Selection of Twin Variants in Dynamic Plastic Deformation of Pure Ti at Liquid Nitrogen Temperature
Received date: 2021-11-12
Revised date: 2021-12-22
Online published: 2022-02-22
Supported by
Joint Research and Development Fund of Liaoning Province and Shenyang National Laboratory for Materials Science(2019JH3/30100030);Young Talents Project of Shenyang National Laboratory for Materials Science, and Natural Science Foundation Project of Liaoning Provincial Department of Education(J2020050)
Pure Ti can form twins during deformation due to the hcp crystal structure, and some kinds of twins can easily form under certain conditions, thus affecting the properties of materials. It has considerable influence on the properties of materials through the regulation of twin types and variants. This work investigates the effect of the dislocation slip of adjacent grains on the selection of twin variants during the deformation of pure Ti. The dynamic plastic deformation (DPD) of commercially pure Ti (99.9%) was performed at liquid nitrogen temperature (-196oC). The microstructure before and after the deformation was observed using EBSD. The influence of twinning on Schmid factor (m) before and after deformation was investigated, and a mechanism for selecting twin variants of polycrystalline pure Ti was proposed. The results show that after DPD at liquid nitrogen temperature, high-density primary twins appeared in pure Ti, followed by secondary and double twins. After twinning, the Schmid factor of basal slip changed noticeably, and the m of a large number of grains was close to 0.5. Based on the geometric compatibility factor (m') of the original slip and twin matching relationship and the Schmid factor of an adjacent grain (m1), a new orientation compatibility factor ω (ω = m1·m') was established, and the selection of twin variants in the plastic deformation of polycrystalline pure titanium was quantitatively analyzed. It was discovered that the ω determines the selection of twin variants in pure Ti, and the pyramidal slip <a> of the adjacent grain plays a significant role in promoting the initiation of twin variants.
Dong GAO , Yu ZHOU , Ze YU , Baoguang SANG . Selection of Twin Variants in Dynamic Plastic Deformation of Pure Ti at Liquid Nitrogen Temperature[J]. Acta Metall Sin, 2022 , 58(9) : 1141 -1149 . DOI: 10.11900/0412.1961.2021.00491
| 1 | Fu J, Ding H, Huang Y, et al. Influence of phase volume fraction on the grain refining of a Ti-6Al-4V alloy by high-pressure torsion [J]. J. Mater. Res. Technol., 2015, 4: 2 |
| 2 | Li X M, Sun W L, Han Y, et al. Preparation of Ti(C x N1 - x ) thick films on titanium by plasma electrolytic carbonitriding [J]. Acta Metall. Sin., 2008, 44: 1105 |
| 2 | 李新梅, 孙文磊, 憨 勇 等. 纯钛表面电解液微弧碳氮化制备碳氮化钛厚膜 [J]. 金属学报, 2008, 44: 1105 |
| 3 | Partridge P G. The crystallography and deformation modes of hexagonal close-packed metals [J]. Int. Mater. Rev., 1967, 12: 169 |
| 4 | Groves G W, Kelly A. Independent slip systems in crystals [J]. Philos. Mag., 1963, 8: 877 |
| 5 | Mises R V. Mechanik der plastischen formänderung von kristallen [J]. Z. Angew. Math. Mech., 1928, 8: 161 |
| 6 | Huang W, Wang Y, Li Z R, et al. Influences of temperature and strain rate on deformation twinning of polycrystalline titanium [J]. Chin. J. Nonferrous. Met., 2008, 18: 1440 |
| 6 | 黄 文, 汪 洋, 李子然 等. 温度和应变率对多晶纯钛孪晶变形的影响 [J]. 中国有色金属学报, 2008, 18: 1440 |
| 7 | Chichili D R, Ramesh K T, Hemker K J. The high-strain-rate response of alpha-titanium: Experiments, deformation mechanisms and modeling [J]. Acta Mater., 1998, 46: 1025 |
| 8 | Choi S W, Won J W, Lee S, et al. Deformation twinning activity and twin structure development of pure titanium at cryogenic temperature [J]. Mater. Sci. Eng., 2018, A738: 75 |
