Effects of Ar Ion Irradiation on Microstructure of Fe-Cu Alloys at 290oC

  • Xiaohui ZHU ,
  • Xiangbing LIU ,
  • Runzhong WANG ,
  • Yuanfei LI ,
  • Wenqing LIU
Expand
  • 1.School of Materials Science and Engineering, Shanghai University, Shanghai 200444, China
    2.Suzhou Nuclear Power Research Institute, Suzhou 215004, China
LIU Wenqing, professor, Tel: 18930623992, E-mail: wqliu@staff.shu.edu.cn

Received date: 2021-08-12

  Revised date: 2021-09-28

  Online published: 2021-10-20

Supported by

National Key Research and Development Program of China(2017YFB0703002);Joint Fund of the National Natural Science Foundation of China(U1530115)

Abstract

Irradiation-enhanced precipitation of Cu clusters is a main factor contributing to the hardening/embrittlement of reactor pressure vessels, and thus, limiting the lifetime of reactors. The Cu clusters are easily formed in ferric alloys under neutron irradiation or ion irradiation, which is used to simulate neutron irradiation. However, the inhibition and even dissolution of Cu clusters in Cu-containing alloys after ion irradiation is also observed in some research. To investigate the reason for ion irradiation-induced dissolution of solute clusters, Fe-1.3%Cu (atomic fraction) alloys were irradiated with Ar ions to the fluence of 4 × 1016 ion/cm2 at 290oC. TEM and atom probe tomography were used to characterize microstructure and solute atom distributions, respectively. Numerous black dot defects and bubbles with average diameters of about 1.3 nm are observed in the irradiated layer. Well-defined Cu-rich clusters are also precipitated in the irradiated layer. The average radius and number density of clusters increase first and then decrease with an increase in distance from the surface. The high displacement damage rate and large cascade size of Ar ions inhibit the irradiation-enhanced diffusion of Cu atoms and bring Cu atoms of the clusters back to matrix, which causes Cu clusters to precipitate weakly near the irradiated surface. With increasing distance from the surface, the Ar ion concentration increases. Ar-vacancy complexes or Ar bubbles form due to the aggregation of Ar ions. Then, the interattraction between Cu atoms and vacancies complexes would enhance the atom diffusion and segregation, which causes an increase in size and number density of the Cu-rich clusters.

Cite this article

Xiaohui ZHU , Xiangbing LIU , Runzhong WANG , Yuanfei LI , Wenqing LIU . Effects of Ar Ion Irradiation on Microstructure of Fe-Cu Alloys at 290oC[J]. Acta Metall Sin, 2022 , 58(7) : 905 -910 . DOI: 10.11900/0412.1961.2021.00328

