Modeling and Application of Deformation Resistance Model for Medium and Heavy Plate Based on Machine Learning
Received date: 2021-07-12
Revised date: 2021-11-09
Online published: 2022-06-16
Based on the actual production data of the plate mill of Xingcheng Special Steel, two machine learning methods for predicting deformation resistance are proposed to improve prediction accuracy. The first is a multi-steel deformation resistance model and modeling method that is combined with an extreme learning machine (ELM) and a traditional mathematical model, and the second is a deformation resistance model and modeling method that is based on the TensorFlow deep learning framework. Method one: The structural form of the original deformation resistance model was improved by referring to the Zhou Jihua-Guan Kezhi deformation resistance model, and the reference deformation resistances of representative steel grades of low alloy steel, alloy steel, and high alloy steel were calculated. The influence coefficient of deformation parameters independent of steel grade was calculated using nonlinear regression. The ELM neural network algorithm was presented, and neural network parameters were optimized using grey correlation analysis and cross-validation. To reduce the residual error of ELM prediction, the prediction results were smoothed using linear interpolation and then combined with the traditional mathematical model to obtain the deformation resistance. Method two: Based on deep learning technology, two types of deep neural networks with different structures were built and combined with the mechanism. To improve the generalizability and stability of the model, the mini-batch and RMSprop optimization algorithms were used in conjunction with batch normalization (BN) and early stopping regularization strategies. Finally, deformation resistance prediction models for roughing mill (RM) and finishing mill (FM) were developed respectively in conjunction with the process characteristics to improve model accuracy. The results showed that the deformation resistance prediction using deep learning has high prediction accuracy. Offline analysis indicated that the mean absolute percentage error decreased from 9.27% of the original model to an average of 2.59%. The online application demonstrated that the ratio of rolling force prediction accuracy within 10% relative error increased from 72.31% to an average of 90.24%, raising the technological level of onsite production.
Xiumei JI , Meiling HOU , Long WANG , Jie LIU , Kewei GAO . Modeling and Application of Deformation Resistance Model for Medium and Heavy Plate Based on Machine Learning[J]. Acta Metall Sin, 2023 , 59(3) : 435 -446 . DOI: 10.11900/0412.1961.2021.00283
| 1 | Zhang D H, Peng W, Sun J, et al. Key intelligent technologies of steel strip rolling process [J]. J. Iron Steel Res., 2019, 31: 174 |
| 1 | 张殿华, 彭 文, 孙 杰 等. 板带轧制过程中的智能化关键技术 [J]. 钢铁研究学报, 2019, 31: 174 |
| 2 | Liu X H, Wang G D. Development of advanced technology in hot strip rolling [J]. Res. Iron Steel, 2000, (5): 1 |
| 2 | 刘相华, 王国栋. 热轧带钢新技术的发展 [J]. 钢铁研究, 2000, (5): 1 |
| 3 | Li Y, Liu J X, Ke X T. Development and research of deformation resistance model in hot rolling process [J]. Res. Iron Steel, 2009, 37(6): 59 |
| 3 | 李 英, 刘建雄, 柯晓涛. 轧制变形抗力数学模型的发展与研究动态 [J]. 钢铁研究, 2009, 37(6): 59 |
| 4 | Zhou J H, Guan K Z. Plastic Deformation Resistance of Metal [M]. Beijing: Machinery Industry Press, 1989: 212 |
| 4 | 周纪华, 管克智. 金属塑性变形阻力 [M]. 北京: 机械工业出版社, 1989: 212 |
| 5 | Wang J, Wang X G, Yang H T, et al. A new mathematical model for predicting flow stress of X70HD under hot deformation [J]. J. Cent. South Univ., 2015, 22: 2052 |
| 6 | Feng Y L, Li J, Ai L Q, et al. Deformation resistance of Fe-Mn-V-N alloy under different deformation processes [J]. Rare Met., 2017, 36: 833 |
| 7 | Kingkam W, Zhao C Z, Li H, et al. Hot deformation and corrosion resistance of high-strength low-alloy steel [J]. Acta Metall. Sin. (Engl. Lett.), 2019, 32: 495 |
