Additive Manufacturing of Magnesium Alloys by Selective Laser Melting Technology: A Review
Received date: 2022-04-09
Revised date: 2022-06-27
Online published: 2022-07-18
Supported by
National Key Research and Development Program of China(2021YFB3701001);National Natural Science Foundation of China(51971130);National Natural Science Foundation of China(U21A2047);National Natural Science Foundation of China(51821001);National Natural Science Foundation of China(U2037601)
Selective laser melting (SLM) additive manufacturing technology holds the broad prospect for the preparation of high-performance complex metal components owing to its high processing accuracy, short manufacturing cycle, and high material usage. Magnesium (Mg) alloys are the lightest metal structural material and provide the benefits of low density, substantial specific strength and specific stiffness, good damping and shock absorption performance, and good biodegradability. Thus, it is worthwhile to employ SLM to manufacture Mg alloys, which is predicted to widen the application scope of Mg alloys. In this study, a comprehensive review on SLM of Mg alloys focusing on the preparation of Mg alloy powders, SLM process parameters, metallurgical defects, microstructure and mechanical properties of the as-built state, post-processing, and special equipment developed for SLM of Mg alloys is given. Finally, the future development trends of the SLM of Mg alloys are explored.
Liming PENG , Qingchen DENG , Yujuan WU , Penghuai FU , Ziyi LIU , Qianye WU , Kai CHEN , Wenjiang DING . Additive Manufacturing of Magnesium Alloys by Selective Laser Melting Technology: A Review[J]. Acta Metall Sin, 2023 , 59(1) : 31 -54 . DOI: 10.11900/0412.1961.2022.00166
| 1 | Wu G H, Wang C L, Sun M, et al. Recent developments and applications on high-performance cast magnesium rare-earth alloys [J]. J. Magnes. Alloy., 2021, 9: 1 |
| 2 | Song J F, Chen J, Xiong X M, et al. Research advances of magnesium and magnesium alloys worldwide in 2021 [J]. J. Magnes. Alloy., 2022, 10: 863 |
| 3 | Fu P H, Peng L M, Jiang H, et al. Tensile properties of high strength cast Mg alloys at room temperature: A review [J]. China Foundry, 2014, 11: 277 |
| 4 | Lu B H, Li D C, Tian X Y. Development trends in additive manufacturing and 3D printing [J]. Engineering, 2015, 1: 85 |
| 5 | Zeng Z R, Salehi M, Kopp A, et al. Recent progress and perspectives in additive manufacturing of magnesium alloys [J]. J. Magnes. Alloy., 2022, 10: 1511 |
| 6 | Tandon R, Palmer T, Gieseke M, et al. Additive manufacturing of magnesium alloy powders: Investigations into process development using Elektron?MAP + 43 via laser powder bed fusion and directed energy deposition [A]. World PM 2016 Congress and Exhibition [C]. European Powder Metallurgy Association (EPMA), 2016: 1 |
| 7 | Liao H G, Fu P H, Peng L M, et al. Microstructure and mechanical properties of laser melting deposited GW103K Mg-RE alloy [J]. Mater. Sci. Eng., 2017, A687: 281 |
| 8 | Zheng D D, Li Z, Jiang Y L, et al. Effect of multiple thermal cycles on the microstructure evolution of GA151K alloy fabricated by laser-directed energy deposition [J]. Addit. Manuf., 2022, 57: 102957 |
| 9 | Madhuri N, Jayakumar V, Sathishkumar M. Recent developments and challenges accompanying with wire arc additive manufacturing of Mg alloys: A review [J]. Mater. Today Proc., 2021, 46: 8573 |
| 10 | Guo J, Zhou Y, Liu C M, et al. Wire arc additive manufacturing of AZ31 magnesium alloy: Grain refinement by adjusting pulse frequency [J]. Materials, 2016, 9: 823480 |
