Theoretical Calculation and Analysis of the Effect of Oxygen Atom on the Grain Boundary of Superalloy Matrices Ni, Co and NiCr

  • Xin LI ,
  • He JIANG ,
  • Zhihao YAO ,
  • Jianxin DONG
Expand
  • School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083, China
JIANG He, Tel: 13811910685, E-mail: jianghe17@sina.cn

Received date: 2021-04-30

  Revised date: 2021-06-03

  Online published: 2021-11-26

Supported by

National Natural Science Foundation of China(51771016)

Abstract

As advanced aero engines and heavy-duty gas turbines require high service temperatures, how to maintain better performance and damage tolerance of superalloys at high service temperatures has emerged as a critical issue in the application of superalloys. Previous research has shown that temperature rise has no effect on the crack growth rate of alloys placed in a vacuum. However, in air, fatigue crack growth rate is observed to significantly depend on temperature. According to the sample fracture, which is an oxide-covered intergranular fracture, oxygen atoms significantly affect the performance of superalloys. As first-principle calculation method has advanced rapidly in recent years, it can eliminate the effect of irrelevant impurity atoms on the weakening of grain boundaries and establish a pure grain boundary system. Thus, this method is an ideal analysis tool for this research. The ideal tensile test combined with ideal separation work and charge density difference of the grain boundary in nickel-based superalloy under different oxygen concentrations, was performed using the first-principle calculation method. The internal reason for the weakening of the Ni grain boundary due to oxygen is given. A similar comparative analysis of Co and NiCr grain boundaries was also performed. Further, the cause of the oxidation and weakening of the grain boundaries is explained. The results demonstrate that the high electronegativity of O atoms weakens the Ni—Ni metal bond at the grain boundary due to the lack of charge. Further, in the stretching process, when the tensile strain reaches 0.10, the strain of the oxygen-containing Ni grain boundary is entirely provided by the Ni—Ni bond present at this boundary. The presence of oxygen significantly accelerates the fracture failure process of the Ni grain boundary. In addition, Co-based alloy has higher strength after grain boundary oxidation and has better oxidation resistance weakening performance than Ni; however, the strain of fracture is small. Although the NiCr-based grain boundary strength is the weakest, the mechanical properties after oxidation are relatively stable. The reason for the weakening of the Ni grain boundary due to oxidation is attributed to structural distortion caused by oxygen atoms, whereas the weakening of Co- and NiCr-based grain boundary due to oxidation is primarily related to changes in the charge density distribution.

Cite this article

Xin LI , He JIANG , Zhihao YAO , Jianxin DONG . Theoretical Calculation and Analysis of the Effect of Oxygen Atom on the Grain Boundary of Superalloy Matrices Ni, Co and NiCr[J]. Acta Metall Sin, 2023 , 59(2) : 309 -318 . DOI: 10.11900/0412.1961.2021.00176

