Effects of Microstructure and Strain Rate on Dynamic Mechanical Properties and Adiabatic Shear Band of TC4 Alloy
Received date: 2021-12-31
Revised date: 2022-03-26
Online published: 2022-05-18
Supported by
National Natural Science Foundation of China(51771049);National Natural Science Foundation of China(51790484);National Key Laboratory Fund of China(JCKYS2020602005)
Under dynamic load, shear bands constitute the main deformation mode comparaed with quasistatic deformation. This study systematically investigates the influence of microstructures and strain rates of Ti-6Al-4V (TC4) alloys on their adiabatic shear behavior. TC4 alloys with three types of microstructures (lamellar, bimodal, and equiaxial) were successfully obtained via different thermal treatments. The dynamic mechanical properties, such as the critical shear strain rates of the hardening, softening transformation, maximum shear strength, critical shear strain rates of adiabatic shear-band nucleation and bearing time of the three types of microstructures were compared. Results indicate that compared with the lamellar bimodal and equiaxial TC4 alloys, the lamellar TC4 alloy shows the best dynamic mechanical properties, achieving higher shear strength and critical shear strain rates as well as the lowest adiabatic shear sensitivity. Microstructural analysis reveals that the adiabatic shear bands that formed in the three types of alloys are brittle. The width of the shear band decreases with increasing shear strain rate. Furthermore, at the same shear strain rate, the order of the widths of the shear bands is as follows: lamellar TC4 alloy > bimodal TC4 alloy > equiaxial TC4 alloy.
Wei CHEN , Huan ZHANG , Juan MU , Zhengwang ZHU , Haifeng ZHANG , Yandong WANG . Effects of Microstructure and Strain Rate on Dynamic Mechanical Properties and Adiabatic Shear Band of TC4 Alloy[J]. Acta Metall Sin, 2022 , 58(10) : 1271 -1280 . DOI: 10.11900/0412.1961.2021.00530
| 1 | Schutz R W, Watkins H B. Recent developments in titanium alloy application in the energy industry [J]. Mater. Sci. Eng., 1998, A243: 305 |
| 2 | Jin H X, Wei K X, Li J M, et al. Research development of titanium alloy in aerospace industry [J]. Chin. J. Nonferrous Met., 2015, 25: 280 |
| 2 | 金和喜, 魏克湘, 李建明 等. 航空用钛合金研究进展 [J]. 中国有色金属学报, 2015, 25: 280 |
| 3 | Boyer R R. An overview on the use of titanium in the aerospace industry [J]. Mater. Sci. Eng., 1996, A213: 103 |
| 4 | Yang R, Ma Y J, Lei J F, et al. Toughening high strength titanium alloys through fine tuning phase composition and refining microstructure [J]. Acta Metall. Sin., 2021, 57: 1455 |
| 4 | 杨 锐, 马英杰, 雷家峰 等. 高强韧钛合金组成相成分和形态的精细调控 [J]. 金属学报, 2021, 57: 1455 |
| 5 | Rae W. Thermo-metallo-mechanical modelling of heat treatment induced residual stress in Ti-6Al-4V alloy [J]. Mater. Sci. Technol., 2019, 35: 747 |
| 6 | Majorell A, Srivatsa S, Picu R C. Mechanical behavior of Ti-6Al-4V at high and moderate temperatures—Part I: Experimental results [J]. Mater. Sci. Eng., 2002, A326: 297 |
| 7 | Du Y X, Yang X L, Li Z S, et al. Shear localization behavior in hat-shaped specimen of near-α Ti-6Al-2Zr-1Mo-1V titanium alloy loaded at high strain rate [J]. Trans. Nonferrous Met. Soc. China, 2021, 31: 1641 |
