Effect of Strain Rate on the Strain Partitioning Behavior of Ferrite/Bainite in X80 Pipeline Steel
Received date: 2021-09-27
Revised date: 2021-12-16
Online published: 2022-07-08
Supported by
Natural Science Foundation of Shaanxi Province(2019JZ-27)
X80 pipeline steel, which is mainly composed of ferrite/bainite, is an important structural steel for pipeline transportation. The plastic deformation of X80 pipeline steel at different strain rates caused by geological and human factors deteriorates its strength. Microstructural transformation and strain localization during deformation are the fundamental factors that deteriorate the mechanical properties of steel. Therefore, in this study, the strain partitioning behavior and microstructure evolution mechanism of ferrite and bainite in X80 pipeline steel at different strain rates (10-4 s-1 to 10-1 s-1) under 5% deformation were revealed using representative volume element models and electron backscatter diffraction technology. The results show that when the strain rate is low (10-4 s-1 to 10-3 s-1), ferrite has sufficient time to complete the evolution of geometrically necessary dislocations (GNDs) to low-angle grain boundaries (LAGBs) and the transformation of LAGBs to high-angle grain boundaries (HAGBs). Ferrite can release strain distortion energy, which can weaken the strain localization behavior of X80 steel. As the strain rate increases, the strain response time decreases, hindering the transition from LAGBs to HAGBs. This results in the accumulation of high-density GNDs and LAGBs in ferrite, thereby intensifying strain localization. Additionally, when the strain rate is high (10-2 s-1 to 10-1 s-1), the strain partitioning coefficient between ferrite and bainite could be reduced, thereby producing the strain gradient in the vicinity of the interface and resulting in GNDs accumulation and back stress formation. Furthermore, ferrite and bainite could show compressive and tensile stresses, respectively, thus limiting the strain coordination between the two phases significantly, increasing the stress concentration near the interface, and reducing the strain hardening ability. The strain partitioning behavior between ferrite and bainite was further revealed to better understand the plastic deformation of X80 pipeline steel.
Key words: X80 steel; strain rate; RVE model; strain localization; strain hardening
WANG Nan , CHEN Yongnan , ZHAO Qinyang , WU Gang , ZHANG Zhen , LUO Jinheng . Effect of Strain Rate on the Strain Partitioning Behavior of Ferrite/Bainite in X80 Pipeline Steel[J]. Acta Metall Sin, 2023 , 59(10) : 1299 -1310 . DOI: 10.11900/0412.1961.2021.00412
| 1 | Tan X D, Ponge D, Lu W J, et al. Carbon and strain partitioning in a quenched and partitioned steel containing ferrite [J]. Acta Mater., 2019, 165: 561 |
| 2 | Han Q N, Rui S S, Qiu W H, et al. Crystal orientation effect on fretting fatigue induced geometrically necessary dislocation distribution in Ni-based single-crystal superalloys [J]. Acta Mater., 2019, 179: 129 |
| 3 | Li S C, Guo C Y, Hao L L, et al. In-situ EBSD study of deformation behaviour of 600 MPa grade dual phase steel during uniaxial tensile tests [J]. Mater. Sci. Eng., 2019, A759: 624 |
| 4 | Das A, Tarafder S, Sivaprasad S, et al. Influence of microstructure and strain rate on the strain partitioning behaviour of dual phase steels [J]. Mater. Sci. Eng., 2019, A754: 348 |
| 5 | Kratochvíl J, Kru?ík M, Sedlá?ek R. Instability origin of subgrain formation in plastically deformed materials [J]. Int. J. Eng. Sci., 2010, 48: 1401 |
| 6 | Wang N, Chen Y N, Wu G, et al. Investigation on micromechanism involved in ferrite hardening after prestraining of dual-phase steel [J]. Mater. Sci. Eng., 2021, A800: 140387 |
| 7 | Dai Q F, Song R B, Fan W Y, et al. Behaviour and mechanism of strain hardening for dual phase steel DP1180 under high strain rate deformation [J]. Acta Metall. Sin., 2012, 48: 1160 |
| 代启锋, 宋仁伯, 范午言 等. DP1180双相钢在高应变速率变形条件下应变硬化行为及机制 [J]. 金属学报, 2012, 48: 1160 | |
| 8 | Shakerifard B, Lopez J G, Legaza M C T, et al. Strain rate dependent dynamic mechanical response of bainitic multiphase steels [J]. Mater. Sci. Eng., 2019, A745: 279 |
| 9 | Dong D Y, Liu Y, Wang L, et al. Effect of strain rate on dynamic deformation behavior of DP780 steel [J]. Acta Metall. Sin., 2013, 49: 159 |
| 董丹阳, 刘 杨, 王 磊 等. 应变速率对DP780钢动态拉伸变形行为的影响 [J]. 金属学报, 2013, 49: 159 | |
