Formation and Evolution of Stray Grains on Remelted Interface in the Seed Crystal During the Directional Solidification of Single-Crystal Superalloys Assisted by Vertical Static Magnetic Field

  • SU Zhenqi ,
  • ZHANG Congjiang ,
  • YUAN Xiaotan ,
  • HU Xingjin ,
  • LU Keke ,
  • REN Weili ,
  • DING Biao ,
  • ZHENG Tianxiang ,
  • SHEN Zhe ,
  • ZHONG Yunbo ,
  • WANG Hui ,
  • WANG Qiuliang
Expand
  • 1School of Materials Science and Engineering, Shanghai University, Shanghai 200444, China
    2State Key Laboratory of Advanced Special Steel, Shanghai University, Shanghai 200444, China
    3Institute of Electrical Engineering, Chinese Academy of Sciences, Beijing 100190, China

Received date: 2022-04-24

  Revised date: 2022-07-05

  Online published: 2022-08-04

Supported by

National Natural Science Foundation of China(51871142);Independent Research and Development Project of State Key Laboratory of Advanced Special Steel, Shanghai Key Laboratory of Advanced Ferrometallurgy, Shanghai University(SKLASS 2021-Z08);Science and Technology Commission of Shanghai Municipality(19DZ2270200)

Abstract

Nickel-based superalloys, especially single-crystal (SC) ones, have long been recognized as important materials for turbine blades used in aerospace and gas engines. Static magnetic fields are effective at controlling the material forming. The use of static magnetic fields during solidification has evolved as a sophisticated approach for efficiently controlling the microstructures and mechanical performance of metallic materials. In recent years, studies have shown that static magnetic fields have a complex effect on dendrites in SC superalloys. However, the mechanism of static magnetic fields regulating stray grains on remelted interface needs to be investigated further. This work studied the generation of stray grains near the seed remelted zone and the evolution mechanism during the directional solidification of the SC superalloy assisted by a magnetic field by tracing the solidification microstructure. The stray grains of large orientation that deviated from the <001> direction appeared on the remelted zone interface of the solidification microstructure when the magnetic field was applied, accompanied by the formation of a large-angle grain boundary (LAGB). Most of the stray grains were distributed at the sample edge. The increase in magnetic field intensity and pulling speed increased the number of stray grains and the length of the LAGB. As the solidification progressed, the large-orientation stray grains and the LAGBs were eliminated at a fast speed and evolved into small-orientation dendrites. During the following solidification, the orientation of the dendrites became even smaller and the evolution speed decreased sharply. The increase in withdrawal speed intensified the evolution process. The stray grains formed in the remelted zone can be attributed to the twisting dendrite by the thermoelectric magnetic force. The distribution of more stray grains around the sample was caused by the circulation from thermoelectric magnetic convection at the macroscopic scale.

Cite this article

SU Zhenqi , ZHANG Congjiang , YUAN Xiaotan , HU Xingjin , LU Keke , REN Weili , DING Biao , ZHENG Tianxiang , SHEN Zhe , ZHONG Yunbo , WANG Hui , WANG Qiuliang . Formation and Evolution of Stray Grains on Remelted Interface in the Seed Crystal During the Directional Solidification of Single-Crystal Superalloys Assisted by Vertical Static Magnetic Field[J]. Acta Metall Sin, 2023 , 59(12) : 1568 -1580 . DOI: 10.11900/0412.1961.2022.00193

