-ferrite and at the δ-ferrite/austenite interface, and subsequently in austenite during hot deformation. The flow stress of as-cast samples was much lower than that of homogenized samples at the same strain because of the presence of soft δ-ferrite. Dynamic recovery occurred easier in δ-ferrite, and the resulting dynamic softening remarkably reduced flow stress with an increase in strain. Discontinuous dynamic recrystallization characterized by original austenite grain boundary bulging was the dominant mechanism in homogenized samples. However, the presence of δ-ferrite promoted the occurrence of continuous dynamic recrystallization in austenite near the δ-ferrite/austenite interface in as-cast samples. Compared with the homogenized samples, a higher degree of recrystallization was observed in as-cast samples because of the combined effects of continuous dynamic recrystallization and discontinuous dynamic recrystallization.

Cite this article

CHEN Shenghu , WANG Qiyu , JIANG Haichang , RONG Lijian . Effect of δ-Ferrite on Hot Deformation and Recrystallization of 316KD Austenitic Stainless Steel for Sodium-Cooled Fast Reactor Application[J]. Acta Metall Sin, 2024 , 60(3) : 367 -376 . DOI: 10.11900/0412.1961.2022.00039

References

1 Sofu T. A review of inherent safety characteristics of metal alloy sodium-cooled fast reactor fuel against postulated accidents [J]. Nucl. Eng. Technol., 2015, 47: 227
2 Dai Y N, Zheng X T, Ding P S. Review on sodium corrosion evolution of nuclear-grade 316 stainless steel for sodium-cooled fast reactor applications [J]. Nucl. Eng. Technol., 2021, 53: 3474
3 Aoto K, Dufour P, Yang H Y, et al. A summary of sodium-cooled fast reactor development [J]. Prog. Nucl. Energy, 2014, 77: 247
4 Yan C G, Li Y P, Wang M Z. Type 316 austenitic steels for reactor vessel and internals in sodium fast reactors and their creep rupture properties [J]. J. Iron Steel Res., 2018, 30: 935
  燕春光, 李雅平, 王明政. 钠冷快堆堆容器堆内构件用316型不锈钢及其持久断裂性能 [J]. 钢铁研究学报, 2018, 30: 935
5 Schaeffler A L. Constitution diagram for stainless steel weld metal [J]. Met. Prog., 1949, 56: 680
6 Delong W T. Ferrite in austenitic stainless steel weld metal [J]. Weld. J., 1974, 53: 273s
7 Espy R H. Weldability of nitrogen-strengthened stainless steels [J]. Weld. J., 1982, 61: 149s
8 Wang Q Y, Chen S H, Rong L J. δ-Ferrite formation and its effect on the mechanical properties of heavy-section AISI 316 stainless steel casting [J]. Metall. Mater. Trans., 2020, 51A: 2998
9 Wang Q Y, Chen S H, Lv X L, et al. Role of δ-ferrite in fatigue crack growth of AISI 316 austenitic stainless steel [J]. J. Mater. Sci. Technol., 2022, 114: 7
10 Zhou Y H, Liu Y C, Zhou X S, et al. Precipitation and hot deformation behavior of austenitic heat-resistant steels: A review [J]. J. Mater. Sci. Technol., 2017, 33: 1448
11 Zhou Y H, Liu Y C, Zhou X S, et al. Processing maps and microstructural evolution of the type 347H austenitic heat-resistant stainless steel [J]. J. Mater. Res., 2015, 30: 2090
12 Guo B F, Ji H P, Liu X G, et al. Research on flow stress during hot deformation process and processing map for 316LN austenitic stainless steel [J]. J. Mater. Eng. Perform., 2012, 21: 1455
