Research paper

Effect of Heat Input on Microstructure and Mechanical Properties of Marine High Strength Steel Fabricated by Wire Arc Additive Manufacturing

  • HOU Xuru ,
  • ZHAO Lin ,
  • REN Shubin ,
  • PENG Yun ,
  • MA Chengyong ,
  • TIAN Zhiling
Expand
  • 1.Institute for Advanced Materials and Technology, University of Science and Technology Beijing, Beijing 100083, China
    2.Central Iron and Steel Research Institute, Beijing 100081, China
ZHAO Lin, professor, Tel: (010)62182946, E-mail: hhnds@aliyun.com;
PENG Yun, professor, Tel: (010)62185578, E-mail: pengyun@cisri.com.cn

Received date: 2022-04-08

  Revised date: 2022-07-12

  Online published: 2022-08-26

Supported by

Key Basic Research Program of Basic Strengthening Plan(2021-JCJQ-ZD-075-11);CISRI Independent R&D Program(21H62630B)

Abstract

Marine-grade high strength steel (yield strength = 590 MPa) is a low-carbon, low-alloy steel characterized by high strength and toughness, excellent weldability, and seawater corrosion resistance. Thus, it is suitable for structural applications and widely used in the shipbuilding industry. Recently, wire arc additive manufacturing (WAAM) has attracted significant attention worldwide because of its high deposition rates and material utilization ratios, low material and equipment costs, and good structural integrity. However, the research on WAAM of 590 MPa marine-grade high strength steel is limited. In this work, 590 MPa marine-grade high strength steel components were produced by cold metal transfer and pulse-arc additive manufacturing (CMT + P-WAAM). The effect of the heat input on the microstructures and mechanical properties of the developed steel were investigated using several techniques, including OM, SEM, EBSD, and TEM. The results indicate that at a heat input of 5.6 kJ/cm, the microstructures of the WAAM deposited metals are mainly upper bainite and granular bainite, the area fraction of the martensite-austenite (M-A) constituents accounts for about 14.82%, the length ratio of the effective high-angle grain boundary (grain boundary angle α > 45°) is 36.3%, the tensile strength of the deposited metals are 843 and 858 MPa in the horizontal and vertical directions, respectively, and the average microhardness is about 286 HV. However, its impact absorbed energy at -50oC is only 15 and 16 J in the horizontal and vertical directions, respectively. At a heat input of 13.5 kJ/cm, the low cooling rate and the high inclusion (inclusion size d > 0.4 μm) content promote the formation of a large quantity of acicular ferrites with lath bainites and a small amount of granular bainites. The area fraction of the M-A constituents is reduced to 4.21%, and the length ratio of the effective high-angle grain boundary is increased to 52.4%. The tensile strength of the deposited metals in the horizontal and vertical directions is reduced to 723 and 705 MPa, respectively. Similarly, the average microhardness is also reduced to 258 HV, but the low-temperature impact absorbed energy is greatly improved, reaching 109 and 127 J, respectively, which is 7-8 times that of the WAAM deposited metal at a low heat input. The impact fracture characteristics also changed from a quasi-cleavage fracture to a typical ductile fracture.

Cite this article

HOU Xuru , ZHAO Lin , REN Shubin , PENG Yun , MA Chengyong , TIAN Zhiling . Effect of Heat Input on Microstructure and Mechanical Properties of Marine High Strength Steel Fabricated by Wire Arc Additive Manufacturing[J]. Acta Metall Sin, 2023 , 59(10) : 1311 -1323 . DOI: 10.11900/0412.1961.2022.00161

