Physical and Mathematical Simulation on the Bubble Entrainment Behavior at Slag-Metal Interface

  • ZHOU Xiaobin ,
  • ZHAO Zhanshan ,
  • WANG Wanxing ,
  • XU Jianguo ,
  • YUE Qiang
Expand
  • 1.School of Metallurgical Engineering, Anhui University of Technology, Ma'anshan 243032, China
    2.ESP Department, Rizhao Steel Holding Group Co., Ltd., Rizhao 276806, China
ZHOU Xiaobin, Tel: 18955536370, E-mail: zxbahut@ahut.edu.cn

Received date: 2022-05-05

  Revised date: 2022-07-28

  Online published: 2022-08-29

Supported by

National Natural Science Foundation of China(51704006);National Natural Science Foundation of China(51774004)

Abstract

The flow and interaction between slag, metals, and bubbles are very complicated phenomena in metallurgical processes, such as desulfurization in hot metal pretreatment, steelmaking process in a converter, and second refining process. The molten steel or hot metal can be entrained into the slag when a bubble or bubbles flow through the slag-metal interface during the metallurgical process. The bubble entrainment behavior can increase the heat and mass transfer and, in turn, increase the chemical reaction efficiency of the slag-metal interface. Investigating the entrainment behavior helps in understanding the interaction between bubbles and liquid phases. The current study focuses on the effects of bubbles and slag properties on the bubble entrainment behaviors at the slag-metal interface. The results show that the bubble size is the most important factor influencing the entrainment, followed by the slag density. The slag viscosity and interfacial tension of the slag-metal interface show a weaker effect on the entrainment. In particular, the entrainment volume of steel and maximum area of the slag-metal interface increase by 7.41 and 3.67 times when the bubble diameter increased from 10 to 16 mm, respectively. When the slag density increases from 2000 to 5000 kg/m3, the entrainment volume of steel and maximum area of the slag-metal interface increase by 62.3% and 13.1%, respectively. The increasing in slag viscosity and interfacial tension is less affected by slag entrainment and interface area. The entrainment volume of steel and maximum area of the slag-metal interface are decreased by 30.6% and 6.4% when the interfacial tension of the slag-metal interface increases from 0.65 to 1.10 N/m, respectively. Similarly, when the slag viscosity increases from 0.05 to 2.0 Pa·s, the entrainment volume of steel and maximum area of the slag-metal decrease by 18.4% and 10.2%, respectively.

Cite this article

ZHOU Xiaobin , ZHAO Zhanshan , WANG Wanxing , XU Jianguo , YUE Qiang . Physical and Mathematical Simulation on the Bubble Entrainment Behavior at Slag-Metal Interface[J]. Acta Metall Sin, 2023 , 59(11) : 1523 -1532 . DOI: 10.11900/0412.1961.2022.00218

