Research paper

Effects of Processing on Microstructures and Properties of FGH4097 Superalloy

  • Leipeng XIE ,
  • Wenyao SUN ,
  • Minghui CHEN ,
  • Jinlong WANG ,
  • Fuhui WANG
Expand
  • Shenyang National Laboratory for Materials Science, Northeastern University, Shenyang 110819, China
SUN Wenyao, Tel: (024)83691562, E-mail: sunwenyao@mail.neu.edu.cnCHEN Minghui, professor, Tel: (024)83691562, E-mail: mhchen@mail.neu.edu.cn

Received date: 2021-09-06

  Revised date: 2021-12-03

  Online published: 2022-03-11

Supported by

National Natural Science Foundation of China(51871051);Ministry of Industry and Information Technology Project(MJ-2017-J-99)

Abstract

Powder metallurgy (PM) nickel-based superalloys are widely used as high-temperature, fatigue-resistant components in aircraft and gas turbines. However, many powder particle boundaries and carbides are found in alloys prepared via traditional methods, such as hot pressing (HP) and hot isostatic pressing, causing serious damage to the properties of PM superalloys. New methods and processes must be developed to improve the performance of PM superalloys. SEM, EBSD, and TEM were used in this work to investigate the microstructure, mechanical properties, and oxidation behavior of FGH4097 alloys prepared via spark plasma sintering (SPS) and HP. Owing to the advantages of uniform microstructure, fine grain, and less carbide precipitation, SPSed alloy has better tensile properties and oxidation resistance than HPed alloy. At 25oC, SPSed alloy's yield, tensile strengths, and elongation are 998 MPa, 1401 MPa, and 17.1%, respectively; whereas those of HPed alloy are 951 MPa, 1262 MPa, and 14.4%, respectively. Although the two alloys exhibit similar yield and tensile strengths at 700oC, SPSed alloy shows merely 80% higher ductility than HPed alloy. The oxidation mass gain of the two alloys oxidized at 900oC for 100 h follows the parabolic law. A continuous and dense Al2O3 scale is formed on the surface of SPSed alloy, which effectively prevents the inward diffusion of O and outward diffusion of Cr and Ti. The mass gain is merely 0.19 mg/cm2, and the oxidation rate is 1.03 × 10-7 mg2/(cm4·s). Conversely, the oxidation rate of HPed alloy is approximately 2.6 times that of SPSed alloy. Severe internal oxidation occurs in HPed alloy, resulting in abundant less protective NiCr2O4 and TiO2 formation on the surface, as well as large cracks and spalling.

Cite this article

Leipeng XIE , Wenyao SUN , Minghui CHEN , Jinlong WANG , Fuhui WANG . Effects of Processing on Microstructures and Properties of FGH4097 Superalloy[J]. Acta Metall Sin, 2022 , 58(8) : 992 -1002 . DOI: 10.11900/0412.1961.2021.00382