References

1 Wu B T, Pan Z X, Ding D H, et al. A review of the wire arc additive manufacturing of metals: Properties, defects and quality improvement [J]. J. Manuf. Process., 2018, 35: 127
2 Tian C L, Chen J L, Dong P, et al. Current state and future development of the wire arc additive manufacture technology abroad [J]. Aeros. Manuf. Technol., 2015, (2): 57
  田彩兰, 陈济轮, 董 鹏 等. 国外电弧增材制造技术的研究现状及展望 [J]. 航天制造技术, 2015, (2): 57
3 Li F Z. Research on development path of additive manufacturing industry in China [J]. Adv. Mater. Indus., 2017, (1): 5
  李方正. 我国增材制造产业发展路径探究 [J]. 新材料产业, 2017, (1): 5
4 Xiong J, Xue Y G, Chen H, et al. Status and development prospects of forming control technology in arc-based additive manufacturing [J]. Elect. Weld. Mach., 2015, 45(9): 45
  熊 俊, 薛永刚, 陈 辉 等. 电弧增材制造成形控制技术的研究现状与展望 [J]. 电焊机, 2015, 45(9): 45
5 Spencer J D, Dickens P M, Wykes C M. Rapid prototyping of metal parts by three-dimensional welding [J]. Proc. Inst. Mech. Eng., 1998, 212B: 175
6 Yan X, Gu P. A review of rapid prototyping technologies and systems [J]. Comput. Aided Des., 1996, 28: 307
7 Debroy T, Wei H L, Zuback J S, et al. Additive manufacturing of metallic components—Process, structure and properties [J]. Prog. Mater. Sci., 2018, 92: 112
8 Williams S W, Martina F, Addison A C, et al. Wire + arc additive manufacturing [J]. Mater. Sci. Technol., 2015, 32: 641
9 Derekar K S. A review of wire arc additive manufacturing and advances in wire arc additive manufacturing of aluminium [J]. Mater. Sci. Technol., 2018, 34: 895
10 Kazanas P, Deherkar P, Almeida P, et al. Fabrication of geometrical features using wire and arc additive manufacture [J]. Proc. Inst. Mech. Eng., 2012, 226B: 1042
11 Bermingham M J, Thomson-Larkins J, St John D H, et al. Sensitivity of Ti-6Al-4V components to oxidation during out of chamber wire + arc additive manufacturing [J]. J. Mater. Process. Technol., 2018, 258: 29
12 Dhinakaran V, Ajith J, Fahmidha A F Y, et al. Wire arc additive manufacturing (WAAM) process of nickel based superalloys—A review [J]. Mater. Today: Proc., 2020, 21: 920
13 Zhou L Z, Liu S H, Ding D P. Rapid prototyping technology based on three-dimensional welding deposition [J]. Electr. Mould, 2004, (4): 1
  周龙早, 刘顺洪, 丁冬平. 基于三维焊接熔敷的快速成形技术 [J]. 电加工与模具, 2004, (4): 1
14 Liu S G, Zheng L, Xie R, et al. Additive manufacturing technology for high strength steel ship structures [J]. Hot Work. Technol., 2018, 47(22): 110
  刘水根, 郑 磊, 谢 锐 等. 高强钢船体结构的增材制造技术 [J]. 热加工工艺, 2018, 47(22): 110
15 Nemani A V, Ghaffari M, Nasiri A. Comparison of microstructural characteristics and mechanical properties of shipbuilding steel plates fabricated by conventional rolling versus wire arc additive manufacturing [J]. Add. Manuf., 2020, 32: 101086
16 Guo C, Ma M L, Hu R Z, et al. Microstructure and properties of 10CrNi3MoV high strength steel for naval ship made by wire and arc additive manufacturing [J]. Mater. Rev., 2019, 33(): 455
  郭 纯, 马明亮, 胡瑞章 等. 电弧增材制造舰船用高强钢10CrNi3MoV的组织及性能 [J]. 材料导报, 2019, 33():455
17 Zhou H L, Song C B, Liu Y S, et al. Development and application of 590 MPa grade 3D-printed surfacing wire material [J]. Weld. Technol., 2019, 48(8): 66
  周海龙, 宋昌宝, 刘玉双 等. 590 MPa级3D打印堆熔丝材的研制与应用 [J]. 焊接技术, 2019, 48(8): 66
18 Huda N, Midawi A R H, Gianetto J, et al. Influence of martensite-austenite (MA) on impact toughness of X80 line pipe steels [J]. Mater. Sci. Eng., 2016, A662: 481