| 11 | Holguin D A M, Han S, Kim N P. Magnesium alloy 3D printing by wire and arc additive manufacturing (WAAM) [J]. MRS Adv., 2018, 3: 2959 |
| 12 | Rong W, Zhang Y, Wu Y J, et al. Fabrication of high-strength Mg-Gd-Zn-Zr alloys via differential-thermal extrusion [J]. Mater. Charact., 2017, 131: 380 |
| 13 | Zhang W N, Wang L Z, Feng Z X, et al. Research progress on selective laser melting (SLM) of magnesium alloys: A review [J]. Optik, 2020, 207: 163842 |
| 14 | Thijs L, Kempen K, Kruth J P, et al. Fine-structured aluminium products with controllable texture by selective laser melting of pre-alloyed AlSi10Mg powder [J]. Acta Mater., 2013, 61: 1809 |
| 15 | Thijs L, Verhaeghe F, Craeghs T, et al. A study of the microstructural evolution during selective laser melting of Ti-6Al-4V [J]. Acta Mater., 2010, 58: 3303 |
| 16 | Gao Y, Zhang D Y, Cao M, et al. Effect of δ phase on high temperature mechanical performances of Inconel 718 fabricated with SLM process [J]. Mater. Sci. Eng., 2019, A767: 138327 |
| 17 | Wang Y M, Voisin T, McKeown J T, et al. Additively manufactured hierarchical stainless steels with high strength and ductility [J]. Nat. Mater., 2018, 17: 63 |
| 18 | Zhang B C, Liao H L, Coddet C. Effects of processing parameters on properties of selective laser melting Mg-9%Al powder mixture [J]. Mater. Des., 2012, 34: 753 |
| 19 | Liu J, Wen P. Metal vaporization and its influence during laser powder bed fusion process [J]. Mater. Des., 2022, 215: 110505 |
| 20 | Deng Q C, Wu Y J, Wu Q Y, et al. Microstructure evolution and mechanical properties of a high-strength Mg-10Gd-3Y-1Zn-0.4Zr alloy fabricated by laser powder bed fusion [J]. Addit. Manuf., 2022, 49: 102517 |
| 21 | Cao X, Jahazi M, Immarigeon J P, et al. A review of laser welding techniques for magnesium alloys [J]. J. Mater. Process. Technol., 2006, 171: 188 |
| 22 | Brandau B, Da Silva A, Wilsnack C, et al. Absorbance study of powder conditions for laser additive manufacturing [J]. Mater. Des., 2022, 216: 110591 |
| 23 | Ng C C, Savalani M M, Man H C, et al. Layer manufacturing of magnesium and its alloy structures for future applications [J]. Virtual Phys. Prototyp., 2010, 5: 13 |
| 24 | Ng C C, Savalani M M, Lau M L, et al. Microstructure and mechanical properties of selective laser melted magnesium [J]. Appl. Surf. Sci., 2011, 257: 7447 |
| 25 | Gieseke M, Noelke C, Kaierle S, et al. Selective laser melting of magnesium and magnesium alloys[A]. Magnesium Technology2013[M]. Cham: Springer, 2013: 65 |
| 26 | Hu D, Wang Y, Zhang D F, et al. Experimental investigation on selective laser melting of bulk net-shape pure magnesium [J]. Mater. Manuf. Process., 2015, 30: 1298 |
| 27 | Niu X M, Shen H Y, Fu J Z, et al. Corrosion behaviour of laser powder bed fused bulk pure magnesium in Hank's solution [J]. Corros. Sci., 2019, 157: 284 |
| 28 | Wei K W, Gao M, Wang Z M, et al. Effect of energy input on formability, microstructure and mechanical properties of selective laser melted AZ91D magnesium alloy [J]. Mater. Sci. Eng., 2014, A611: 212 |
| 29 | Pawlak A, Rosienkiewicz M, Chlebus E. Design of experiments approach in AZ31 powder selective laser melting process optimization [J]. Arch. Civ. Mech. Eng., 2017, 17: 9 |
| 30 | He C X, Bin S, Wu P, et al. Microstructure evolution and biodegradation behavior of laser rapid solidified Mg-Al-Zn alloy [J]. Metals, 2017, 7: 105 |
| 31 | Niu X M, Shen H Y, Fu J Z. Microstructure and mechanical properties of selective laser melted Mg-9?wt%Al powder mixture [J]. Mater. Lett., 2018, 221: 4 |
