Overview

Progress in Strengthening and Toughening Mechanisms of Heterogeneous Nanostructured Metals

  • Lei LU ,
  • Huaizhi ZHAO
Expand
  • Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
LU Lei, professor, Tel: (024)23971939, E-mail: llu@imr.ac.cn

Received date: 2022-06-20

  Online published: 2022-08-30

Supported by

National Natural Science Foundation of China(51931010);National Natural Science Foundation of China(92163202);Key Research Program of Frontier Science and International Partnership Program, Chinese Academy of Sciences(GJ-HZ2029);Liaoning Revitalization Talents Program(XLYC1802026)

Abstract

Heterostructured metals typically exhibit excellent mechanical properties, such as high strength, plasticity, and fracture toughness, which are not present in conventional homogeneous materials. This is primarily due to the synergistic effects arising from the interactions between the internal components including the stress/strain gradients, geometrically necessary dislocations, and unique interfacial behavior. This study focuses on two typical heterogeneous nanostructures (laminated and nanotwinned) by reviewing the recent progress in their strengthening and toughening mechanisms. The analysis highlights the effects of the properties and sizes of the individual components, interfaces, and loading directions on the macroscopic strengthening and toughening behavior.

Cite this article

Lei LU , Huaizhi ZHAO . Progress in Strengthening and Toughening Mechanisms of Heterogeneous Nanostructured Metals[J]. Acta Metall Sin, 2022 , 58(11) : 1360 -1370 . DOI: 10.11900/0412.1961.2022.00303