| 9 | Xu F, Zhang X Y, Ni H T, et al. {11 2 ¯ 4} deformation twinning in pure Ti during dynamic plastic deformation [J]. Mater. Sci. Eng., 2012, A541: 190 |
| 10 | Gurao N P, Kapoor R, Suwas S. Deformation behaviour of commercially pure titanium at extreme strain rates [J]. Acta Mater., 2011, 59: 3431 |
| 11 | Zherebtsov S V, Dyakonov G S, Salem A A, et al. Formation of nanostructures in commercial-purity titanium via cryorolling [J]. Acta Mater., 2013, 61: 1167 |
| 12 | Li Q, Xu Y B, Bassim M N. Dynamic mechanical behavior of pure titanium [J]. J. Mater. Process. Technol., 2004, 155-156: 1889 |
| 13 | Tao N R, LU K. Dynamic plastic deformation (DPD): A novel technique for synthesizing bulk nanostructured metals [J]. J. Mater. Sci. Technol., 2007, 23: 771 |
| 14 | Li Y S, Zhang Y, Tao N R, et al. Effect of the Zener-Hollomon parameter on the microstructures and mechanical properties of Cu subjected to plastic deformation [J]. Acta Mater., 2009, 57: 761 |
| 15 | Guan D K, Wynne B, Gao J H, et al. Basal slip mediated tension twin variant selection in magnesium WE43 alloy [J]. Acta Mater., 2019, 170: 1 |
| 16 | Christian J W. Deformation twinning [A]. The Theory of Transformations in Metals and Alloys [M]. Oxford: Elsevier Ltd., 2002: 859 |
| 17 | Lebensohn R A, Tomé C N. A self-consistent anisotropic approach for the simulation of plastic deformation and texture development of polycrystals: Application to zirconium alloys [J]. Acta Metall. Mater., 1993, 41: 2611 |
| 18 | Reid C N, Gilbert A, Hahn G T. Twinning, slip and catastrophic flow in niobium [J]. Acta Metall., 1966, 14: 975 |
| 19 | Wang L, Yang Y, Eisenlohr P, et al. Twin nucleation by slip transfer across grain boundaries in commercial purity titanium [J]. Metall. Mater. Trans., 2009, 41A: 421 |
| 20 | Chun Y B, Yu S H, Semiatin S L, et al. Effect of deformation twinning on microstructure and texture evolution during cold rolling of CP-titanium [J]. Mater. Sci. Eng., 2005, A398: 209 |
| 21 | Lee M S, Jo A R, Hwang S K, et al. The role of strain rate and texture in the deformation of commercially pure titanium at cryogenic temperature [J]. Mater. Sci. Eng., 2021, A827: 142042 |
| 22 | Won J W, Lee J H, Jeong J S, et al. High strength and ductility of pure titanium via twin-structure control using cryogenic deformation [J]. Scr. Mater., 2020, 178: 94 |
| 23 | Zeng Z P, Zhang Y S, Jonsson S. Deformation behaviour of commercially pure titanium during simple hot compression [J]. Mater. Des., 2009, 30: 3105 |
| 24 | Dahlgren S D, Nicholson W L, Merz M D, et al. Microstructural analysis and tensile properties of thick copper and nickel sputter deposits [J]. Thin Solid Films, 1977, 40: 345 |
| 25 | Yoo M H. Slip, twinning, and fracture in hexagonal close-packed metals [J]. Metall. Trans., 1981, 12A: 409 |
| 26 | Qin H, Jonas J J, Yu H B, et al. Initiation and accommodation of primary twins in high-purity titanium [J]. Acta Mater., 2014, 71: 293 |
| 27 | Zhang Z F, Shao C W, Wang B, et al. Tensile and fatigue properties and deformation mechanisms of twinning-induced plasticity steels [J]. Acta Metall. Sin., 2020, 56: 476 |
| 27 | 张哲峰, 邵琛玮, 王 斌 等. 孪生诱发塑性钢拉伸与疲劳性能及变形机制 [J]. 金属学报, 2020, 56: 476 |
| 28 | Yoo M H, Morris J R, Ho K M, et al. Nonbasal deformation modes of HCP metals and alloys: Role of dislocation source and mobility [J]. Metall. Mater. Trans., 2002, 33A: 813 |
| 29 | Luster J, Morris M A. Compatibility of deformation in two-phase Ti Al alloys: Dependence on microstructure and orientation relationships [J]. Metall. Mater. Trans., 1995, 26A: 1745 |
/
| 〈 |
|
〉 |