Corrosion Behaviors of Fe13Cr5Al4Mo Alloy in High-Temperature High-Pressure Water Environments
Received date: 2021-12-22
Revised date: 2022-03-27
Online published: 2022-05-05
Supported by
National Natural Science Foundation of China(51871141)
FeCrAl alloys are promising candidate materials for accident-tolerant-fuel (ATF) claddings owing to their good high-temperature mechanical property, irradiation-swelling resistance, and high-temperature steam-oxidation performance. However, excellent corrosion resistance is also required in high-temperature high-pressure water environments when the alloys are used as ATF claddings. Therefore, in this work, the corrosion behavior of a Fe13Cr5Al4Mo alloy in 360oC, 18.6 MPa deionized water and 360oC, 18.6 MPa, 3.5 mg/L Li + 1000 mg/L B aqueous solution was studied. Results revealed that the weight gain and growth rate of the Fe13Cr5Al4Mo alloy were lower than that of the reference zirconium alloy, indicating a better corrosion property of the Fe13Cr5Al4Mo alloy. Moreover, an oxide film comprising Fe(Cr, Al)2O4 nanospinels formed on the Fe13Cr5Al4Mo alloy in both water environments, and Fe3O4 outer-oxide particles were observed in deionized water. The good corrosion performance of Fe13Cr5Al4Mo alloy was attributed to the compact spinel-oxide film, which could inhibit the diffusion of oxygen ions and metal cations. Adding Li + B into water changed the corrosion weight gain and oxide-film thickness of the Fe13Cr5Al4Mo alloy and impeded the formation of outer-oxide particles, which may be related to the high pH of alkaline Li + B aqueous solution and the interactions between Li+ and B3+.
Xiaodong LIN , Haibin MA , Qisen REN , Rongrong SUN , Wenhuai ZHANG , Lijuan HU , Xue LIANG , Yifeng LI , Meiyi YAO . Corrosion Behaviors of Fe13Cr5Al4Mo Alloy in High-Temperature High-Pressure Water Environments[J]. Acta Metall Sin, 2022 , 58(12) : 1611 -1622 . DOI: 10.11900/0412.1961.2021.00574
| 1 | Charit I. Accident tolerant nuclear fuels and cladding materials [J]. JOM, 2018, 70: 173 |
| 2 | Zinkle S J, Terrani K A, Gehin J C, et al. Accident tolerant fuels for LWRs: A perspective [J]. J. Nucl. Mater., 2014, 448: 374 |
| 3 | Field K G, Yamamoto Y, Pint B A, et al. Accident tolerant FeCrAl fuel cladding: Current status towards commercialization [A]. Proceedings of the 18th International Conference on Environmental Degradation of Materials in Nuclear Power Systems—Water Reactors [C]. New York: Springer, 2019: 1381 |
| 4 | Huang X, Li X Y, Fang X D, et al. Research progress in FeCrAl alloys for accident-tolerant fuel cladding [J]. J. Mater. Eng., 2020, 48(3): 19 |
| 4 | 黄希, 李小燕, 方晓东 等. 容错事故燃料包壳用FeCrAl合金的研究进展 [J]. 材料工程, 2020, 48(3): 19 |
| 5 | Tao X K, Huang Z G, Guo Q M, et al. Research progress of FeCrAl alloy for cladding material of new type of light water reactor [J]. Hot Work. Technol., 2018, 47(6): 23 |
| 5 | 陶小康, 黄重国, 郭青苗 等. 新型轻水反应堆包壳材料FeCrAl合金的研究进展 [J]. 热加工工艺, 2018, 47(6): 23 |
| 6 | Zhang Y Y, Wang H, An X G, et al. Dynamic strain aging behavior of accident tolerance fuel cladding FeCrAl-based alloy for advanced nuclear energy [J]. J. Mater. Sci., 2021, 56: 8815 |
| 7 | Opila E J, Myers D L. Alumina volatility in water vapor at elevated temperatures [J]. J. Am. Ceram. Soc., 2004, 87: 1701 |
