Research paper

Erosion-Corrosion Performance of EH36 Steel Under Sand Impacts of Different Particle Sizes

  • ZHANG Qiliang ,
  • WANG Yuchao ,
  • LI Guangda ,
  • LI Xianjun ,
  • HUANG Yi ,
  • XU Yunze
Expand
  • 1School of Naval Architecture and Ocean Engineering, Dalian University of Technology, Dalian 116024, China
    2CGN New Energy Offshore Wind Power Co., Ltd., Shanwei 516600, China
    3China Nuclear Power Design Co. Ltd., Shenzhen 518000, China
XU Yunze, associate professor, Tel: (0411)84706061, E-mail: xuyunze123@163.com

Received date: 2021-07-02

  Revised date: 2021-07-27

  Online published: 2021-11-22

Supported by

National Key Research and Development Program of China(2022YFC2806204);High-Tech Ship Pr-oject of MIIT(MC-202030-H04);National Natural Science Foundation of China(52001055)

Abstract

Marine carbon steels are constantly subjected to active corrosion due to significant amounts of aggressive agents in seawater. Once sand particles are entrained in seawater, the relative movement between the seawater and marine structures could further lead to erosion-corrosion of marine carbon steels. The size of the sand particles would play an important role in the synergy of erosion and corrosion. In this work, the erosion-corrosion performances of the EH36 marine carbon steel at sand impacts of different particle sizes were studied in 3.5%NaCl solution using the EIS, gravimetric measurements, and surface morphology characterization. A computational fluid dynamics simulation is used to simulate the impact velocity and trajectory of the sand particles in the test cell. The simulation results reveal that at a relatively lower flow velocity of 2 m/s, the average impact velocity of the sand particles on the electrode surface is presented as a decreasing trend along with increasing size (100-850 μm). However, increment in the particle size could still lead to rise in the impact energy due to mass increase. The EIS and gravimetric measurement results show that at low flow rate conditions, corrosion is the main contributor to the steel degradation in the sand-containing electrolyte. Meanwhile, corrosion is the prerequisite for severe erosion in this case. The steel loss induced by erosion would rise with an increase in the particle size. The surface characterization results show that the erosion-corrosion pattern changed from the typical “flow mark” to pitting damage with increasing particle size. It suggests that the increase in the impact energy could lead to a pitting initiation, thereby accelerating localized corrosion. It was determined that the particle size increase would promote the synergy of erosion and corrosion compared to pure corrosion, pure erosion, and erosion-corrosion performances. The initiation and propagation of localized erosion-corrosion are determined by the coupled effect of local sand impacts, anodic dissolution, and flow-enhanced analyte transportation. When the diameter of the sand particle is 100 μm, the erosion-corrosion process is controlled by the analyte transportation, leading to the formation of a typical “flow mark”. When the diameter of the sand particle ranges from 430 μm to 850 μm, the synergy of the sand impact and local anodic dissolution would effectively retard the analyte transportation, resulting in the formation of stable pitting damage.

Cite this article

ZHANG Qiliang , WANG Yuchao , LI Guangda , LI Xianjun , HUANG Yi , XU Yunze . Erosion-Corrosion Performance of EH36 Steel Under Sand Impacts of Different Particle Sizes[J]. Acta Metall Sin, 2023 , 59(7) : 893 -904 . DOI: 10.11900/0412.1961.2021.00267