| 10 | Kundu A, Field D P, Chakraborti P C. Effect of strain and strain rate on the development of deformation heterogeneity during tensile deformation of a solution annealed 304 LN austenitic stainless steel: An EBSD study [J]. Mater. Sci. Eng., 2020, A773: 138854 |
| 11 | Ghassemi-Armaki H, Maa? R, Bhat S P, et al. Deformation response of ferrite and martensite in a dual-phase steel [J]. Acta Mater., 2014, 62: 197 |
| 12 | Nguyen T T, Park J S, Kim W S, et al. Environment hydrogen embrittlement of pipeline steel X70 under various gas mixture conditions with in situ small punch tests [J]. Mater. Sci. Eng., 2020, A781: 139114 |
| 13 | Zhang J, Liang Z, Zhao G H. Mechanical behaviour analysis of a buried steel pipeline under ground overload [J]. Eng. Failure Anal., 2016, 63: 131 |
| 14 | Sodjit S, Uthaisangsuk V. Microstructure based prediction of strain hardening behavior of dual phase steels [J]. Mater. Des., 2012, 41: 370 |
| 15 | Chen Y N, Wu Z C, Wu G, et al. Investigation on micromechanism of ferrite hardening after pre-straining with different strain rates of dual-phase steel [J]. Mater. Sci. Eng., 2021, A802: 140657 |
| 16 | Fillafer A, Krempaszky C, Werner E. On strain partitioning and micro-damage behavior of dual-phase steels [J]. Mater. Sci. Eng., 2014, A614: 180 |
| 17 | Ma J, Tian C C, Ma A B. Effect on microstructure and properties of X80 high steel grade pipeline steel by prestrain [J]. Ind. Heat., 2021, 50(2): 49 |
| 马 晶, 田晨超, 马安博. 预应变对X80高钢级管线钢力学性能的影响 [J]. 工业加热, 2021, 50(2): 49 | |
| 18 | Park S, Jung J, Cho W, et al. Predictive dual-scale finite element simulation for hole expansion failure of ferrite-bainite steel [J]. Int. J. Plast., 2021, 136: 102900 |
| 19 | Kuang S, Kang Y L, Yu H, et al. Stress-strain partitioning analysis of constituent phases in dual phase steel based on the modified law of mixture [J]. Int. J. Miner. Metall. Mater., 2009, 16: 393 |
| 20 | Oliver W C, Pharr G M. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments [J]. J. Mater. Res., 1992, 7: 1564 |
| 21 | Zhao Z T, Wang X S, Qiao G Y, et al. Effect of bainite morphology on deformation compatibility of mesostructure in ferrite/bainite dual-phase steel: Mesostructure-based finite element analysis [J]. Mater. Des., 2019, 180: 107870 |
| 22 | Zhang C Z, Yang S H, Gong B M, et al. Effects of post weld heat treatment (PWHT) on mechanical properties of C-Mn weld metal: Experimental observation and microstructure-based simulation [J]. Mater. Sci. Eng., 2018, A712: 430 |
| 23 | Werner E, Wesenjak R, Fillafer A, et al. Microstructure-based modelling of multiphase materials and complex structures [J]. Contin. Mech. Thermodyn., 2016, 28: 1325 |
| 24 | Bintu A, Vincze G, Picu C R, et al. Strain hardening rate sensitivity and strain rate sensitivity in TWIP steels [J]. Mater. Sci. Eng., 2015, A629: 54 |
| 25 | Shamsujjoha M. Evolution of microstructures, dislocation density and arrangement during deformation of low carbon lath martensitic steels [J]. Mater. Sci. Eng., 2020, A776: 139039 |
| 26 | Feaugas X. On the origin of the tensile flow stress in the stainless steel AISI 316L at 300 K: Back stress and effective stress [J]. Acta Mater., 1999, 47: 3617 |
| 27 | Sedlá?ek R, Blum W. Internal stresses in dislocation subgrain structures [J]. Comput. Mater. Sci., 1998, 13: 148 |
| 28 | Liu X L, Xue Q Q, Wang W, et al. Back-stress-induced strengthening and strain hardening in dual-phase steel [J]. Materialia, 2019, 7: 100376 |
| 29 | Yang M X, Pan Y, Yuan F P, et al. Back stress strengthening and strain hardening in gradient structure [J]. Mater. Res. Lett., 2016, 4: 145 |
| 30 | Orowan E. Problems of plastic gliding [J]. Proc. Phys. Soc., 1940, 52: 8 |
| 31 | Zhou N G, Zhou L. Structure and nucleation mechanisms of misfit dislocations in epitaxial FCC thin films with positive and negative mismatches [J]. Mater. Chem. Phys., 2006, 100: 168 |
| 32 | Olmsted D L, Holm E A, Foiles S M. Survey of computed grain boundary properties in face-centered cubic metals-II: Grain boundary mobility [J]. Acta Mater., 2009, 57: 3704 |
| 33 | Liu Q, Fang L M, Xiong Z W, et al. The response of dislocations, low angle grain boundaries and high angle grain boundaries at high strain rates [J]. Mater. Sci. Eng., 2021, A822: 141704 |
| 34 | Hasan S M, Mandal A, Singh S B, et al. Work hardening behaviour and damage mechanisms in carbide-free bainitic steel during uni-axial tensile deformation [J]. Mater. Sci. Eng., 2019, A751: 142 |
/
| 〈 |
|
〉 |