| 8 | Pramanik A, Littlefair G. Machining of titanium alloy (Ti-6Al-4V)-theory to application [J]. Mach. Sci. Technol., 2015, 19: 1 |
| 9 | Zhu Z S, Shang G Q, Wang X N, et al. Microstructure controlling technology and mechanical properties relationship of titanium alloys for aviation applications [J]. J. Aeronaut. Mater., 2020, 40(3): 1 |
| 9 | 朱知寿, 商国强, 王新南 等. 航空用钛合金显微组织控制和力学性能关系 [J]. 航空材料学报, 2020, 40(3): 1 |
| 10 | Yang Y, Cheng X L. Current status and trends in researches on adiabatic shearing [J]. Chin. J. Nonferrous Met., 2002, 12: 401 |
| 10 | 杨 扬, 程信林. 绝热剪切的研究现状及发展趋势 [J]. 中国有色金属学报, 2002, 12: 401 |
| 11 | Liao S C, Duffy J. Adiabatic shear bands in a Ti-6Al-4V titanium alloy [J]. J. Mech. Phys. Solids, 1998, 46: 2201 |
| 12 | Yu J Q, Zhou H H, Shen L T, et al. Thermo-plastic shear bands induced during dynamic loading in Ti-55 alloys [J] Acta Metall. Sin., 1999, 35: 379 |
| 12 | 禹金强, 周惠华, 沈乐天 等. Ti-55合金中的热塑剪切带 [J]. 金属学报, 1999, 35: 379 |
| 13 | Wang B F, Li J, Sun J Y, et al. Adiabatic shear bands in Ti-6Al-4V alloy with lamellar microstructure [J]. J. Mater. Eng. Perform., 2014, 23: 1896 |
| 14 | Sun X R, Wang H Z, Yang P, et al. Mechanical behaviors and micro-shear structures of metals with different structures by high-speed compression [J]. Acta Metall. Sin., 2014, 50: 387 |
| 14 | 孙秀荣, 王会珍, 杨 平 等. 不同结构金属高速压缩力学行为及微观剪切结构差异 [J]. 金属学报, 2014, 50: 387 |
| 15 | Peirs J, Verleysen P, Degrieck J, et al. The use of hat-shaped specimens to study the high strain rate shear behaviour of Ti-6Al-4V [J]. Int. J. Impact Eng., 2010, 37: 703 |
| 16 | Lee D G, Lee S, Lee C S, et al. Effects of microstructural factors on quasi-static and dynamic deformation behaviors of Ti-6Al-4V alloys with Widmanstatten structures [J]. Metall. Mater. Trans., 2003, 34A: 2541 |
| 17 | Zheng C, Wang F C, Cheng X W, et al. Capturing of the propagating processes of adiabatic shear band in Ti-6Al-4V alloys under dynamic compression [J]. Mater. Sci. Eng., 2016, A658: 60 |
| 18 | Li W Q, Geng T Q, Ge S F, et al. Effect of strain rate on compressive behavior of a Zr-based metallic glass under a wide range of strain rates [J]. Materials, 2020, 13: 2861 |
| 19 | Guo X R, Zhang J X, Yi X B, et al. Influence of volume fraction of secondary α phase on dynamic compression properties and adiabatic shear sensitivity of TC18 titanium alloy [J]. Trans. Mater. Heat Treat., 2020, 41(10): 24 |
| 19 | 郭小汝, 张俊喜, 易湘斌 等. 次生α相含量对TC18钛合金动态压缩性能和绝热剪切敏感性的影响 [J]. 材料热处理学报, 2020, 41(10): 24 |
| 20 | Chen Y, Pei C H, Li Z X, et al. Dynamic mechanical behavior of α + β titanium alloys at high strain rate [J]. J. Aeronaut. Mater., 2013, 33(6): 8 |
| 20 | 陈 洋, 裴传虎, 李臻熙 等. α + β钛合金在高应变率下的动态力学性能 [J]. 航空材料学报, 2013, 33(6): 8 |
| 21 | Yi X B, Zhang J X, Li B D, et al. Dynamic compressive mechanical properties of TB6 titanium alloy under high temperature and high strain rate [J]. Rare Met. Mater. Eng., 2019, 48: 1220 |
| 21 | 易湘斌, 张俊喜, 李宝栋 等. 高温、高应变率下TB6钛合金的动态压缩性能 [J]. 稀有金属材料与工程, 2019, 48: 1220 |
| 22 | Yang H B, Xiang W L, Xu Y, et al. Effect of cooling ways on adiabatic shear sensitivity of TC21 titanium alloy [J]. Chin. J. Nonferrous Met., 2017, 27: 920 |
| 22 | 杨红斌, 向文丽, 徐 媛 等. 冷却方式对TC21钛合金绝热剪切敏感性的影响 [J]. 中国有色金属学报, 2017, 27: 920 |
