Strain-Controlled Fatigue Behavior of Nanotwin- Strengthened 304 Austenitic Stainless Steel
Received date: 2021-08-17
Revised date: 2021-09-04
Online published: 2021-10-13
Supported by
National Natural Science Foundation of China(51931010);Key Research Program of Frontier Science and International Partnership Program, Chinese Academy of Sciences(GJHZ2029);Liaoning Revitalization Talents Program(XLYC1802026);Youth Innovation Promotion Association, Chinese Academy of Sciences(2019196)
Engineering nano-scale twin boundaries has been recognized as a novel strategy to achieve a superior combination of tensile strength, ductility, and fatigue limit in metallic materials. However, to date, the strain-controlled fatigue behavior of nanotwin (NT)-strengthened metals is still rarely explored, most possibly owing to the difficulty in preparing bulk fatigue samples. In this work, a bulk heterogeneously structured 304 stainless steel (304 SS) containing 30% volume fraction of NT bundles embedded in the micrometer-sized grain matrix was prepared and studied under constant plastic strain amplitude-controlled fatigue tests. A considerable fatigue life and much higher cyclic flow stress level, while maintaining a weaker degree of cyclic softening at larger strain amplitude, was achieved in NT-strengthened 304 SS, compared with its coarse-grained counterpart in the same strain-controlled fatigue tests. This is fundamentally distinct from the more obvious softening behavior of conventional nanostructured metals induced by strain localization at larger strain amplitude. Such exceptional low-cycle fatigue properties were attributed to the presence of a high-strength NT structure associated with novel mechanical stability and its co-deformation with surrounding grains, effectively suppressing strain localization and fatigue crack initiation.
Qingsong PAN , Fang CUI , Nairong TAO , Lei LU . Strain-Controlled Fatigue Behavior of Nanotwin- Strengthened 304 Austenitic Stainless Steel[J]. Acta Metall Sin, 2022 , 58(1) : 45 -53 . DOI: 10.11900/0412.1961.2021.00342
| 1 | Suresh S . Fatigue of Materials [M]. 2nd Ed., Cambridge, UK: Cambridge University Press, 1998: 679 |
| 2 | Pineau A , Benzerga A A , Pardoen T . Failure of metals III: Fracture and fatigue of nanostructured metallic materials [J]. Acta Mater., 2016, 107: 508 |
| 3 | Meyers M A , Chawla K K . Mechanical Behavior of Materials [M]. 2nd Ed., Cambridge, UK: Cambridge University Press, 2009: 739 |
| 4 | Li Q , Yan F K , Tao N R , et al . Deformation compatibility between nanotwinned and recrystallized grains enhances resistance to interface cracking in cyclic loaded stainless steel [J]. Acta Mater., 2019, 165: 87 |
| 5 | Majumdar S , Roy S , Ray K K . Fatigue performance of dual-phase steels for automotive wheel application [J]. Fatigue Fract. Eng. Mater. Struct., 2017, 40: 315 |
| 6 | Wang Z G , Wang G N , Ke W , et al . Influence of the martensite content on the fatigue behavior of a dual-phase steel [J]. Mater. Sci. Eng., 1987, 91: 39 |
| 7 | Anbarlooie B , Hosseini-Toudeshky H , Kadkhodapour J . High cycle fatigue micromechanical behavior of dual phase steel: Damage initiation, propagation and final failure [J]. Mech. Mater., 2017, 106: 8 |
| 8 | B?hner A , Niendorf T , Amberger D , et al . Martensitic transformation in ultrafine-grained stainless steel AISI 304L under monotonic and cyclic loading [J]. Metals, 2012, 2: 56 |
| 9 | Kaneko Y , Hayashi S , Vinogradov A . Cyclic response of SUS316L stainless steel processed by ECAP [J]. Mater. Trans., 2013, 54: 1612 |
| 10 | Renk O , Hohenwarter A , Pippan R . Cyclic deformation behavior of a 316L austenitic stainless steel processed by high pressure torsion [J]. Adv. Eng. Mater., 2012, 14: 948 |
| 11 | Ueno H , Kakihata K , Kaneko Y , et al . Enhanced fatigue properties of nanostructured austenitic SUS 316L stainless steel [J]. Acta Mater., 2011, 59: 7060 |
| 12 | H?ppel H W , Zhou Z M , Mughrabi H , et al . Microstructural study of the parameters governing coarsening and cyclic softening in fatigued ultrafine-grained copper [J]. Philos. Mag., 2002, 82A: 1781 |
| 13 | Mughrabi H , H?ppel H W , Kautz M . Fatigue and microstructure of ultrafine-grained metals produced by severe plastic deformation [J]. Scr. Mater., 2004, 51: 807 |
| 14 | Kunz L , Luká? P , Svoboda M . Fatigue strength, microstructural stability and strain localization in ultrafine-grained copper [J]. Mater. Sci. Eng., 2006, A424: 97 |
| 15 | Mughrabi H , H?ppel H W . Cyclic deformation and fatigue properties of very fine-grained metals and alloys [J]. Int. J. Fatigue, 2010, 32: 1413 |
| 16 | Lu K . Stabilizing nanostructures in metals using grain and twin boundary architectures [J]. Nat. Rev. Mater., 2016, 1: 1 |
