Effect of Gallium Addition on Mechanical and Antibacterial Properties of 304L Stainless Steel
Received date: 2022-07-20
Revised date: 2022-09-01
Online published: 2022-09-15
Supported by
National Natural Science Foundation of China(52171242);Peak Climbing Project of Foshan Hospital of Traditional Chinese Medicine(202000206);Youth Innovation Promotion Association CAS(2018221)
As a new antibacterial metal element, Ga is widely used in the medical field and always added to compounds in ionic form to form Ga complexes for medicinal use. However, related research on the mechanical properties, antibacterial properties, and antibacterial mechanism of Ga-bearing alloys is still very limited. In this work, the effect of Ga addition on the mechanical properties of 304L austenitic stainless steel (304L SS) after solution treatment was investigated via metallographic observations and tensile strength and hardness tests. Moreover, the antibacterial properties of Ga-bearing 304L stainless steel (304L-Ga SS) were tested using plate counting and the activity state of bacteria on the surface of the material was detected using SEM. Based on the known Ga ion sterilization principle, the antibacterial mechanism of 304L-Ga SS was preliminarily discussed using the reactive oxygen species (ROS) fluorescence reaction and ion dissolution results of the material in different solution tests. Results showed that the structure of 304L-Ga SS is still austenitic like that of 304L SS. The Ga addition increases the yield strength and elongation of the material but decreases its tensile strength and hardness. The change in strength and elongation is the result of the synergistic effect of the increase in stacking fault energy and the solid solution strengthening. The Ga addition also slightly increases the lattice constant of stainless steel due to the replacement solid solution effect. In the passive film of 304L-Ga SS, Ga exists in alloy form. Because of their similarity to Fe ions, Ga ions dissolved from Ga in the passive film are inhaled into bacteria cells and cause high expression of ROS in the bacteria, causing oxidative stress, and bactericidal effect. Contact sterilization is one of the main bactericidal mechanisms of 304L-Ga SS. Adequate contact between the bacteria and stainless steel improves the dissolution of Ga due to the proton (H+) depletion reaction in the bacteria. At the same time, the production of additional ROS during the proton consumption reaction further enhances the antibacterial effect.
MENG Yujia , XI Tong , YANG Chunguang , ZHAO Jinlong , ZHANG Xinrui , YU Yingjie , YANG Ke . Effect of Gallium Addition on Mechanical and Antibacterial Properties of 304L Stainless Steel[J]. Acta Metall Sin, 2024 , 60(7) : 890 -900 . DOI: 10.11900/0412.1961.2022.00351
| 1 | Oh K T, Choo S U, Kim K M, et al. A stainless steel bracket for orthodontic application [J]. Eur. J. Orthod., 2005, 27: 237 |
| 2 | Winters G L, Nutt M J. Stainless Steels for Medical and Surgical Applications [M]. West Conshohocken: ASTM International, 2003: 13 |
| 3 | Bomba? D, Brojan M, Fajfar P, et al. Review of materials in medical applications [J]. RMZ-Mater. Geoenviron., 2007, 54: 471 |
| 4 | Simionescu N, Benea L, Dumitrascu V M. The synergistic effect of proteins and reactive oxygen species on electrochemical behaviour of 316L stainless steel for biomedical applications [J]. IOP Conf. Ser.: Mater. Sci. Eng., 2018, 374: 012058 |
| 5 | Chen Q Z, Thouas G A. Metallic implant biomaterials [J]. Mater. Sci. Eng., 2015, R87: 1 |
| 6 | Wen M, Li W, Cao X M. Research on the mechanical properties for medical stainless steel [J]. Adv. Mater. Res., 2012, 383-390: 3976 |
| 7 | Padilha A F, Plaut R L, Rios P R. Annealing of cold-worked austenitic stainless steels [J]. ISIJ Int., 2003, 43: 135 |
| 8 | McGuire M F. Stainless Steels for Design Engineers [M]. New York: ASM International, 2008: 69 |