References

1 Lu K. The future of metals [J]. Science, 2010, 328: 319
2 Meyers M A, Mishra A, Benson D J. Mechanical properties of nanocrystalline materials [J]. Prog. Mater. Sci., 2006, 51: 427
3 Xie J J, Wu X L, Hong Y S. Shear bands at the fatigue crack tip of nanocrystalline nickel [J]. Scr. Mater., 2007, 57: 5
4 Kumar K S, Suresh S, Chisholm M F, et al. Deformation of electrodeposited nanocrystalline nickel [J]. Acta Mater., 2003, 51: 387
5 Farkas D, Van Petegem S, Derlet P M, et al. Dislocation activity and nano-void formation near crack tips in nanocrystalline Ni [J]. Acta Mater., 2005, 53: 3115
6 Pippan R, Hohenwarter A. The importance of fracture toughness in ultrafine and nanocrystalline bulk materials [J]. Mater. Res. Lett., 2016, 4: 127
7 Wu X L, Zhu Y T. Heterogeneous materials: A new class of materials with unprecedented mechanical properties [J]. Mater. Res. Lett., 2017, 5: 527
8 Lu K. Making strong nanomaterials ductile with gradients [J]. Science, 2014, 345: 1455
9 Cheng Z, Zhou H F, Lu Q H, et al. Extra strengthening and work hardening in gradient nanotwinned metals [J]. Science, 2018, 362: eaau1925
10 Calcagnotto M, Adachi Y, Ponge D, et al. Deformation and fracture mechanisms in fine- and ultrafine-grained ferrite/martensite dual-phase steels and the effect of aging [J]. Acta Mater., 2011, 59: 658
11 Park K, Nishiyama M, Nakada N, et al. Effect of the martensite distribution on the strain hardening and ductile fracture behaviors in dual-phase steel [J]. Mater. Sci. Eng., 2014, A604: 135
12 Ma X L, Huang C X, Moering J, et al. Mechanical properties of copper/bronze laminates: Role of interfaces [J]. Acta Mater., 2016, 116: 43
13 Wang Y M, Chen M W, Zhou F H, et al. High tensile ductility in a nanostructured metal [J]. Nature, 2002, 419: 912
14 Zhu Y T, Wu X L. Perspective on hetero-deformation induced (HDI) hardening and back stress [J]. Mater. Res. Lett., 2019, 7: 393
15 Wu X L, Yang M X, Yuan F P, et al. Heterogeneous lamella structure unites ultrafine-grain strength with coarse-grain ductility [J]. Proc. Natl. Acad. Sci. USA, 2015, 112: 14501
16 Zhao H Z, You Z S, Tao N R, et al. Anisotropic toughening of nanotwin bundles in the heterogeneous nanostructured Cu [J]. Acta Mater., 2022, 228: 117748
17 ASTM. Standard test method for measurement of fracture toughness [S]. West Conshchocken: American Society of Testing and Materials, 2015
18 Smith D L, Hoffman D W. Thin-film deposition: Principles and practice [J]. Phys. Today, 1996, 49: 60
19 Ross C A. Electrodeposited multilayer thin films [J]. Annu. Rev. Mater. Sci., 1994, 24: 159
20 Bakonyi I, Péter L. Electrodeposited multilayer films with giant magnetoresistance (GMR): Progress and problems [J]. Prog. Mater. Sci., 2010, 55: 107
21 Fang T H, Li W L, Tao N R, et al. Revealing extraordinary intrinsic tensile plasticity in gradient nano-grained copper [J]. Science, 2011, 331: 1587
22 Wu X L, Yang M X, Yuan F P, et al. Combining gradient structure and TRIP effect to produce austenite stainless steel with high strength and ductility [J]. Acta Mater., 2016, 112: 337
23 You Z S, Qu S D, Luo S S, et al. Fracture toughness evaluation of nanostructured metals via a contactless crack opening displacement gauge [J]. Materialia, 2019, 7: 100430
24 Luo S S, You Z S, Lu L. Intrinsic fracture toughness of bulk nanostructured Cu with nanoscale deformation twins [J]. Scr. Mater., 2017, 133: 1
25 Ashby M F. The deformation of plastically non-homogeneous materials [J]. Philos. Mag., 1970, 21: 399
26 Fleck N A, Muller G M, Ashby M F, et al. Strain gradient plasticity: theory and experiment [J]. Acta Metall. Mater., 1994, 42: 475
27 Gao H J, Huang Y G. Geometrically necessary dislocation and size-dependent plasticity [J]. Scr. Mater., 2003, 48: 113
28 Mughrabi H. On the role of strain gradients and long-range internal stresses in the composite model of crystal plasticity [J]. Mater. Sci. Eng., 2001, A317: 171
29 Mughrabi H. The effect of geometrically necessary dislocations on the flow stress of deformed crystals containing a heterogeneous dislocation distribution [J]. Mater. Sci. Eng., 2001, A319-321: 139
30 Wu H, Fan G H. An overview of tailoring strain delocalization for strength-ductility synergy [J]. Prog. Mater. Sci., 2020, 113: 100675
31 Yang M X, Pan Y, Yuan F P, et al. Back stress strengthening and strain hardening in gradient structure [J]. Mater. Res. Lett., 2016, 4: 145
32 Wang Y F, Yang M X, Ma X L, et al. Improved back stress and synergetic strain hardening in coarse-grain/nanostructure laminates [J]. Mater. Sci. Eng., 2018, A727: 113
33 Cao Z, Cheng Z, Xu W, et al. Effect of work hardening discrepancy on strengthening of laminated Cu/CuZn alloys [J]. J. Mater. Sci. Technol., 2022, 103: 67
34 Wan T, Cheng Z, Bu L F, et al. Work hardening discrepancy designing to strengthening gradient nanotwinned Cu [J]. Scr. Mater., 2021, 201: 113975
