A Quantitative and Statistical Method of γ' Precipitates in Superalloy Based on the High-Throughput Field Emission Scanning Eelectron Microscope
Received date: 2021-09-07
Revised date: 2021-11-11
Online published: 2022-04-09
Supported by
National Key Research and Development Program of China(2016YFB0701401)
Superalloys are used widely in national defense, energy, maritime, aviation, and other vital areas requiring stable and reliable materials owing to their excellent oxidation and heat corrosion resistance, high-temperature strength, good fatigue performance, and fracture toughness. The presence of a coherent gamma prime (γ') precipitate is the main factor affecting the high-temperature mechanical properties. Therefore, obtaining the quantitative and statistical γ' precipitate data is indispensable for examining and developing new superalloys. On the other hand, conventional instruments and methods barely achieve this goal. In this study, high-throughput field emission scanning electron microscope (high-throughput SEM) was introduced because of its high-speed imaging and original position visualization. Based on the high-throughput SEM, an innovative deformation GH4096 superalloy prepared at five different solution cooling rates were used as an object to establish a quantitative and statistical method for characterizing the primary, secondary, and tertiary γ' precipitates. Many images of γ' precipitates with magnifications of ×57000 and ×3000 were obtained rapidly, and methodologies for recognizing the γ' precipitates were developed using MIPAR software. Matrices of images of different amounts were formed. Through these methodologies, information on these matrices was obtained, including the ratio of the primary γ' precipitates area fractions between images with magnifications of ×57000 and ×3000. The ratio between the amounts of secondary and tertiary γ' precipitates and the area fraction of the secondary and tertiary γ' precipitates varied with the number of images investigated, respectively. By comparing the tendencies of these three results, the minimum field of view that could represent the actual distribution of γ' precipitates was set to a matrix of 13 × 13 images with a magnification of ×57000 and a pixels square of 2048 × 2048. Considering the consistency between the results of the standardized small-angle X-ray scattering (SAXS) and γ' precipitates in the 13 × 13 images, the established method was quantitative in characterizing the primary, secondary, and tertiary γ' precipitates of GH4096 superalloy. The results of the samples with five different solution cooling rates showed that the solution cooling rates strongly influenced the morphology and quantitative results of the γ' precipitates. Moreover, the behavior of the precipitates corresponded to the classical nucleation growth mechanism and Ostwald Ripening. The solution cooling rates influenced the tensile strength of the samples. The samples exhibited excellent tensile strengths at relatively faster cooling rates, more secondary γ' precipitates, and a higher total area fraction of secondary and tertiary γ' precipitates. Overall, a GH4096 superalloy was prepared using the established method. The statistical and quantitative results of the γ' precipitates highlight a novel way of studying the impact of the solution cooling process on γ' precipitates that can predict the performance of GH4096 superalloys.