References

1 Zeng L, Guo X P, Zhang G A. Inhibition of the erosion-corrosion of a 90° low alloy steel bend [J]. J. Alloys Compd., 2017, 724: 827
2 Zayed A, Garbatov Y, Soares C G. Corrosion degradation of ship hull steel plates accounting for local environmental conditions [J]. Ocean Eng., 2018, 163: 299
3 Chen F, Li Y D, Yang J, et al. Corrosion behavior of X80 steel welded joint in simulated natural gas condensate solutions [J]. Acta Metall. Sin., 2020, 56: 137
  陈 芳, 李亚东, 杨 剑 等. X80钢焊接接头在模拟天然气凝析液中的腐蚀行为 [J]. 金属学报, 2020, 56: 137
4 Liu C S, Tian Z H, Zhang Z M, et al. Corrosion behaivour of X65 low carbon steel during redox state transition process of high level nuclear waste disposal [J]. Acta Metall. Sin., 2019, 55: 849
  刘灿帅, 田朝晖, 张志明 等. 地质处置低氧过渡期X65低碳钢腐蚀行为研究 [J]. 金属学报, 2019, 55: 849
5 Xia D X, Song S Z, Behnamian Y, et al. Review—Electrochemical noise applied in corrosion science: Theoretical and mathematical models towards quantitative analysis [J]. J. Electrochem. Soc., 2020, 167: 081507
6 Xu Y Z, Liu L, Zhou Q P, et al. An overview of major experimental methods and apparatus for measuring and investigating erosion-corrosion of ferrous-based steels [J]. Metals, 2020, 10: 180
7 Huang Y, Yang L J, Xu Y Z, et al. A novel system for corrosion protection of reinforced steels in the underwater zone [J]. Corros. Eng., Sci. Technol., 2016, 51: 566
8 Liu L, Xu Y Z, Xu C B, et al. Detecting and monitoring erosion-corrosion using ring pair electrical resistance sensor in conjunction with electrochemical measurements [J]. Wear, 2019, 428-429: 328
9 Xia D H, Song S Z, Tao L, et al. Review-material degradation assessed by digital image processing: Fundamentals, progresses, and challenges [J]. J. Mater. Sci. Technol., 2020, 53: 146
10 Yi J Z, He S Y, Wang Z B, et al. Effect of impact angle on the critical flow velocity for erosion-corrosion of 304 stainless steel in simulated sand-containing sea water [J]. J. Bio Tribo Corros., 2021, 7: 99
11 Shang T, Zhong X K, Zhang C F, et al. Erosion-corrosion and its mitigation on the internal surface of the expansion segment of N80 steel tube [J]. Int. J. Miner., Metall. Mater., 2021, 28: 98
12 Zhong X K, Shang T, Zhang C F, et al. In situ study of flow accelerated corrosion and its mitigation at different locations of a gradual contraction of N80 steel [J]. J. Alloys Compd., 2020, 824: 153947
13 Yi J Z, Hu H X, Wang Z B, et al. On the critical flow velocity for erosion-corrosion in local eroded regions under liquid-solid jet impingement [J]. Wear, 2019, 422-423: 94
14 Yi J Z, Hu H X, Wang Z B, et al. On the critical flow velocity for erosion-corrosion of Ni-based alloys in a saline-sand solution [J]. Wear, 2020, 458-459: 203417
15 Li K Q, Yang L J, Xu Y Z, et al. Influence of S O 4 2 - on the corrosion behavior of Q235B steel bar in simulated pore solution [J]. Acta Metall. Sin., 2019, 55: 457
  李恺强, 杨璐嘉, 徐云泽 等. S O 4 2 - 对模拟孔隙液中Q235B钢筋腐蚀行为的影响 [J]. 金属学报, 2019, 55: 457
16 Stack M M, James J S, Lu Q. Erosion-corrosion of chromium steel in a rotating cylinder electrode system: Some comments on particle size effects [J]. Wear, 2004, 256: 557
17 Zheng Y G, Yu H, Jiang S L, et al. Effect of the sea mud on erosion-corrosion behaviors of carbon steel and low alloy steel in 2.4%NaCl solution [J]. Wear, 2008, 264: 1051
18 Luo S Z, Zheng Y G, Li J, et al. Slurry erosion resistance of fusion-bonded epoxy powder coating [J]. Wear, 2001, 249: 733
19 Jiang Z C, Yang Y, Peng H P, et al. Erosion corrosion behavior of X80 steel in multiphase flow with different sand particle sizes [J]. Oil-Gas Field Surface Eng., 2018, 37(11): 76
  姜志超, 杨 燕, 彭浩平 等. X80钢在不同砂粒粒径下的多相流中的冲刷腐蚀行为 [J]. 油气田地面工程, 2018, 37(11): 76
20 Chen Z X, Hu H X, Guo X M, et al. Effect of groove depth on the slurry erosion of V-shaped grooved surfaces [J]. Wear, 2021, 488-489: 204133
21 Peng X, Wang J, Shan C, et al. Corrosion behavior of long-time immersed rusted carbon steel in flowing seawater [J]. Acta Metall. Sin., 2012, 48: 1260
  彭 欣, 王 佳, 山 川 等. 带锈碳钢在流动海水中的长期腐蚀行为 [J]. 金属学报, 2012, 48: 1260
22 Xu Y Z, Zhang Q L, Gao S, et al. Exploring the effects of sand impacts and anodic dissolution on localized erosion-corrosion in sand entraining electrolyte [J]. Wear, 2021, 478-479: 203907
23 He L M, Xu Y Z, Wang X N, et al. Understanding the propagation of nonuniform corrosion on a steel surface covered by marine sand [J]. Corrosion, 2019, 75: 1487
24 Stuparu A, Susan-Resiga R, Tanasa C. CFD assessment of the hydrodynamic performance of two impellers for a baffled stirred reactor [J]. Appl. Sci., 2021, 11: 4949
25 Xu Y Z, Zhou Q P, Liu L, et al. Exploring the corrosion performances of carbon steel in flowing natural sea water and synthetic sea waters [J]. Corros. Eng., Sci. Technol., 2020, 55: 579
26 Liu L, Xu Y Z, Zhu Y S, et al. The roles of fluid hydrodynamics, mass transfer, rust layer and macro-cell current on flow accelerated corrosion of carbon steel in oxygen containing electrolyte [J]. J. Electrochem. Soc., 2020, 167: 141510
27 Zhu Y S, Xu Y Z, Wang M Y, et al. Understanding the influences of temperature and microstructure on localized corrosion of subsea pipeline weldment using an integrated multi-electrode array [J]. Ocean Eng., 2019, 189: 106351
28 Stern M, Geary A L. Electrochemical polarization: I. A theoretical analysis of the shape of polarization curves [J]. J. Electrochem. Soc., 1957, 104: 56
29 Xu Y Z, Liu L, Xu C B, et al. Electrochemical characteristics of the dynamic progression of erosion-corrosion under different flow conditions and their effects on corrosion rate calculation [J]. J. Solid State Electrochem, 2020, 24: 2511
30 Xu Y Z, Tan M Y. Visualising the dynamic processes of flow accelerated corrosion and erosion corrosion using an electrochemically integrated electrode array [J]. Corros. Sci., 2018, 139: 438
31 Xu Y Z, Tan M Y. Probing the initiation and propagation processes of flow accelerated corrosion and erosion corrosion under simulated turbulent flow conditions [J]. Corros. Sci., 2019, 151: 163
32 Guo H X, Lu B T, Luo J L. Interaction of mechanical and electrochemical factors in erosion-corrosion of carbon steel [J]. Electrochim. Acta, 2005, 51: 315
33 Xu Y Z, Liu L, Zhou Q P, et al. Understanding the influences of pre-corrosion on the erosion-corrosion performance of pipeline steel [J]. Wear, 2020, 442-443: 203151
Outlines

/