References

1 Guo J T. The current situation of application and development of superalloys in the fields of energy industry[J]. Acta Metall. Sin., 2010, 46: 513
  郭建亭. 高温合金在能源工业领域中的应用现状与发展[J]. 金属学报, 2010, 46: 513
2 Ma D X. Development of single crystal solidification technology for production of superalloy turbine blades[J]. Acta Metall. Sin., 2015, 51: 1179
  马德新. 高温合金叶片单晶凝固技术的新发展[J]. 金属学报, 2015, 51: 1179
3 Sun X F, Jin T, Zhou Y Z, et al. Research progress of nickel-base single crystal superalloys[J]. Mater. China, 2012, 31(12): 1
  孙晓峰, 金 涛, 周亦胄 等. 镍基单晶高温合金研究进展[J]. 中国材料进展, 2012, 31(12): 1
4 Zhang J, Huang T W, Liu L, et al. Advances in solidification characteristics and typical casting defects in nickel-based single crystal superalloys[J]. Acta Metall. Sin., 2015, 51: 1163
  张 军, 黄太文, 刘 林 等. 单晶高温合金凝固特性与典型凝固缺陷研究[J]. 金属学报, 2015, 51: 1163
5 Ren N, Panwisawas C, Li J, et al. Solute enrichment induced dendritic fragmentation in directional solidification of nickel-based superalloys[J]. Acta Mater., 2021, 215: 117043
6 Zhang J, Wang L, Wang D, et al. Recent progress in research and development of nickel-based single crystal superalloys[J]. Acta Metall. Sin., 2019, 55: 1077
  张 健, 王 莉, 王 栋 等. 镍基单晶高温合金的研发进展[J]. 金属学报, 2019, 55: 1077
7 D'Souza N, Newell M, Devendra K, et al. Formation of low angle boundaries in Ni-based superalloys[J]. Mater. Sci. Eng., 2005, A413-414: 567
8 Zhou Y Z. Formation of stray grains during directional solidification of a nickel-based superalloy[J]. Scr. Mater., 2011, 65: 281
9 Yang X L, Dong H B, Wang W, et al. Microscale simulation of stray grain formation in investment cast turbine blades[J]. Mater. Sci. Eng., 2004, A386: 129
10 Meng X B, Lu Q, Li J G, et al. Modes of grain selection in spiral selector during directional solidification of nickel-base superalloys[J]. J. Mater. Sci. Technol., 2012, 28: 214
11 Li Y F, Liu L, Huang T W, et al. The process analysis of seeding-grain selection and its effect on stray grain and orientation control[J]. J. Alloys Compd., 2016, 657: 341
12 Hu S S, Yang W C, Li Z R, et al. Formation mechanisms and control method for stray grains at melt-back region of Ni-based single crystal seed[J]. Prog. Nat. Sci., 2021, 31: 624
13 Hallensleben P, Schaar H, Thome P, et al. On the evolution of cast microstructures during processing of single crystal Ni-base superalloys using a Bridgman seed technique[J]. Mater. Des., 2017, 128: 98
14 Zhang T, Ren W L, Dong J W, et al. Effect of high magnetic field on the primary dendrite arm spacing and segregation of directionally solidified superalloy DZ417G[J]. J. Alloys Compd., 2009, 487: 612
15 Dong J W, Ren Z M, Ren W L, et al. Effect of horizontal magnetic field on the microstructure of directionally solidified Ni-based superalloy[J]. Acta Metall. Sin., 2010, 46: 71
  董建文, 任忠鸣, 任维丽 等. 横向磁场对镍基高温合金定向凝固组织的影响[J]. 金属学报, 2010, 46: 71
16 Ren W L, Lu L, Yuan G Z, et al. The effect of magnetic field on precipitation phases of single-crystal nickel-base superalloy during directional solidification[J]. Mater. Lett., 2013, 100: 223
17 Xuan W D, Song G, Duan F M, et al. Enhanced creep properties of nickel-base single crystal superalloy CMSX-4 by high magnetic field[J]. Mater. Sci. Eng., 2021, A803: 140729
18 Li Q D, Shen J, Qin L, et al. Effect of traveling magnetic field on freckle formation in directionally solidified CMSX-4 superalloy[J]. Mater. Process. Technol., 2019, 274: 116308
19 Xuan W D, Ren Z M, Li C J. Effect of a high magnetic field on microstructures of Ni-based superalloy during directional solidification[J]. J. Alloys Compd., 2015, 620: 10
20 Zhang K L, Li Y J, Yang Y S. Influence of the low voltage pulsed magnetic field on the columnar-to-equiaxed transition during directional solidification of superalloy K4169[J]. J. Mater. Sci. Technol., 2020, 48: 9