References

1 Feng J X. Application of desulphurization technique by magnesium injection in molten iron [J]. Met. Mater. Metall. Eng., 2007, 35(4): 21
  冯建新. 铁水喷镁脱硫技术的应用 [J]. 金属材料与冶金工程, 2007, 35(4): 21
2 Wang D G, Cheng N L, Zhou X B. Research on the effect of bottom blowing on bath stirring in a 250 t converter [J]. Chin. J. Process Eng., 2020, 20: 678
  王多刚, 程乃良, 周小宾. 250吨转炉底吹对熔池搅拌的影响研究 [J]. 过程工程学报, 2020, 20: 678
3 Mazumdar D, Dhandapani P, Sarvanakumar R. Modeling and optimisation of gas stirred ladle systems [J]. ISIJ Int., 2017, 57: 286
4 Iguchi M, Nakamura K I, Tsujino R. Mixing time and fluid flow phenomena in liquids of varying kinematic viscosities agitated by bottom gas injection [J]. Metall. Mater. Trans., 1998, 29B: 569
5 Chen Z P, Zhu M Y, Wen G H, et al. Effect of submerged entry nozzle argon blowing on slab quality [J]. Iron Steel, 2009, 44(7): 28
  陈志平, 朱苗勇, 文光华 等. 连铸板坯浸入式水口吹氩工艺研究 [J]. 钢铁, 2009, 44(7): 28
6 Li B K, Yin H B, Zhou C Q, et al. Modeling of three-phase flows and behavior of slag/steel interface in an argon gas stirred ladle [J]. ISIJ Int., 2008, 48: 1704
7 Wei G S, Zhu R, Cheng T, et al. Study on the impact characteristics of coherent supersonic jet and conventional supersonic jet in EAF steelmaking process [J]. Metall. Mater. Trans., 2018, 49B: 361
8 Zhao C, Chen W, Zhang L F, et al. Numerical simulation of multiphase flow in converter top blowing process [J]. China Metall., 2018, 28(suppl.1) : 1
  赵 冲, 陈 威, 张立峰 等. 转炉顶吹过程多相流数值模拟 [J]. 中国冶金, 2018, 28(): 1
9 De Jesús Villela-Aguilar J, Ramos-Banderas J á, Hernández-Bocanegra C A, et al. Optimization of the mixing time using asymmetrical arrays in both gas flow and injection positions in a dual-plug ladle [J]. ISIJ Int., 2020, 60: 1172
10 Hibbeler L C, Liu R, Thomas B G. Review of mold flux entrainment mechanisms and model investigation of entrainment by shear-layer instability [A]. Proceedings of the 7th ECCC [C]. Dusseldorf, Germany, 2011: 1
11 Yu H Q, Zhu M Y. The interfacial behavior of molten steel and liquid slag in slab continuous casting mold with electromagnetic brake and argon gas injection [J]. Acta Metall. Sin., 2008, 44: 1141
  于海岐, 朱苗勇. 板坯结晶器电磁制动和吹氩过程的钢/渣界面行为 [J]. 金属学报, 2008, 44: 1141
12 Yang H L, He P, Zhai Y C. Removal behavior of inclusions in molten steel by bubble wake flow based on water model experiment [J]. ISIJ Int., 2014, 54: 578
13 Li B, Lu H B, Zhong Y B, et al. Numerical simulation for the influence of EMS position on fluid flow and inclusion removal in a slab continuous casting mold [J]. ISIJ Int., 2020, 60: 1204
14 Han Z J, Holappa L. Formation of metal droplets from gas bubbles bursting on iron melt [J]. Steel Res., 2001, 72: 434
15 Han Z J, Holapp L. Bubble bursting phenomenon in gas/metal/slag systems [J]. Metall. Mater. Trans., 2003, 34B: 525
16 Han Z J, Holappa L. Characteristics of iron entrainment into slag due to rising gas bubbles [J]. ISIJ Int., 2003, 43: 1698
17 Ekeng?rd J, Andersson A M T, J?nsson P G. Distribution of metal droplets in top slags during ladle treatment [J]. Ironmaking Steelmaking, 2008, 35: 575
18 Yoshida H, Liu J, Kim S J, et al. Influence of the interfacial tension on the droplet formation by bubble rupture in Sn(Te) and salt system [J]. ISIJ Int., 2016, 56: 1902
19 Song D Y, Maruoka N, Gupta G S, et al. Influence of bottom bubbling rate on formation of metal emulsion in Al-Cu alloy and molten salt system [J]. ISIJ Int., 2012, 52: 1018
20 Reiter G, Schwerdtfeger K. Observations of physical phenomena occurring during passage of bubbles through liquid/liquid interfaces [J]. ISIJ Int., 1992, 32: 50
21 Greene G A, Chen J C, Conlin M T. Onset of entrainment between immiscible liquid layers due to rising gas bubbles [J]. Int. J. Heat Mass Trans., 1988, 31: 1309
22 Zhao H L, Wang J Q, Zhang W L, et al. Bubble motion and interfacial phenomena during bubbles crossing liquid-liquid interfaces [J]. Processes, 2019, 7: 719
23 Singh K K, Gebauer F, Bart H J. CFD Simulation of the phenomenon of passage of a bubble through the interface between two initially quiescent liquids [J]. Chem. Ing. Tech., 2015, 87: 1047
24 Natsui S, Takai H, Kumagai T, et al. Multiphase particle simulation of gas bubble passing through liquid/liquid interfaces [J]. Mater. Trans., 2014, 55: 1707
25 Boyer F, Lapuerta C. Study of a three component Cahn-Hilliard flow model [J]. ESAIM: Math. Model. Numer. Anal., 2006, 40: 653
26 Boyer F, Lapuerta C, Minjeaud S, et al. Cahn-Hilliard/Navier-Stokes model for the simulation of three-phase flows [J]. Transp. Porous Med., 2010, 82: 463
27 Chen J X. Handbook of Steelmaking Data and Diagrams [M]. 2nd Ed., Beijing: Metallurgical Industry Press, 2010: 275
  陈家祥. 炼钢常用图表数据手册 [M]. 第 2版, 北京: 冶金工业出版社, 2010: 275
Outlines

/