13 Mataya M C, Nilsson E R, Brown E L, et al. Hot working and recrystallization of as-cast 316L [J]. Metall. Mater. Trans., 2003, 34A: 1683
14 Dehghan-Manshadi A, Barnett M R, Hodgson P D. Hot deformation and recrystallization of austenitic stainless steel: Part I. Dynamic recrystallization [J]. Metall. Mater. Trans., 2008, 39A: 1359
15 Wang S L, Zhang M X, Wu H C, et al. Study on the dynamic recrystallization model and mechanism of nuclear grade 316LN austenitic stainless steel [J]. Mater. Charact., 2016, 118: 92
16 Chen L, Wang L M, Du X J, et al. Hot deformation behavior of 2205 duplex stainless steel [J]. Acta Metall. Sin., 2010, 46: 52
  陈 雷, 王龙妹, 杜晓建 等. 2205双相不锈钢的高温变形行为 [J]. 金属学报, 2010, 46: 52
17 Ni K, Yang Y H, Cao J C, et al. Softening behavior of 18.7Cr-1.0Ni-5.8Mn-0.2N low nickel-type duplex stainless steel during hot compression deformation under large strain [J]. Acta Metall. Sin., 2021, 57: 224
  倪 珂, 杨银辉, 曹建春 等. 18.7Cr-1.0Ni-5.8Mn-0.2N节Ni型双相不锈钢的大变形热压缩软化行为 [J]. 金属学报, 2021, 57: 224
18 Fang Y L, Liu Z Y, Zhang W N, et al. Microstructure evolution of lean duplex stainless steel 2101 during hot deformation [J]. Acta Metall. Sin., 2010, 46: 641
  方轶琉, 刘振宇, 张维娜 等. 节约型双相不锈钢2101高温变形过程中微观组织演化 [J]. 金属学报, 2010, 46: 641
19 Dehghan-Manshadi A, Hodgson P D. Effect of δ-ferrite co-existence on hot deformation and recrystallization of austenite [J]. J. Mater. Sci., 2008, 43: 6272
20 Dehghan-Manshadi A, Barnett M R, Hodgson P D. Microstructural evolution during hot deformation of duplex stainless steel [J]. Mater. Sci. Technol., 2007, 23: 1478
21 Ruitenberg G, Woldt E, Petford-Long A K. Comparing the Johnson-Mehl-Avrami-Kolmogorov equations for isothermal and linear heating conditions [J]. Thermochim. Acta, 2001, 378: 97
22 Ham F S. Theory of diffusion-limited precipitation [J]. J. Phys. Chem. Solids, 1958, 6: 335
23 Alberry P J, Haworth C W. Interdiffusion of Cr, Mo, and W in iron [J]. Met. Sci., 1974, 8: 407
24 Ponge D, Gottstein G. Necklace formation during dynamic recrystallization: Mechanisms and impact on flow behavior [J]. Acta Mater., 1998, 46: 69
25 Pi?ol-Juez A, Iza-Mendia A, Gutiérrez I. δ /γ Interface bondary sliding as a mechanism for strain accommodation during hot deformation in a duplex stainless steel [J]. Metall. Mater. Trans., 2000, 31A: 1671
26 Chen S H, Rong L J. Effect of silicon on the microstructure and mechanical properties of reduced activation ferritic/martensitic steel [J]. J. Nucl. Mater., 2015, 459: 13
27 Yanushkevich Z, Belyakov A, Kaibyshev R. Microstructural evolution of a 304-type austenitic stainless steel during rolling at temperatures of 773-1273 K [J]. Acta Mater., 2015, 82: 244
28 Arun Babu K, Mozumder Y H, Saha R, et al. Hot-workability of super-304H exhibiting continuous to discontinuous dynamic recrystallization transition [J]. Mater. Sci. Eng., 2018, A734: 269
29 Dehghan-Manshadi A, Hodgson P D. Dependency of recrystallization mechanism to the initial grain size [J]. Metall. Mater. Trans., 2008, 39A: 2830
30 Gourdet S, Montheillet F. A model of continuous dynamic recrystallization [J]. Acta Mater., 2003, 51: 2685
31 Gourdet S, Montheillet F. Effects of dynamic grain boundary migration during the hot compression of high stacking fault energy metals [J]. Acta Mater., 2002, 50: 2801
Outlines

/