| 32 | Liu S, Yang W S, Shi X, et al. Influence of laser process parameters on the densification, microstructure, and mechanical properties of a selective laser melted AZ61 magnesium alloy [J]. J. Alloys Compd., 2019, 808: 151160 |
| 33 | Proa?o B, Miyahara H, Matsumoto T, et al. Weakest region analysis of non-combustible Mg products fabricated by selective laser melting [J]. Theor. Appl. Fract. Mech., 2019, 103: 102291 |
| 34 | Pawlak A, Szymczyk P E, Kurzynowski T, et al. Selective laser melting of magnesium AZ31B alloy powder [J]. Rapid Prototyp. J., 2019, 26: 249 |
| 35 | Liu S, Guo H J. Influence of hot isostatic pressing (HIP) on mechanical properties of magnesium alloy produced by selective laser melting (SLM) [J]. Mater. Lett., 2020, 265: 127463 |
| 36 | Liu L, Ma H T, Gao C D, et al. Island-to-acicular alteration of second phase enhances the degradation resistance of biomedical AZ61 alloy [J]. J. Alloys Compd., 2020, 835: 155397 |
| 37 | Liu S, Guo H J. Balling behavior of selective laser melting (SLM) magnesium alloy [J]. Materials (Basel), 2020, 13: 3632 |
| 38 | Proa?o B, Miyahara H, Matsumoto T, et al. Plastic strain distribution throughout the microstructure duality during the fracture process of non-combustible Mg products fabricated by selective laser melting [J]. Theor. Appl. Fract. Mech., 2020, 110: 102805 |
| 39 | Xu C J, Hua X Y, Ma D, et al. Study on microstructure and properties of selective laser melted (SLM) magnesium alloy AZ91D [J]. Foundry Technol., 2021, 42: 749 |
| 39 | 徐春杰, 华心雨, 马 东 等. 选区激光熔化AZ91D镁合金的组织与性能 [J]. 铸造技术, 2021, 42: 749 |
| 40 | Wang J Y, Chang Z P, Yue Y F, et al. Effect of particle size distribution of AZ91D magnesium alloy powder on selective laser melting process [J]. Hebei J. Ind. Sci. Technol., 2022, 39: 79 |
| 40 | 王金业, 常志鹏, 岳彦芳 等. AZ91D镁合金粉末粒度分布对其选区激光熔化成形的影响 [J]. 河北工业科技, 2022, 39: 79 |
| 41 | Zeng Z R, Choudhary S, Esmaily M, et al. An additively manufactured magnesium-aluminium alloy withstands seawater corrosion [J]. npj Mater. Degrad., 2022, 6: 32 |
| 42 | Wei K W, Wang Z M, Zeng X Y. Influence of element vaporization on formability, composition, microstructure, and mechanical performance of the selective laser melted Mg-Zn-Zr components [J]. Mater. Lett., 2015, 156: 187 |
| 43 | Shuai C J, Yang Y W, Wu P, et al. Laser rapid solidification improves corrosion behavior of Mg-Zn-Zr alloy [J]. J. Alloys Compd., 2017, 691: 961 |
| 44 | Zhang M, Chen C J, Liu C, et al. Study on porous Mg-Zn-Zr ZK61 alloys produced by laser additive manufacturing [J]. Metals, 2018, 8: 635 |
| 45 | Shuai C J, Liu L, Zhao M C, et al. Microstructure, biodegradation, antibacterial and mechanical properties of ZK60-Cu alloys prepared by selective laser melting technique [J]. J. Mater. Sci. Technol., 2018, 34: 1944 |
| 46 | Wei K W, Zeng X Y, Wang Z M, et al. Selective laser melting of Mg-Zn binary alloys: Effects of Zn content on densification behavior, microstructure, and mechanical property [J]. Mater. Sci. Eng., 2019, A756: 226 |
| 47 | Yin Y, Huang Q L, Liang L X, et al. In vitro degradation behavior and cytocompatibility of ZK30/bioactive glass composites fabricated by selective laser melting for biomedical applications [J]. J. Alloys Compd., 2019, 785: 38 |
| 48 | Shuai C J, Liu L, Gao C D, et al. Uniform degradation mode and enhanced degradation resistance of Mg alloy via a long period stacking ordered phase in the grain interior [J]. Mater. Res. Express, 2019, 6: 065406 |