| 23 | Mao P L, Sun Q H, Liu Z, et al. Mechanical properties and adiabatic shear sensitivity of Ti-6Al-4V alloy with different microstructures [J]. Chin. J. Rare Met., 2016, 40: 1207 |
| 23 | 毛萍莉, 孙庆海, 刘 正 等. 微观组织状态对Ti-6Al-4V合金动态力学性能和绝热剪切敏感性的影响 [J]. 稀有金属, 2016, 40: 1207 |
| 24 | Zheng C, Wang F C, Cheng X W, et al. Effect of microstructures on ballistic impact property of Ti-6Al-4V targets [J]. Mater. Sci. Eng., 2014, A608: 53 |
| 25 | Huang S S, Ma Y J, Zhang S L, et al. Influence of alloying elements partitioning behaviors on the microstructure and mechanical propertiesin α + β titanium alloy [J]. Acta Metall. Sin., 2019, 55: 741 |
| 25 | 黄森森, 马英杰, 张仕林 等. α + β两相钛合金元素再分配行为及其对显微组织和力学性能的影响 [J]. 金属学报, 2019, 55: 741 |
| 26 | Sun K, Yu X D, Tan C W, et al. Influence of adiabatic shear bands intersection on the ballistic impact of Ti-6Al-4V alloys with three microstructures [J]. Mater. Sci. Eng., 2014, A606: 257 |
| 27 | Bai L Y. A criterion for thermo-plastic shear instability [A]. Shock Waves and High-Strain-Rate Phenomena in Metals [M]. New York: Springer, 1981: 277 |
| 28 | Wang Z M, Chen Z Y, Zhan C K, et al. Quasi-static and dynamic forced shear deformation behaviors of Ti-5Mo-5V-8Cr-3Al alloy [J]. Mater. Sci. Eng., 2017, A691: 51 |
| 29 | Yan N, Li Z Z, Xu Y B, et al. Shear localization in metallic materials at high strain rates [J]. Prog. Mater. Sci., 2021, 119: 100755 |
| 30 | Recht R F. Catastrophic thermoplastic shear [J]. J. Appl. Mech., 1964, 31: 189 |
| 31 | Xu Y, Sun K, Zi X F, et al. Study on adiabatic shearing sensitivity of different microstructures of TC6 titanium alloy at different stress states [J]. Rare Met. Mater. Eng., 2011, 40: 2002 |
| 31 | 徐 媛, 孙 坤, 自兴发 等. 不同应力状态下TC6钛合金不同组织绝热剪切敏感性研究 [J]. 稀有金属材料与工程, 2011, 40: 2002 |
| 32 | Sun Q H. Adiabatic shearing mechanism of Ti- 6Al-4V [D]. Shenyang: Shenyang University of Technology, 2016 |
| 32 | 孙庆海. Ti-6Al-4V 绝热剪切机理 [D]. 沈阳: 沈阳工业大学, 2016 |
| 33 | Zhou T F, Wu J J, Che J T, et al. Dynamic shear characteristics of titanium alloy Ti-6Al-4V at large strain rates by the split Hopkinson pressure bar test [J]. Int. J. Impact Eng., 2017, 109: 167 |
| 34 | Wu G Q, Song H, Sha W, et al. Relationship between microstructure and deformation behaviour during dynamic compression in Ti-3Al-5Mo-5V alloy [J]. Mater. Sci. Technol., 2011, 27: 1399 |
| 35 | Ran C, Chen P W, Li L, et al. Dynamic shear deformation and failure of Ti-5Al-5Mo-5V-1Cr-1Fe titanium alloy [J]. Mater. Sci. Eng., 2017, A694: 41 |
| 36 | Ran C, Chen P W, Li L, et al. High-strain-rate plastic deformation and fracture behaviour of Ti-5Al-5Mo-5V-1Cr-1Fe titanium alloy at room temperature [J]. Mech. Mater., 2018, 116: 3 |
| 37 | Dodd B, Bai Y L. Introduction to Adiabatic Shear Localization [M]. London: Imperial College Press, 2014: 33 |
| 38 | Xue Q, Meyers M A, Nesterenko V F. Self-organization of shear bands in titanium and Ti-6Al-4V alloy [J]. Acta Mater., 2002, 50: 575 |
| 39 | Lee W S, Lin C F. Plastic deformation and fracture behaviour of Ti-6Al-4V alloy loaded with high strain rate under various temperatures [J]. Mater. Sci. Eng., 1998, A241: 48 |
| 40 | Ran C, Chen P W. Shear localization and recrystallization in high strain rate deformation in Ti-5Al-5Mo-5V-1Cr-1Fe alloy [J]. Mater. Lett., 2018, 232: 142 |
/
| 〈 |
|
〉 |