Research paper

Modelling of the Plastic Behavior of Cu Crystal with Twinning-Induced Softening and Strengthening Effects

  • Xiangru GUO ,
  • Junjie SHEN
Expand
  • 1.Tianjin Key Laboratory for Advanced Mechatronic System Design and Intelligent Control, School of Mechanical Engineering, Tianjin University of Technology, Tianjin 300384, China
    2.National Demonstration Center for Experimental Mechanical and Electrical Engineering Education, Tianjin University of Technology, Tianjin 300384, China
SHEN Junjie, associate professor, Tel: (022)60214133, E-mail: sjj1982428@sina.com

Received date: 2021-05-27

  Revised date: 2021-07-30

  Online published: 2021-09-07

Supported by

National Natural Science Foundation of China(52105393);Natural Science Foundation of Tianjin(18JCYBJC88700)

Abstract

Dislocation slip and twinning are the main deformation mechanisms dominating plastic behavior of crystalline materials, such as twinning-induced plasticity steel, Cu, Mg, and their alloys. The influence of twinning and interaction between dislocations and twins on the plastic deformation of crystal materials is complex. On the one hand, a sudden stress drop in the stress-strain curve during twin nucleation, propagation, and growth (TNPG) of crystal materials, i.e., the twinning softening effect, is evident. On the other hand, the interaction between twins and dislocations demonstrates the strengthening effect of plastic deformation. Polycrystalline materials are used in engineering applications, and twin nucleation corresponds to different strains in each grain. Therefore, determining the influence of twin softening and strengthening effects on plastic deformation of polycrystalline materials is difficult. In this work, a crystal plastic finite element model of Cu, considering the twinning softening effect, was developed to describe the TNPG process based on the crystal plasticity theory. The method was used to reveal the influence of twins' activation and their interaction with dislocations on strain hardening during the tension of Cu single crystal and polycrystal. The results show that twinning has an evident orientation effect. Under twinning favorable orientation, a sudden stress drop in the stress-strain curve caused by twinning propagation during plastic deformation of Cu single crystal is evident, and the total plastic deformation can be divided into three stages: slip, twinning, and interaction between dislocations and twins. Compared with Cu single crystal, the stress-strain curve changes smoothly and the strain hardening rate is higher during the tension of Cu polycrystal. Meanwhile, the dislocation density is concentrated at the grain boundary, and twins are easy to form at the grain boundary during the plastic deformation of Cu polycrystal.

Cite this article

Xiangru GUO , Junjie SHEN . Modelling of the Plastic Behavior of Cu Crystal with Twinning-Induced Softening and Strengthening Effects[J]. Acta Metall Sin, 2022 , 58(3) : 375 -384 . DOI: 10.11900/0412.1961.2021.00230