References

1 Li H Y, Sun J F, Hardy M C, et al. Effects of microstructure on high temperature dwell fatigue crack growth in a coarse grain PM nickel based superalloy[J]. Acta Mater., 2015, 90: 355
2 Tong J, Dalby S, Byrne J, et al. Creep, fatigue and oxidation in crack growth in advanced nickel base superalloys[J]. Int. J. Fatigue, 2001, 23: 897
3 Xu C, Nai Q L, Yao Z H, et al. Grain boundary oxidation effect of GH4738 superalloy on fatigue crack growth [J]. Acta Metall. Sin., 2017, 53: 1453
3 徐 超, 佴启亮, 姚志浩 等. 晶界氧化对GH4738高温合金疲劳裂纹扩展的作用[J]. 金属学报, 2017, 53: 1453
4 Xu C, Yao Z H, Dong J X. The sharp drop in fatigue crack growth life at a critical elevated temperature for a PM Ni-based superalloy FGH97[J]. Mater. Sci. Eng., 2019, A761: 138038
5 Ghonem H, Zheng D. Oxidation-assisted fatigue crack growth behavior in alloy 718-part I. Quantitative modeling[J]. Fatigue Fract. Eng. Mater. Struct., 1991, 14: 749
6 Thomas L E, Bruemmer S M. High-resolution characterization of intergranular attack and stress corrosion cracking of alloy 600 in high-temperature primary water[J]. Corrosion, 2000, 56: 572
7 Was G S, Lian K. Role of carbides in stress corrosion cracking resistance of alloy 600 and controlled-purity Ni-16% Cr-9% Fe in primary water at 360oC[J]. Corrosion, 1998, 54: 675
8 Chen J, Dongare A M. Role of grain boundary character on oxygen and hydrogen segregation-induced embrittlement in polycrystalline Ni[J]. J. Mater. Sci., 2017, 52: 30
9 Yamaguchi M. First-principles study on the grain boundary embrittlement of metals by solute segregation: Part I. Iron (Fe)-solute (B, C, P, and S) systems[J]. Metall. Mater. Trans., 2011, 42A: 319
10 Yamaguchi M, Shiga M, Kaburaki H. Energetics of segregation and embrittling potency for non-transition elements in the Ni Σ5(012) symmetrical tilt grain boundary: A first-principles study[J]. J. Phys.: Condens. Matter, 2004, 16: 3933
11 Wang L G, Wang C Y. First-principles calculations of energies of impurities and doping effects at grain boundaries in nickel[J]. Mater. Sci. Eng., 1997, A234-236: 521
12 Lefkaier I K, Bentria E T. The effect of impurities in nickel grain boundary: density functional theory study[A]. Study of Grain Boundary Character[M]. Rijeka: InTech, 2016: 1
13 Vargas-Hernández R A. Bayesian optimization for calibrating and selecting hybrid-density functional models[J]. J. Phys. Chem., 2020, 124A: 4053
14 Liu W G, Ren C L, Han H, et al. First-principles study of the effect of phosphorus on nickel grain boundary[J]. J. Appl. Phys., 2014, 115: 043706
15 Rühl S. The inorganic crystal structure database (ICSD): A tool for materials sciences[A]. Materials Informatics: Methods, Tools and Applications [M]. Weinheim: Wiley-VCH, 2019: 41
16 Rouquette J, Haines J, Fraysse G, et al. High-pressure structural and vibrational study of PbZr0.40Ti0.60O3 [J]. Inorg. Chem., 2008, 47: 9898
17 Cheng J L, Jian L, Yang K S. Aimsgb: An algorithm and open-source python library to generate periodic grain boundary structures[J]. Comput. Mater. Sci., 2018, 155: 92
18 Yamaguchi M, Shiga M, Kaburaki H. Grain boundary decohesion by impurity segregation in a nickel-sulfur system[J]. Science, 2005, 307: 393
19 Momma K, Izumi F. VESTA 3 for three‐dimensional visualization of crystal, volumetric and morphology data[J]. J. Appl. Cryst., 2011, 44: 1272
20 Zhang M, Liu H Y, Li Q, et al. Superhard BC3 in cubic diamond structure[J]. Phys. Rev. Lett., 2015, 114: 015502
21 Li X. ArticleAttachment, 2023, https://github.com/lixin555/ArticleAttachment
22 Sun S N, Kioussis N, Lim S P, et al. Impurity effects on atomic bonding in Ni3Al[J]. Phys. Rev., 1995, 52B: 14421
23 Rice J R, Wang J S. Embrittlement of interfaces by solute segregation[J]. Mater. Sci. Eng., 1989, A107: 23
24 Razumovskiy V I, Lozovoi A Y, Razumovskii I M. First-principles-aided design of a new Ni-base superalloy: Influence of transition metal alloying elements on grain boundary and bulk cohesion[J]. Acta Mater., 2015, 82: 369
25 Lozovoi A Y, Paxton A T, Finnis M W. Structural and chemical embrittlement of grain boundaries by impurities: A general theory and first-principles calculations for copper[J]. Phys. Rev., 2006, 74B: 155416
26 H?glund J, Guillermet A F, Grimvall G, et al. Theory of bonding in transition-metal carbides and nitrides[J]. Phys. Rev., 1993, 48B: 11685
27 Abe F, Tanabe T. Change in lattice spacing of nickel by dissolved chromium and tungsten[J]. Int. J. Mater. Res., 1985, 76: 420
28 Kim J J, Shin S H, Jung J A, et al. First-principles study of interstitial diffusion of oxygen in nickel chromium binary alloy[J]. Appl. Phys. Lett., 2012, 100: 131904
Outlines

/