| 9 | Singh N, Nanda T, Kumar B R, et al. In situ investigations of microstructural changes during tensile deformation of AISI 304L stainless steels [J]. Arch. Civ. Mech. Eng., 2019, 19: 672 |
| 10 | Zhang E L, Zhao X T, Hu J L, et al. Antibacterial metals and alloys for potential biomedical implants [J]. Bioact. Mater., 2021, 6: 2569 |
| 11 | Costerton J W, Lewandowski Z, Caldwell D E, et al. Microbial biofilms [J]. Annu. Rev. Microbiol., 1995, 49: 711 |
| 12 | Sutherland I W. The biofilm matrix—An immobilized but dynamic microbial environment [J]. Trends Microbiol., 2001, 9: 222 |
| 13 | Hall-Stoodley L, Costerton J W, Stoodley P. Bacterial biofilms: From the natural environment to infectious diseases [J]. Nat. Rev. Microbiol., 2004, 2: 95 |
| 14 | An Y H, Friedman R J. Concise review of mechanisms of bacterial adhesion to biomaterial surfaces [J]. J. Biomed. Mater. Res., 1998, 43: 338 |
| 15 | Simchi A, Tamjid E, Pishbin F, et al. Recent progress in inorganic and composite coatings with bactericidal capability for orthopaedic applications [J]. Nanomedicine, 2011, 7: 22 |
| 16 | Ye L F, Chen H B, Lin Z L, et al. Research progress in antibacterial stainless steel [J]. Hot Work. Technol., 2014, 43(20): 10 |
| 叶丽芳, 陈惠波, 林照亮 等. 不锈钢抗菌技术研究进展 [J]. 热加工工艺, 2014, 43(20): 10 | |
| 17 | Xu M Y, Wang C, Li Y G. Research progress of antibacterial stainless steel [J]. Foundry Technol., 2016, 37(6): 1085 |
| 徐鸣悦, 王 丛, 李运刚. 抗菌不锈钢的研究进展 [J]. 铸造技术, 2016, 37(6): 1085 | |
| 18 | Kircheva N, Dudev T. Competition between abiogenic and biogenic metal cations in biological systems: Mechanisms of gallium's anticancer and antibacterial effect [J]. J. Inorg. Biochem., 2021, 214: 111309 |
| 19 | Chitambar C R. Gallium complexes as anticancer drugs [A]. Metallo-Drugs: Development and Action of Anticancer Agents [M]. Berlin: De Gruyter, 2018: 281 |
| 20 | Wazzan N, Soliman K A, Halim W S A. Theoretical study of gallium nitride nanocage as a carrier for 5-fluorouracil anticancer drug [J]. J. Mol. Model., 2019, 25: 265 |
| 21 | Yin H Y, Gao J J, Chen X M, et al. A gallium(III) complex that engages protein disulfide isomerase A3 (PDIA3) as an anticancer target [J]. Angew. Chem. Int. Ed., 2020, 59: 20147 |
| 22 | Halevas E, Mavroidi B, Antonoglou O, et al. Structurally characterized gallium-chrysin complexes with anticancer potential [J]. Dalton Trans., 2020, 49: 2734 |
| 23 | Auger C, Lemire J, Appanna V, et al. Gallium in bacteria, metabolic and medical implications [A]. Encyclopedia of Metalloproteins [M]. New York: Springer, 2013: 800 |
| 24 | Minandri F, Bonchi C, Frangipani E, et al. Promises and failures of gallium as an antibacterial agent [J]. Future Microbiol., 2014, 9: 379 |
| 25 | Verron E, Bouler J M, Scimeca J C. Gallium as a potential candidate for treatment of osteoporosis [J]. Drug Discov. Today, 2012, 17: 1127 |
| 26 | Kaneko Y, Thoendel M, Olakanmi O, et al. The transition metal gallium disrupts Pseudomonas aeruginosa iron metabolism and has antimicrobial and antibiofilm activity [J]. J. Clin. Invest., 2007, 117: 877 |
| 27 | Olakanmi O, Britigan B E, Schlesinger L S. Gallium disrupts iron metabolism of mycobacteria residing within human macrophages [J]. Infect. Immun., 2000, 68: 5619 |
| 28 | Harrington J R, Martens R J, Cohen N D, et al. Antimicrobial activity of gallium against virulent Rhodococcus equiin vitro and in vivo [J]. J. Vet. Pharmacol. Ther., 2006, 29: 121 |
| 29 | Coleman M, Kuskie K, Liu M, et al. In vitro antimicrobial activity of gallium maltolate against virulent Rhodococcus equi [J]. Vet. Microbiol., 2010, 146: 175 |
| 30 | Baldoni D, Steinhuber A, Zimmerli W, et al. In vitro activity of gallium maltolate against staphylococci in logarithmic, stationary, and biofilm growth phases: Comparison of conventional and calorimetric susceptibility testing methods [J]. Antimicrob. Agents. Chemother., 2010, 54: 157 |
| 31 | Chitambar C R. Gallium and its competing roles with iron in biological systems [J]. Biochim. Biophys. Acta., 2016, 1863: 2044 |