| 8 | Pan D, Zhang R Q, Wang H, et al. Formation and stability of oxide layer in FeCrAl fuel cladding material under high-temperature steam [J]. J. Alloys Compd., 2016, 684: 549 |
| 9 | Park D J, Kim H G, Park J Y, et al. A study of the oxidation of FeCrAl alloy in pressurized water and high-temperature steam environment [J]. Corros. Sci., 2015, 94: 459 |
| 10 | Parker S S, White J, Hosemann P, et al. Oxidation kinetics of ferritic alloys in high-temperature steam environments [J]. JOM, 2018, 70: 186 |
| 11 | Pint B A. Performance of FeCrAl for accident-tolerant fuel cladding in high-temperature steam [J]. Corros. Rev., 2017, 35: 167 |
| 12 | Stott F H, Wood G C, Stringer J. The influence of alloying elements on the development and maintenance of protective scales [J]. Oxid. Met., 1995, 44: 113 |
| 13 | Yamamoto Y, Pint B A, Terrani K A, et al. Development and property evaluation of nuclear grade wrought FeCrAl fuel cladding for light water reactors [J]. J. Nucl. Mater., 2015, 467: 703 |
| 14 | Rebak R B. Versatile oxide films protect FeCrAl alloys under normal operation and accident conditions in light water power reactors [J]. JOM, 2018, 70: 176 |
| 15 | Rebak R B, Larsen M, Kim Y J. Characterization of oxides formed on iron-chromium-aluminum alloy in simulated light water reactor environments [J]. Corros. Rev., 2017, 35: 177 |
| 16 | Ning F Q, Wang X, Yang Y, et al. Uniform corrosion behavior of FeCrAl alloys in borated and lithiated high temperature water [J]. J. Mater. Sci. Technol., 2021, 70: 136 |
| 17 | Song L J, Liu F H, Li C T, et al. Effect of B-Li water chemistry on corrosion of metal materials of nuclear power plant [J]. Nucl. Sci. Eng., 2014, 34: 97 |
| 17 | 宋利君, 刘飞华, 李成涛 等. B-Li水化学对核电站金属材料腐蚀的影响 [J]. 核科学与工程, 2014, 34: 97 |
| 18 | Betova I, Bojinov M, Karastoyanov V, et al. Effect of water chemistry on the oxide film on alloy 690 during simulated hot functional testing of a pressurised water reactor [J]. Corros. Sci., 2012, 58: 20 |
| 19 | Wei K J, Wang X P, Zhu M H, et al. Effects of Li, B and H elements on corrosion property of oxide films on ZIRLO alloy in 300oC/14 MPa lithium borate buffer solutions [J]. Corros. Sci., 2021, 181: 109216 |
| 20 | Molander A, Norring K, Andersson P O, et al. Environmental effects on PWSCC initiation and propagation in alloy 600 [A]. Proceedings of the 15th International Conference on Environmental Degradation of Materials in Nuclear Power Systems—Water Reactors [C]. New York: Springer, 2011: 1699 |
| 21 | Vankeerberghen M, Weyns G, Gavrilov S, et al. Crack propagation rate modelling for 316SS exposed to PWR-relevant conditions [J]. J. Nucl. Mater., 2009, 384: 274 |
| 22 | Liu W Q, Zhou B X, Li Q, et al. Detrimental role of LiOH on the oxide film formed on zircaloy-4 [J]. Corros. Sci., 2005, 47: 1855 |
| 23 | Billot P, Yagnik S, Ramasubramanian N, et al. The role of lithium and boron on the corrosion of zircaloy-4 under demanding PWR-type conditions [A]. Zirconium in the Nuclear Industry: 13th International Symposium [C]. West Conshohocken: American Society for Testing and Materials, 2002: 169 |
| 24 | Zhao Y F, Tang M, Jiang E, et al. Inhibition effects of low concentration of boron on corrosion of zirconium alloy [J]. Nucl. Power Eng., 2019, 40(2): 32 |
| 24 | 赵永福, 唐敏, 姜峨 等. 低浓度硼对锆合金缓蚀作用研究 [J]. 核动力工程, 2019, 40(2): 32 |
| 25 | Li J. The focused-ion-beam microscope—More than a precision ion milling machine [J]. JOM, 2006, 58(3): 27 |