LU Yuhua , WANG Haizhou , LI Dongling , FU Rui , LI Fulin , SHI Hui . A Quantitative and Statistical Method of γ' Precipitates in Superalloy Based on the High-Throughput Field Emission Scanning Eelectron Microscope[J]. Acta Metall Sin, 2023 , 59(7) : 841 -854 . DOI: 10.11900/0412.1961.2021.00376
| 1 | Reed R C. The Superalloys: Fundamentals and Applications [M]. Cambridge: Cambridge University Press, 2006: 1 |
| 2 | Chen M S, Wang G Q, Li H B, et al. Annealing treatment methods and mechanisms for refining mixed and coarse grains in a solution treatment nickel-based superalloy [J]. Adv. Eng. Mater., 2019, 21: 1900558 |
| 3 | Guo J T. The current situation of application and development of superalloys in the fields of energy industry [J]. Acta Metall. Sin., 2010, 46: 513 |
| 郭建亭. 高温合金在能源工业领域中的应用现状与发展 [J]. 金属学报, 2010, 46: 513 | |
| 4 | Zhang R, Liu P, Cui C Y, et al. Present research situation and prospect of hot working of cast & wrought superalloys for aero-engine turbine disk in China [J]. Acta Metall. Sin., 2021, 57: 1215 |
| 张 瑞, 刘 鹏, 崔传勇 等. 国内航空发动机涡轮盘用铸锻难变形高温合金热加工研究现状与展望 [J]. 金属学报, 2021, 57: 1215 | |
| 5 | Polkowska A, Polkowski W, Warmuzek M, et al. Microstructure and hardness evolution in Haynes 282 nickel-based superalloy during multi-variant aging heat treatment [J]. J. Mater. Eng. Perform., 2019, 28: 3844 |
| 6 | Huang Q Y, Li H K. Superalloys [M]. Beijing: Metallurgical Industry Press, 2000: 24 |
| 黄乾尧, 李汉康. 高温合金 [M]. 北京: 冶金工业出版社, 2000: 24 | |
| 7 | Wu H Y, Huang Z W, Zhou N, et al. A study of solution cooling rate on γ′ precipitate and hardness of a polycrystalline Ni-based superalloy using a high-throughput methodology [J]. Mater. Sci. Eng., 2019, A739: 473 |
| 8 | Mao J, Chang K M, Yang W H, et al. Cooling precipitation and strengthening study in powder metallurgy superalloy U720LI [J]. Metall. Mater. Trans., 2001, 32A: 2441 |
| 9 | Lin D L, Yao D L, Lin X J, et al. Effect of volume fraction and size of fine γ′ on creep strength of a DS nickel-base superalloy [J]. Acta Metall. Sin., 1982, 18: 104 |
| 林栋梁, 姚德良, 林先进 等. 细小γ′粒子的数量和尺寸对提高定向凝固高强度镍基高温合金蠕变强度的作用 [J]. 金属学报, 1982, 18: 104 | |
| 10 | Jiang H F. Requirements and forecast of turbine disk materials [J]. Gas Turb. Exp. Res., 2002, 15(4): 1 |
| 江和甫. 对涡轮盘材料的需求及展望 [J]. 燃气涡轮试验与研究, 2002, 15(4): 1 | |
| 11 | Zhang Y W, Chi Y. Recent developments of powder metallurgy superalloy in Russia [J]. Powder Metall. Ind., 2012, 22(5): 37 |
| 张义文, 迟 悦. 俄罗斯粉末冶金高温合金研制新进展 [J]. 粉末冶金工业, 2012, 22(5): 37 | |
| 12 | Shi C X, Zhong Z Y. Development and innovation of superalloy in China [J]. Acta Metall. Sin., 2010, 46: 1281 |
| 师昌绪, 仲增墉. 我国高温合金的发展与创新 [J]. 金属学报, 2010, 46: 1281 | |
| 13 | Chen Y Q, Prasath babu R, Slater T J A, et al. An investigation of diffusion-mediated cyclic coarsening and reversal coarsening in an advanced Ni-based superalloy [J]. Acta Mater., 2016, 110: 295 |
| 14 | Singh A R P, Nag S, Hwang J Y, et al. Influence of cooling rate on the development of multiple generations of γ′ precipitates in a commercial nickel base superalloy [J]. Mater. Charact., 2011, 62: 878 |