19 Moeinifar S, Kokabi A H, Hosseini H R M. Effect of tandem submerged arc welding process and parameters of Gleeble simulator thermal cycles on properties of the intercritically reheated heat affected zone [J]. Mater. Des., 2011, 32: 869
20 Matsuda F, Ikeuchi K, Fukada Y, et al. Review of mechanical and metallurgical investigations of M-A constituent in welded joint in Japan [J]. Trans. JWRI, 1995, 24: 1
21 Zhong Y, Xiao F R, Zhang J W, et al. In situ TEM study of the effect of M/A films at grain boundaries on crack propagation in an ultra-fine acicular ferrite pipeline steel [J]. Acta Mater., 2006, 54: 435
22 Zhang D Q. Study on the acicular ferrite formation mechanism of weld metal in microalloyed steel [D]. Tianjin: Tianjin University, 2000
  张德勤. 微合金钢焊缝金属中针状铁素体形成机理的研究 [D]. 天津: 天津大学, 2000
23 Gourgues A F, Flower H M, Lindley T C. Electron backscattering diffraction study of acicular ferrite, bainite, and martensite steel microstructures [J]. Mater. Sci. Technol., 2000, 16: 26
24 Daz-Fuentes M, Iza-Mendia A, Gutiérrez I. Analysis of different acicular ferrite microstructures in low-carbon steels by electron backscattered diffraction. Study of their toughness behavior [J]. Metall. Mater. Trans., 2003, 34A: 2505
25 Zeng L. Welding Engineering [M]. Beijing: New Era Press, 1986: 123
  曾 乐. 焊接工程学 [M]. 北京: 新时代出版社, 1986: 123
26 Cao R, Feng W, Peng Y, et al. Analysis on impact property of welded joint HAZ of 980 MPa high strength steel [J]. Trans. China Weld. Inst., 2010, 31(8): 93
  曹 睿, 冯 伟, 彭 云 等. 980 MPa级高强钢焊接接头HAZ冲击性能的分析 [J]. 焊接学报, 2010, 31(8): 93
27 Ricks R A, Howell P R, Barritte G S. The nature of acicular ferrite in HSLA steel weld metals [J]. J. Mater. Sci., 1982, 17: 732
28 Han S C. Physical metallurgy of acicular ferrite (Continued) [J]. Dev. Appl. Mater., 1995, 10(6): 2
  韩顺昌. 针状铁素体的物理冶金学(续) [J]. 材料开发与应用, 1995, 10(6): 2
29 Barbaro F J, Krauklis P, Easterling K E. Formation of acicular ferrite at oxide particles in steels [J]. Mater. Sci. Technol., 1989, 5: 1057
30 Lee T K, Kim H J, Kang B Y, et al. Effect of inclusion size on the nucleation of acicular ferrite in welds [J]. ISIJ Int., 2000, 40: 1260
31 Liu Z C, Ji Y P, Ren H P. Morphology and substructure of bainite in steel (2) [J]. Heat Treat. Technol. Equip., 2016, 37(4): 1
  刘宗昌, 计云萍, 任慧平. 钢中贝氏体组织形态和亚结构(二) [J]. 热处理技术与装备, 2016, 37(4): 1
32 Zhang Y Q, Zhang R J, Su H, et al. Effect of granular bainite on mechanical properties of microalloyed 10MnNiCr steel [J]. Iron Steel, 2003, 38(11): 45
  张永权, 张荣久, 苏 航 等. 粒状贝氏体对10MnNiCr微合金钢力学性能的影响 [J]. 钢铁, 2003, 38(11): 45
33 Davis C L, King J E. Effect of cooling rate on intercritically reheated microstructure and toughness in high strength low alloy steel [J]. Mater. Sci. Technol., 1993, 9: 8
34 Li Y, Crowther D N, Green M J W, et al. The effect of vanadium and niobium on the properties and microstructure of the intercritically reheated coarse grained heat affected zone in low carbon microalloyed steels [J]. ISIJ Int., 2001, 41: 46
35 Lee S, Kim B C, Kwon D. Fracture toughness analysis of heat-affected zones in high-strength low-alloy steel welds [J]. Metall. Mater. Trans., 1993, 24A: 1133
36 Li X D, Shang C J, Han C C, et al. Influence of necklace-type M-A constituent on impact toughness and fracture mechanism in the heat affected zone of X100 pipeline steel [J]. Acta Metall. Sin., 2016, 52: 1025
  李学达, 尚成嘉, 韩昌柴 等. X100管线钢焊接热影响区中链状M-A组元对冲击韧性和断裂机制的影响 [J]. 金属学报, 2016, 52: 1025
37 Davis C L, King J E. Cleavage initiation in the intercritically reheated coarse-grained heat-affected zone: Part I. Fractographic evidence [J]. Metall. Mater. Trans., 1994, 25A: 563
Outlines

/