| 17 | Lu K , Lu L , Suresh S . Strengthening materials by engineering coherent internal boundaries at the nanoscale [J]. Science, 2009, 324: 349 |
| 18 | Sansoz F , Lu K , Zhu T , et al . Strengthening and plasticity in nanotwinned metals [J]. MRS Bull., 2016, 41: 292 |
| 19 | Zhang X , Wang H , Chen X H , et al . High-strength sputter-deposited Cu foils with preferred orientation of nanoscale growth twins [J]. Appl. Phys. Lett., 2006, 88: 173116 |
| 20 | Lu L , Chen X , Huang X , et al . Revealing the maximum strength in nanotwinned copper [J]. Science, 2009, 323: 607 |
| 21 | Lu L , Shen Y F , Chen X H , et al . Ultrahigh strength and high electrical conductivity in copper [J]. Science, 2004, 304: 422 |
| 22 | Lu L , You Z S . Plastic deformation mechanisms in nanotwinned metals [J]. Acta Metall. Sin., 2014, 50: 129 |
| 22 | 卢 磊, 尤泽升 . 纳米孪晶金属塑性变形机制 [J]. 金属学报, 2014, 50: 129 |
| 23 | Hodge A M , Furnish T A , Shute C J , et al . Twin stability in highly nanotwinned Cu under compression, torsion and tension [J]. Scr. Mater., 2012, 66: 872 |
| 24 | Pan Q S , Lu L . Strain-controlled cyclic stability and properties of Cu with highly oriented nanoscale twins [J]. Acta Mater., 2014, 81: 248 |
| 25 | Pan Q S , Lu Q H , Lu L . Fatigue behavior of columnar-grained Cu with preferentially oriented nanoscale twins [J]. Acta Mater., 2013, 61: 1383 |
| 26 | Pan Q S , Zhou H F , Lu Q H , et al . History-independent cyclic response of nanotwinned metals [J]. Nature, 2017, 551: 214 |
| 27 | Li X Y , Dao M , Eberl C , et al . Fracture, fatigue, and creep of nanotwinned metals [J]. MRS Bull., 2016, 41: 298 |
| 28 | Lu L , Pan Q S , Hattar K , et al . Fatigue and fracture of nanostructured metals and alloys [J]. MRS Bull., 2021, 46: 258 |
| 29 | You Z S , Li X Y , Gui L J , et al . Plastic anisotropy and associated deformation mechanisms in nanotwinned metals [J]. Acta Mater., 2013, 61: 217 |
| 30 | Lu K , Yan F K , Wang H T , et al . Strengthening austenitic steels by using nanotwinned austenitic grains [J]. Scr. Mater., 2012, 66: 878 |
| 31 | Yan F K , Liu G Z , Tao N R , et al . Strength and ductility of 316L austenitic stainless steel strengthened by nano-scale twin bundles [J]. Acta Mater., 2012, 60: 1059 |
| 32 | Yi H Y , Yan F K , Tao N R , et al . Comparison of strength-ductility combinations between nanotwinned austenite and martensite-austenite stainless steels [J]. Mater. Sci. Eng., 2015, A647: 152 |
| 33 | Yi H Y , Yan F K , Tao N R , et al . Work hardening behavior of nanotwinned austenitic grains in a metastable austenitic stainless steel [J]. Scr. Mater., 2016, 114: 133 |
| 34 | Cui F , Pan Q S , Tao N R , et al . Enhanced high-cycle fatigue resistance of 304 austenitic stainless steel with nanotwinned grains [J]. Int. J. Fatigue, 2021, 143: 105994 |
| 35 | Li Q , Yan F K , Tao N R . Enhanced fatigue damage resistance of nanotwinned austenitic grains in a nanotwinned stainless steel [J]. Scr. Mater., 2017, 136: 59 |
| 36 | Meyers M A , Mishra A , Benson D J . Mechanical properties of nanocrystalline materials [J]. Prog. Mater Sci., 2006, 51: 427 |
| 37 | Mughrabi H . Fatigue, an everlasting materials problem-still en vogue [J]. Proc. Eng., 2010, 2: 3 |
| 38 | Peralta P , Laird C . Fatigue of metals [A]. Physical Metallurgy [M]. 5th Ed., Oxford: Elsevier, 2014: 1765 |
| 39 | Bayerlein M , Christ H J , Mughrabi H . Plasticity-induced martensitic transformation during cyclic deformation of AISI 304L stainless steel [J]. Mater. Sci. Eng., 1989, A114: L11 |
| 40 | Kelly P M . The martensite transformation in steels with low stacking fault energy [J]. Acta Metall., 1965, 13: 635 |
| 41 | Krupp U , Roth I , Christ H J , et al . In situ SEM observation and analysis of martensitic transformation during short fatigue crack propagation in metastable austenitic steel [J]. Adv. Eng. Mater., 2010, 12: 255 |
| 42 | Maier H J , Schneeweiss O , Donth B . Kinetics of fatigue-induced phase transformation in a metastable austenitic 304 L-type steel at low temperatures [J]. Scr. Metall. Mater., 1993, 29: 521 |
| 43 | Yan F K , Tao N R , Archie F , et al . Deformation mechanisms in an austenitic single-phase duplex microstructured steel with nanotwinned grains [J]. Acta Mater., 2014, 81: 487 |
| 44 | Shute C J , Myers B D , Xie S , et al . Microstructural stability during cyclic loading of multilayer copper/copper samples with nanoscale twinning [J]. Scr. Mater., 2009, 60: 1073 |
| 45 | Shute C J , Myers B D , Xie S , et al . Detwinning, damage and crack initiation during cyclic loading of Cu samples containing aligned nanotwins [J]. Acta Mater., 2011, 59: 4569 |
| 46 | Hong C S , Tao N R , Huang X , et al . Nucleation and thickening of shear bands in nano-scale twin/matrix lamellae of a Cu-Al alloy processed by dynamic plastic deformation [J]. Acta Mater., 2010, 58: 3103 |
/
| 〈 |
|
〉 |