| 49 | Tao J X, Zhao M C, Zhao Y C, et al. Influence of graphene oxide (GO) on microstructure and biodegradation of ZK30-xGO composites prepared by selective laser melting [J]. J. Magnes. Alloy., 2020, 8: 952 |
| 50 | Yang Y W, Lu C F, Peng S P, et al. Laser additive manufacturing of Mg-based composite with improved degradation behaviour [J]. Virtual Phys. Prototyp., 2020, 15: 278 |
| 51 | Liu J G, Yin B Z, Sun Z R, et al. Hot cracking in ZK60 magnesium alloy produced by laser powder bed fusion process [J]. Mater. Lett., 2021, 301: 130283 |
| 52 | Wu C L, Zai W, Man H C. Additive manufacturing of ZK60 magnesium alloy by selective laser melting: Parameter optimization, microstructure and biodegradability [J]. Mater. Today Commun., 2021, 26: 101922 |
| 53 | Xie B, Zhao M C, Tao J X, et al. Comparison of the biodegradation of ZK30 subjected to solid solution treating and selective laser melting [J]. J. Mater. Res. Technol., 2021, 10: 722 |
| 54 | Benn F, D'Elia F, Van Gaalen K, et al. Printability, mechanical and degradation properties of Mg-(x)Zn elemental powder mixes processed by laser powder bed fusion [J]. Addit. Manuf. Lett., 2022, 2: 100025 |
| 55 | Liang J W, Lei Z L, Chen Y B, et al. Microstructure evolution of laser powder bed fusion ZK60 Mg alloy after different heat treatment [J]. J. Alloys Compd., 2022, 898: 163046 |
| 56 | Liang J W, Lei Z L, Chen Y B, et al. Elimination of extraordinarily high cracking susceptibility of ZK60 Mg alloy fabricated by laser powder bed fusion [J]. Mater. Lett., 2022, 312: 131731 |
| 57 | Liang J W, Lei Z L, Chen Y B, et al. Formability, microstructure, and thermal crack characteristics of selective laser melting of ZK60 magnesium alloy [J]. Mater. Sci. Eng., 2022, A839: 142858 |
| 58 | Zhou Y Z, Wu P, Yang Y W, et al. The microstructure, mechanical properties and degradation behavior of laser-melted Mg-Sn alloys [J]. J. Alloys Compd., 2016, 687: 109 |
| 59 | Yang Y W, Wu P, Wang Q Y, et al. The enhancement of Mg corrosion resistance by alloying Mn and laser-melting [J]. Materials (Basel), 2016, 9: 216 |
| 60 | Liu C, Zhang M, Chen C J. Effect of laser processing parameters on porosity, microstructure and mechanical properties of porous Mg-Ca alloys produced by laser additive manufacturing [J]. Mater. Sci. Eng., 2017, A703: 359 |
| 61 | Jauer L, Meiners W, Vervoort S, et al. Selective laser melting of magnesium alloys [J]. European Congress and Exhibition on Powder Metallurgy. European PM Conference Proceedings, 2016: 1 |
| 62 | Li Y, Zhou J, Pavanram P, et al. Additively manufactured biodegradable porous magnesium [J]. Acta Biomater., 2018, 67: 378 |
| 63 | Zumdick N A, Jauer L, Kersting L C, et al. Additive manufactured WE43 magnesium: A comparative study of the microstructure and mechanical properties with those of powder extruded and as-cast WE43 [J]. Mater. Charact., 2019, 147: 384 |
| 64 | Gangireddy S, Gwalani B, Liu K M, et al. Microstructure and mechanical behavior of an additive manufactured (AM) WE43-Mg alloy [J]. Addit. Manuf., 2019, 26: 53 |
| 65 | B?r F, Berger L, Jauer L, et al. Laser additive manufacturing of biodegradable magnesium alloy WE43: A detailed microstructure analysis [J]. Acta Biomater., 2019, 98: 36 |
| 66 | Hyer H, Zhou L, Benson G, et al. Additive manufacturing of dense WE43 Mg alloy by laser powder bed fusion [J]. Addit. Manuf., 2020, 33: 101123 |
| 67 | Esmaily M, Zeng Z, Mortazavi A N, et al. A detailed microstructural and corrosion analysis of magnesium alloy WE43 manufactured by selective laser melting [J]. Addit. Manuf., 2020, 35: 101321 |