| 15 | Baldan A. Review progress in Ostwald ripening theories and their applications to nickel-base superalloys Part I: Ostwald ripening theories [J]. J. Mater. Sci., 2002, 37: 2171 |
| 16 | Dwarapureddy A K, Balikci E, Ibekwe S, et al. Activation energy for growth in single size distribution and the dissolution features of γ′ precipitates in the superalloy IN738LC [J]. J. Mater. Sci., 2008, 43: 1802 |
| 17 | Hwang J Y, Banerjee R, Tiley J, et al. Nanoscale characterization of elemental partitioning between gamma and gamma prime phases in René 88 DT nickel-base superalloy [J]. Metall. Mater. Trans., 2009, 40A: 24 |
| 18 | Hwang J Y, Nag S, Singh A R P, et al. Compositional variations between different generations of γ′ precipitates forming during continuous cooling of a commercial nickel-base superalloy [J]. Metall. Mater. Trans., 2009, 40A: 3059 |
| 19 | Chen Y Q, Francis E, Robson J, et al. Compositional variations for small-scale gamma prime (γ′) precipitates formed at different cooling rates in an advanced Ni-based superalloy [J]. Acta Mater., 2015, 85: 199 |
| 20 | Mao J, Chang K M, Yang W H, et al. Cooling precipitation and strengthening study in powder metallurgy superalloy Rene88DT [J]. Mater. Sci. Eng., 2002, A332: 318 |
| 21 | Sharghi-Moshtaghin R, Asgari S. The influence of thermal exposure on the γ' precipitates characteristics and tensile behavior of superalloy IN-738LC [J]. J. Mater. Process. Technol., 2004, 147: 343 |
| 22 | Wang H Z, Wang H, Ding H, et al. Progress in high-throughput materials synthesis and characterization [J]. Sci. Technol. Rev., 2015, 33(10): 31 |
| 王海舟, 汪 洪, 丁 洪 等. 材料的高通量制备与表征技术 [J]. 科技导报, 2015, 33(10): 31 | |
| 23 | Wang H Z, Zhao L, Jia Y H, et al. State-of-the-art review of high-throughput statistical spatial-mapping characterization technology and its application [J]. Engineering, 2020, 6: 621 |
| 24 | Picó Y, Andreu V. Nanosensors and other techniques for detecting nanoparticles in the environment [A]. Nanosensors for Chemical and Biological Applications: Sensing with Nanotubes, Nanowires and Nanoparticles [M]. Amsterdam: Woodhead Publishing, 2014: 295 |
| 25 | Yokoyama T, Masuda H, Suzuki M, et al. Basic properties and measuring methods of nanoparticles [A]. Nanoparticle Technology Handbook [M]. 2nd Ed., Amsterdam: Elsevier, 2012: 3 |
| 26 | Smith T M, Bonacuse P, Sosa J, et al. A quantifiable and automated volume fraction characterization technique for secondary and tertiary γ' precipitates in Ni-based superalloys [J]. Mater. Charact., 2018, 140: 86 |
| 27 | Chen N, Guo J J, Gong H F. The research progress of methods for characterizing nanoparticles [J]. Mod. Sci. Instrum., 2012, (2): 160 |
| 陈 宁, 果晶晶, 宫惠峰. 纳米颗粒粒度测量方法进展 [J]. 现代科学仪器, 2012, (2): 160 | |
| 28 | Smith T M, Senanayake N M, Sudbrack C K, et al. Characterization of nanoscale precipitates in superalloy 718 using high resolution SEM imaging [J]. Mater. Charact., 2019, 148: 178 |
| 29 | Cao B, Chen M, Zhou Q. Comparison of three methods of measuring nano-particles size [J]. Phys. Examinat. Test., 2005, 23(6): 27 |
| 曹 标, 陈 明, 周 崎. 三种纳米颗粒粒径测量方法的比较 [J]. 物理测试, 2005, 23(6): 27 | |
| 30 | General Administration of Quality Supervision, Inspection and Quarantine of the People's Republic of China, Standardization Administration. Nanometer powder—Determinaiton of particle size distribution—Small angle X-ray [S]. Beijing: Standards Press of China, 2005 |