References

1 Backman D G, Williams J C. Advanced materials for aircraft engine applications [J]. Science, 1992, 255: 1082
2 Reed R C. The Superalloys: Fundamentals and Applications [M]. London: Cambridge University Press, 2008: 33
3 Schafrik R, Sprague R. Superalloy technology: A perspective on critical innovations for turbine engines [J]. Key Eng. Mater., 2008, 380: 113
4 Fecht H, Furrer D. Processing of nickel-base superalloys for turbine engine disc applications [J]. Adv. Eng. Mater., 2000, 2: 777
5 Liu F F, Chen J Y, Dong J X, et al. The hot deformation behaviors of coarse, fine and mixed grain for Udimet 720Li superalloy [J]. Mater. Sci. Eng., 2016, A651: 102
6 Zhang G Q, Zhang Y W, Zheng L, et al. Research progress in powder metallurgy superalloys and manufacturing technologies for aero-engine application [J]. Acta Metall. Sin., 2019, 55: 1133
6 张国庆, 张义文, 郑 亮 等. 航空发动机用粉末高温合金及制备技术研究进展 [J]. 金属学报, 2019, 55: 1133
7 Raisson G. Evolution of PM nickel base superalloy processes and products [J]. Powder Metall., 2008, 51: 10
8 Qu X H, Zhang G Q, Zhang L, Applications of powder metallurgy technologies in aero-engines [J]. J. Aeronaut. Mater., 2014, 34(1): 1
8 曲选辉, 张国庆, 章 林. 粉末冶金技术在航空发动机中的应用 [J]. 航空材料学报, 2014, 34(1): 1
9 Miner R V, Gayda J. Effects of processing and microstructure on the fatigue behaviour of the nickel-base superalloy René 95 [J]. Int. J. Fatigue, 1984, 6: 189
10 Radavich J, Furrer D. Assessment of Russian P/M superalloy EP741NP [A]. Superalloys 2004 [C]. Pittsburgh: The Minerals, Metals & Materials Society, 2004: 381
11 Ma W B, Liu G Q, Hu B F, et al. Effect of Hf on carbides of FGH4096 superalloy produced by hot isostatic pressing [J]. Mater. Sci. Eng., 2013, A587: 313
12 Qiu C L, Attallah M M, Wu X H, et al. Influence of hot isostatic pressing temperature on microstructure and tensile properties of a nickel-based superalloy powder [J]. Mater. Sci. Eng., 2013, A564: 176
13 Roncery L M, Lopez-Galilea I, Ruttert B, et al. Influence of temperature, pressure, and cooling rate during hot isostatic pressing on the microstructure of an SX Ni-base superalloy [J]. Mater. Des., 2016, 97: 544
14 Khoshghadam-Pireyousefan M, Mohammadzadeh A, Heidarzadeh A, et al. Fundamentals of spark plasma sintering for metallic, ceramic, and polymer matrix composites production [J]. Encycl. Mater.: Compos., 2021, 2: 822
15 Guillon O, Gonzalez-Julian J, Dargatz B, et al. Field-assisted sintering technology/spark plasma sintering: Mechanisms, materials, and technology developments [J]. Adv. Eng. Mater., 2014, 16: 830
16 Yang W P, Liu G Q, Wu K, et al. Influence of sub-solvus solution heat treatment on γ′ morphological instability in a new Ni-Cr-Co-based powder metallurgy superalloy [J]. J. Alloys Compd., 2014, 582: 515
17 Galindo-Nava E I, Connor L D, Rae C M F. On the prediction of the yield stress of unimodal and multimodal γ′ nickel-base superalloys [J]. Acta Mater., 2015, 98: 377
18 Wang L. Mechanical Properties of Materials [M]. 3rd Ed., Shenyang: Northeast University Press, 2014: 89
18 王 磊. 材料的力学性能 [M]. 第 3版, 东北大学出版社, 2014: 89
19 Thébaud L, Villechaise P, Crozet C, et al. Is there an optimal grain size for creep resistance in Ni-based disk superalloys? [J]. Mater. Sci. Eng., 2018, A716: 274
20 Kozar R W, Suzuki A, Milligan W W, et al. Strengthening mechanisms in polycrystalline multimodal nickel-base superalloys [J]. Metall. Mater. Trans., 2009, 40A: 1588
21 Roth H A, Davis C L, Thomson R C. Modeling solid solution strengthening in nickel alloys [J]. Metall. Mater. Trans., 1997, 28A: 1329
22 Dong X M, Zhang X L, Du K, et al. Microstructure of carbides at grain boundaries in nickel-based superalloys [J]. J. Mater. Sci. Technol., 2012, 28: 1031
23 Sundararaman M, Mukhopadhyay P, Banerjee S. Carbide precipitation in nickel base superalloys 718 and 625 and their effect on mechanical properties [A]. Superalloys 718, 625, 706 and Various Derivatives [C]. Pittsburgh: The Minerals, Metals & Materials Society, 1997: 367
24 Sreenu B, Sarkar R, Kumar S S S, et al. Microstructure and mechanical behaviour of an advanced powder metallurgy nickel base superalloy processed through hot isostatic pressing route for aerospace applications [J]. Mater. Sci. Eng., 2020, A797: 140254
25 Pérez P, González-Carrasco J L, Adeva P. Influence of exposure time and grain size on the oxidation behaviour of a PM Ni3Al alloy at 635oC [J]. Corros. Sci., 1998, 40: 631
26 Wang J L, Chen M H, Yang L L, et al. Nanocrystalline coatings on superalloys against high temperature oxidation: A review [J]. Corros. Commun., 2021, 1: 58
27 Zhao W, Gleeson B. Assessment of the detrimental effects of steam on Al2O3-scale establishment [J]. Oxid. Met., 2015, 83: 607
28 Sun W Y, Chen M H, Bao Z B, et al. Breakaway oxidation of a low-Al content nanocrystalline coating at 1000℃ [J]. Surf. Coat. Technol., 2019, 358: 958
29 Yang S S, Yang L L, Chen M H, et al. Understanding of failure mechanisms of the oxide scales formed on nanocrystalline coatings with different Al content during cyclic oxidation [J]. Acta Mater., 2021, 205: 116576
30 Yu H, Ukai S, Hayashi S, et al. Effect of Al content on the high-temperature oxidation of Co-20Cr-(5, 10) Al oxide dispersion strengthened superalloys [J]. Corros. Sci., 2017, 118: 49
31 Guo C, Yu Z R, Liu C, et al. Effects of Y2O3 nanoparticles on the high-temperature oxidation behavior of IN738LC manufactured by laser powder bed fusion [J]. Corros. Sci., 2020, 171: 108715
Outlines

/