References

1 Guo X R, Sun C Y, Li R, et al. A dislocation density based model for twinning induced softening of TWIP steel [J]. Comput. Mater. Sci., 2017, 139: 8
2 Niewczas M, Basinski Z S, Basinski S J, et al. Deformation of copper single crystals to large strains at 4.2K—I. Mechanical response and electrical resistivity [J]. Philos. Mag., 2001, 81A: 1121
3 Seo J H, Park H S, Yoo Y, et al. Origin of size dependency in coherent-twin-propagation-mediated tensile deformation of noble metal nanowires [J]. Nano Lett., 2013, 13: 5112
4 Liang Z Y, Li Y Z, Huang M X. The respective hardening contributions of dislocations and twins to the flow stress of a twinning-induced plasticity steel [J]. Scr. Mater., 2016, 112: 28
5 Luo Z C, Huang M X. Revisit the role of deformation twins on the work-hardening behaviour of twinning-induced plasticity steels [J]. Scr. Mater., 2018, 142: 28
6 Paramatmuni C, Zheng Z B, Rainforth W M, et al. Twin nucleation and variant selection in Mg alloys: An integrated crystal plasticity modelling and experimental approach [J]. Int. J. Plast., 2020, 135: 102778
7 Zhi H H, Zhang C, Antonov S, et al. Investigations of dislocation-type evolution and strain hardening during mechanical twinning in Fe-22Mn-0.6C twinning-induced plasticity steel [J]. Acta Mater., 2020, 195: 371
8 Bertin N, Sills R B, Cai W. Frontiers in the simulation of dislocations [J]. Annu. Rev. Mater. Res., 2020, 50: 437
9 Zhang J, Li H W, Sun X X, et al. A multi-scale MCCPFEM framework: Modeling of thermal interface grooving and deformation anisotropy of titanium alloy with lamellar colony [J]. Int. J. Plast., 2020, 135: 102804
10 Agaram S, Kanjarla A K, Bhuvaraghan B, et al. Dislocation density based crystal plasticity model incorporating the effect of precipitates in IN718 under monotonic and cyclic deformation [J]. Int. J. Plast., 2021, 141: 102990
11 Sun C Y, Guo N, Fu M W, et al. Modeling of slip, twinning and transformation induced plastic deformation for TWIP steel based on crystal plasticity [J]. Int. J. Plast., 2016, 76: 186
12 Guo N, Tang B T, Liu J Y, et al. Characteristic stepwise strain hardening behaviour induced by slip and twinning of large-deformed copper single crystals: Crystal plasticity modelling and simulation [J]. Philos. Mag., 2021, 101: 1245
13 Li X X, Xu D S, Yang R. Crystal plasticity finite element method investigation of the high temperature deformation consistency in dual-phase titanium alloy [J]. Acta Metall. Sin., 2019, 55: 928
13 李学雄, 徐东生, 杨 锐. 双相钛合金高温变形协调性的CPFEM研究 [J]. 金属学报, 2019, 55: 928
14 Chin G Y, Hosford W F, Mendorf D R. Accommodation of constrained deformation in f.c.c. metals by slip and twinning [J]. Proc. Roy. Soc., 1969, 309A: 433
15 Van Houtte P. Simulation of the rolling and shear texture of brass by the Taylor theory adapted for mechanical twinning [J]. Acta Metall., 1978, 26: 591
16 Choi S H, Shin E J, Seong B S. Simulation of deformation twins and deformation texture in an AZ31 Mg alloy under uniaxial compression [J]. Acta Mater., 2007, 55: 4181
17 Tomé C N, Lebensohn R A, Kocks U F. A model for texture development dominated by deformation twinning: Application to zirconium alloys [J]. Acta Metall. Mater., 1991, 39: 2667
18 Kalidindi S R. Modeling anisotropic strain hardening and deformation textures in low stacking fault energy fcc metals [J]. Int. J. Plast., 2001, 17: 837
19 Sun C Y, Guo X R, Huang J, et al. Modelling of plastic deformation on coupling twinning of single crystal TWIP steel [J]. Acta Metall. Sin., 2015, 51: 357
19 孙朝阳, 郭祥如, 黄 杰等. 耦合孪生的TWIP钢单晶体塑性变形行为模拟研究 [J]. 金属学报, 2015, 51: 357
20 Sun C Y, Guo X R, Guo N, et al. Investigation of plastic deformation behavior on coupling twinning of polycrystal TWIP steel [J]. Acta Metall. Sin., 2015, 51: 1507
20 孙朝阳, 郭祥如, 郭 宁等. 耦合孪生的TWIP钢多晶体塑性变形行为研究 [J]. 金属学报, 2015, 52: 1507
21 Beyerlein I J, Mara N A, Bhattacharyya D, et al. Texture evolution via combined slip and deformation twinning in rolled silver-copper cast eutectic nanocomposite [J]. Int. J. Plast., 2011, 27: 121
22 Wu P D, Guo X Q, Qiao H, et al. A constitutive model of twin nucleation, propagation and growth in magnesium crystals [J]. Mater. Sci. Eng., 2015, A625: 140
23 Qiao H, Barnett M R, Wu P D. Modeling of twin formation, propagation and growth in a Mg single crystal based on crystal plasticity finite element method [J]. Int. J. Plast., 2016, 86: 70
24 Wang H, Clausen B, Capolungo L, et al. Stress and strain relaxation in magnesium AZ31 rolled plate: In-situ neutron measurement and elastic viscoplastic polycrystal modeling [J]. Int. J. Plast., 2016, 79: 275
25 Kalidindi S R. Incorporation of deformation twinning in crystal plasticity models [J]. J. Mech. Phys. Solids, 1998, 46: 267
26 Allain S, Chateau J P, Bouaziz O. A physical model of the twinning-induced plasticity effect in a high manganese austenitic steel [J]. Mater. Sci. Eng., 2004, A387: 143
27 Arsenlis A, Parks D M. Modeling the evolution of crystallographic dislocation density in crystal plasticity [J]. J. Mech. Phys. Solids, 2002, 50: 1979
28 Sun Z K, Li F G, Zhu J M. Radial micro-cracks in pile-up region of single-crystal Cu in spherical indentation: Experimental observation and crystal plastic simulation [J]. J. Mater. Sci., 2019, 54: 9875
29 Khan A S, Liu J, Yoon J W, et al. Strain rate effect of high purity aluminum single crystals: Experiments and simulations [J]. Int. J. Plast., 2015, 67: 39
30 Dancette S, Delannay L, Renard K, et al. Crystal plasticity modeling of texture development and hardening in TWIP steels [J]. Acta Mater., 2012, 60: 2135
31 Blewitt T H, Coltman R R, Redman J K. Low-temperature deformation of copper single crystals [J]. J. Appl. Phys., 1957, 28: 651
32 Quey R, Dawson P R, Barbe F. Large-scale 3D random polycrystals for the finite element method: Generation, meshing and remeshing [J]. Comput. Methods Appl. Mech. Eng., 2011, 200: 1729
Outlines

/