References

1 Odette G R, Yamamoto T, Williams T J, et al. On the history and status of reactor pressure vessel steel ductile to brittle transition temperature shift prediction models [J]. J. Nucl. Mater., 2019, 526: 151863
2 Zelenty J E. Understanding thermally induced embrittlement in low copper RPV steels utilising atom probe tomography [J]. Mater. Sci. Technol., 2015, 31: 981
3 Zinkle S J, Terrani K A, Snead L L. Motivation for utilizing new high-performance advanced materials in nuclear energy systems [J]. Curr. Opin. Solid State Mater. Sci., 2016, 20: 401
4 Zinkle S J, Snead L L. Opportunities and limitations for ion beams in radiation effects studies: Bridging critical gaps between charged particle and neutron irradiations [J]. Scr. Mater., 2018, 143: 154
5 Ding Z N, Yang Y T, Song Y, et al. Hardening of reduced activation ferritic/martensitic steels under the irradiation of high-energy heavy-ion [J]. Acta Phys. Sin., 2017, 66: 112501
5 丁兆楠, 杨义涛, 宋 银 等. 高能重离子辐照的低活化钢硬化效应 [J]. 物理学报, 2017, 66: 112501
6 Liu X B, Wang R S, Ren A, et al. Evaluation of radiation hardening in ion-irradiated Fe based alloys by nanoindentation [J]. J. Nucl. Mater., 2014, 444: 1
7 He L, Tan L Z, Yang Y, et al. Evolution of B2 and Laves phases in a ferritic steel under Fe2+ ion irradiation at 475oC [J]. J. Nucl. Mater., 2019, 525: 102
8 Yang T F, Guo W, Poplawsky J D, et al. Structural damage and phase stability of Al0.3CoCrFeNi high entropy alloy under high temperature ion irradiation [J]. Acta Mater., 2020, 188: 1
9 Zhu X H, Liu X B, Wang R Z, et al. Hardening effects of He irradiation on Fe-Cu alloy [J]. Nuclear Inst. Methods Phys. Res. Sect., 2020, 479B: 211
10 Shu S, Almirall N, Wells P B, et al. Precipitation in Fe-Cu and Fe-Cu-Mn model alloys under irradiation: Dose rate effects [J]. Acta Mater., 2018, 157: 72
11 Jiao Z, Was G S. Precipitate evolution in ion-irradiated HCM12A [J]. J. Nucl. Mater., 2012, 425: 105
12 Stoller R E, Toloczko M B, Was G S, et al. On the use of SRIM for computing radiation damage exposure [J]. Nucl. Inst. Methods Phys. Res. Sect., 2013, 310B: 75
13 Egeland G W, Valdez J A, Maloy S A, et al. Heavy-ion irradiation defect accumulation in ZrN characterized by TEM, GIXRD, nanoindentation, and helium desorption [J]. J. Nucl. Mater., 2013, 435: 77
14 Deng P, Peng Q J, Han E H, et al. Study of irradiation damage in domestically fabricated nuclear grade stainless steel [J]. Acta Metall. Sin., 2017, 53: 1588
14 邓 平, 彭群家, 韩恩厚 等. 国产核用不锈钢辐照损伤研究 [J]. 金属学报, 2017, 53: 1588
15 Miller M K, Russell K F, Thompson G B. Strategies for fabricating atom probe specimens with a dual beam FIB [J]. Ultramicroscopy, 2005, 102: 287
16 Luo F F, Guo L P, Chen J H, et al. Damage behavior in helium-irradiated reduced-activation martensitic steels at elevated temperatures [J]. J. Nucl. Mater., 2014, 455: 339
17 Yeli G, Chen D, Yabuuchi K, et al. The stability of γ' precipitates in a multi-component FeCoNiCrTi0.2 alloy under elevated-temperature irradiation [J]. J. Nucl. Mater., 2020, 540: 152364
18 Cairney J M, Rajan K, Haley D, et al. Mining information from atom probe data [J]. Ultramicroscopy, 2015, 159: 324
19 Marquis E, Wirth B, Was G. Characterization and modeling of grain boundary chemistry evolution in ferritic steels under irradiation [R]. Ann Arbor, MI, USA: USDOE Office of Nuclear Energy (NE), 2016
20 Horton L L, Bentley J, Jesser W A. The microstructure of “triple-beam” ion irradiated Fe and Fe-Cr alloys [J]. J. Nucl. Mater., 1981, 104: 1085
21 Ke J H, Reese E R, Marquis E A, et al. Flux effects in precipitation under irradiation-simulation of Fe-Cr alloys [J]. Acta Mater., 2019, 164: 586
22 Was G S. Fundamentals of Radiation Materials Science: Metals and Alloys [M]. 2nd Ed., Berlin: Springer-Verlag, 2017: 488
23 Xu D H, Certain A, Voigt H J L, et al. Ballistic effects on the copper precipitation and re-dissolution kinetics in an ion irradiated and thermally annealed Fe-Cu alloy [J]. J. Chem. Phys., 2016, 145: 104704
24 Hu Z Y, Xu C, Liang Y X, et al. The radiation effect of ion species on the microstructure of nanoporous gold [J]. Scr. Mater., 2021, 190: 136.
25 Belkacemi L T, Meslin E, Décamps B, et al. Role of displacement cascades in Ni clustering in a ferritic Fe-3.3 at%Ni model alloy: Comparison of heavy and light particle irradiations [J]. Scr. Mater., 2020, 188: 169
Outlines

/