| 32 | Wu H X, Li R, Ge X. In vitro clearance effects of gallium nitrate on biofilms of clinically isolated Staphylococcus aureus [J]. Chin. J. Infect. Control, 2015, 14: 223 |
| 吴浩昕, 李 蓉, 葛 新. 硝酸镓对临床分离金黄色葡萄球菌生物膜的体外清除作用 [J]. 中国感染控制杂志, 2015, 14: 223 | |
| 33 | Rimondini L, Valle C D, Cochis A, et al. The biofilm formation onto implants and prosthetic materials may be contrasted using gallium (3+) [J]. Key Eng. Mater., 2013, 587: 315 |
| 34 | Bernstein L R, Zhang L K. Gallium maltolate has in vitro antiviral activity against SARS-CoV-2 and is a potential treatment for COVID-19 [J]. Antivir. Chem. Chemother., 2020, 28: 2040206620983780 |
| 35 | Xu G M, Zhang C X, Ning L, et al. Evaluation on the cytotoxicity of gallium alloy by MTT-assay [J]. Chin. J. Stomatol., 2001, 36: 189 |
| 徐钢梅, 张彩霞, 宁 丽 等. MTT法评价镓合金的细胞毒性[J]. 中华口腔医学杂志, 2001, 36: 189 | |
| 36 | Goss C H, Kaneko Y, Khuu L, et al. Gallium disrupts bacterial iron metabolism and has therapeutic effects in mice and humans with lung infections [J]. Sci. Transl. Med., 2018, 10: eaat7520 |
| 37 | Li L, Chang H, Yong N, et al. Superior antibacterial activity of gallium based liquid metals due to Ga3+ induced intracellular ROS generation [J]. J. Mater. Chem., 2021, 9B: 85 |
| 38 | Cochis A, Azzimonti B, Chiesa R, et al. Metallurgical gallium additions to titanium alloys demonstrate a strong time-increasing antibacterial activity without any cellular toxicity [J]. ACS Biomater. Sci. Eng., 2019, 5: 2815 |
| 39 | Choi S R, Britigan B E, Narayanasamy P. Iron/heme metabolism-targeted gallium(III) nanoparticles are active against extracellular and intracellular Pseudomonas aeruginosa and Acinetobacter baumannii [J]. Antimicrob. Agents. Chemother., 2019, 63: e02643-18 |
| 40 | Piatek M, Griffith D M, Kavanagh K. Quantitative proteomic reveals gallium maltolate induces an iron-limited stress response and reduced quorum-sensing in Pseudomonas aeruginosa [J]. J. Biol. Inorg. Chem., 2020, 25: 1153 |
| 41 | Gao C D, Zeng Z H, Peng S P, et al. Magnetostrictive alloys: Promising materials for biomedical applications [J]. Bioact. Mater., 2022, 8: 177 |
| 42 | Eshed M, Lellouche J, Gedanken A, et al. A Zn-doped CuO nanocomposite shows enhanced antibiofilm and antibacterial activities against Streptococcus mutans compared to nanosized CuO [J]. Adv. Funct. Mater., 2014, 24: 1382 |
| 43 | Hu G X, Cai X, Rong Y H. Fundamentals of Materials Science [M]. Shanghai: Shanghai Jiaotong University Press, 2010: 111 |
| 胡赓祥, 蔡 珣, 戎咏华. 材料科学基础[M]. 上海: 上海交通大学出版社, 2010: 111 | |
| 44 | Cai T, Li K Q, Zhang Z J, et al. Predicting the variation of stacking fault energy for binary Cu alloys by first-principles calculations [J]. J. Mater. Sci. Technol., 2020, 53: 61 |
| 45 | Hacht B. Gallium(III) ion hydrolysis under physiological conditions [J]. Bull. Korean Chem. Soc., 2008, 29: 372 |
| 46 | Orlov Y F, Maslov E I, Belkina E I. Solubilities of metal hydroxides [J]. Russ. J. Inorg. Chem., 2013, 58: 1306 |
| 47 | Moeller T, King G L. The some physicochemical studies on Gallium(III) salt solutions [J]. J. Phys. Chem., 1950, 54: 999 |
| 48 | Hijazi S, Visca P, Frangipani E. Gallium-protoporphyrin IX inhibits Pseudomonas aeruginosa growth by targeting cytochromes [J]. Front. Cell. Infect. Microbiol., 2017, 7: 12 |
| 49 | Braud A, Hoegy F, Jezequel K, et al. New insights into the metal specificity of the Pseudomonas aeruginosa pyoverdine-iron uptake pathway [J]. Environ. Microbiol., 2009, 11: 1079 |
| 50 | Todorov L, Kostova I, Lanthanum Traykova M. gallium and their impact on oxidative stress [J]. Curr. Med. Chem., 2019, 26: 4280 |
| 51 | Cao H L, Liu X Y, Meng F H, et al. Biological actions of silver nanoparticles embedded in titanium controlled by micro-galvanic effects [J]. Biomaterials, 2011, 32: 693 |
| 52 | Wang G M, Jin W H, Qasim A M, et al. Antibacterial effects of titanium embedded with silver nanoparticles based on electron-transfer-induced reactive oxygen species [J]. Biomaterials, 2017, 124: 25 |
/
| 〈 |
|
〉 |