21 Ren W L, Niu C L, Ding B, et al. Improvement in creep life of a nickel-based single-crystal superalloy via composition homogeneity on the multiscales by magnetic-field-assisted directional solidification[J]. Sci. Rep., 2018, 8: 1452
22 Xuan W D, Liu H, Lan J, et al. Effect of a transverse magnetic field on stray grain formation of Ni-based single crystal superalloy during directional solidification[J]. Metall. Mater. Trans., 2016, 47B: 3231
23 Xuan W D, Liu H, Li C J, et al. Effect of a high magnetic field on microstructures of Ni-based single crystal superalloy during seed melt-back[J]. Metall. Mater. Trans., 2016, 47B: 828
24 Xuan W D, Lan J, Liu H, et al. Effects of a high magnetic field on the microstructure of Ni-based single-crystal superalloys during directional solidification[J]. Metall. Mater. Trans., 2017, 48A: 3804
25 Yuan X T, Zhou T, Ren W L, et al. Nondestructive effect of the cusp magnetic field on the dendritic microstructure during the directional solidification of nickel-based single crystal superalloy[J]. J. Mater. Sci. Technol., 2021, 62: 52
26 Liu C L, Su H J, Zhang J, et al. Effect of electromagnetic field on microstructure of Ni-based single crystal superalloys[J]. Acta Metall. Sin., 2018, 54: 1428
  刘承林, 苏海军, 张 军 等. 电磁场对镍基单晶高温合金组织的影响[J]. 金属学报, 2018, 54: 1428
27 Li Y J, Teng Y F, Feng X H, et al. Effects of pulsed magnetic field on microsegregation of solute elements in a Ni-based single crystal superalloy[J]. J. Mater. Sci. Technol., 2017, 33: 105
28 Niu C L, Ren W L, Ding B, et al. The change of mushy-zone length of a nickel-based single-crystal superalloy during the static-magnetic-field-assisted directional solidification[J]. Cryst. Res. Technol., 2018, 53: 1700187
29 Liu Q. EBSD technique and its applications in materials science[J]. Chin. J. Stereol. Image Anal., 2005, 10: 205
  刘 庆. 电子背散射衍射技术及其在材料科学中的应用[J]. 中国体视学与图像分析, 2005, 10: 205
30 Xu W L, Wang F, Ma D X, et al. Sliver defect formation in single crystal Ni-based superalloy castings[J]. Mater. Des., 2020, 196: 109138
31 Ren Z M, Lei Z S, Li C J, et al. New study and development on electromagnetic field technology in metallurgical processes[J]. Acta Metall. Sin., 2020, 56: 583
  任忠鸣, 雷作胜, 李传军 等. 电磁冶金技术研究新进展[J]. 金属学报, 2020, 56: 583
32 Wang J, Fautrelle Y, Ren Z M, et al. Thermoelectric magnetic force acting on the solid during directional solidification under a static magnetic field[J]. Appl. Phys. Lett., 2012, 101: 251904
33 Dahle A K, Arnberg L. Development of strength in solidifying aluminium alloys[J]. Acta Mater., 1997, 45: 547
34 Khine Y Y, Walker J S. Thermoelectric magnetohydrodynamic effects during Bridgman semiconductor crystal growth with a uniform axial magnetic field[J]. J. Cryst. Growth, 1998, 183: 150
35 Ma D X. Freckle formation during directional solidification of complex castings of superalloys[J]. Acta Metall. Sin., 2016, 52: 426
  马德新. 定向凝固的复杂形状高温合金铸件中的雀斑形成[J]. 金属学报, 2016, 52: 426
36 Walton D, Chalmers B. The origin of the preferred orientation in the columnar zone of ingots[J]. Trans. Am. Inst. Min. Metall. Eng., 1959, 215: 447
37 Zhou Y Z, Volek A, Green N R. Mechanism of competitive grain growth in directional solidification of a nickel-base superalloy[J]. Acta Mater., 2008, 56: 2631
38 Hu S S, Liu L, Cui Q W, et al. Converging competitive growth in bi-crystal of Ni-based superalloy during directional solidification[J]. Acta. Metall. Sin., 2016, 52: 897
  胡松松, 刘 林, 崔强伟 等. 镍基高温合金定向凝固过程中的汇聚型双晶竞争生长[J]. 金属学报, 2016, 52: 897
39 Guo C W, Takaki T, Sakane S, et al. Overgrowth behavior at converging grain boundaries during competitive grain growth: A two-dimensional phase-field study[J]. Int. J. Heat Mass Transfer, 2020, 160: 120196
40 Zhou Y Z, Jin T, Sun X F. Structure evolution in directionally solidified bicrystals of nickel base superalloys[J]. Acta Metall. Sin., 2010, 46: 1327
  周亦胄, 金 涛, 孙晓峰. 双晶镍基高温合金定向凝固过程的结构演化[J]. 金属学报, 2010, 46: 1327
Outlines

/