35 Lu K, Lu L, Suresh S. Strengthening materials by engineering coherent internal boundaries at the nanoscale [J]. Science, 2009, 324: 349
36 Lu K, Yan F K, Wang H T, et al. Strengthening austenitic steels by using nanotwinned austenitic grains [J]. Scr. Mater., 2012, 66: 878
37 Xiong L, You Z S, Qu S D, et al. Fracture behavior of heterogeneous nanostructured 316L austenitic stainless steel with nanotwin bundles [J]. Acta Mater., 2018, 150: 130
38 You Z S, Luo S S, Lu L. Size effect of deformation nanotwin bundles on their strengthening and toughening in heterogeneous nanostructured Cu [J]. Sci. China Technol. Sci., 2021, 64: 23
39 Yan F K, Liu G Z, Tao N R, et al. Strength and ductility of 316L austenitic stainless steel strengthened by nano-scale twin bundles [J]. Acta Mater., 2012, 60: 1059
40 Zhang Y, Tao N R, Lu K. Mechanical properties and rolling behaviors of Nano-grained copper with embedded nano-twin bundles [J]. Acta Mater., 2008, 56: 2429
41 Yan F, Zhang H W, Tao N R, et al. Quantifying the microstructures of pure cu subjected to dynamic plastic deformation at cryogenic temperature [J]. J. Mater. Sci. Technol., 2011, 27: 673
42 Yan F K, Tao N R, Archie F, et al. Deformation mechanisms in an austenitic single-phase duplex microstructured steel with nanotwinned grains [J]. Acta Mater., 2014, 81: 487
43 Li Q, Yan F K, Tao N R, et al. Deformation compatibility between nanotwinned and recrystallized grains enhances resistance to interface cracking in cyclic loaded stainless steel [J]. Acta Mater., 2019, 165: 87
44 You Z S, Li X Y, Gui L J, et al. Plastic anisotropy and associated deformation mechanisms in nanotwinned metals [J]. Acta Mater., 2013, 61: 217
45 Zhao H Z, You Z S, Tao N R, et al. Anisotropic strengthening of nanotwin bundles in heterogeneous nanostructured Cu: Effect of deformation compatibility [J]. Acta Mater., 2021, 210: 116830
46 Ritchie R O. The conflicts between strength and toughness [J]. Nat. Mater., 2011, 10: 817
47 Lesuer D R, Syn C K, Sherby O D, et al. Mechanical behaviour of laminated metal composites [J]. Int. Mater. Rev., 1996, 41: 169
48 Hunt W H, Osman T M, Lewandowski J J. Micro- and macrostructural factors in DRA fracture resistance [J]. JOM, 1993, 45(1): 30
49 Dehm G, Jaya B N, Raghavan R, et al. Overview on micro- and nanomechanical testing: New insights in interface plasticity and fracture at small length scales [J]. Acta Mater., 2018, 142: 248
50 Liu B X, Huang L J, Rong X D, et al. Bending behaviors and fracture characteristics of laminatedductile-tough composites under different modes [J]. Compos. Sci. Technol., 2016, 126: 94
51 Pippan R. The crack driving force for fatigue crack propagation [J]. Eng. Fract. Mech., 1993, 44: 821
52 Wang Y Q, Fritz R, Kiener D, et al. Fracture behavior and deformation mechanisms in nanolaminated crystalline/amorphous micro-cantilevers [J]. Acta Mater., 2019, 180: 73
53 Ohashi Y, Wolfenstine J, Koch R, et al. Fracture behavior of a laminated steel-brass composite in bend tests [J]. Mater. Sci. Eng., 1992, A151: 37
54 Cepeda-Jiménez C M, García-Infanta J M, Pozuelo M, et al. Impact toughness improvement of high-strength aluminium alloy by intrinsic and extrinsic fracture mechanisms via hot roll bonding [J]. Scr. Mater., 2009, 61: 407
55 Venkateswara Rao K T, Yu W K, Ritchie R O. Cryogenic toughness of commercial aluminum-lithium alloys: Role of delamination toughening [J]. Metall. Trans., 1989, 20A: 485
56 Liu L, Yu Q, Wang Z, et al. Making ultrastrong steel tough by grain-boundary delamination [J]. Science, 2020, 368: 1347
57 Cepeda-Jiménez C M, Pozuelo M, García-Infanta J M, et al. Influence of the alumina thickness at the interfaces on the fracture mechanisms of aluminium multilayer composites [J]. Mater. Sci. Eng., 2008, A496: 133
58 Kum D W, Oyama T, Wadsworth J, et al. The impact properties of laminated composites containing ultrahigh carbon (UHC) steels [J]. J. Mech. Phys. Solids, 1983, 31: 173
59 Lee S, Oyama T, Wadsworth J, et al. Impact properties of a laminated composite based on ultrahigh carbon steel and brass [J]. Mater. Sci. Eng., 1992, A154: 133
60 Zhang J Y, Zhang X, Wang R H, et al. Length-scale-dependent deformation and fracture behavior of Cu/X (X = Nb, Zr) multilayers: The constraining effects of the ductile phase on the brittle phase [J]. Acta Mater., 2011, 59: 7368
61 Nasim M, Li Y C, Wen M, et al. A review of high-strength nanolaminates and evaluation of their properties [J]. J. Mater. Sci. Technol., 2020, 50: 215
62 Misra A, Krug H. Deformation behavior of nanostructured metallic multilayers [J]. Adv. Eng. Mater., 2001, 3: 217
63 Zhang J Y, Liu G, Zhang X, et al. A maximum in ductility and fracture toughness in nanostructured Cu/Cr multilayer films [J]. Scr. Mater., 2010, 62: 333
64 Qin E W, Lu L, Tao N R, et al. Enhanced fracture toughness and strength in bulk nanocrystalline Cu with nanoscale twin bundles [J]. Acta Mater., 2009, 57: 6215
Outlines

/