| 26 | Cao X Y, Zhu P, Wang W, et al. Effect of thermal aging on oxide film of stainless steel weld overlay cladding exposed to high temperature water [J]. Mater. Charact., 2018, 138: 195 |
| 27 | Hanbury R D, Was G S. Oxide growth and dissolution on 316L stainless steel during irradiation in high temperature water [J]. Corros. Sci., 2019, 157: 305 |
| 28 | Kuang W J, Han E H, Wu X Q, et al. Microstructural characteristics of the oxide scale formed on 304 stainless steel in oxygenated high temperature water [J]. Corros. Sci., 2010, 52: 3654 |
| 29 | Terachi T, Yamada T, Miyamoto T, et al. Corrosion behavior of stainless steels in simulated PWR primary water—Effect of chromium content in alloys and dissolved hydrogen [J]. J. Nucl. Sci. Technol., 2008, 45: 975 |
| 30 | Lister D H, Davidson R D, Mcalpine E. The mechanism and kinetics of corrosion product release from stainless steel in lithiated high temperature water [J]. Corros. Sci., 1987, 27: 113 |
| 31 | Macdonald D D, Urquidi-Macdonald M. Theory of steady-state passive films [J]. J. Electrochem. Soc., 1990, 137: 2395 |
| 32 | Robertson J. The mechanism of high temperature aqueous corrosion of stainless steels [J]. Corros. Sci., 1991, 32: 443 |
| 33 | Matthews R P, Knusten R D, Westraadt J E, et al. Intergranular oxidation of 316L stainless steel in the PWR primary water environment [J]. Corros. Sci., 2017, 125: 175 |
| 34 | Macdonald D D. Passivity—The key to our metals-based civilization [J]. Pure Appl. Chem., 1999, 71: 951 |
| 35 | Wu W S, Ran G, Li Y P, et al. Early corrosion behaviour of irradiated FeCrAl alloy in a simulated pressurized water reactor environment [J]. Corros. Sci., 2020, 174: 108824 |
| 36 | Shen Z, Tweddle D, Yu H B, et al. Microstructural understanding of the oxidation of an austenitic stainless steel in high-temperature steam through advanced characterization [J]. Acta Mater., 2020, 194: 321 |
| 37 | Robino C V. Representation of mixed reactive gases on free energy (Ellingham-Richardson) diagrams [J]. Metall. Mater. Trans., 1996, 27B: 65 |
| 38 | Sun H, Wu X Q, Han E H, et al. Effects of pH and dissolved oxygen on electrochemical behavior and oxide films of 304SS in borated and lithiated high temperature water [J]. Corros. Sci., 2012, 59: 334 |
| 39 | Shu M, Wang C L, Chen Y. Studies on electrochemical corrosion behaviors and 316NG stainless steel in boron-lithium solutions [J]. Nucl. Power Eng., 2018, 39(5): 63 |
| 39 | 舒茗, 王丛林, 陈勇. 316NG不锈钢在硼-锂溶液中的电化学腐蚀行为研究 [J]. 核动力工程, 2018, 39(5): 63 |
| 40 | Kaczorowski D, Combrade P, Vernot J P, et al. Water chemistry effect on the wear of stainless steel in nuclear power plant [J]. Tribol. Int., 2006, 39: 1503 |
| 41 | Park Y J, Choi K C, Ha Y K. Solubility study of nickel ferrite in boric acid using a flow-through autoclave system under high temperature and high pressure [J]. Nucl. Eng. Technol., 2016, 48: 554 |
| 42 | Tremaine P R, Leblanc J C. The solubility of magnetite and the hydrolysis and oxidation of Fe2+ in water to 300oC [J]. J. Solution Chem., 1980, 9: 415 |
| 43 | Cox B, Ungurelu M, Wong Y M, et al. Mechanisms of LiOH degradation and H3BO3 repair of ZrO2 films [A]. Zirconium in the Nuclear Industry: 11th International Symposium [C]. West Conshohocken: American Society for Testing and Materials, 1996: 114 |
/
| 〈 |
|
〉 |