| 8 | Wei L X, Zhang Y, Sun H, et al. Online cold rolling prediction based on improved OS-ELM [J]. Acta Metrol. Sin., 2019, 40: 111 |
| 8 | 魏立新, 张 宇, 孙 浩 等. 基于改进OS-ELM的冷连轧在线轧制力预报 [J]. 计量学报, 2019, 40: 111 |
| 9 | Wang J, Wang Y, Xie H B, et al. Deformation resistance model based on measured data of hot rolling [J]. J. Plast. Eng., 2015, 22(1): 55 |
| 9 | 王 健, 王 宇, 谢红飙 等. 基于热连轧实测数据的金属材料变形抗力模型 [J]. 塑性工程学报, 2015, 22(1): 55 |
| 10 | Li W G, Liu C, Zhao Y T, et al. Modeling deformation resistance for hot rolling based on generalized additive model [J]. J. Iron Steel Res. Int., 2017, 24: 1177 |
| 11 | Xie X Q, Li W G, Fu W P, et al. Deformation resistance model for hot-rolled strip based on measured data [J]. Metall. Ind. Autom., 2019, 43(2): 29 |
| 11 | 谢向群, 李维刚, 付文鹏 等. 基于实测数据的热轧带钢变形抗力模型 [J]. 冶金自动化, 2019, 43(2): 29 |
| 12 | Su Y J, Fu H D, Bai Y, et al. Progress in materials genome engineering in China [J]. Acta Metall. Sin., 2020, 56: 1313 |
| 12 | 宿彦京, 付华栋, 白 洋 等. 中国材料基因工程研究进展 [J]. 金属学报, 2020, 56: 1313 |
| 13 | Wang T, Wan Z P, Sun Y, et al. Dynamic softening behavior and microstructure evolution of nickel base superalloy [J]. Acta Metall. Sin., 2018, 54: 83 |
| 13 | 王 涛, 万志鹏, 孙 宇 等. 镍基变形高温合金动态软化行为与组织演变规律研究 [J]. 金属学报, 2018, 54: 83 |
| 14 | Li M Q, Yao X Y, Luo J, et al. Modeling for flow stress of the nickel-based GH4169 superalloy at high temperature deformation [J]. Acta Metall. Sin., 2007, 43: 937 |
| 14 | 李淼泉, 姚晓燕, 罗 皎 等. 镍基高温合金GH4169高温变形流动应力模型研究 [J]. 金属学报, 2007, 43: 937 |
| 15 | Phaniraj M P, Lahiri A K. The applicability of neural network model to predict flow stress for carbon steels [J]. J. Mater. Process. Technol., 2003, 141: 219 |
| 16 | Zhou J H, Guan K Z, Liu J, et al. An mathematical model of flow stress for hot strip mill [J]. J. Univ. Sci. Technol. Beijing, 1991, 13: 20 |
| 16 | 周纪华, 管克智, 刘 玠 等. 热轧碳钢流动应力的数学模型 [J]. 北京科技大学学报, 1991, 13: 20 |
| 17 | Zhao M M, Qin S, Feng J, et al. Effect of Al and Ni on hot deformation behavior of 1Cr9Al(1~3)Ni(1~7)WVNbB steel [J]. Acta Metall. Sin., 2020, 56: 960 |
| 17 | 赵嫚嫚, 秦 森, 冯 捷 等. Al、Ni对1Cr9Al(1~3)Ni(1~7)WVNbB钢热变形行为的影响 [J]. 金属学报, 2020, 56: 960 |
| 18 | Ji X M, Wang L, Gao K W, et al. Application of ELM to predict plate rolling force [J]. J. Iron Steel Res., 2020, 32: 393 |
| 18 | 冀秀梅, 王 龙, 高克伟 等. 极限学习机在中厚板轧制力预报中的应用 [J]. 钢铁研究学报, 2020, 32: 393 |
| 19 | Mei Y, Sun Q L, Yu L H, et al. Grain size prediction of aluminum alloy dies castings based on GA-ELM [J]. Acta Metall. Sin., 2017, 53: 1125 |
| 19 | 梅 益, 孙全龙, 喻丽华 等. 基于GA-ELM的铝合金压铸件晶粒尺寸预测 [J]. 金属学报, 2017, 53: 1125 |
| 20 | Huang G B, Zhu Q Y, Siew C K. Extreme learning machine: Theory and applications [J]. Neurocomputing, 2006, 70: 489 |
| 21 | Deng C W, Huang G B, Xu J, et al. Extreme learning machines: New trends and applications [J]. Sci. China Inform. Sci., 2015, 58: 1 |
| 22 | Huang G B, Zhou H M, Ding X J, et al. Extreme learning machine for regression and multiclass classification [J]. IEEE Trans. Syst. Man Cybern., 2012, 42B: 513 |
| 23 | Poudel P, Bae S H, Jang B. Comparison of different deep learning optimizers for modeling photovoltaic power [J]. J. Chosun Nat. Sci., 2018, 11: 204 |
| 24 | Li W G, Yang W, Zhao Y T, et al. Modeling hot strip rolling process under framework of generalized additive model [J]. J. Cent. South Univ., 2019, 26: 2379 |
| 25 | Ma W, Li W G, Zhao Y T, et al. Prediction of hot-rolled roll force based on deep learning[J]. J. Iron Steel Res., 2019, 31: 805 |
| 25 | 马 威, 李维刚, 赵云涛 等. 基于深度学习的热连轧轧制力预测 [J]. 钢铁研究学报, 2019, 31: 805 |
| 26 | Liu D H, Li J H, Peng Y, et al. Comprehensive evaluation of sintering basic characteristics of iron ore based on grey relational analysis [J]. J. Iron Steel Res. Int., 2019, 26: 691 |
| 27 | Zhang T, Zhang Z H, Tian Y, et al. Research and application of deep learning method for plate ultra fast cooling [J]. J. Northeastern Univ. (Nat. Sci.), 2019, 40: 635 |
| 27 | 张 田, 张子豪, 田 勇 等. 深度学习在中厚板轧后超快速冷却系统中的研究与应用 [J]. 东北大学学报(自然科学版), 2019, 40: 635 |
/
| 〈 |
|
〉 |