| 68 | Li M Z, Benn F, Derra T, et al. Microstructure, mechanical properties, corrosion resistance and cytocompatibility of WE43 Mg alloy scaffolds fabricated by laser powder bed fusion for biomedical applications [J]. Mater. Sci. Eng., 2021, C119: 111623 |
| 69 | Suchy J, Klakurková L, Man O, et al. Corrosion behaviour of WE43 magnesium alloy printed using selective laser melting in simulation body fluid solution [J]. J. Manuf. Process., 2021, 69: 556 |
| 70 | Liu J G, Liu B C, Min S Y, et al. Biodegradable magnesium alloy WE43 porous scaffolds fabricated by laser powder bed fusion for orthopedic applications: Process optimization, in vitro and in vivo investigation [J]. Bioact. Mater., 2022, 16: 301 |
| 71 | Attarzadeh F, Asadi E. Analysis of element loss, densification, and defects in laser-based powder-bed fusion of magnesium alloy WE43 [J]. J. Magnes. Alloy., 2022, doi: 10.1016/j.jma.2022.02.011 |
| 72 | Wang W L, Wang D, He L, et al. Thermal behavior and densification during selective laser melting of Mg-Y-Sm-Zn-Zr alloy: Simulation and experiments [J]. Mater. Res. Express, 2020, 7: 116519 |
| 73 | Wang W L, Yang X, Wang K K. Research on formability, microstructure and mechanical properties of selective laser melted Mg-Y-Sm-Zn-Zr magnesium alloy [J]. Mater. Charact., 2022, 189: 111980 |
| 74 | Wu J J, Wang L Z. Selective laser melting manufactured CNTs/AZ31B composites: Heat transfer and vaporized porosity evolution [J]. J. Mater. Res., 2018, 33: 2752 |
| 75 | Niu X M, Shen H Y, Fu J Z, et al. Effective control of microstructure evolution in AZ91D magnesium alloy by SiC nanoparticles in laser powder-bed fusion [J]. Mater. Des., 2021, 206: 109787 |
| 76 | Wang X C, Chen C J, Zhang M. Effect of heat treatment on microstructure and micro-wear resistance of selective laser melted Mg-Al-Zn alloy with La2O3 addition [J]. J. Mater. Eng. Perform., 2021, 30: 2316 |
| 77 | Wits W W, Smit M D, Al-Hamdani K, et al. Laser powder bed fusion of a magnesium-SiC metal matrix composite [J]. Proced. CIRP, 2019, 81: 506 |
| 78 | Wang C M, Shuai Y, Yang Y W, et al. Amorphous magnesium alloy with high corrosion resistance fabricated by laser powder bed fusion [J]. J. Alloys Compd., 2022, 897: 163247 |
| 79 | Deng Q C, Wu Y J, Luo Y H, et al. Fabrication of high-strength Mg-Gd-Zn-Zr alloy via selective laser melting [J]. Mater. Charact., 2020, 165: 110377 |
| 80 | Deng Q C, Wu Y J, Su N, et al. Influence of friction stir processing and aging heat treatment on microstructure and mechanical properties of selective laser melted Mg-Gd-Zr alloy [J]. Addit. Manuf., 2021, 44: 102036 |
| 81 | Fu P H, Wang N Q, Liao H G, et al. Microstructure and mechanical properties of high strength Mg-15Gd-1Zn-0. 4Zr alloy additive-manufactured by selective laser melting process [J]. Trans. Nonferrous Met. Soc. China, 2021, 31: 1969 |
| 82 | Deng Q C, Wu Y J, Zhu W X, et al. Effect of heat treatment on microstructure evolution and mechanical properties of selective laser melted Mg-11Gd-2Zn-0.4Zr alloy [J]. Mater. Sci. Eng., 2022, A829: 142139 |
| 83 | Deng Q C, Wang X C, Lan Q, et al. Limitations of linear energy density for laser powder bed fusion of Mg-15Gd-1Zn-0.4Zr alloy [J]. Mater. Charact., 2022, 190: 112071 |
| 84 | Deng Q C, Zhang Y, Liu Z Y, et al. Laser powder bed fusion of an age-hardenable Mg-10Gd-0.2Zr alloy with excellent strength-ductility synergy [J]. J. Alloys Compd., 2022, 910: 164863 |