| 中华人民共和国国家质量监督检验检疫总局, 中国国家标准化管理委员会. 纳米粉末粒度分布的测定X射线小角散射法 [S]. 北京: 中国标准出版社, 2005 | |
| 31 | Goertz V, Dingenouts N, Nirschl H. Comparison of nanometric particle size distributions as determined by SAXS, TEM and analytical ultracentrifuge [J]. Part. Part. Syst. Charact., 2009, 26: 17 |
| 32 | Xiang Y W, Zhang J Y, Liu C L. Verification for particle size distribution of ultrafine powders by the SAXS method [J]. Mater. Charact., 2000, 44: 435 |
| 33 | Liu Q B, Lu C F, Yan P. Physicochemical phase analysis of a directionally solidified Ni-based cast superalloy [J]. Metall. Anal., 2006, 26(2): 9 |
| 刘庆斌, 卢翠芬, 燕 平. 一种定向凝固镍基铸造高温合金的物理化学相分析 [J]. 冶金分析, 2006, 26(2): 9 | |
| 34 | Li L X, Zhao X L, Li N, et al. Physicochemical phase analysis of iron-nickel based high temperature alloy with high chromium [J]. Metall. Anal., 2015, 35(2): 6 |
| 李玲霞, 赵晓丽, 李 南 等. 一种高铬的铁镍基高温合金物理化学相分析 [J]. 冶金分析, 2015, 35(2): 6 | |
| 35 | Ju Y W, Li S, Yuan X F, et al. A macro-nano-atomic-scale high-throughput approach for material research [J]. Sci. Adv., 2021, 7: eabj8804 |
| 36 | Sosa J M, Huber D E, Welk B, et al. Development and application of MIPAR?: A novel software package for two- and three-dimensional microstructural characterization [J]. Integr. Mater. Manuf. Innov., 2014, 3: 123 |
| 37 | Fu R, Feng D, Chen X C, et al. Research of ESR-CDS technology [J]. J. Iron Steel Res., 2011, 23(suppl.2) : 1 |
| 付 锐, 冯 涤, 陈希春 等. 电渣重熔连续定向凝固技术研究 [J]. 钢铁研究学报, 2011, 23(): 1 | |
| 38 | Fu R, Chen X C, Ren H, et al. Structure and hot deformation behavior of ESR-CDS René88DT [J]. J. Aeronaut. Mater., 2011, 31(3): 8 |
| 付 锐, 陈希春, 任 昊 等. 电渣重熔连续定向凝固René88DT合金的组织与热变形行为 [J]. 航空材料学报, 2011, 31(3): 8 | |
| 39 | Chen X C, Fu R, Feng D, et al. Calculation on technological parameters of electroslag remelting continuous-directionally solidified René88DT nickel alloy ingot [J]. Spec. Steel, 2011, 32(5): 31 |
| 陈希春, 付 锐, 冯 涤 等. 电渣重熔连续定向凝固René88DT镍基合金锭工艺参数的计算 [J]. 特殊钢, 2011, 32(5): 31 | |
| 40 | Chen X C, Ren H, Fu R, et al. Recent development of solidified structure controlling of superalloy during ESR process [J]. Spec. Steel Technol., 2011, 17(3): 1 |
| 陈希春, 任 昊, 付 锐 等. 电渣重熔高温合金凝固组织控制的研究进展 [J]. 特钢技术, 2011, 17(3): 1 | |
| 41 | Li F L, Fu R, Feng D, et al. Hot deformation characteristics of Ni-base wrought superalloy CDS&W FGH96 [J]. Chin. J. Rare Met., 2015, 39: 201 |
| 李福林, 付 锐, 冯 涤 等. 镍基变形高温合金CDS&W FGH96热变形行为研究 [J]. 稀有金属, 2015, 39: 201 | |
| 42 | Xu Y M, Li Q, Luo X M. Several development priorities of heat treatment technology in our country [J]. Heat Treat. Met., 2017, 42(4): 1 |
| 徐跃明, 李 俏, 罗新民. 我国热处理技术发展的几个重点 [J]. 金属热处理, 2017, 42(4): 1 | |
| 43 | General Administration of Quality Supervision, Inspection and Quarantine of the People's Republic of China, Standardization Administration. Particle size analysis—image analysis methods—part 1: Static image analysis method [S]. Beijing: Standards Press of China, 2008 |
| 中华人民共和国国家质量监督检验检疫总局, 中国国家标准化管理委员会. 粒度分析 图像分析法 第1部分: 静态图像分析法 [S]. 北京: 中国标准出版社, 2008 | |
| 44 | Semiatin S L, Kim S L, Zhang F, et al. An investigation of high-temperature precipitation in powder-metallurgy, gamma/gamma-prime nickel-base superalloys [J]. Metall. Mater. Trans., 2015, 46A: 1715 |
/
| 〈 |
|
〉 |