Grain Boundary Structure and Coercivity Enhancement of Nd90Al10 Alloy Modified NdFeB Permanent Magnets by GBD Process
Received date: 2021-11-01
Revised date: 2022-04-24
Online published: 2022-07-25
Supported by
High Technology Research and Development Program of China(2010AA03A0401)
The grain boundary diffusion (GBD) process is a remarkable achievement in sintered Nd-Fe-B permanent magnet manufacturing. Furthermore, the coercivity can be considerably improved by diffusing heavy rare earth (HRE) elements into the magnet along the grain boundary, and the reduced HRE consumption can also be realized. However, compared with parameters of GBD, previous research has focused less on improving the magnet. In this study, the magnet was prepared using low melting point alloy Nd90Al10 before GBD modification, after which the corresponding Tb-GBD was completed. The magnetic property results indicated that the coercivity increased to 1439 kA/m, which was 530 kA/m higher than the unmodified magnet. Thus, the effects of the grain boundary structure and composition on the coercivity were analyzed. The addition of Nd90Al10 did not affect the Curie temperature of the magnet, but it reduced the low-temperature phase transition temperature. The Tb replaced Nd at the margin of main phase, which moved the diffraction peak to the right in the XRD spectrum. Moreover, a clear Tb-rich shell surrounding the main phase formed in the diffused magnet modified by Nd90Al10 at the depth of 20 μm, and the shell could still be clearly observed at 100 μm. However, the main phase was surrounded by the continuous grain boundary when the depth increased to 500 μm in Nd90Al10 modified magnet by GBD. The Tb-rich shell was observed by TEM and a noncrystalline Nd-rich phase was observed. The content peak of the Nd element appeared in the central region of the Nd-rich phase. This, the diffused depth and usage efficiency remarkably improved, because the Nd-rich phase acted as a channel for Tb diffusion, with the concentration of Tb being as high as 35%.
LIU Lujun , LIU Zheng , LIU Renhui , LIU Yong . Grain Boundary Structure and Coercivity Enhancement of Nd90Al10 Alloy Modified NdFeB Permanent Magnets by GBD Process[J]. Acta Metall Sin, 2023 , 59(11) : 1457 -1465 . DOI: 10.11900/0412.1961.2021.00471
| 1 | Bai G, Gao R. W, Sun Y, et al. Study of high-coercivity sintered NdFeB magnets [J]. J. Magn. Magn. Mater., 2007, 308: 20 |
| 2 | Yan G H, Chen R J, Ding Y, et al. The preparation of sintered NdFeB magnet with high-coercivity and high temperature-stability [J]. J. Phys. Conf. Ser., 2011, 266: 012052 |
| 3 | Hirosawa S, Matsuura Y, Yamamoto H, et al. Magnetization and magnetic anisotropy of R2Fe14B measured on single crystals [J]. J. Appl. Phys., 1986, 59: 873 |
| 4 | Oono N, Sagawa M, Kasada R, et al. Production of thick high-performance sintered neodymium magnets by grain boundary diffusion treatment with dysprosium-nickel-aluminum alloy [J]. J. Magn. Magn. Mater., 2011, 323: 297 |
| 5 | Wang J, Liang L, Wu M Y, et al. Research progress on grain boundary fine microstructure and magnetic properties of sintered NdFeB magnet [J]. Chin. J. Nonferrous Met., 2014, 24: 1562 |
| 王 静, 梁 乐, 武梦艳 等. 烧结NdFeB永磁体的晶界微细结构及性能研究进展 [J]. 中国有色金属学报, 2014, 24: 1562 | |
| 6 | Wang X L, Zhao L N, Ding K H, et al. Influence of dysprosium distribution on properties of sintered and aged Dy-doped NdFeB permanent magnets [J]. Rare Met. Mater. Eng., 2016, 45: 309 |
| 7 | Chen B C, Liu X M, Chen R J, et al. Design and fabrication of Dy-free sintered permanent magnets with high coercivity [J]. J. Appl. Phys., 2012, 111: 07A710 |
| 8 | Dormidontov N A, Dormidontov A G, Lileev A S, et al. Effect of partial substitution of neodymium with praseodymium on the magnetic and process properties of sintered magnets of type NdFeB [J]. Met. Sci. Heat Treat., 2017, 58: 608 |
| 9 | Park K T, Hiraga K, Sagawa M. Effect of metal-coating and consecutive heat treatment on coercivity of thin Nd-Fe-B sintered magnets [A]. Proceeding of the 16th International Workshop on Rare-Earth Magnets and Their Applications [C]. Sendai, Japan: Japan Institute of Metals, 2000: 257 |