| 85 | Wang Y C, Fu P H, Wang N Q, et al. Challenges and solutions for the additive manufacturing of biodegradable magnesium implants [J]. Engineering, 2020, 6: 1267 |
| 86 | Xie K, Wang N Q, Guo Y, et al. Additively manufactured biodegradable porous magnesium implants for elimination of implant-related infections: An in vitro and in vivo study [J]. Bioact. Mater., 2022, 8: 140 |
| 87 | Zheng Y F, Xia D D, Shen Y N, et al. Additively manufactured biodegrabable metal implants [J]. Acta Metall. Sin., 2021, 57: 1499 |
| 87 | 郑玉峰, 夏丹丹, 谌雨农 等. 增材制造可降解金属医用植入物 [J]. 金属学报, 2021, 57: 1499 |
| 88 | Cunningham R, Zhao C, Parab N, et al. Keyhole threshold and morphology in laser melting revealed by ultrahigh-speed X-ray imaging [J]. Science, 2019, 363: 849 |
| 89 | Zhao C, Parab N D, Li X X, et al. Critical instability at moving keyhole tip generates porosity in laser melting [J]. Science, 2020, 370: 1080 |
| 90 | Wang L, Zhang Y M, Chia H Y, et al. Mechanism of keyhole pore formation in metal additive manufacturing [J]. npj Comput. Mater., 2022, 8: 22 |
| 91 | Kou S. Solidification and liquation cracking issues in welding [J]. JOM, 2003, 55(6): 37 |
| 92 | Mercelis P, Kruth J P. Residual stresses in selective laser sintering and selective laser melting [J]. Rapid Prototyp. J., 2006, 12: 254 |
| 93 | Roehling J D, Smith W L, Roehling T T, et al. Reducing residual stress by selective large-area diode surface heating during laser powder bed fusion additive manufacturing [J]. Addit. Manuf., 2019, 28: 228 |
| 94 | Chen C P, Xiao Z X, Wang Y L, et al. Prediction study on in-situ reduction of thermal stress using combined laser beams in laser powder bed fusion [J]. Addit. Manuf., 2021, 47: 102221 |
| 95 | Kalentics N, Sohrabi N, Tabasi H G, et al. Healing cracks in selective laser melting by 3D laser shock peening [J]. Addit. Manuf., 2019, 30: 100881 |
| 96 | Salehi M, Maleksaeedi S, Farnoush H, et al. An investigation into interaction between magnesium powder and Ar gas: Implications for selective laser melting of magnesium [J]. Powder Technol., 2018, 333: 252 |
| 97 | Wen P, Qin Y, Chen Y Z, et al. Laser additive manufacturing of Zn porous scaffolds: Shielding gas flow, surface quality and densification [J]. J. Mater. Sci. Technol., 2019, 35: 368 |
| 98 | Rong W, Wu Y J, Zhang Y, et al. Characterization and strengthening effects of γ′ precipitates in a high-strength casting Mg-15Gd-1Zn-0.4Zr (wt.%) alloy [J]. Mater. Charact., 2017, 126: 1 |
| 99 | Ozaki T, Kuroki Y, Yamada K, et al. Mechanical properties of newly developed age hardenable Mg-3.2 mol%Gd-0.5 mol%Zn casting alloy [J]. Mater. Trans., 2008, 49: 2185 |
| 100 | Li J C, He Z L, Fu P H, et al. Heat treatment and mechanical properties of a high-strength cast Mg-Gd-Zn alloy [J]. Mater. Sci. Eng., 2016, A651: 745 |
| 101 | Zhang J H, Leng Z, Liu S J, et al. Microstructure and mechanical properties of Mg-Gd-Dy-Zn alloy with long period stacking ordered structure or stacking faults [J]. J. Alloys Compd., 2011, 509: 7717 |
| 102 | Zhang Y, Wu Y J, Peng L M, et al. Microstructure evolution and mechanical properties of an ultra-high strength casting Mg-15.6Gd-1.8Ag-0.4Zr alloy [J]. J. Alloys Compd., 2014, 615: 703 |
| 103 | Wang Q D, Chen J, Zhao Z, et al. Microstructure and super high strength of cast Mg-8.5Gd-2.3Y-1.8Ag-0.4Zr alloy [J]. Mater. Sci. Eng., 2010, A528: 323 |
| 104 | Macías J G S, Elangeswaran C, Zhao L, et al. Ductilisation and fatigue life enhancement of selective laser melted AlSi10Mg by friction stir processing [J]. Scr. Mater., 2019, 170: 124 |
/
| 〈 |
|
〉 |