| 10 | Nakamura H, Hirota K, Shimao M, et al. Magnetic properties of extremely small Nd-Fe-B sintered magnets [J]. IEEE Trans. Magnet., 2005, 41: 3844 |
| 11 | Cui X G, Wang X H, Cui C Y, et al. Research progress in Grain boundary diffusion modification, microstructures and properties of sintered Nd-Fe-B magnets [J]. Chin. J. Rare Met., 2018, 42: 315 |
| 崔熙贵, 王兴华, 崔承云 等. 烧结钕铁硼的晶界扩散改性、结构与性能研究进展 [J]. 稀有金属, 2018, 42: 315 | |
| 12 | Tan M, Zhao Y, Chen H S, et al. Research progress on grain boundary diffused Nd-Fe-B magnets [J]. Powder Metall. Ind., 2019, 29(2): 66 |
| 谭 敏, 赵 扬, 陈红升 等. 钕铁硼晶界扩散研究进展 [J]. 粉末冶金工业, 2019, 29(2): 66 | |
| 13 | Suzuki H, Satsu Y, Komuro M. Magnetic properties of a Nd-Fe-B sintered magnet with Dy segregation [J]. J. Appl. Phys., 2009, 105: 07A734 |
| 14 | Li D S, Suzuki S, Kawasaki T, et al. Grain interface modification and magnetic properties of Nd-Fe-B sintered magnets [J]. Jpn. J. Appl. Phys., 2008, 47: 7876 |
| 15 | Popov A G, Vasilenko D Y, Puzanova T Z, et al. Effect of diffusion annealing on the hysteretic properties of sintered Nd-Fe-B magnets [J]. Phys. Met. Metall., 2011, 111: 471 |
| 16 | Sun X X, Bao X Q, Gao X X, et al. Effect of dysprosium addition by pack cementation on magnetic properties and microstructure of Nd-Fe-B sintered magnets [J]. Chin. J. Rare Met., 2009, 27: 86 |
| 孙绪新, 包小倩, 高学绪 等. 烧结Nd-Fe-B磁体表面渗镀Dy2O3对磁体显微组织和磁性能的影响 [J]. 中国稀土学报, 2009, 27: 86 | |
| 17 | Zhang L G, Liu L B, Jin Z P. The Phase Diagrams and Application of Al-Cu-Re System [M]. Changsha: Central South University Press, 2015: 1 |
| 章立钢, 刘立斌, 金展鹏. 稀土A1-Cu合金相图及应用 [M]. 长沙: 中南大学出版社, 2015: 1 | |
| 18 | Di J H. Study on the effect of Al and rare earth grain boundary Co-diffusion on the microstructure and coercivity of sintered Nd-Fe-B magnets [D]. Ningbo: Ningbo Institute of Material Technology and Engineering, Chinese Academy of Science, 2019 |
| 邸敬慧. Al和稀土元素共晶界扩散对烧结Nd-Fe-B磁体微观结构和矫顽力影响的研究 [D]. 宁波: 中国科学院大学(中国科学院宁波材料技术与工程研究所), 2019 | |
| 19 | Kim T H, Lee S R, Namkumg S, et al. A study on the Nd-rich phase evolution in the Nd-Fe-B sintered magnet and its mechanism during post-sintering annealing [J]. J. Alloys Compd., 2012, 537: 261 |
| 20 | Knoch K G, Grieb B, Henig E T, et al. Upgraded Nd-Fe-B-AD (AD = Al,Ga) magnets: Wettability and microstructure [J]. IEEE Trans. Magnet., 1990, 26: 1951 |
| 21 | Goto R, Nishio S, Matsuura M, et al. Wettability and interfacial microstructure between Nd2Fe14B and Nd-rich phases in Nd-Fe-B alloys [J]. IEEE Trans. Magnet., 2008, 44: 4232 |
| 22 | Nishio S, Sugimoto S, Goto R, et al. Effect of Cu addition on the phase equilibria in Nd-Fe-B sintered magnets [J]. Mater. Trans., 2009, 50: 723 |
| 23 | Kim T H, Lee S R, Bae K H, et al. Effects of Al/Cu co-doping on crystal structure and chemical composition of Nd-rich phases in Nd-Fe-B sintered magnet [J]. Acta Mater., 2017, 133: 200 |
| 24 | Chen F G, Jin Y X, Cheng Y, et al. Investigation of the wettability and the interface feature of the melted Nd70Cu30 alloy on the surface of a sintered Nd-Fe-B magnet [J]. Scr. Mater., 2018, 157: 135 |
| 25 | Kim T H, Lee S R, Yun S J, et al. Anisotropic diffusion mechanism in grain boundary diffusion processed Nd-Fe-B sintered magnet [J]. Acta Mater., 2016, 112: 59 |
| 26 | You C Y, Lu Z X, Qiao Y, et al. Microstructure characterization and its relationship with magnetic properties of sintered Nd-Fe-B magnet [A]. Proceedings of the 7th Chinese Academic Conference on Functional Materials and Their Applications [C]. Changsha: China Instrumentation Society, China Metal Society, 2010: 314 |
| 游才印, 卢正欣, 乔 玉 等. 烧结钕铁硼磁体的微结构表征及其与磁性能的关系研究 [A]. 第七届中国功能材料及其应用学术会议论文集 [C]. 长沙: 中国仪器仪表学会, 中国金属学会, 2010: 314 | |
| 27 | Xu F. Effects of grain boundary structure and chemistry on the coercivity of NdFeB materials [D]. Shanghai: Shanghai Jiao Tong University, 2011 |
| 徐 芳. 晶界结构和晶界化学对NdFeB材料矫顽力的影响 [D]. 上海: 上海交通大学, 2011 | |
| 28 | Oikawa T, Yokota H, Ohkubo T, et al. Large-scale micromagnetic simulation of Nd-Fe-B sintered magnets with Dy-rich shell structures [J]. AIP Adv., 2016, 6: 056006 |
| 29 | Périgo E A, Titov I, Weber R, et al. Small-angle neutron scattering study of coercivity enhancement in grain-boundary-diffused Nd-Fe-B sintered magnets [J]. J. Alloys Compd., 2016, 677: 139 |
/
| 〈 |
|
〉 |